At least 37 records · Page 2

Multi-phase characterization of pitch-carbon coated nano-silicon anodes for lithium-ion batteries

Silicon (Si) is a leading next-generation Li-ion battery anode candidate that meets rigorous performance demands for portable power including enhanced power and energy density with robust cycling performance. However, a series of complex and interrelated reactions lead to reduced calendar life in Si-containing systems and therefore challenge practical adoption. In the present work, we probe the mechanisms underlying observed performance improvements by adding a pitch-carbon coating onto nano-Si material. We pair solid-phase (X-ray photoemission spectroscopy, Fourier-transform infrared), semi-volatile phase (solid-phase microextraction-gas chromatography-mass spectrometry), and gas-phase (gas chromatography-flame-ionization detector) characterization signals to comprehensively evaluate the impact of pitch-carbon coating on the evolution of the Si solid-electrolyte interphase (SEI) and the associated impacts on electrode/electrolyte reactivity. The pitch-carbon is found to serve as a physicochemical barrier, reducing the electro-active surface area for Si/electrolyte reactivity and preventing Si oxidation. Further, the pitch-carbon coating promotes the evolution of a more-favorable SEI by subsuming substantial functionality typically associated with the fluoroethylene carbonate (FEC) electrolyte additive - such as alkoxide scavenging and suppression of transesterification pathways - and by shifting the competitive electrolyte degradation pathways' favorability. The multi-phase characterization approach enables holistic end-products evaluation from complex (electro)chemical interfacial reactions, which informs a robust interpretation of the carbon coating's role in electrochemical performance improvements. The present mechanistic evaluation aids the rational design for improved nano-Si materials.

25 ENERGY STORAGE↗

Investigation of SiO x anode fading mechanism with limited capacity cycling

Silicon suboxide (SiO x ) is one of the promising anode materials for the next-generation lithium-ion batteries. However, SiO x has a severe capacity fading problem during cycling. It is thus desired to investigate the detailed fading mechanisms of SiO x anode materials. In this study, limited capacity cycling was employed to examine the electrochemical behaviors of the SiO x anode, and the lithiation/delithiation cycling was limited within a range of 10% theoretical capacity. This strategy minimizes the volume variation of SiO x materials upon charging/discharging, which helps to reveal their decay factors other than volume fluctuation. It is demonstrated that the instability of the SiO x surface during cycling was likely a parallel factor of active material fading, which seems to cause unfavored electrode interface rearrangements with lowered electric conductivity.

electric vehicles↗

Graphene coating on silicon anodes enabled by thermal surface modification for high-energy lithium-ion batteries

Silicon is a high-energy density anode material for lithium-ion batteries, but it possesses shortcomings such as poor electronic conductivity, interfacial instability and mechanical fracturing that hinder its battery cycling. Carbon coating has been an important strategy for stabilizing silicon anodes, but the effects of the silicon surface properties on carbon coating morphology and the consequent silicon cycling stability have not been clearly elucidated. Herein, we find that thermal oxidation of the silicon anodes followed by chemical vapor deposition of carbonaceous precursors leads to a well-ordered graphene coating, whereas disordered graphite coating is formed on the native silicon surface. Graphene-coated silicon exhibits superior cycling performance, retaining a discharge capacity of ~1300 mAh g -1 after 300 cycles, whereas the disordered graphite-coated silicon suffers continuous degradation, retaining only~600 mAh g -1 after 300 cycles. Cryogenic electron microscopy reveals the mechanism behind the difference in cycling stabilities; graphene coated silicon is able to withstand the large mechanical strains induced during extended cycling, whereas disordered graphite coating is ruptured, exposing silicon surfaces to the electrolyte, leading to extensive buildup of SEI and poor cycling performance. Characterization of the silicon surface reveals that thermal treatment yields an oxygen-rich surface layer, which is hypothesized to play a decisive role in dictating the carbon coating. This work highlights the effect of silicon surface properties on carbon coating microstructure, and presents thermal treatment as a facile avenue to attain graphene coating on silicon anodes.

25 ENERGY STORAGE↗

Evaluating temperature dependent degradation mechanisms of silicon-graphite electrodes and the effect of fluoroethylene carbonate electrolyte additive

Understanding and overcoming the relatively high rate of degradation observed with silicon (Si)-based anodes in lithium (Li)-ion batteries (LiBs) is crucial for developing cells with increased energy density. The capacity fade of Si-graphite (Gr) electrodes in electrolytes with and without 10 wt% fluoroethylene carbonate (FEC) is explored during cycling at temperatures of 25, 45, and 70 °C, focusing on the complex degradation modes arising from loss of active material, loss of Li inventory, and cell resistance growth. We first show the common half-cell testing cannot be used at elevated temperatures as the performance of Li metal overshadows the behavior of Si-Gr electrode. Symmetric cell configuration successfully eliminates the effect of foreign materials, and reveals that while the presence of FEC provides better passivation of Si, it also results in greater parasitic reactions at 70 °C and faster capacity fade. The electrolyte without FEC, on the other hand, shows higher capacity retention at 70 °C. Finally, we propose a multi-step test protocol which can successfully deconvolute the information on loss of Li inventory and of active material. By combining half-cell and symmetric cell test methods, we demonstrate that loss of active material is reduced at higher temperatures and the dominant mechanisms of capacity loss for Si-Gr electrodes at elevated temperatures is loss of Li inventory.

25 ENERGY STORAGE↗

A Micrometer‐Sized Silicon/Carbon Composite Anode Synthesized by Impregnation of Petroleum Pitch in Nanoporous Silicon

Porous silicon (Si)/carbon nanocomposites have been extensively explored as a promising anode material for high-energy lithium (Li)-ion batteries (LIBs). However, shrinking of the pores and sintering of Si in the nanoporous structure during fabrication often diminishes the full benefits of nanoporous Si. Herein, a scalable method is reported to preserve the porous Si nanostructure by impregnating petroleum pitch inside of porous Si before high-temperature treatment. The resulting micrometer-sized Si/C composite maintains a desired porosity to accommodate large volume change and high conductivity to facilitate charge transfer. It also forms a stable surface coating that limits the penetration of electrolyte into nanoporous Si and minimizes the side reaction between electrolyte and Si during cycling and storage. A Si-based anode with 80% of pitch-derived carbon/nanoporous Si enables very stable cycling of a Si||Li(Ni0.5Co0.2Mn0.3)O 2 (NMC532) battery (80% capacity retention after 450 cycles). It also leads to low swelling in both particle and electrode levels required for the next generation of high-energy LIBs. In conclusion, the process also can be used to preserve the porous structure of other nanoporous materials that need to be treated at high temperatures.

anode materials↗

Development of Next Generation Hierarchical Hybrid Cu-Si anode Batteries via Direct-Ink Writing Application: End of (6th) Month Report - November 2025

Sustainable renewable energy continues to be in dire need to effectively combat global warming. Emerging technology for electric vehicles/ devices remains in high demand that is not only lower in cost, more efficient, but safer in comparison to commercial materials on the market. Although first-generation lithium-ion batteries have exhibited extensive commercial application, conventional graphite no longer meets this increasing demand as an efficient anode material. Due to the fact that graphite has a subpar theoretical specific capacity (372 mAh g -1 ), thus significant limitations in rate capability (for potential faster charging at higher C-rates currently commercially available.). Alternatively, silicon has gained significant attention as a superior candidate to potentially surpass graphite. Due to silicon’s exceedingly high theoretical capacity (4,200 mAh g -1 ) in comparison to standard graphite, its abundance thus in turn it’s low-cost, in addition to exhibiting a significantly low working potential (< 0.4 V vs Li/Li + ). However, one of the main (and most detrimental) challenges is silicon’s tendency to expand in volume (> 300%) upon discharge as it begins the lithiation process. As a direct result, it causes not only for the particles to both crack and pulverize under mechanical stress as the volume continues to expand and contract during cycling. Upon assembling the cell, it needs to undergo ‘charging’ for initially discharging/ ‘activating’ the cell, otherwise commonly known as the ‘formation’ step. As a result a solid electrolyte interface (SEI) layer begins to form at the anode surface because some of the electrolyte begins to react during the formation process. However, this (SEI) layer is deemed as a ‘protective’ interlayer because in theory it prevents further reaction as the cell continues to cycle. However, due to the volume change it causes significant degradation at the interface. As cracking starts to occur at the anode surface, it results in a ‘new’ altered surface with each cycle that causes further reaction with the electrolyte as a byproduct quickly consuming active Li/ and more electrolyte. Thus, fracturing this ‘protective layer,’ causing significantly higher impedance as a result, and in turn a decline in capacity due to active Li-loss. In addition to the active material exfoliating off from the current collector, further contributing to the steady decline in capacity and overall performance. Current state of the art Si-anode batteries on the market range between a maximum content of 5-10 Si wt%. It has been previously reported Tesla has utilized SiO x -C anodes containing 5 wt% Si within their ‘Model 3/ Model X’ electric vehicles. However, more recent ‘Model 3’ vehicles have started to incorporate 10 Si wt%, in which they were able to increase their energy density upwards by approximately 30%. Recent effort has been focused on continuing to increase the wt% of Si being utilized, eventually to 100 wt% of Si, to maximize the energy density even further.

36 MATERIALS SCIENCE↗

Understanding why poly(acrylic acid) works: decarbonylation and cross-linking provide an ionically conductive passivation layer in silicon anodes

Poly(acrylic acid) (PAA) is commonly used as a binder for fabricating silicon (Si) anode active materials in lithium-ion batteries due to its useful properties including high polar solvent solubility, good rheology, and strong adhesive properties. However, the role and evolution of PAA during electrode fabrication, cycling, and calendar aging are not well understood. In this work, we reveal the evolution of PAA during electrode curing and relate its chemical change to the final electrode properties and performance. These studies are made possible using two types of in situ attenuated total reflectance-infrared Fourier transform (ATR-FTIR) spectroscopy: thermal ATR-FTIR to probe the cross-linking reaction, and ATR-FTIR spectroelectrochemistry of three-dimensional composite electrodes, a unique technique developed herein that probes the solvation dynamics of lithium ions at the silicon anode interface under electrochemical polarization. Specifically, we show that PAA undergoes a thermally-mediated, cross-linking decarbonylation reaction to form an ether-based network polymer. To show the importance of the polyether moieties, we synthesize partially esterified PAA analogues that do not undergo this cross-linking decarbonylation reaction and correlate the degree of cross-linking to half-cell performance metrics. Finally, we unveil the mechanism of the polyether binder performance through in situ ATR-FTIR spectroelectrochemistry and show that PAA acts as an interfacial material that conducts lithium-ions, limits solvent molecule access to the Si surface, and stabilizes the electrode against parasitic lithium inventory loss at high state of charge for an extended period of time.

25 ENERGY STORAGE↗

Characterization of pitch carbon coating properties affecting the electrochemical behavior of silicon nanoparticle lithium-ion battery anodes

Silicon is an exciting material for next-generation lithium-ion battery anodes, due to its high theoretical capacity and availability, but its widespread implementation has been limited by extensive volume changes during cycling that causes mechanical damage and limits cycle life. One approach to mitigating these deleterious effects while still maintaining silicon's benefits is the addition of a pitch carbon coating to nanometer-sized silicon particles. Here, in this study, we present characterization of pitch-coated silicon electrodes without annealing and annealed at 700 °C and 1000 °C to determine the optimum temperature treatment, as well as pitch-only and silicon-only electrodes with and without annealing to elucidate the impacts of each component on early electrochemical behavior. Using Fourier transform infrared and Raman spectroscopies, atomic force and scanning spreading resistance microscopy, and electrochemical analysis, we find 700 °C to be the optimal annealing temperature, as amorphous carbon is created, which improves conductivity prior to cycling and facilitates ion storage during cycling that increases capacity. We also present in situ Raman spectroscopy data demonstrating the heterogeneous aging that occurs across the electrode surface during cycling.

25 ENERGY STORAGE↗

Functionalized Silicon Particles for Enhanced Half- and Full-Cell Cycling of Si-Based Li-Ion Batteries

Vinylene carbonate (VC) and polyethylene oxide (PEO) have been investigated as functional agents that mimic the solid electrolyte interphase (SEI) chemistry of silicon (Si). VC and PEO are known to contribute to the stability of Si-based lithium-ion batteries as an electrolyte additive and as a SEI component, respectively. In this work, covalent surface functionalization was achieved via a facile route, which involves ball-milling the Si particles with sacrificial VC and PEO. Thermogravimetric analysis (TGA), X-ray photoelectron spectroscopy (XPS), and magic angle spinning nuclear magnetic resonance (MAS NMR) spectroscopy indicate that the additives are strongly bound to Si. In particular, MAS NMR shows Si–R or Si–O–R groups, which confirm functionalization of the Si after milling in VC or PEO. Particle size analysis by dynamic light scattering reveals that the additives facilitate particle size reduction and that the functionalized particles result in more stable dispersions based on zeta potential measurements. Raman mapping of the electrodes fabricated from the VC and PEO-coated active material with a polyacrylic acid (PAA) binder reveals a more homogenous distribution of Si and the carbon conductive additive compared to the electrodes prepared from the neat Si. Furthermore, the VC-milled Si strikingly exhibited the highest capacity in both half- and full-cell configurations, with more than 200 mAh g –1 measured capacity compared to the neat Si in the half-cell format. This is linked to an improved electrode processing based on the Raman and zeta potential measurements as well as a thinner SEI (with more organic components for the functionalized Si relative to the neat Si) based on XPS analysis of the cycled electrodes. In conclusion, the effect of binder was also investigated by comparing PAA with P84 (polyimide type), where an increased capacity is observed in the latter case.

25 ENERGY STORAGE↗

Mitigating Calendar Aging in Si-NMC Batteries with Advanced Dual-Salt Glyme Electrolytes

In addressing the critical challenge of calendar aging in silicon (Si)-based lithium-ion batteries, this study introduces a groundbreaking strategy utilizing glyme-type dual-salt electrolytes (lithium bis(trifluoromethanesulfonyl)imide [LiTFSI] and lithium difluoro(oxalato)borate [LiDFOB]). These electrolytes are demonstrated to significantly mitigate parasitic reactions and capacity loss in Si-NMC (lithium nickel manganese cobalt oxide) full cells, especially when compared with traditional carbonate-based electrolytes. Further, our exhaustive mechanistic analysis reveals that such electrolytes not only preserve the integrity of the Si anode but also improve the cathode/electrolyte interphases (CEI) through the formation of a conformal coating on the high-voltage cathode surface. This dual-salt approach, enhanced by the addition of a phosphate additive, effectively decelerates calendar aging, marking a substantial advance in the quest for durable and reliable Si-based energy storage technologies. The findings underscore the vital role of electrolyte composition in extending the calendar life of Si batteries, offering an alternative avenue toward maximizing the performance and longevity of next-generation Li-Si batteries.

36 MATERIALS SCIENCE↗

Insights into Chemical Prelithiation of SiO x /Graphite Composite Anodes through Scanning Electron Microscope Imaging

Initial Coulombic efficiency (ICE) is critical for determining the energy density of lithium-ion batteries (LIBs) used for practical applications; however, it is typically disregarded in anode research. We used SiO x and graphite composite anodes for commercial lithium-ion batteries in our preliminary research to achieve a balance between ICE, capacity, and cycling life. ICE reached 88%; however, it needs further improvement for commercial applications. Prelithiation is a process that involves the introduction of extra lithium ions into LIBs during their manufacturing to enhance the overall performance of the LIBs. We applied a chemical prelithiation method on our SiO x /graphite composite anodes, which comprised 95 wt % of the active material mass loading on the electrode. The ICE increased from 88% to 98% using an aryllithium reagent impregnation method within 2 min of prelithiation. The anode’s specific capacity density, rate, and cycle performance also significantly improved. Scanning electron microscopy (SEM) imaging enhanced by an osmium tetroxide staining method indicated that the P-anode contained a stable solid electrolyte interface (SEI) layer after the prelithiation process and cycling electrochemical test. The P-anode’s stable charge differential peak over 500 cycles also showcases a robust artificial SEI layer that was generated by the prelithiation procedure. Here, this prelithiation process has significant potential for adoption in the LIB industry’s current electrode manufacturing process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Prelithiated SiO x /Graphite-NMC811 Cells: Capacity Loss, Impedance Rise and Hidden Degradation Pathways Revealed Using Three-Electrode Diagnostics

Electrodes containing SiO x /graphite (Gr) materials are attractive as anodes for high-energy lithium-ion batteries. However, their mechanical deformation, electrochemical response, and impedance evolution during long-term cycling are strongly coupled, complicating accurate diagnosis of performance fade mechanisms. In this work, the behavior of electrochemically prelithiated SiO x /Gr anodes paired with NMC811 cathodes is systematically investigated using techniques that include in-situ dilatometry, three-electrode electrochemistry, and multiscale post-cycling microscopy. The SiO x /Gr electrode exhibits a maximum expansion of 49% upon lithiation to 10 mV vs Li + /Li, with 84% of the expansion and 91% of the capacity being reversible. In full cells, relatively stable cycling with only 12% capacity fade over 500 cycles is observed. Three-electrode experiments reveal cell-level impedance growth, which is dominated by the NMC811 cathode: the SiO x /Gr anode exhibits minimal net impedance rise and an initial impedance decrease at low potentials. Despite this apparent electrochemical stability, cross-sectional SEM, PFIB tomography, and cryo-STEM reveal irreversible anode thickening caused by the accumulation of an inorganic-rich solid electrolyte interphase (SEI) permeating the anode bulk. Electrode potential-shift analysis further demonstrates that Li + ions released from lithium reservoirs in the prelithiated anode mask true lithium inventory loss during aging. These results demonstrate that low-expansion SiO x /Gr anodes can simultaneously exhibit favorable cycling and impedance metrics while undergoing substantial, hidden degradation, underscoring the importance of electrode-resolved diagnostics for evaluating prelithiated silicon-based anodes.

25 ENERGY STORAGE↗

Effect of electrochemical cycling on microstructures of nanocomposite silicon electrodes using hyperpolarized 129 Xe and 7 Li NMR spectroscopy

The microstructural stability of composite electrodes during electrochemical cycling is critically important as it dictates the performance of Li-ion batteries. The issue becomes even more important for the high capacity alloying anode such as silicon that typically exhibits dramatic lithiation–delithiation-induced volume changes. The solid electrolyte interphase (SEI) layer formed on the active electrode surface has a profound effect on the overall microstructural stability of composite electrodes. An ideal SEI layer allows Li+ ions in and out of the electrode, but is an insulator to electrons, preventing the electrolyte from being further reduced. However, the SEI layers formed during initial lithiation may experience changes or degradation with subsequent cycling, adversely affecting the electrode performance. A combination of hyperpolarized 129 Xe and 7 Li nuclear magnetic resonance spectroscopies was applied to probe the microstructures of nanocomposite silicon electrodes at various stages of the lithiation–delithiation cycle. The results obtained from this study shed light on the degradation mechanism of nanocomposite Si electrodes upon electrochemical cycling and should prove useful in the effort to design more robust electrodes in the future.

36 MATERIALS SCIENCE↗

LiH formation and its impact on Li batteries revealed by cryogenic electron microscopy

Little is known about how evolved hydrogen affects the cycling of Li batteries. Hypotheses include the formation of LiH in the solid-electrolyte interphase (SEI) and dendritic growth of LiH. Here, we discover that LiH formation in Li batteries likely follows a different pathway: Hydrogen evolved during cycling reacts to nucleate and grow LiH within already deposited Li metal, consuming active Li. We provide the evidence that LiH formed in Li batteries electrically isolates active Li from the current collector that degrades battery capacity. We detect the coexistence of Li metal and LiH also on graphite and silicon anodes, showing that LiH forms in most Li battery anode chemistries. Last, we find that LiH has its own SEI layer that is chemically and structurally distinct from the SEI on Li metal. Our results highlight the formation mechanism and chemical origins of LiH, providing critical insight into how to prevent its formation.

25 ENERGY STORAGE↗

Electrochemical Formation of Li-M-(M')-Si Phases Using Multivalent Electrolyte Salt Additives

Lithium-rich silicides (Li 15 Si 4 ), formed during the electrochemical lithiation of silicon, show high reactivity with electrolyte components that contribute to capacity decay, formal lithium loss, and low coulombic efficiency. Recently, the reactivity of lithium silicides was found to be suppressed by substituting a multivalent cation (i.e. Mg, Ca) for lithium that results in the room temperature formation of a ternary Li-M-Si phase. In this study, we explored a range of multivalent electrolyte salt additives (M = Ni, Cu, La, Ce, Sr, Ba, and Ca-Mg mixed salt) in a lithium-ion cell configuration and identified a room temperature electrochemical route to the formation of new ternary and quaternary lithium silicides. Using this method, both nickel and copper salts were found to plate onto the silicon electrode surface upon lithiation. Further, based on refined synchrotron XRD data, multivalent cations with an ionic radius similar to Na (~1.03 Å) or smaller can be inserted electrochemically into a formally cation-deficient Li 15 Si 4 host lattice to form new ternary (or quartenary) phases. The electrochemical synthesis of a new quaternary Li-M-M’-Si phase represents a facile route to preparing and scaling materials isostructural to the Heusler phase and electron-precise Li 14 MgSi 4 phase that results in enhanced cycling and calendar life performance.

25 ENERGY STORAGE↗

Assessing Electrolyte Fluorination Impact on Calendar Aging of Blended Silicon-Graphite Lithium-Ion Cells Using Potentiostatic Holds

Silicon-based lithium-ion batteries have started to meet cycle life metrics, but they exhibit poor calendar life. Here, electrolyte fluorination impact on calendar fade of blended silicon-graphite anodes is explored using a LiPF 6 in EC:EMC:FEC electrolyte vs LiBOB in EC:EMC electrolyte. We utilize a combined experimental-modeling approach applying potentiostatic voltage holds (V-hold) to evaluate electrolyte suitability for calendar life in a shortened testing timeframe (~2 months). Our theoretical framework deconvolutes the irreversible parasitic capacity losses (lithium lost to the solid electrolyte interphase) from the V-hold electrochemical data. Unfluorinated electrolyte (dominant LiBOB reduction) exhibits higher cell resistance as compared to fluorinated electrolyte (dominant FEC reduction). Both systems have similar irreversible capacities during the voltage hold duration with slower rate of parasitic capacity loss for the LiBOB system. Extrapolation of the parasitic losses to end of life capacity fade of 20% shows LiBOB electrolyte outperforming LiPF 6 electrolyte in calendar life. The results demonstrate the applicability of the V-hold protocol as a rapid material screening tool providing semi-quantitative calendar lifetime estimates.

25 ENERGY STORAGE↗

Evaluating Contributions of Pitch-Carbon Coating to Improved Stability of Si Anodes Through Voltage-Resolved Multi-Phase Characterization

Silicon nanoparticles have emerged as a promising alternative to graphite to improve the energy density of next-generation lithium-ion battery anodes. Nano-sized Si domains facilitate rapid ion transport and minimize particle-scale mechanical degradation, but also exhibit increased (electro)chemical reactivity with Li-ion electrolyte components due to their high surface area. We have previously demonstrated that surface modification of Si nanoparticles with pitch-carbon is an effective strategy to reduce these parasitic reactions. In the present work, we holistically evaluate the mechanistic contribution of pitch-carbon coating to the observed stability improvement over uncoated Si. We utilize coupled in situ and ex situ methods to probe changes to solid-surface, volatile headspace, and gas-phase chemistry occurring during initial cycling. Measurements taken at targeted potentials associated with electrolyte species reduction enables the decoupling of specific reaction pathways tied to interfacial stability. Further, we demonstrate the non-trivial role of gas reconsumption in dictating the nature of the passivating surface layer evolved on both uncoated and pitch-coated Si. This multi-phase analysis offers insights into the mechanism of effective surface passivation, which may be applied to inform future Si material development.

ENERGY STORAGE↗

Study on the Carbon Nanostructures for Nanosized Si Electrodes

Silicon (Si) has been considered as a next-generation anode material due to natural abundance, low operating potential (<0.5 V vs. Li/Li+), and high theoretical specific capacity of 4200 mAh g-1.[1] However, the electrochemical alloying reaction of Si involves large volume changes of 400% during lithiation and delithiation, causing cracking and pulverization of Si.[1] In addition, solid electrolyte interface (SEI) of Si anode experiences constant changes due to unstable SEI reactivity.[2] Considerable efforts have been made to design nanostructured Si materials to address the issues because nanostructuring can relieve the mechanical strain.[3] However, when compared to micrometer-sized active materials having sufficient electrolyte pathway through interparticle space, the nanoparticle (NP)-based electrodes tend to be densely packed. As mass loading is higher and electrode is thicker, ion transport issue can become more severe in the densely packed electrodes.[4] In this work, we will present studies on engineered porosity impacts performance in Si NP electrodes by altering carbon nanostructures. We explore the extreme limit of effectively non-porous electrodes using quasi-spherical, Si NPs, which result in densely packed electrodes when slurry is prepared with conventional carbon black. We engineer porosity using carbon nanostructures including multi-walled carbon nanotubes and carbon nanorods in place of conventional carbon black to create pore structure in Si NP-based electrodes. These experiments provide a correlation between mass loading, porosity and silicon utilization in Si NP-based electrodes. References: [1] C. K. Chan, H. Peng, G. Liu, K. Mcllwrath, X. F. Zhang, R. A. Huggins, Y. Cui, "High-performance lithium battery anodes using silicon nanowires", Nat. Nanotechnol., 2008, 3, 31, [2] J. D. McBrayer, M.-T. F. Rodrigues, M. C. Schulze, D. P. Abraham, C. A. Apblett, I. Bloom, G. M. Carroll, A. M. Coclasure, C. Fang, K. L. Harrison, G. Liu, S. D. Minteer, N. R. Neale, G. M. Veith, C. S. Johnson, J. T. Vaughey, A. K. Burrel, B. Cunningham, "Calendar aging of silicon-containing batteries", Nat. Energy, 2021, 6, 1164, [3] H. Wu, G. Zheng, N. Liu, T. J. Carney, Y. Yang, Y. Cui, "Engineering Empty space between Si Nanoparticles for Lithium-Ion Battery Anodes", Nano Lett., 2012, 12, 904, [4] X. Zhang, Z. Ju, Y. Zhu, K. J. Takeuchi, E. S. Takeuchi, A. C. Marschilok, G. Yu, "Multiscale Understanding and Architecture Design of High Energy/Power Lithium-Ion Battery Electrodes", Adv. Energy Mater., 2021, 11, 2000808

carbon nanostructure↗