Search NASA⌕ Search

SEARCH · Search NASA

Results for “MARTENSITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Crystallographic analysis of lenticular martensite in Fe–1.0C–17Cr stainless steel by electron backscatter diffraction

The crystallography of lenticular martensite, which formed in coarse austenite grains (size about 80 μm) after subzero treatment at − 196 °C (liquid nitrogen) for different holding times, was investigated using electron backscatter diffraction (EBSD). For the sample treated with 15 min of isothermal holding, more than 50 martensite plates (with a thickness of larger than 1 μm) that formed within a coarse austenite grain were employed to obtain the pole figures. The pole figures clearly indicated that the individual plate of lenticular martensite approximately adopted the Kurdjumov–Sachs (K–S) orientation relationship with respect to the austenite matrix. For the sample treated with 30 s of isothermal holding, a few martensite plates that formed in variant pairings in a coarse austenite grain were analyzed. The results showed that zigzag couplings (including spear couplings), the major product of plate martensite, had an absolute dominance of a specific variant pair (V1/V17). The orientation gradient within a lenticular martensite plate was also measured using convergent beam electron diffraction (CBED). The evidence strongly suggests that the spread in diffracted intensity within pole figures is related to the misorientation gradient within the lenticular martensite plate. - Highlights: • The orientation relationship between lenticular martensite and austenite was investigated by pole figures via Electron Backscatter Diffraction (EBSD). • The initial stage of lenticular martensite formation was investigated, excluding interference from hard impingement. • In addition to EBSD, convergent beam electron diffraction (CBED) was used to measure the misorientation angle from the midrib to the untwinned region in lenticular martensite plate. • Zigzag couplings (including spear couplings), the major product of plate martensite, had an absolute dominance of a specific variant pair (V1/V17).

36 MATERIALS SCIENCE↗

Structure and crystallography of martensite–austenite constituent in the intercritically reheated coarse-grained heat affected zone of a high strength pipeline steel

Highlights: • Structure and crystallography of M-A constituent in ICCGHAZ of X100 weld joint was studied via multi-scale characterization. • Majority of M-A constituent preferred to form lamellar lath structure, which primarily consisted of lath martensite (87%). • The retained austenite had K-S orientation relationship with its neighboring martensite. • Adjacent martensite laths within M-A had large misorientation but no fixed crystallographic orientation relationship. • Martensite laths within the M-A constituent did not inherit the crystallographic orientation of the parent matrix. - Abstract: The structure and crystallography of martensite-austenite (M-A) constituent in the intercritically reheated coarse-grained heat affected zone (ICCGHAZ) of X100 (690 MPa) pipeline steel weld joint was studied via multi-scale characterization. The results suggested that majority of the necklace-type M-A constituent in the ICCGHAZ preferred to form lamellar lath structure, which primarily consisted of lath martensite (87%). Only small fraction of retained austenite (9%) was found between martensite laths. The retained austenite had K-S orientation relationship with its neighboring martensite: (10-1){sub M} // (11-1){sub γ} and [111]{sub M} // [011]{sub γ}. Adjacent martensite laths within M-A constituent had large misorientation but no fixed crystallographic orientation relationship which implied that martensite laths may nucleate independently and encounter with each other during growth. M-A constituent and matrix microstructure belonged to different prior austenite grains. The martensite laths within the M-A constituent did not inherit the crystallographic orientation of the parent matrix during the intercritical reheating and subsequent cooling process of the second pass welding.

36 MATERIALS SCIENCE↗

Characteristics of martensite transformed from deformed austenite with various states of ultrahigh strength 300 M steel

Highlights: • Fractions of lath martensite and its packets decrease with the increasing of strain. • Length and width of blocks of lath martensite decrease with an increase in strain. • Severe work-hardening and completed DRX hamper transformation of lath martensite. • As for austenite with the state of work-hardening, the lath width changes little. • As for austenite with the state of DRX and subsequent growth, the lath width changes. - Abstract: 300 M steel was isothermally compressed on a Gleeble 1500 simulator at a deformation temperature of 1173 K, a strain rate of 0.1 s{sup −1} and strains ranging from 0.11 to 1.20. The morphologies and structure characteristics of martensite transformed from deformed austenite during water quenching were observed and analysed via scanning electron microscope and transmission electron microscope. Subsequently, effects of prior austenite state on martensitic transformation behavior of 300 M steel were analysed. The experimental results showed that predominant lath martensite and complemental twinned martensite and retained austenite coexisted in deformation-quenched 300 M steel at various strains. The volume fraction of lath martensite and packets of lath martensite decreased with the increasing of strain, and the length and width of the blocks in lath martensite concurrently decreased. Prior austenite with the state of severely work-hardening or just completed dynamic recrystallization would hamper the nucleation and subsequent growth of lath martensite. Additionally, as for austenite with the state of work-hardening, the morphologies and width of laths changed little with the increasing of strain, whereas dislocations in the interior of laths dramatically increased. However, as for austenite with the state of dynamic recrystallization and subsequent growth, the width of laths obviously increased with the increasing of austenite grain size.

36 MATERIALS SCIENCE↗

Structural and Magnetic Properties of Thermal- and Deformation-Induced Martensite in an Fe-27%Ni-4%Mn-1%Zn Alloy

Deformation- and thermal-induced martensite properties were examined according to existing martensite morphology and magnetic properties for same prior austenite homogenization conditions in Fe-27%Ni-4%Mn-1%Zn alloy. Scanning electron microscope (SEM) and vibrating sample magnetometer (VSM) characterization techniques were employed for the investigation. Scanning electron microscope observations showed that while martensite formation in the austenite phase of alloy exhibited a lath morphology by thermal effect, elongated deformation-induced martensite morphology exists after deformation. The Curie temperatures were detected at about 201 K for thermal-induced martensite and at about 226 K for deformation-induced martensite from VSM measurements. The magnetic saturation values were determined as about 21 emu g{sup −1} for thermal-induced martensite and 23 emu g{sup −1} for deformation-induced martensite. We found that magnetic saturation increased with deformation effect. On the other hand, VSM offered the soft ferromagnetic characteristic with coersive values of 36 Oe for thermal-induced martensite and the soft ferromagnetic characteristic with 47 Oe for deformation-induced martensite. The changes in the magnetic properties resulting from the thermal and deformation affect were clearly determined. Deformation caused magnetic stabilization in Fe-27%Ni-4%Mn-1%Zn alloy.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characteristics and mechanisms of hydrogen-induced quasi-cleavage fracture of lath martensitic steel

Here this study presents an in-depth characterization of the microstructures, crystallographic orientations, and dislocation characteristics beneath hydrogen-induced quasi-cleavage fracture features of an as-quenched, lath martensitic (α') 22MnB5 steel. The fracture surfaces of gaseous hydrogen-embrittled martensitic specimens were analyzed by a combination of multiple analytical tools: scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM), and transmission Kikuchi diffraction (TKD). The dominant fracture mode in the hydrogen-affected zones was quasi-cleavage fracture, which involved significant plasticity, evidenced by plastic zones near tear ridges and a high density of dislocations beneath the quasi-cleavage facets. The martensite constituent sizes, variant orientations, and boundaries influenced the quasi-cleavage surface morphologies. Fractography revealed the occurrence of {100} α' -type cleavage across martensitic laths, developing relatively “flat” quasi-cleavage surfaces, in addition to {110} α' -type cracking likely along lath and block boundaries, and fracture along non-cleavage planes. The likelihood of the formation of the relatively “flat” quasi-cleavage surfaces increased with increasing martensitic constituent sizes. Substantial dislocation bands formed on intersecting {112} α' slip planes within a martensite block below the hydrogen-induced cleavage fractures on {100} α' planes. River markings on the quasi-cleavage surfaces were found to originate from the complex, hierarchical lath martensitic microstructure. Steps and ridges on the quasi-cleavage facets generally linked with the various martensitic boundaries, suggesting that they were produced as a result of crack deviations at those boundaries. The fracture paths and martensite quasi-cleavage mechanisms are discussed in the context of the role of hydrogen and Cottrell cleavage model.

36 MATERIALS SCIENCE↗

Nano/ultrafine grained austenitic stainless steel through the formation and reversion of deformation-induced martensite: Mechanisms, microstructures, mechanical properties, and TRIP effect

A comprehensive study was carried out on the strain-induced martensitic transformation, its reversion to austenite, the resultant grain refinement, and the enhancement of strength and strain-hardening ability through the transformation-induced plasticity (TRIP) effect in a commercial austenitic 304L stainless steel with emphasis on the mechanisms and the microstructural evolution. A straightforward magnetic measurement device, which is based on the measurement of the saturation magnetization, for evaluating the amount of strain-induced martensite after cold rolling and reversion annealing in metastable austenitic stainless steels was used, which its results were in good consistency with those of the X-ray diffraction (XRD) method. A new parameter called the effective reduction in thickness was introduced, which corresponds to the reasonable upper bound on the obtainable martensite fraction based on the saturation in the martensitic transformation. By means of thermodynamics calculations, the reversion mechanisms were estimated and subsequently validated by experimental results. The signs of thermal martensitic transformation at cooling stage after reversion at 850 °C were found, which was attributed to the rise in the martensite start temperature due to the carbide precipitation. After the reversion treatment, the average grain sizes were around 500 nm and the nanometric grains of the size of ~ 65 nm were also detected. The intense grain refinement led to the enhanced mechanical properties and observation of the change in the work-hardening capacity and TRIP effect behavior. A practical map as a guidance for grain refining and characterizing the stability against grain growth was proposed, which shows the limitation of the reversion mechanism for refinement of grain size. - Graphical abstract: Display Omitted - Highlights: • Nano/ultrafine grained austenitic stainless steel through martensite treatment • A parameter descriptive of a reasonable upper bound on the obtainable martensite • Characterization of martensite by virtue of a new developed magnetic device • Investigation of mechanical properties and TRIP effect and the effect of grain size.

36 MATERIALS SCIENCE↗

Twinning and martensitic transformations in nickel-enriched 304 austenitic steel during tensile and indentation deformations

Twinning and martensitic transformation have been investigated in nickel-enriched AISI 304 stainless steel subjected to tensile and indentation deformation. Using electron backscatter diffraction (EBSD), the morphology of alpha- and epsilon-martensite and the effect of grain orientation to load axis on phase and structure transformations were analyzed in detail. It was found that the twinning occurred less frequently under indentation than under tension; also, twinning was not observed in [001] and [101] grains. In tensile tests, the martensite particles preferably formed at the deformation twins, intersections between twins, or at twin-grain boundary intersections. Conversely, martensite formation in the indentation tests was not closely associated with twinning; instead, the majority of martensite was concentrated in the dense colonies near grain boundaries. Martensitic transformation seemed to be obstructed in the [001] grains in both tensile and indentation test cases. Under a tensile stress of 800 MPa, both alpha- and epsilon-martensite were found in the microstructure, but at 1100 MPa only -martensite presented in the specimen. Under indentation, alpha- and epsilon-martensite were observed in the material regardless of stress level.

Gussev, Maxim N↗

Effects of heat treatment and build orientation on the evolution of $ϵ$ and $α'$ martensite and strength during compressive loading of additively manufactured 304L stainless steel

In this paper, the effect of heat-treatment and build orientation on martensitic phase transformation in additively manufactured (AM) 304L stainless steel is studied and compared with conventionally produced wrought material. The relationships between observed martensitic transformations and material microstructures and their effects on mechanical strength are established through experimental observations. In situ high-energy X-ray powder diffraction measurements were performed to monitor the evolution of $ϵ$ and $α'$ martensite during compressive loading of stainless steel. Electron backscatter diffraction (EBSD) was used to provide insight on initial grain morphology, crystallographic misorientation within grains, and crystallographic texture. Heat treatment alters the microstructure of AM samples creating different initial conditions. This difference in starting microstructure resulted in variability in martensitic transformation during compressive deformation. The rate of martensitic transformation decreased for AM samples treated with temperatures up to 1100°C, after which the AM microstructures recrystallized, resulting in increased rate of martensitic transformation for those samples treated at higher temperatures. It was also observed that aligning the axis of compression with the AM build direction resulted in a lower rate of strain-induced martensite formation as opposed to aligning the compression axis perpendicular to it. More favorable distribution of crystal orientations in the latter loading orientation promoted martensitic transformation. These and additional experimental observations from EBSD in terms of kernel average misorientation, mean grain orientation spread, and mean crystallite size reveal strong microstructural effects on strength of additively manufactured metallic materials.

304L stainless steel↗

Martensitic transformations in Ti-6Al-4V (ELI) alloy manufactured by 3D Printing

Highlights: • Two metastable martensitic phases, namely α′′ and α′ may be formed in Ti-6Al-4V during 3D manufacturing process. In the present investigation, Ti-6Al-4V ELI samples were manufactured by the powder-bed fusion (PBF) process using the laser sintering (LS) technology. Microstructure, chemical and phase constitution, and mechanical properties were studied by means of the transmission electron microscopy, atom probe tomography, X-ray diffraction, nanoindentation and mechanical testing. It was found that the structure of LS samples consisted of two different variants of metastable phases, namely the hexagonal α′ martensitic phase and small amounts of the orthorhombic α″ martensitic phase. The martensitic α′-phase was formed because of the high cooling rates of the LS method. The {10 1-bar 2} 1-bar 011 hexagonal martensite tensile twins were observed in the microstructure of the as-build alloy. Small areas with inner twinning martensitic plates, which are typical for the metastable orthorhombic martensitic phase in titanium alloys, were identified by the transmission electron microscopy. Atom probe tomography (APT) confirmed localization of β-stabilizing elements at interfaces, presumably at the twin or lamella boundaries. The structure and origin of the martensitic phases in 3D printed Ti-6Al-4V alloys are discussed with respect to in-situ heat treatment during manufacturing.

36 MATERIALS SCIENCE↗