Microwave Absorbing Perovskite Catalysts for Efficient Electrification of Syngas Production from CO2 and Methane

Microwave absorbing catalysts have the potential to make thermal reactions such as methane reforming (CH4 + CO2 + H2O → H2 + CO) into carbon negative processes when coupled with decarbonized electricity. Due to microwaves directly heating the catalyst rather than heating the reactor and gases, even high temperature reactions such as dry reforming methane (DRM, CH4 + CO2 → H2 + CO) can be achieved rapidly, efficiently, and on-demand, ideal for coupling with intermittent renewable electricity. However, microwave catalysts present unique design challenges due to the same material needing to both efficiently absorb microwaves in oxidative and reductive reaction conditions and be an efficient and stable catalyst in inherently non-isothermal reactors. We screened from over 28 catalysts in the La0.8Sr0.2(Co-Ni-Mn)O3 perovskite solid-solution family to determine promising microwave reforming catalysts and identify design principles for effective materials. The best performing catalyst candidate was able to produce syngas ratios (H2:CO) from 1-3, and scale up testing showed CO and H2 production efficiencies rivaling conventional carbon intensive steam reforming efficiencies at the liters per minute level of production.

Marin, Christopher↗

Low temperature dry reforming of methane using Ru-Ni-Mg/ceria-zirconia catalysts: Effect of Ru loading and reduction temperature

Dry reforming catalysts, especially those with activity at moderate temperatures, have been intensely investigated to enhance the conversion of biogas. Here, Ru is evaluated as a promoter for Ni-Mg based catalysts. Catalysts based on 1.4 wt%Ni-1.0 wt%Mg-Ce 0.6 Zr 0.4 O 2 with Ru (0.02–0.32 wt%) were prepared using incipient wetness. The reducibility of the catalysts and conversions increased with increasing Ru content. Increases in conversions with increasing Ru loading was attributed to the additional active sites and synergistic effect between Ru and Ni, which weakened Ni-Mg interactions. Samples showed dry reforming activity at low temperatures (450–510 °C). Reaction rates and activation energies of higher loading Ru samples (1.4 wt%Ni-1.0 wt%Mg/Ce 0.6 Zr 0.4 O 2 with 0.16 and 0.32 wt%Ru) decreased when the reduction temperature was raised from 300 to 400 °C. A 20 h TOS study showed stable catalytic activity with minimal coke deposition. Furthermore, the results suggest that Ru is an alternative to Pt in promoting low temperature dry reforming of methane.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structurally Regenerable High Entropy Aluminate Spinel Catalysts for Dry Reforming of Methane

The dry reforming of methane reaction is a promising means to convert two potent greenhouse gases, methane and carbon dioxide, into industrially valuable synthesis gas. However, the presence of reducing gases and high operating temperatures degrade conventional nickel catalysts via excessive coke formation and particle sintering. These catalysts are not readily regenerated because the oxidative heat treatments employed to remove coke further promote active particle sintering. In this work, we designed high entropy aluminate spinel oxides (MAl 2 O 4 where M = Co, Mg, Ni, and divalent site vacancies in nominal equimolar concentration) as selective and regenerable reforming catalysts. Under reaction conditions, reducible nickel and cobalt cations exsolved from the spinel lattice to form highly selective bimetallic particles on the oxide surface. Instead of sintering, these particles uniquely redissolved back into the aluminate lattice upon reoxidation and regained the original spinel structure. This phenomenon is ascribed to entropic stabilization, wherein an increase in configurational entropy creates a thermodynamic driving force for redispersing supported metal particles back into the multi‐cationic oxide structure. During the dry reforming reaction, nickel atoms similarly exsolved from a NiAl 2 O 4 sample and reduced to form metallic nickel particles. However, subsequent oxidation of this sample promoted sintering and oxidation of the nickel particles to an inactive state. High entropy materials thus provide a unique mechanism of regeneration, which is inaccessible in conventional catalysts.

coke deposition↗

Confined Ni-In intermetallic alloy nanocatalyst with excellent coking resistance for methane dry reforming

Carbon dioxide and methane are two main greenhouse gases which are contributed to serious global warming. Fortunately, dry reforming of methane (DRM), a very important reaction developed decades ago, can convert these two major greenhouse gases into value-added syngas or hydrogen. The main problem retarding its industrialization is the seriously coking formation upon the nickel-based catalysts. Herein, a series of confined indium-nickel (In-Ni) intermetallic alloy nanocatalysts (In x Ni@SiO 2 ) have been prepared and displayed superior coking resistance for DRM reaction. The sample containing 0.5 wt.% of In loading (In 0.5 Ni@SiO 2 ) shows the best balance of carbon deposition resistance and DRM reactivity even after 430 h long term stability test. The boosted carbon resistance can be ascribed to the confinement of core–shell structure and to the transfer of electrons from Indium to Nickel in In-Ni intermetallic alloys due to the smaller electronegativity of In. Additionally, both the silica shell and the increase of electron cloud density on metallic Ni can weaken the ability of Ni to activate C–H bond and decrease the deep cracking process of methane. The reaction over the confined InNi intermetallic alloy nanocatalyst was conformed to the Langmuir-Hinshelwood (L-H) mechanism revealed by in situ diffuse reflectance infrared Fourier transform spectroscopy (in-situ DRIFTS). This work provides a guidance to design high performance coking resistance catalysts for methane dry reforming to efficiently utilize these two main greenhouse gases.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Stable Catalysts for Combined Dry and Steam Reforming of Methane and Carbon Dioxide

The specific aim of this project is to develop a comprehensive understanding of cheaper and more stable methane and carbon dioxide reforming catalysts with an optimal introduction of steam to reduce carbon deposits that typically prevent the catalytic systems from transferring to commercial implementation. The work was proposed as a two-year project with the end goal of to show a reliable catalyst system run for at least 400 hours at temperatures less than 800 °C with less than 5% loss of activity of the catalyst and a carbon monoxide to hydrogen product ratio of at least 1:1. The project went for one-year and met the end of year milestone by developing two strategies (use of a cerium co-catalyst and introducing 5% water) that reduced the carbon deposition rates by at least 20% relative to the baseline 10% NiMgAlO methane reforming of CO 2 at < 800 °C in order to shown technical feasibility of the concept.

36 MATERIALS SCIENCE↗

Catalytic reforming of methane with H 2 S via dynamically stabilized sulfur on transition metal oxides and sulfides

Reforming of methane with H 2 S is a promising path to directly utilize sour natural gas reserves, although some aspects of the mechanism and structure–function relations remain elusive. In this report we show that metal oxides of group 4–6 elements, which are inert for steam and dry methane reforming reactions, are active and stable (pre)catalysts for the H 2 S reforming of methane. The key active sites are sulfur species (S*) that are dynamically bound to metal cations during catalysis. Similar H/D isotope exchange patterns and universal rate inhibition by H 2 on representative catalysts indicate that H 2 S decomposition and recombination of surface hydrogen atoms are quasi-equilibrated, whereas CH 4 dissociation steps are reversible, yet not quasi-equilibrated. An in-depth analysis of the kinetic data and isotopic substitution effects identifies S*-mediated C–H bond cleavage as the most plausible rate-limiting step common for all catalysts, with subtle yet essential differences between 3d and 4d/5d catalysts in the thermodynamic stability of S*.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

AUTOIGNITION DELAY TIMES FOR REFORMATE GAS MIXTURES FROM METHANE GAS ENGINES

Methane slip is a prominent issue in natural gas reciprocating engines that are used in transportation and marine applications. The incomplete combustion that results in methane slip can be resolved with the introduction of hydrogen within the combustion mixture to improve methane oxidation and further enable combustion within the engine crevices where methane has previously remained unreacted. Steam methane reforming (SMR) is a common method used to produce hydrogen and can be used to design an onboard device to reduce methane slip from reciprocating engines. The development of this reformer device requires the validation of high-fidelity chemical kinetic models at the low temperatures of the crevice volumes of these engines. In this work, auto-ignition data is obtained using a shock tube at lean (φ—0.714 or λ—1.4) and stoichiometric (φ, λ = 1) equivalence ratios spanning a temperature range of 1042–1234 K at the 80-bar operating pressure of the test engine. Blends of methane, hydrogen, and reformate products from the SMR reaction are shock-heated in synthetic air, with the ignition delay time measured using an OH* chemiluminescence detector at 310 nm and a CH* detector at 430 nm. The experimental results are compared to several state-of-the-art chemical kinetic mechanisms from the literature. In general, most of the mechanisms show very good agreement with experiments at higher temperatures, with simulation results showing little deviation from experiments at lower temperatures. A sensitivity analysis was conducted, and the results reveal that the reaction H2 + CH3O2 = H + CH3O2H has a very significant role in determining low-temperature ignition delay times (IDTs) of SMR mixtures. These findings provide valuable insights into the chemical kinetics governing methane reformate combustion and contribute to the optimization of onboard reformer designs aimed at mitigating methane slip in natural gas-fueled engines.

Fraze, Matthew↗

Utilizing bimetallic catalysts to mitigate coke formation in dry reforming of methane

We report dry reforming of methane (DRM) involves the conversion of carbon dioxide (CO 2 ) and methane (CH 4 ) into syngas (a mixture of hydrogen, H 2 , and carbon monoxide, CO), which can then be used to produce a wide range of products by means of Fischer-Tropsch synthesis. DRM has gained much attention as a means of mitigating damage from anthropogenic greenhouse gas (GHGs) emissions to the environment and instead utilizing these gases as precursors for value-added chemicals or to synthesize sustainable fuels and chemicals. Carbon deposition or coke formation, a primary cause of catalyst deactivation, has proven to be a major challenge in the development of DRM catalysts. The use of nickel- and cobalt-based catalysts has been extensively explored for DRM for their high activity and low cost but suffer from poor stability due to coke formation that has hindered their commercialization. Numerous articles have reviewed the various aspects of catalyst deactivation and strategies for mitigation, but few has focused on the benefit of bimetallic catalysts for mitigating coke formation. Bimetallic catalysts, often improve the catalytic stability over their monometallic counterparts due to synergistic effects resulting from two metal-to-metal interactions. This review will cover DRM literature for various bimetallic catalyst systems, including the effect of supports and promoters, on the mitigation of carbonaceous deactivation

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Steering the Methane Dry Reforming Reactivity of Ni/La 2 O 3 Catalysts by Controlled In Situ Decomposition of Doped La 2 NiO 4 Precursor Structures

The influence of A- and/or B-site doping of Ruddlesden-Popper perovskite materials on the crystal structure, stability, and dry reforming of methane (DRM) reactivity of specific A 2 BO 4 phases (A = La, Ba; B = Cu, Ni) has been evaluated by a combination of catalytic experiments, in situ X-ray diffraction, X-ray absorption spectroscopy (XAS), X-ray photoelectron spectroscopy (XPS), and aberration-corrected electron microscopy. At room temperature, B-site doping of La 2 NiO 4 with Cu stabilizes the orthorhombic structure ( Fmmm ) of the perovskite, while A-site doping with Ba yields a tetragonal space group ( I 4/ mmm ). We observed the orthorhombic-to-tetragonal transformation above 170 °C for La 2 Ni 0.9 Cu 0.1 O 4 and La 2 Ni 0.8 Cu 0.2 O 4 , slightly higher than for undoped La 2 NiO 4 . Loss of oxygen in interstitial sites of the tetragonal structure causes further structure transformations for all samples before decomposition in the temperature range of 400 °C-600 °C. Controlled in situ decomposition of the parent or A/B-site doped perovskite structures in a DRM mixture (CH 4 :CO 2 = 1:1) in all cases yields an active phase consisting of exsolved nanocrystalline metallic Ni particles in contact with hexagonal La 2 O 3 and a mixture of (oxy)carbonate phases (hexagonal and monoclinic La 2 O 2 CO 3 , BaCO 3 ). Differences in the catalytic activity evolve because of (i) the in situ formation of Ni-Cu alloy phases (in a composition of >7:1 = Ni:Cu) for La 2 Ni 0.9 Cu 0.1 O 4 , La 2 Ni 0.8 Cu 0.2 O 4 , and La 1.8 Ba 0.2 Ni 0.9 Cu 0.1 O 4 , (ii) the resulting Ni particle size and amount of exsolved Ni, and (iii) the inherently different reactivity of the present (oxy)carbonate species. Based on the onset temperature of catalytic DRM activity, the latter decreases in the order of La 2 Ni 0.9 Cu 0.1 O 4 ~ La 2 Ni 0.8 Cu 0.2 O 4 ≥ La 1.8 Ba 0.2 Ni 0.9 Cu 0.1 O 4 > La 2 NiO 4 > La 1.8 Ba 0.2 NiO 4 . Simple A-site doped La 1.8 Ba 0.2 NiO 4 is essentially DRM inactive. The Ni particle size can be efficiently influenced by introducing Ba into the A site of the respective Ruddlesden-Popper structures, allowing us to control the Ni particle size between 10 nm and 30 nm both for simple B-site and A-site doped structures. Hence, it is possible to steer both the extent of the metal-oxide-(oxy)carbonate interface and its chemical composition and reactivity. Counteracting the limitation of the larger Ni particle size, the activity can, however, be improved by additional Cu-doping on the B-site, enhancing the carbon reactivity. Exemplified for the La 2 NiO 4 based systems, we show how the delicate antagonistic balance of doping with Cu (rendering the La 2 NiO 4 structure less stable and suppressing coking by efficiently removing surface carbon) and Ba (rendering the La 2 NiO 4 structure more stable and forming unreactive surface or interfacial carbonates) can be used to tailor prospective DRM-active catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Elucidating the role of earth alkaline doping in perovskite-based methane dry reforming catalysts

To elucidate the role of earth alkaline doping in perovskite-based dry reforming of methane (DRM) catalysts, we embarked on a comparative and exemplary study of a Ni-based Sm perovskite with and without Sr doping. While the Sr-doped material appears as a structure-pure Sm 1.5 Sr 0.5 NiO 4 Ruddlesden Popper structure, the undoped material is a NiO/monoclinic Sm 2 O 3 composite. Hydrogen pre-reduction or direct activation in the DRM mixture in all cases yields either active Ni/Sm 2 O 3 or Ni/Sm 2 O 3 /SrCO 3 materials, with albeit different short-term stability and deactivation behavior. The much smaller Ni particle size after hydrogen reduction of Sm 1.5 Sr 0.5 NiO 4 , and of generally all undoped materials stabilizes the short and long-term DRM activity. Carbon dioxide reactivity manifests itself in the direct formation of SrCO 3 in the case of Sm 1.5 Sr 0.5 NiO 4 , which is dominant at high temperatures. For Sm 1.5 Sr 0.5 NiO 4 , the CO : H 2 ratio exceeds 1 at these temperatures, which is attributed to faster direct carbon dioxide conversion to SrCO 3 without catalytic DRM reactivity. As no Sm 2 O 2 CO 3 surface or bulk phase as a result of carbon dioxide activation was observed for any material – in contrast to La 2 O 2 CO 3 – we suggest that oxy-carbonate formation plays only a minor role for DRM reactivity. Rather, we identify surface graphitic carbon as the potentially reactive intermediate. Graphitic carbon has already been shown as a crucial reaction intermediate in metal-oxide DRM catalysts and appears both for Sm 1.5 Sr 0.5 NiO 4 and NiO/monoclinic Sm 2 O 3 after reaction as crystalline structure. It is significantly more pronounced for the latter due to the higher amount of oxygen-deficient monoclinic Sm 2 O 3 facilitating carbon dioxide activation. Despite the often reported beneficial role of earth alkaline dopants in DRM catalysis, we show that the situation is more complex. In our studies, the detrimental role of earth alkaline doping manifests itself in the exclusive formation of the sole stable carbonated species and a general destabilization of the Ni/monoclinic Sm 2 O 3 interface by favoring Ni particle sintering.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Enhanced activity and stability of MgO-promoted Ni/Al 2 O 3 catalyst for dry reforming of methane: Role of MgO

Highly dispersed nickel nanoparticles (NPs) were deposited on Al 2 O 3 NPs by atomic layer deposition (ALD). Various amounts of MgO were loaded on Ni/Al 2 O 3 catalysts by the incipient wetness (IW) method for dry reforming of methane. Fresh and used catalysts were systematically characterized to reveal the effects of MgO on the catalytic performance. MgO was found to increase the basic amount and basic strength of catalyst surfaces, which provided additional surface oxygen species and assisted the adsorption and activation of CO 2 . Although the formation of NiO-MgO solid solution, during the calcination of incipient wetness, did not improve the overall reducibility, the Ni NPs from NiO-MgO solid solution after reduction formed an intimate interaction with MgO, which could inhibit Ni NPs from sintering and provide sufficient metal-support interface for CO 2 activation. The MgO-promoted Ni/Al 2 O 3 reached a methane reforming rate of 1780 L CH4 g Ni -1 h -1 at 850 °C, which is 26% more than that of the pristine Ni/Al 2 O 3 . Finally, the higher CO 2 activity enhanced the oxidation rate of the surface carbon generated from side-reactions, thereby resulting in a higher reforming rate and inhibiting coke formation, especially the detrimental graphitic encapsulating carbon on the active nickel surface.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Reforming of methane with carbon dioxide over cerium oxide promoted nickel nanoparticles deposited on 4-channel hollow fibers by atomic layer deposition

Ni nanoparticles were deposited on four-channel structured α-Al2O3 hollow fibers by atomic layer deposition (ALD). CeO 2 was loaded by a liquid phase incipient wetness method to promote Ni catalysts for dry reforming of methane. For Ni/Al 2 O 3 prepared by ALD, inactive NiAl2O4 that originated from the Ni ALD process was incompletely reduced. The introduced CeO 2 was found to weaken the NiO–Al 2 O 3 interaction, free NiO from NiO–Al 2 O 3 or NiAl 2 O 4 , and improve the reducibility of NiO. The higher reducibility of NiAl 2 O 4 , tuned by CeO 2 , further activated the catalyst during DRM, because a larger proportion of NiAl 2 O 4 was gradually reduced to metallic nickel by the reaction products. The optimal catalytic performance reached a methane reforming rate of 2410 L h -1 gNi -1 at 850 °C. The CeO 2 promoted catalyst also exhibited an excellent performance after regeneration. In addition, the inhibition effect of CeO 2 on coke formation was observed, due to the enhanced CO 2 dissociative adsorption by CeO 2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Field-assisted suppression of coke in the methane steam reforming reaction

Electric fields were applied to an unsupported nickel catalyst during methane steam reforming with a low steam-to-methane ratio of 2:1. As expected, catalysts operated in standard mode (without an applied field) experienced high levels of coking. Coke formation was almost completely suppressed by the application of a positive electric field. This is explained using density functional theory computations which indicate that positive electric fields (1) increase the affinity for water adsorption on the surface, thereby increasing the amount of oxygen available to remove carbon, (2) stabilize individual carbon fragments, thus reducing their tendency to polymerize, and (3) increase the oxygen storage capabilities of the catalyst by inducing sub-surface oxygen formation and bulk oxidation.

Gray, Jake T.↗