Search NASA⌕ Search

SEARCH · Search NASA

Results for “MAX phase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Synthesis of Mo 4 VAlC 4 MAX Phase and Two-Dimensional Mo 4 VC 4 MXene with Five Atomic Layers of Transition Metals

MXenes are a family of two-dimensional (2D) transition metal carbides, nitrides, and carbonitrides with a general formula of M n+1 X n T x , in which two, three, or four atomic layers of a transition metal (M: Ti, Nb, V, Cr, Mo, Ta, etc.) are interleaved with layers of C and/or N (shown as X), and T x represents surface termination groups such as –OH, =O, and –F. Here, we report the scalable synthesis and characterization of a MXene with five atomic layers of transition metals (Mo 4 VC 4 T x ), by synthesizing its Mo 4 VAlC 4 MAX phase precursor that contains no other MAX phase impurities. These phases display twinning at their central M layers which is not present in any other known MAX phases or MXenes. Transmission electron microscopy and X-ray diffraction were used to examine the structure of both phases. Energy-dispersive X-ray spectroscopy, X-ray photoelectron spectroscopy, Raman spectroscopy, and high-resolution scanning transmission electron microscopy with energy-dispersive X-ray spectroscopy were used to study the composition of these materials. Density functional theory calculations indicate that other five transition metal-layer MAX phases (M' 4 M"AlC 4 ) may be possible, where M' and M" are two different transition metals. The predicted existence of additional Al-containing MAX phases suggests that more M 5 C 4 T x MXenes can be synthesized. Additionally, we characterized the optical, electronic, and thermal properties of Mo 4 VC 4 T x . Here, this study demonstrates the existence of an additional subfamily of M 5 X 4 T x MXenes as well as a twinned structure, allowing for a wider range of 2D structures and compositions for more control over properties, which could lead to many different applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

MAX-Phase Partial Optical Properties

The optical and electrical properties of MAX-phase materials have been thoroughly studied in the past. We present here a new technique to determine and study the partial contributions to the optical properties. Following the same methodology as the decomposition of the density of states to the partial density of states, we have decomposed the optical properties into the partial optical properties. Using this technique the differences of elemental and layer resolved optical properties are displayed for both the 211 and 312 phase of TiSiC and TiAlC MAX-phase materials.

Weigand, Alysse↗

Modeling the non-Schmid crystallographic slip in MAX phases

We present a crystal plasticity constitutive relation for the description of experimentally observed non-Schmid crystallographic slip in a class of ternary carbides and nitrides commonly referred to as MAX phases. In the constitutive relation, we assume that the evolution of the slip system strength in MAX phases has two components – a classical component that depends on the Taylor cumulative shear strain and a non-Schmid component that depends on the stress normal to the slip plane. The non-Schmid crystal plasticity constitutive relation is then used to carry out finite element simulations of micropillar compression of single crystals of two MAX phases, Ti 2 AlC and Ti 3 AlC 2 . The finite element simulations not only quantitatively predict the stress – strain response of a wide range of crystallographic orientations of the micropillars but also rationalize the non-uniform deformation and the deformed shape of the micropillars observed in the experiments for the two materials. As a result, parametric studies are also carried out to quantify the role of the non-Schmid effect and understand the effects of key experimental parameters on the stress – strain response of the micropillars of the two MAX phases.

36 MATERIALS SCIENCE↗

Synthesis, microstructure and micro-mechanical characterization of metal (Nb, Ti) – MAX phase (Ti 2 AlC) nanolaminates

We utilize elevated temperature physical vapor deposition (PVD) techniques to design metal/MAX multilayered nanocomposite thin films with alternating nanoscale metallic (Nb, Ti) and MAX phase (Ti 2 AlC) layer thicknesses. These metal/MAX nanolaminate architectures attempt to exploit a unique hierarchical topology – as interfaces between the layers are expected to be in direct competition with the internal interfaces within the MAX layers, to drive their tunable macroscopic mechanical behavior. Two metal/MAX nanolaminates – Nb/Ti 2 AlC and Ti/Ti 2 AlC – were deposited. The Nb/Ti 2 AlC metal/MAX system showed highly diffused layer interfaces with distinct Ti – rich and Nb–Al – rich layers, with the presence of MAX phase alongside TiC and other Ti–Al and Nb–Al intermetallic phases. The Nb/Ti 2 AlC system possessed a layered architecture, though the MAX phases were not found to be continuously present in each alternating layer. The second Ti/Ti 2 AlC system showed a non-lamellar nanocomposite microstructure and the formation of mixed Ti n+1 AlC n phases (a mix of n = 1, 2), and no indication of layering. Diffusion occurring between the metal/MAX layers in both cases, likely due to the elevated temperatures during the deposition process, is speculated as the likely cause of these resultant microstructures. The mechanical properties of both systems were evaluated using micromechanical (nanoindentation and micro-pillar compression) techniques, which demonstrated high strengths for both systems (Nb system: yield and instability strengths of 4.88 ± 0.1 GPa and 5.57 ± 0.03 GPa, Ti system: yield and instability strength of 5.61 ± 0.28 GPa and 6.21 ± 0.25 GPa). In conclusion, this work highlights the promising mechanical properties of metal/MAX multilayered depositions and summarizes the challenges in PVD synthesis of metal/MAX multilayered nanolaminates.

MAX phase↗

Robust Solar Receivers Using MAX Phase Materials

This work was supported by the U.S. Department of Energy’s Office of Energy Efficiency and Renewable Energy under the Solar Energy Technologies Office Award Number 35928. The objective of the proposed effort was to develop and optimize additive manufacturing technologies for low-cost fabrication of high-temperature receivers using MAX phase-based materials (Ti 3 SiC 2 and Ti 3 AlC 2 ). MAX phase materials are a group of ternary metal carbides and nitrides where M stands for an early transition metal element, A is a group 13–16 element, and X is C and/or N. In Phase 1, the binder jetting additive manufacturing process was used to synthesize and characterize the Ti 3 SiC 2 MAX phase material. The typical process involved first producing a TiC preform using binder jetting followed by infiltration of the preform with silicon melt to form Ti 3 SiC 2 in situ. The reaction-infiltrated samples showed formation of MAX phase in the sample core; however, the surface showed cracking. Various process conditions—cooling rates, hold times, Si proportion, etc.—were varied to minimize the surface cracking. The fabricated MAX phase core was characterized by microstructure analysis and evaluations of mechanical properties such as hardness and thermal shock. In Phase 2, the focus included fabrication of Ti 3 SiC 2 MAX phase materials by spark plasma sintering (SPS) and synthesis of Ti 3 AlC 2 MAX phase materials by the Al melt infiltration process. It is expected that Al infiltration will not cause sample cracking, since Al does not expand during solidification. In addition, other processing approaches were investigated to fabricate the MAX phase materials, such as SPS with a graphite bedding approach for producing short-length Ti 3 AlC 2 MAX phase tubes for demonstration of prototypical Concentrating Solar Power receiver tubes. Fabricated samples underwent thermo-mechanical testing to validate the materials for the solar receiver application at temperatures >1000°C. In Phase 3, the effort focused on the development and optimization of the Ti-Al-C MAX phase composite material using the Al melt infiltration approach. We started with optimization of precursor powders and making preform structures by either pressing them in a die or using the binder jetting additive manufacturing process followed by Al melt infiltration. In addition, we investigated the formation of preform structures by cold isostatic pressing followed by Al melt infiltration for making Ti-Al-C MAX phase composite. Thermo-mechanical characterizations, such as creep, strength, and thermal shock, were conducted to establish the structures’ performance.

36 MATERIALS SCIENCE↗

Ti{sub 2}GaC, Ti{sub 4}GaC{sub 3} and Cr{sub 2}GaC-Synthesis, crystal growth and structure analysis of Ga-containing MAX-phases M{sub n+1}GaC{sub n} with M=Ti, Cr and n=1, 3

Single crystals of Ga-containing MAX-phases Ti{sub 2}GaC, Ti{sub 4}GaC{sub 3}, and Cr{sub 2}GaC were grown from a metallic melt generated by an excess of Ga. This technique allows the crystal growth at different temperatures to control the product distribution. Compounds developed were Ti{sub 2}GaC and TiC at 1500 deg. C, and Ti{sub 2}GaC and Ti{sub 4}GaC{sub 3} at 1300 deg. C. Crystal structures were refined from single crystal data. Ti{sub 2}GaC and Cr{sub 2}GaC were previously known, and belong to the Cr{sub 2}AlC type as well as the solid solutions V{sub 2}Ga{sub 1-x}Al{sub x}C and Cr{sub 2}Ga{sub 1-x}Al{sub x}C. Ti{sub 4}GaC{sub 3} is one of the few 413-phases (P6{sub 3}/mmc, a=3.0690(4) A, c=23.440(5) A) and the first Ga-containing representative. The crystal structures of MAX-phases are intergrowths of layers of an intermetallic MGa in a hexagonal stacking sequence with carbidic layers (MC){sub n} of the NaCl type. The thickness of the layer depends from the value of n. The results of the structure refinements also demonstrate that also the structural details follow this description. - Graphical abstract: Single crystals of Ga-containing MAX-Phases (TiC){sub n}(TiGa) (n=1, 3) were grown from a metallic melt including and characterised by X-ray diffraction. Ti{sub 4}GaC{sub 3} is one of the few 413-phase and the first containing Ga.

36 MATERIALS SCIENCE↗

New insight into the helium-induced damage in MAX phase Ti{sub 3}AlC{sub 2} by first-principles studies

In the present work, the behavior of He in the MAX phase Ti{sub 3}AlC{sub 2} material is investigated using first-principle methods. It is found that, according to the predicted formation energies, a single He atom favors residing near the Al plane in Ti{sub 3}AlC{sub 2}. The results also show that Al vacancies are better able to trap He atoms than either Ti or C vacancies. The formation energies for the secondary vacancy defects near an Al vacancy or a C vacancy are strongly influenced by He impurity content. According to the present results, the existence of trapped He atoms in primary Al vacancy can promote secondary vacancy formation and the He bubble trapped by Al vacancies has a higher tendency to grow in the Al plane of Ti{sub 3}AlC{sub 2}. The diffusion of He in Ti{sub 3}AlC{sub 2} is also investigated. The energy barriers are approximately 2.980 eV and 0.294 eV along the c-axis and in the ab plane, respectively, which means that He atoms exhibit faster migration parallel to the Al plane. Hence, the formation of platelet-like bubbles nucleated from the Al vacancies is favored both energetically and kinetically. Our calculations also show that the conventional spherical bubbles may be originated from He atoms trapped by C vacancies. Taken together, these results are able to explain the observed formation of bubbles in various shapes in recent experiments. This study is expected to provide new insight into the behaviors of MAX phases under irradiation from electronic structure level in order to improve the design of MAX phase based materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

An Efficient Electrolytic Preparation of MAX-Phased Ti-Al-C

Large-scale deployment of MAX-phased Ti-Al-C with intriguing mechanical and physicochemical properties is significantly retarded by its harsh preparation conditions, in which costly precursors, high temperature and non-atmospheric pressure are generally imperative. We herein report an efficient electrolytic preparation of MAX-phased Ti-Al-C by direct electro-reduction of solid TiO{sub 2}-Al{sub 2}O{sub 3}-C in molten CaCl{sub 2} at 1223 K under normal pressure. Homogeneous layered Ti{sub 3}AlC{sub 2} with an oxygen content of 4300 ppm is prepared under a voltage of 3 V between the solid cathode and graphite anode for only 4 hours. The electro-reduction of TiO{sub 2}-Al{sub 2}O{sub 3}-C exhibits a much faster speed compared with the electrolysis employing TiO{sub 2}, TiO{sub 2}-C and TiO{sub 2}-Al{sub 2}O{sub 3} as the precursors. Time-dependent electrolysis indicates that TiC{sub x}O{sub y} is the main intermediate. The generation of refractory and highly conducting TiC{sub x}O{sub y} intermediate enhances the reduction. Density functional theory simulations show a weak affinity towards oxygen of the resulting Ti{sub 3}AlC{sub 2}, which is beneficial to fast and thorough deoxidation. The formation of a layered structure of Ti{sub 3}AlC{sub 2} is attributed to the template effect of the precursory graphite. By simply varying the precursory stoichiometry, layered Ti{sub 2}AlC is also prepared. The present protocol featuring affordable feedstock, low temperature, ambient pressure, high energy efficiency and controllable stoichiometry is promising for large-scale application.

36 MATERIALS SCIENCE↗

The correlation between N deficiency and the mechanical properties of the Ti 2 AlNy MAX phase

The role of X deficiency on the mechanical properties of MAX phases was studied by synthesizing Ti 2 AlN through powder metallurgy in stoichiometric and sub/extra-stoichiometric nitrogen compositions. XRD analyses and ab initio calculations indicate that nitrogen vacancies result in a lattice contraction predominantly along the c-axis. The elastic moduli and intrinsic hardness of substoichiometric Ti 2 AlN 0.9 measured from nanoindentation tests are shown to be slightly smaller than that of Ti 2 AlN. The key mechanical indexes, bulk (B), shear (G) and Young’s (E) moduli as well as the hardness variation are calculated in density functional theory, and show different responses depending on the concentration of N vacancies. Overall, this joint experimental and theoretical study provides a full understanding of the energetics, chemical bonding, electronic structure, and mechanics of the N deficient MAX phases which would increase the application of nitride ceramics.

36 MATERIALS SCIENCE↗

Elemental and layer based analysis of optical properties: A new technique applied to four MAX-phases

Here we present here a novel technique to calculate partial contributions to the optical properties by atoms, elements, and layers. Following the same methodology as the calculation of the partial density of states from the density of states, we have decomposed the optical properties into the partial optical properties. Using this technique the differences of elemental resolved optical properties as well as layer-resolved optical properties are displayed for both the 211 and 312 phases of TiSiC and TiAlC MAX-phase materials.

36 MATERIALS SCIENCE↗

MAX Phases for the Nuclear Industry: Possibilities and Pitfalls

By now it is well-established that the layered, machinable, hexagonal carbides and nitrides, with the general formula, M{sub n+1}AX{sub n}, (MAX) where n = 1 to 3, M is an early transition metal, A is an A-group (mostly groups 13 and 14) element and X is either C and/or N - sometimes referred to as polycrystalline nanolaminates because every basal plane is a potential deformation or delamination plane - combine some of the best attributes of metals and ceramics. Like metals, they are electrically and thermally conductive, most readily machinable (manual hack saw will suffice) not susceptible to thermal shock, plastic at high temperatures, and exceptionally damage tolerant. Like ceramics, some of them are elastically quite rigid, lightweight, and maintain their strengths to high temperatures. The ternaries Ti{sub 3}SiC{sub 2} and Ti{sub 2}AlC are also creep, fatigue and oxidation resistant. The impetus for this work was our conjecture - proven herein - that the presence of the pure A-layers in the MAX phases would result in extraordinary damage tolerance to neutron. After irradiation to 0.14 dpa at 121 deg. C and 735 deg. C, black spots are observed in both ternaries. After irradiation to higher doses, at 735 deg. C, basal dislocation loops, with a Burgers vector of b = 1/2 [0001] are observed in TAC with loop diameters of the order of the order of 25 nm. In TAC larger dislocation loops (75±34 nm) are observed after 3.4 dpa at 735 deg. C, in addition to stacking faults. In sharp contrast to the MAX phases, the TiC impurity particles in the former, form extensive dislocation loops at all conditions. Voids are observed at grain boundaries and within stacking faults after 3.4 dpa irradiation, with extensive void formation in the TiC regions at 1085 deg. C. Most remarkably, defect free, denuded zones, of the order of 1 μm, were observed after irradiation to 3.4 dpa at 735 deg. C. Small grains, 3-5 μm in diameter were totally damage free after irradiation at 1085 deg. C to this dose. When these results are compared to those of TiC, there is little doubt that the A-layers in the MAX phases, provide enhanced neutron irradiation tolerance. Based on these, and other results that will be touched upon, it is reasonable to conclude that Ti{sub 3}SiC{sub 2} is quite a promising candidate for high (> 500 deg. C) temperature nuclear applications. At lower temperatures anisotropic swelling results in microcracking. (authors)

36 MATERIALS SCIENCE↗

Atomically Layered and Ordered Rare-Earth i -MAX Phases: A New Class of Magnetic Quaternary Compounds

In 2017, we discovered quaternary i -MAX phases—atomically layered solids, where M is an early transition metal, A is an A group element, and X is C—with a (M 1 2/3 M 2 1/3 ) 2 AC chemistry, where the M 1 and M 2 atoms are in-plane ordered. Herein, we report the discovery of a class of magnetic i -MAX phases in which bilayers of a quasi-2D magnetic frustrated triangular lattice overlay a Mo honeycomb arrangement and an Al Kagomé lattice. The chemistry of this family is (Mo 2/3 RE 1/3 ) 2 AlC, and the rare-earth, RE, elements are Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Tm, and Lu. Here, the magnetic properties were characterized and found to display a plethora of ground states, resulting from an interplay of competing magnetic interactions in the presence of magnetocrystalline anisotropy.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Experimental and theoretical characterization of ordered MAX phases Mo{sub 2}TiAlC{sub 2} and Mo{sub 2}Ti{sub 2}AlC{sub 3}

Herein, we report on the phase stabilities and crystal structures of two newly discovered ordered, quaternary MAX phases—Mo{sub 2}TiAlC{sub 2} and Mo{sub 2}Ti{sub 2}AlC{sub 3}—synthesized by mixing and heating different elemental powder mixtures of mMo:(3-m)Ti:1.1Al:2C with 1.5 ≤ m ≤ 2.2 and 2Mo: 2Ti:1.1Al:2.7C to 1600 °C for 4 h under Ar flow. In general, for m ≥ 2 an ordered 312 phase, (Mo{sub 2}Ti)AlC{sub 2}, was the majority phase; for m < 2, an ordered 413 phase (Mo{sub 2}Ti{sub 2})AlC{sub 3}, was the major product. The actual chemistries determined from X-ray photoelectron spectroscopy (XPS) are Mo{sub 2}TiAlC{sub 1.7} and Mo{sub 2}Ti{sub 1.9}Al{sub 0.9}C{sub 2.5}, respectively. High resolution scanning transmission microscopy, XPS and Rietveld analysis of powder X-ray diffraction confirmed the general ordered stacking sequence to be Mo-Ti-Mo-Al-Mo-Ti-Mo for Mo{sub 2}TiAlC{sub 2} and Mo-Ti-Ti-Mo-Al-Mo-Ti-Ti-Mo for Mo{sub 2}Ti{sub 2}AlC{sub 3}, with the carbon atoms occupying the octahedral sites between the transition metal layers. Consistent with the experimental results, the theoretical calculations clearly show that M layer ordering is mostly driven by the high penalty paid in energy by having the Mo atoms surrounded by C in a face-centered configuration, i.e., in the center of the M{sub n+1}X{sub n} blocks. At 331 GPa and 367 GPa, respectively, the Young's moduli of the ordered Mo{sub 2}TiAlC{sub 2} and Mo{sub 2}Ti{sub 2}AlC{sub 3} are predicted to be higher than those calculated for their ternary end members. Like most other MAX phases, because of the high density of states at the Fermi level, the resistivity measurement over 300 to 10 K for both phases showed metallic behavior.

36 MATERIALS SCIENCE↗

MAX phase – Alumina composites via exchange reaction in the M{sub n+1}AlC{sub n} systems (M=Ti, V, Cr, Nb, or Ta)

MAX phases have been produced for the first time via an exchange reaction between the M-element oxide and Al leading to an M–Al–C–Al{sub 2}O{sub 3} composite in the V–Al–C, Cr–Al–C, Nb–Al–C and Ta–Al–C systems in addition to the previously known Ti–Al–C system. The reduction reaction was first investigated by forming the binary M–X carbide and then proven to be generic across all M–Al–C systems with the production of the M{sub 2}AlC phase in each case. The work was extended to the other M{sub 3}AlC{sub 2} and M{sub 4}AlC{sub 3} phases in the respective systems, and was successful in 4 of the 5 cases with moderate yield. - Graphical abstract: A range of M{sub n+1}AX{sub n} phases (M-octahedra with X centres and A layers) were synthesised directly from the M oxide via exchange reactions for the 5 M-elements shown. - Highlights: • Ten M{sub n+1}AlC{sub n} phases were produced from M-oxides via a single step exchange reaction. • Eight of these MAX phases had not been produced via this method before. • Al was found to be a suitable reducing agent in all cases. • The process was also discovered to work under SHS and MASHS conditions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crystallographic and TEM Features of a TBC/Ti2AlC MAX Phase Interface after 1300°C Burner Rig Oxidation

A FIB/STEM interfacial study was performed on a TBC/Ti 2 AlC MAX phase system, oxidized in an aggressive burner rig test (Mach 0.3 at 1300 °C for 500 h). The 7YSZ TBC, α-Al 2 O 3 TGO, and MAXthal 211 TM Ti 2 AlC base were variously characterized by TEM/STEM, EDS, SADP, and HRTEM. The YSZ was a mix of “clean” featureless and “faulted” high contrast grains. The latter exhibited ferro-elastic domains of high Y content tetragonal t″ variants. No martensite was observed. The TGO was essentially a duplex α-Al 2 O 3 structure of inner columnar plus outer equiaxed grains. It maintained a perfectly intact, clean interface with the Ti 2 AlC substrate. The Ti 2 AlC substrate exhibited no interfacial Al-depletion zone but, rather, numerous faults along the basal plane of the hexagonal structure. These are believed to offer a means of depleting Al by forming crystallographic, low-Al planar defects, proposed as Ti 2.5 AlC 1.5 . These characterizations support and augment prior optical, SEM, and XRD findings that demonstrated remarkable durability for the YSZ/Ti 2 AlC MAX phase system in aggressive burner tests.

TI2AlC↗

Alumina-Forming MAX Phases in Turbine Material Systems

Coatings for high temperature turbine components are based on low conductivity YSZ thermal barriers and protective NiAl, NiCoCrAlY bond coats. Good oxidation hot corrosion resistance, intermediate CTE, and strain tolerance of Ti2AlC and Cr2AlC MAX phases are thus of special interest. Their alumina scale growth follows a cubic law in accord with FeCrAlY alloys, with oxygen grain boundary diffusivity: Dgb 1.8 x 10-10 exp(-375 kJmole) m3s. Protective cubic kinetics are also found in high pressure burner rig (6 atm., 25 ms) and TGA tests of MAXthal 211Ti2AlC. The initial portion (0.1 hr) is dominated by fast TiO2 growth (with little evidence of scale volatility in high pressure water vapor, as found for SiO2 scales). Bulk Ti2AlC and Cr2AlC substrates show promise as potential bond coats for YSZ TBCs in 1000-1200 C furnace life (500 h) tests. Cr2AlC is proving to be very resistant to 700-900 C Na2SO4 hot corrosion and is of interest for disk alloys. Preliminary diffusion bonded Cr2AlC-superalloy hybrid couples have survived 1000 hr interrupted furnace tests at 800C with no indication of cracking or debonding. Diffusion zones of -NiAl+Cr7C3 were produced in these above 1000 C, but did not grow to any great extent after 1000 hr at 800 C. Processing as coatings presents challenges, however the basic properties of MAX phases provide novel opportunities for high temperature turbine components.

MAX phase↗

MAX phase – Alumina composites via elemental and exchange reactions in the Ti{sub n+1}AC{sub n} systems (A=Al, Si, Ga, Ge, In and Sn)

Extension of the aluminothermal exchange reaction synthesis of M{sub n+1}AX{sub n} phases to systems where the element ‘A’ is not the reducing agent was investigated in systems TiO{sub 2}–A–Al–C for A=Al, Si, Ga, Ge, In and Sn as well as Cr{sub 2}O{sub 3}–Ga–Al–C. MAX phase-Al{sub 2}O{sub 3} composites were made in all systems except those with A=Ga or In. The effectiveness of conversion to MAX phases was generally in the range 63–96% without optimisation of starting ratios. Optimisation in the Ti–Si–C system gave a MAX phase component with >98% Ti{sub 3}SiC{sub 2}. - Graphical abstract: A range of Ti{sub n+1}AX{sub n} phases with different A elements were synthesised directly from the M oxide via exchange reactions. The process has now been shown to be general in all the systems marked in green in the table. - Highlights: • Ti{sub n+1}AC{sub n} phases were produced via a single step exchange reaction. • 3 MAX phase systems were successful via this method for the first time. • Cr{sub 2}GeC was also able to be produced via an exchange reaction. • The interconversion reaction in MAX phases is more general than previously thought.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Oxidation of Alumina-Forming MAX Phases in Turbine Environments

Protective coatings for high temperature turbine components are based on YSZ thermal barriers and oxidation resistant, alumina-forming NiAl or NiCoCrAlY bond coats. Ti2AlC and Cr2AlC MAX phases are thus of special interest because of good oxidation resistance and CTE that can match Al2O3 and YSZ. Their alumina scales grow according to cubic kinetics due to grain growth in the scale, with initial heating dominated by fast TiO2 growth. Protective cubic kinetics are also found in high pressure burner rig tests of MAXthal 211 Ti2AlC, but with reduced rates due to volatile TiO(OH)2 formation in water vapor. YSZ-coatings on bulk Ti2AlC exhibit remarkable durability up to 1300C in furnace tests and at least a 25x life advantage compared to superalloys. At another extreme, Cr2AlC is resistant to low temperature Na2SO4 hot corrosion and exhibits thermal cycling stability bonded to a superalloy disk material. Accordingly, sputtered Cr2AlC coatings on disk specimens prevented hot corrosion detriments on LCF. Breakaway oxidation (Ti2AlC), scale spallation (Cr2AlC), interdiffusion, and processing as coatings still present serious challenges. However the basic properties of MAX phases provide some unusual opportunities for use in high temperature turbines.

ceramics↗