At least 37 records · Page 2

Comparison of Bond in Roll-bonded and Adhesively Bonded Aluminums

Lap-shear and peel test measurements of bond strength have been carried out as part of an investigation of roll bonding of 2024 and 7075 aluminum alloys. Shear strengths of the bonded material in the F temper are in the range of 14 to 16 ksi. Corresponding peel strengths are 120 to 130 lb/inch. These values, which are three to five times those reported in the literature for adhesively bonded 2024 and 7075, are a result of the true metallurgical bond achieved. The effects of heat-treating the bonded material are described and the improvements in bond strength discussed relative to the shear strength of the parent material. The significance of the findings for aerospace applications is discussed.

Schwensfeir, R. J., Jr.↗

Copper-Tantalum Metal Matrix Composites Consolidated from Powder Blends by Severe Plastic Deformation

We investigated the effectiveness of severe plastic deformation by equal channel angular extrusion (ECAE) for consolidation of metal powders into metal matrix composites. Equal volumes of copper (Cu) and tantalum (Ta) powders were consolidated at ambient temperature via different ECAE routes. Composites processed by ECAE routes 4E and 4Bc were also processed at 300 °C. The resulting materials were characterized by scanning electron microscopy (SEM) and compression testing. Processing by route 4Bc at 300 °C resulted in the highest compressive strength, lowest anisotropy, and least strain rate sensitivity. We conclude that the superior properties achieved by this route arise from mechanical bonding due to interlocking Cu and Ta phases as well as enhanced metallurgical bonds from contact of pristine metal surfaces when the material is sheared along orthogonal planes.

36 MATERIALS SCIENCE↗

Al-Ce Alloy-Based Compact Heat Exchanger for Refrigerant Charge Reduction and Unprecedented Durability (CRADA NFE-21-08888 Final Report)

Oak Ridge National Laboratory and Eck Industries produced and characterized durable and corrosion resistant Al-Ce-Mg alloy-based heat exchanger. Eck Industries successfully casted Al-Ce-Mg heat exchanger. ORNL characterized reaction bonding between Al-2Ce-6Mg alloy and stainless-steel tube in a heat exchanger header. Metallurgical bonds were achieved between stainless steel tubes and Al-Ce-Mg alloy cast headers. ORNL performed corrosion testing on Al-Ce-Mg alloy/stainless steel tube reactive bond interface. In most cases no significant changes to the reactive bond morphology or compositional distribution were observed in the samples after exposure to acid for 267h acid.

36 MATERIALS SCIENCE↗

Al-Ce Alloy-Based Compact Heat Exchanger for Refrigerant Charge Reduction and Unprecedented Durability

• Oak Ridge National Laboratory and Eck Industries produced and characterized durable and corrosion resistant Al-Ce-Mg alloy-based heat exchanger. • Eck Industries successfully casted Al-Ce-Mg heat exchanger. • ORNL characterized reaction bonding between Al-2Ce-6Mg alloy and stainless-steel tube in a heat exchanger header. • Metallurgical bonds were achieved between stainless steel tubes and Al-Ce-Mg alloy cast headers. • ORNL performed corrosion testing on Al-Ce-Mg alloy/stainless steel tube reactive bond interface. • In most cases no significant changes to the reactive bond morphology or compositional distribution were observed in the samples after exposure to acid for 267h acid.

36 MATERIALS SCIENCE↗

Temperature dependent interfacial microstructure in HIP-bonded Al6061/Zr joints

Pressing (HIP) at 450 °C and 560 °C under 103 MPa for 90 minutes to evaluate interfacial diffusion and microstructural evolution. Sound metallurgical bonding was achieved at both temperatures, with Zr serving as an effective diffusion barrier. Microstructural analysis revealed the the formation of a (Al,Si)3Zr intermetallic layer at the Al/Zr interface, whose thickness increased from ~100 nm at 450 °C to ~2100 nm at 560 °C, consistent with temperature-driven diffusion kinetics. The thin and continuous reaction layer observed at 450 °C indicates controlled interdiffusion and minimal reaction zone growth, favorable for maintaining interface stability and ductility. At 560 °C, enhanced atomic mobility led to pronounced intermetallic development, confirming diffusion-controlled growth behavior. These results provide valuable insights for optimizing Al/Zr interface design and diffusion barrier performance in advanced structural and energy systems.

Al/Zr interface↗

Explosive bonded TZM-wire-reinforced C129Y columbium composites

Technique consists of positioning layers of TZM metal filaments between thin C129Y columbium sheets and joining multiple sheet stacks by single explosive joining operation. Metallurgical bonds are excellent, external heat is not required, process is relatively inexpensive, and resulting composites are considerably stronger than base alloy.

Reece, O. Y.↗

Fabrication of stainless steel clad tubing

The feasibility of producing stainless steel clad carbon steel tubing by a gas pressure bonding process was evaluated. Such a tube product could provide substantial chromium savings over monolithic stainless tubing in the event of a serious chromium shortage. The process consists of the initial assembly of three component tubesets from conventionally produced tubing, the formation of a strong metallurgical bond between the three components by gas pressure bonding, and conventional cold draw and anneal processing to final size. The quality of the tubes produced was excellent from the standpoint of bond strength, mechanical, and forming properties. The only significant quality problem encountered was carburization of the stainless clad by the carbon steel core which can be overcome by further refinement through at least three different approaches. The estimated cost of clad tubing produced by this process is greater than that for monolithic stainless tubing, but not so high as to make the process impractical as a chromium conservation method.

Kovach, C. W.↗

Fuel Retention Improvement at High Temperatures in Tungsten-Uranium Dioxide Dispersion Fuel Elements by Plasma-Spray Cladding

An investigation was undertaken to determine the feasibility of depositing integrally bonded plasma-sprayed tungsten coatings onto 80-volume-percent tungsten - 20-volume-percent uranium dioxide composites. These composites were face clad with thin tungsten foil to inhibit uranium dioxide loss at elevated temperatures, but loss at the unclad edges was still significant. By preheating the composite substrates to approximately 3700 degrees F in a nitrogen environment, metallurgically bonded tungsten coatings could be obtained directly by plasma spraying. Furthermore, even though these coatings were thin and somewhat porous, they greatly inhibited the loss of uranium dioxide. For example, a specimen that was face clad but had no edge cladding lost 5.8 percent uranium dioxide after 2 hours at 4750 dgrees F in flowing hydrogen. A similar specimen with plasma-spray-coated edges, however, lost only 0.75 percent uranium dioxide under the same testing conditions.

Grisaffe, Salvatore J.↗

Multi-scale characterization and simulation of impact welding between immiscible Mg/steel alloys

Vaporizing foil actuator spot welding method is used in this paper to join magnesium alloy AZ31 and uncoated high-strength steel DP590, which are typically considered as un-weldable due to their high physical property disparities, low mutual solubility, and the lack of any intermetallic phases. Characterization results from scanning electron microscopy (SEM) and high-resolution transmission electron microscopy (HRTEM) of the weld interface indicate that the impact creates an Mg nanocrystalline interlayer with abundant Fe particles. The interlayer exhibits intact bonding with both DP590 and AZ31 substrates. To investigate the fundamental bond formation mechanisms at the interface, a finite element (FE)-based process simulation is first performed to calculate the local temperature and deformation at the interface under the given macroscopic experimental condition. Finally, taking the FE results at the interface as inputs, molecular dynamics (MD) simulations are conducted to study the interlayer formation at the Mg/Fe interface during the impact and cooling. The results found a high velocity shearing-induced mechanical mixing mechanism that mixes Mg/Fe atoms at the interface and creates the interlayer, leading to the metallurgical bond between Mg/steel alloys.

36 MATERIALS SCIENCE↗

Aluminum/SmCo 5 composites for structural and magnetic applications

Metal-bonded magnetic composites (MBMCs) present a promising alternative to dense sintered magnets, particularly for intricate components. Compared to polymer-based bonded magnets, MBMCs have wider applicability in harsh environments. In this paper, we demonstrate a solid-state shear-based manufacturing technique to introduce localized magnetization into a paramagnetic aluminum matrix by embedding SmCo5 permanent magnet particles. Our magnetic composites display hard magnetic behavior with a coercivity of 13 kOe and a remanent magnetization of 4.32 emu/g. In addition to magnetization, we also report a 9% improvement in Young’s modulus. Despite the local temperature rise during processing, the magnetic phases didn’t decompose into unwanted phases, preserving the composite's hard magnetic properties. Creation of an interfacial metallurgical bond with the matrix ensured the suitability of the composites for structural applications. Our study investigates the mechanical, and functional properties of composites, paving the way for lightweight structural magnetic composites with a transformative potential in the aerospace, nuclear, and automotive applications. This work underscores the potential for further optimization and development to drive innovations in magnet and equipment design.

36 MATERIALS SCIENCE↗

Co-extrusion of dissimilar Al alloys via shear assisted processing and extrusion

Cladded tubes are generally used where two distinct properties are required at the outer and inner part of a tube, for instance, strength and corrosion resistance. In this investigation, shear assisted processing and extrusion (ShAPE) was employed to fabricate bi-metallic tubes from 1100 and 7075, and 1100 and 2024 dissimilar Al alloy combinations. Surface defect-free bi-metallic tubes were fabricated via the ShAPE process. Detailed microstructural characterization of the interface and various locations of the cladded tubes were carried out using light and scanning electron microscopy techniques. A defect-free, metallurgically bonded interface between the cladded layer and high strength Al (7075 and 2024 Al) was observed. Furthermore, hardness and tensile properties of the cladded ShAPE tubes were examined in the as-extruded conditions.

Komarasamy, Mageshwari↗

A non-melting additive approach to structural repair of aluminum aircraft fastener holes

The damage to fastener holes in aerospace aluminum structures presents significant challenges for aircraft durability, and conventional bushing methods for repairing oversized holes often fall short due to the lack of metallurgical bonding and limited edge distance availability. This study investigates additive friction stir deposition, a non-melting additive process, as a viable alternative for the structural repair of aerospace fastener holes. The repair process, demonstrated on AA7050 (Al-Zn-Mg-Cu-Zr) hole structures, involves filling oversized holes with new material and machining to restore the original hole size. The repaired hole coupons are defect-free and exhibit good fatigue performance under fully reversed tension-compression loading (R = -1). At a nominal stress amplitude of 123.5 MPa, the average number of cycles to failure is 12,666 for unrepaired baseline coupons and 17,372 for effectively repaired coupons. Restoring complex geometries without compromising fatigue performance has been difficult in aerospace applications; this study marks the first demonstration of additive repair that consistently outperforms the unrepaired baseline coupons. Notably, the result is achieved through a low-energy, cost-effective solution without the need for post-repair heat treatment. Except for a few outliers, the post-repair fatigue performance generally remains inferior to that of undamaged, pristine coupons, likely due to precipitate evolution in AA7050 caused by the thermomechanical processing nature of additive friction stir deposition. This evolution weakens the repair region and the adjacent base material, leading to faster crack initiation and growth compared to the properly aged base material, AA7050-T7451.

36 MATERIALS SCIENCE↗

Friction-based riveting technique for AZ31 magnesium alloy

Rivet materials used in the aerospace and automotive industries are typically alloys of aluminum (Al) or steel. Magnesium (Mg) is an attractive alternative because it is 33% and 75% lighter than Al and steel, respectively. However, a primary barrier for using Mg as rivet material is its poor formability at room temperature, resulting in brittle fracture of the rivet head during cold riveting. Hot riveting is possible but suffers from high cycle time due to the need for pre-heating. A new friction-based riveting technique, Rotating Hammer Riveting (RHR), is reported to fully form AZ31 Mg rivet heads in a mere 0.23 seconds cycle time. Heat and pressure generated through severe plastic deformation during the process was sufficient to form the Mg rivet head without the need for a separate pre-heating operation. Due to dynamic recrystallization, AZ31 Mg grains in the rivet head were significantly refined from about 15 to 2.6 µm during RHR, which favors the formability of Mg rivet by triggering grain boundary sliding and reducing plastic anisotropy of Mg. In addition, RHR joints showed a metallurgical bond between the rivet head and top sheet, which eliminates a significant pathway for corrosion.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of ultrasonic spot welding of AA7075-T6 and A380 casting aluminum alloy

Ultrasonic spot welding (USW) was employed to join AA7075-T6 and casting Al alloy A380. Under a constant welding power, the influence of the welding time duration (from 1 s to 3 s) on peak temperature, microstructure, hardness, and mechanical strength of the joints were studied. It was found that the peak temperature increased with welding time. A sound solid-state metallurgical bonding was obtained at the joint interface. The cracks occurred at the edge of the joints were eventually eliminated as the welding time increased. A layer of refined grains formed in A380 adjacent to the bonding line. Further, hardness reduction occurred in AA7075 at the joint interface and the degree of hardness reduction and the volume increased with the peak temperature. By increasing welding time, lap shear tensile tests show that the peak load increased from 5.3 kN to 6.55 kN. The corresponding interfacial shear strength ranged from 96.29 MPa to 99.72 MPa, lower than the shear strength of both base materials (331 MPa for AA7075 and 185 MPa for A380). All joint samples exhibited interfacial fracture after lap shear tensile testing, with a thin layer of A380 remnant attached to AA7075 at the center of the fractured surface.

36 MATERIALS SCIENCE↗

Numerical Simulation and Experimental Validation of Joint Performance in Aluminum-Steel Lap Welds Formed by Friction Stir Dovetailing

Friction stir dovetailing (FSD) is a new dissimilar material joining process that simultaneously forms a mechanical interlock and metallurgical bond at the dissimilar material interface. This work presents development of a modeling and simulation approach to predict mechanical performance of FSD thick section aluminum to steel joints. A finite element analysis (FEA) was carried out in order to predict the load-carrying capacity and failure location for aluminum thicknesses between 12.7 mm and 50.8 mm with different numbers of dovetails. The numerical results and corresponding experimental investigation are in agreement and suggest that the developed methods can be used effectively for design and analysis of FSD joints using standard FEA tools.

Friction stir dovetailing, Friction stir welding, ↗

Feasibility of Lead Fast Reactor Heat Exchanger Tube Online Monitoring

Within virtually all reactor systems with heat exchangers, the thinnest barriers between primary and secondary fluids are the heat exchanger tubes. Consistent with light water reactor experience, the advanced reactor heat exchangers are the most susceptible regions for corrosion and leakage (NRC, 2019). Moreover, traditional inspections and repairs using robotics will be expensive or impractical. On-line structural health corrosion monitoring (OLSHM) is therefore desirable to detect tube degradation prior to leaks that may allow mixing of heat exchanger fluids. Rhetorically many molten salt reactor (MSR) designers plan for on-line monitoring of critical reactor components including heat exchangers but there are no proven OLSHM sensors or systems for MSR heat exchangers. Guided wave ultrasound from the tube-end or ID using conventional low-temperature piezoelectric sensors has been shown to be sensitive to pits and cracks less than 50% through-wall in long pipes and tubes (Narayanan M.M., 2019) . Mode and frequency selection are important for practical sensor design decisions and ultimate performance. The L-0 wave-mode is easily excited by L-mode transducers but they have surface normal wave motion that will be sensitive to and more attenuative because of fluid interaction with the tube surface (Rose J.L., 1994). Shear Horizontal (SH) wave modes have material motion parallel to the tube surface therefore are virtually unaffected by fluid interaction. For SH-0 to be nondispersive in steel, the frequency-thickness product (MHz-mm) must be less than approximately 1.5. SH mode transducers must be coupled by a material that can support shear stress; a thin layer of honey works well for temporary sensors and an adhesive or a brazed metallurgical bond for permanent sensors. If sensors are incorporated into the fabrication process, the same kinds of SH-0 waves can be generated from the stagnant flow area of the tube OD without compromising the heat-exchange tube function. Piezoelectric materials are also available that can withstand harsh temperatures of molten salt heat exchangers (Stevenson T., 2015) (Machura et al., 2008). Though they may not have as high-performance characteristics, their performance only needs to be good enough to detect flaws of interest. This project attempts to demonstrate feasibility to develop a sensor that can be sensitive to flaws of interest and perform long-term monitoring of a molten salt reactor heat exchanger. Benefits to the advanced reactor system include: • Minimizing the expense of a reactor shut down for periodic inspection—only shutdown for cause. • Reduce risk of unexpected tube rupture by detecting flaws before they grow to through-wall leaks. • Cost reduction by minimizing need to design for manual/robotic inspectability. Transducer design, characterization of the beam profile, wedges vs. direct application of piezoelectric sensors, and ultrasonic pulse-echo responses from a representative heat exchange tube with fabricated flaw types are discussed.

On-Line Tube Monitor, Guided Wave Ultrasound, SH-0↗

Progress Toward Molten Salt Reactor Heat Exchanger On-Line Monitoring

Within virtually all reactor systems with heat exchangers, the thinnest barriers between primary and secondary fluids are the heat exchanger tubes. Consistent with light water reactor experience, the advanced reactor heat exchangers are the most susceptible regions for corrosion and leakage (NRC, 2019). Moreover, traditional inspections and repairs using robotics will be expensive or impractical. On-line structural health corrosion monitoring (OLSHM) is therefore desirable to detect tube degradation prior to leaks that may allow mixing of heat exchanger fluids. Rhetorically many molten salt reactor (MSR) designers plan for on-line monitoring of critical reactor components including heat exchangers but there are no proven OLSHM sensors or systems for MSR heat exchangers. Guided wave ultrasound from the tube-end or ID using conventional low-temperature piezoelectric sensors has been shown to be sensitive to pits and cracks less than 50% through-wall in long pipes and tubes (Narayanan M.M., 2019) . Mode and frequency selection are important for practical sensor design decisions and ultimate performance. The L-0 wave-mode is easily excited by L-mode transducers but they have surface normal wave motion that will be sensitive to and more attenuative because of fluid interaction with the tube surface (Rose J.L., 1994). Shear Horizontal (SH) wave modes have material motion parallel to the tube surface therefore are virtually unaffected by fluid interaction. For SH-0 to be nondispersive in steel, the frequency-thickness product (MHz-mm) must be less than approximately 1.5. SH mode transducers must be coupled by a material that can support shear stress; a thin layer of honey works well for temporary sensors and an adhesive or a brazed metallurgical bond for permanent sensors. If sensors are incorporated into the fabrication process, the same kinds of SH-0 waves can be generated from the stagnant flow area of the tube OD without compromising the heat-exchange tube function. Piezoelectric materials are also available that can withstand harsh temperatures of molten salt heat exchangers (Stevenson T., 2015) (Machura et al., 2008). Though they may not have as high-performance characteristics, their performance only needs to be good enough to detect flaws of interest. This project attempts to demonstrate feasibility to develop a sensor that can be sensitive to flaws of interest and perform long-term monitoring of a molten salt reactor heat exchanger. Benefits to the advanced reactor system include: • Minimizing the expense of a reactor shut down for periodic inspection—only shutdown for cause. • Reduce risk of unexpected tube rupture by detecting flaws before they grow to through-wall leaks. • Cost reduction by minimizing need to design for manual/robotic inspectability. Transducer design, characterization of the beam profile, and ultrasonic pulse-echo responses from a representative heat exchange tube with fabricated flaw types are discussed.

On-Line Tube Monitor, Guided Wave Ultrasound, SH-0↗

Evaluation of tantalum 316 stainless steel transition joints

Tubular transition joints providing a metallurgically bonded connection between tantalum and 316 stainless steel pipe sections were comparatively evaluated for durability under thermal cycling conditions approximating the operation of a SNAP-8 mercury boiler. Both coextruded and vacuum brazed transition joints of 50mm (2 inch) diameter were tested by thermal cycling 100 times between 730 C and 120 C(1350 F and 250 F) in a high vacuum environment. The twelve evaluated transition joints survived the full test sequence without developing leaks, although liquid penetrant bond line indications eventually developed in all specimens. The brazed transition joints exhibited the best dimensional stability and bond line durability.

Stoner, D. R.↗