F and N Rich Solid Electrolyte for Stable All-Solid-State Battery

We report the instability of sulfide solid electrolytes to Li anode and high-voltage LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes limits the cyclic performance of all-solid-state lithium battery (ASSLB). Herein, the stability of Li 6 PS 5 Cl against Li anode is enhanced by mixing a small amount (0.32 wt%) of CuF 2 -LiNO 3 (CL) into Li 6 PS 5 Cl electrolyte layer to in-situ form a mixed-conductive-lithiophobic and self-healing LiF-Li 3 N-Cu solid electrolyte interphase (SEI) at Li 6 PS 5 Cl-CL/Li interface. The critical current density (CCD) of Li 6 PS 5 Cl-CuF 2 -LiNO 3 increases to 1.4 mA cm –2 /1.4 mAh cm –2 at room temperature, which is much higher than that of pristine Li 6 PS 5 Cl (0.4 mA cm –2 /0.4 mAh cm –2 ) even though mixing 0.32 wt% CL into Li 6 PS 5 Cl slightly reduces the ionic conductivity from 2.9 × 10 –3 to 1.5 × 10 –3 S cm –1 . The compatibility of Li 6 PS 5 Cl-CL electrolyte to single-crystalline NMC811 (S-NMC811) is further enhanced by adding a small amount (0.02 wt%) of AlF 3 into Li 6 PS 5 Cl-CL forming Li 6 PS 5 Cl-CuF 2- LiNO 3 -AlF 3 (Li 6 >PS 5 Cl-CLA) as a cathode electrolyte and by doing Cl – on S-NMC811 (Cl@S-NMC811) surface. The Cl@S-NMC811-Li 6 PS 5 Cl-CLA|Li 6 PS 5 Cl-CL|Li cells with areal capacity of 2.55 mAh cm -2 achieve a capacity retention of 69.4% after 100 cycles at 1C (1C = 200 mAh g -1 ). Adding a small amount of SEI and cathode/electrolyte interphase (CEI) former into the sulfide electrolytes with minimal reduction (48.3%) of ionic conductivity is an effective method to enhance the performance of ASSLB.

36 MATERIALS SCIENCE↗

An Oxygen‐Scavenger Sulfide Coating Enabling Long‐Term Stable Nickel‐Rich Cathodes

Oxygen release is a major issue associated with layer-structured metal oxide cathodes in lithium batteries, which can further cause a series of problems, such as irreversible phase transition, microcracking, and electrolyte decomposition. Eventually, these issues jointly result in cell performance degradation and safety hazards. Thus, it is very significant to tackle oxygen release for achieving long-term stable cyclability, but very challenging. Although intensive efforts have been invested to date, there still lacks a feasible solution. In this study, nanoscale ZrS 2 coatings are applied on prefabricated LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes directly via atomic layer deposition (ALD). Very encouragingly, we reveal that this ALD-deposited conformal ZrS 2 nanocoating can serve as an exceptional oxygen scavenger and then convert into a stable sulfate (Zr(SO 4 ) 2 ) coating. Such an in situ conversion is very beneficial and effective for protecting the electrolyte from decomposition. In addition, the resultant Zr(SO 4 ) 2 coating further inhibits undesirable reactions, stabilizes the interface between NMC811 and the electrolyte, suppresses microcracking, mitigates transition metal dissolution, and maintains the structural stability of the NMC811 cathode. Consequently, the ZrS 2 -coated NMC811 cathode has demonstrated extraordinary performance. Thus, this study advances the understanding of interface engineering while paving a new technical pathway for commercializing NMC811 cathodes.

Nickel-rich cathodes↗

To Pave the Way for Large-Scale Electrode Processing of Moisture-Sensitive Ni-Rich Cathodes

High-capacity Ni-rich cathode such as LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) has a great potential to enable high energy lithium-ion batteries (LIBs) for long-range electrical vehicles. However, the utilization of NMC 811 in large-scale application is still challenging. While many published papers on NMC811 focus on materials modification, the moisture sensitivity of NMC811 and its implications in storage and large-scale electrode coating are not well explored, not to mention how to overcome those challenges for industry application. This work discusses the key parameters impacting the rheological properties of NMC811 slurries and their correlations to the properties of dried electrodes. Effective solutions are proposed to address the gelation issue of NMC811 slurry during large-scale coating to hopefully inspire more effective and practical approaches to tackle the grand challenges in electrochemical energy storage.

25 ENERGY STORAGE↗

LiNi0.8Mn0.1Co0.1O2 Thin Films Prepared by Polymer-Assisted Deposition for the Study of Cathode-Electrolyte Interphases in Lithium-Ion Batteries

High-nickel layered oxide cathodes such as LiNi0.8Mn0.1Co0.1O2 (NMC811) are critical for next-generation lithium-ion batteries (LIBs) due to their superior energy density and reduced reliance on cobalt. However, many Ni-rich cathodes suffer from rapid capacity fade and structural instability originating from complex interfacial reactions at the cathode-electrolyte interface. Traditional composite electrodes exhibit degradation mechanisms that are challenging to quantitatively understand due to additives, including binders and carbon black. In this study, we demonstrate a new synthesis approach for binder- and additive-free NMC811 thin films using polymer-assisted deposition (PAD). PAD-NMC811 are model thin-film cathodes for investigating interfacial phenomena that can be obscured in composite cathodes. Structural and chemical characterization by X-ray diffraction, soft X-ray absorption spectroscopy, and atomic force microscopy show that PAD-NMC811 films possess high phase purity, crystallinity, chemical homogeneity, and morphological uniformity. Electrochemical analyses using cyclic voltammetry and galvanostatic cycling revealed electrochemical behavior consistent with that of composite electrodes, along with a moderate capacity fade indicative of cathode-electrolyte interphase (CEI) formation. Our findings illustrate the effectiveness of PAD synthesis of thin films tailored for detailed mechanistic studies, which offer critical insights into CEI evolution and cathode degradation pathways.

25 ENERGY STORAGE↗

Anomalous Thermal Decomposition Behavior of Polycrystalline LiNi 0.8 Mn 0.1 Co 0.1 O 2 in PEO-Based Solid Polymer Electrolyte

we report that replacing liquid electrolytes (LEs) with polymer electrolytes has been considered a promising approach to developing next-generation lithium-ion batteries (LIBs) with high energy density and superior safety. Nevertheless, compared with the extensive research on the electrochemical stability of the cathode/polymer electrolyte interfaces, reports on their thermal behaviors are rare to date. Herein, this work systematically investigates the thermal stability of two typical layered oxide cathodes, LiCoO 2 (LCO) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), with poly(ethylene oxide) (PEO) electrolyte and with carbonate LEs, respectively. It is found that the oxygen release from the cathodes plays a central role in thermal runaway. Replacing the LE with PEO electrolyte can considerably improve the thermal stability of LCO, but surprisingly, deteriorate that of NMC811. The reason is that the surface of single-crystalline LCO particles can be effectively passivated by the PEO electrolyte during heating, but PEO cannot sufficiently passivate all the primary particles of NMC811 owing to insufficient interface wettability of PEO electrolyte within the polycrystalline secondary NMC811 particles. The findings in this work collectively formulate valuable guidance for improving the safety of polymer-electrolyte-based as well as other types of all-solid-state lithium-ion batteries.

25 ENERGY STORAGE↗

Stabilizing high-Ni cathodes with gradient surface Ti-enrichment

High-Ni cathodes are being intensely pursued worldwide for electric vehicles and other energy-dense applications due to their high capacity and low cost. However, structural instabilities during electrochemical cycling and when subjected to thermal treatment have been the major issues hindering their practical deployment. We here report a rational design of coating-integrated-into-synthesis protocol for fabricating surface Ti-enriched LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811#Ti) material. The coating to intermediates is crucial to obtain high structural ordering, both in the bulk and surface of high-Ni cathodes, and the Ti substitute has a unique tri-valence (Ti 3+ ) in a gradient surface distribution. Further, the simulations of projected density of states in the atomistic understanding further certify significantly enhanced stability of lattice oxygen for the NMC811 through such a Ti 3+ -based structure reinforcement. Consequently, the NMC811#Ti cathode delivers a high capacity up to 200mAhg -1 at 0.1 C, along with superior stabilities during air-storage and thermal treatment (up to 297°C at the fully charged state under differential scanning calorimetric measurements). The corresponding NMC811#Ti||graphite full cell exhibits a desired 83.6% capacity retention after 1000 cycles at 0.5 C in a voltage range of 2.8–4.3V. This work demonstrates a delicate surface reinforcement to stabilize high-Ni cathodes for long-life and safe lithium-ion batteries.

36 MATERIALS SCIENCE↗

High-performance LiNi 0.8 Mn 0.1 Co 0.1 O 2 cathode by nanoscale lithium sulfide coating via atomic layer deposition

The commercialization of nickel-rich LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) has been hindered by its continuous loss of practical capacity and reduction in average working voltage. To address these issues, surface modification has been well-recognized as an effective strategy. Different from the coatings reported in literature to date, in this work, we for the first time report a sulfide coating, amorphous Li 2 S via atomic layer deposition (ALD). Here, our study revealed that the conformal nano-Li 2 S coating shows exceptional protection over the NMC811 cathodes, accounting for the dramatically boosted capacity retention from ~11.6% to ~71% and the evidently mitigated voltage reduction from 0.39 to 0.18 V after 500 charge–discharge cycles. In addition, the Li 2 S coating remarkably improved the rate capability of the NMC811 cathode. Our investigation further revealed that all these beneficial effects of the ALD-deposited nano-Li 2 S coating lie in the following aspects: (i) maintain the mechanical integrity of the NMC811 electrode; (ii) stabilize the NMC electrode/electrolyte interface; and (iii) suppress the irreversible phase transition of NMC structure. Particularly, this study also has revealed that the nano-Li 2 S coating has played some unique role not associated with traditional non-sulfide coatings such as oxides. In this regard, we disclosed that the Li 2 S layer has reacted with the released O 2 from the NMC lattices, and thereby has dramatically mitigated electrolyte oxidation and electrode corrosion. Thus, this study is significant and has demonstrated that sulfides may be an important class of coating materials to tackle the issues of NMCs and other layered cathodes in lithium batteries.

36 MATERIALS SCIENCE↗

Substitution-Mediated Calcination of Nickel-Based Cathodes: Decoupling Lithiation and Crystallization

Nickel-based layered cathodes such as LiNiO 2 offer high energy density for lithium-ion batteries, yet improvements in cycling performance and safety are required for practical use–often achieved through manganese and cobalt substitution as in LiNi 0.80 Mn 0.10 Co 0.10 O 2 (NMC811). However, how such substitution impacts calcination, the key process that governs lithiation, structural ordering, crystallization, and ultimately the resulting material properties, remains unclear. Here, in this study, we investigate substitution-mediated calcination dynamics in NMC811 compared to LiNiO 2 using multiscale-correlated in situ spectroscopy and atomistic-to-mesoscale modeling. While both systems progress through the same sequence of intermediates toward the thermodynamically favored layered phase, NMC811 exhibits an earlier onset of layering, concurrent with hydroxide decomposition followed by sluggish crystallization. Modeling reveals that Mn and Co lower the energy barrier for lithium incorporation and ordering but increase the penalty for interlayer gliding, thereby slowing crystal growth at elevated temperatures. This substitution-mediated decoupling of lithiation and crystallization explains the fine-grained microstructure observed in NMC811 versus coarsened particles in LiNiO 2 and establishes a mechanistic framework for predictive microstructure engineering of Ni-based cathodes.

Calcination↗

Electrolyte design for Li-ion batteries under extreme operating conditions

The ideal electrolyte for the widely used LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)||graphite lithium-ion batteries is expected to have the capability of supporting higher voltages (≥4.5 volts), fast charging (≤15 minutes), charging/discharging over a wide temperature range (±60 degrees Celsius) without lithium plating, and non-flammability. No existing electrolyte simultaneously meets all these requirements and electrolyte design is hindered by the absence of an effective guiding principle that addresses the relationships between battery performance, solvation structure and solid-electrolyte-interphase chemistry. Here we report and validate an electrolyte design strategy based on a group of soft solvents that strikes a balance between weak Li+-solvent interactions, sufficient salt dissociation and desired electrochemistry to fulfil all the aforementioned requirements. Remarkably, the 4.5-volt NMC811||graphite coin cells with areal capacities of more than 2.5 milliampere hours per square centimetre retain 75 per cent (54 per cent) of their room-temperature capacity when these cells are charged and discharged at -50 degrees Celsius (-60 degrees Celsius) at a C rate of 0.1C, and the NMC811||graphite pouch cells with lean electrolyte (2.5 grams per ampere hour) achieve stable cycling with an average Coulombic efficiency of more than 99.9 per cent at -30 degrees Celsius. The comprehensive analysis further reveals an impedance matching between the NMC811 cathode and the graphite anode owing to the formation of similar lithium-fluoride-rich interphases, thus effectively avoiding lithium plating at low temperatures. Additionally, this electrolyte design principle can be extended to other alkali-metal-ion batteries operating under extreme conditions.

25 ENERGY STORAGE↗

Effects of catholyte aging on high-nickel NMC cathodes in sulfide all-solid-state batteries

Sulfide solid-state electrolytes (SSEs) in all-solid-state batteries (SSBs) are recognized for their high ionic conductivity and inherent safety. The LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathode offers a high thermodynamic potential of approximately 3.8 V vs. Li/Li + and a theoretical specific capacity of 200 mA h g −1 . However, the practical utilization of NMC811 in sulfide SSBs faces significant interfacial challenges. The oxidation instability of sulfide solid electrolytes against NMC811 and the formation of the cathode electrolyte interphase (CEI) during cycling lead to degradation and reduced cell performance. Volumetric changes in NMC during lithiation and de-lithiation can also cause detachment from sulfide electrolytes or internal particle cracking. Despite extensive galvanostatic cycling studies to address the issues, the calendar life of sulfide SSBs remains poorly understood. Here, we systematically studied the effects of four different catholytes on the calendar aging of LiNbO 3 (LNO)-coated NMC811, including Li 6 PS 5 Cl (LPSCl), Li 3 InCl 6 –Li 6 PS 5 Cl (LIC–LPSCl), Li 3 YCl 6 –Li 6 PS 5 Cl (LYC–LPSCl), and Li 10 GeP 2 S 12 (LGPS). Our results indicate that LPSCl provides optimal capacity retention when stored at high state-of-charge (SOC) at room temperature, but the LIC–LPSCl cathode shows significant capacity degradation and chemical incompatibility. We also established an effective electrochemical calendar aging testing protocol to simulate daily usage, enabling quick inference of the calendar life of SSBs. In conclusion, this new testing approach accelerates materials selection strategies for high-nickel NMC composite cathodes in sulfide SSBs.

25 ENERGY STORAGE↗

Effects of cathode loadings and anode protection on the performance of lithium metal batteries

Abstract While lithium-ion batteries (LIBs) are approaching their energy limits, lithium metal batteries (LMBs) are undergoing intensive investigation for higher energy density. Coupling LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathode with lithium (Li) metal anode, the resultant Li||NMC811 LMBs are among the most promising technologies for future transportation electrification, which have the potential to realize an energy density two times higher than that of state-of-the-art LIBs. To maximize their energy density, the Li||NMC811 LMBs are preferred to have their cathode loading as high as possible while their Li anode as thin as possible. To this end, we investigated the effects of different cathode active material loadings (2–14 mg cm −2 ) on the performance of the Li||NMC811 LMBs. Our study revealed that the cathode loadings have remarkably affected the cell performance, in terms of capacity retention and sustainable capacity. Cells with high cathode loadings are more liable to fade in capacity, due to more severe formation of the CEI and more sluggish ion transport. In this study, we also verified that the protection of the Li anode is significant for achieving better cell performance. In this regard, our newly developed Li-containing glycerol (LiGL) via molecular layer deposition (MLD) is promising to help boost the cell performance, which was controllably deposited on the Li anode.

Materials Science↗

Unravelling electro-chemo-mechanical interplay in layered oxide cathode degradation in solid-state batteries

Solid-state batteries (SSBs) hold notable promise for advancing energy storage technologies. However, their commercial viability is limited by the poor cycle stability and complex degradation mechanism. This study underscores the pivotal role of electro-chemo-mechanical interactions in driving the failure of SSBs. Leveraging advanced x-ray imaging and spectroscopy techniques, we analyzed LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes from cycled Li x In||Li 6 PS 5 Cl (LPSC)||NMC811 SSBs, uncovering the interplay between microstructure, chemical heterogeneity, mechanical characteristics, and electrochemical performance. Our results show that revealing electro-chemo-mechanical interactions is essential to develop strategies to suppress the degradation of SSBs. Particularly, we revisit a LiNbO 3 (LNO) coating layer to mitigate electrochemical degradation. The LNO@NMC811 cathode retains 116 milliampere-hours per gram after 200 cycles, showing excellent stability, while the uncoated NMC811 cathode keeps degrading over time, with suppressed chemical heterogeneity and mechanical failure. This work highlights the importance of synergizing advanced material design with coating techniques, ensuring uniform lithium flux and improving mechanical properties to achieve stable, high-performance SSBs.

Zheng, Xueli [SLAC National Accelerator Laboratory↗

Capacity Fade of Graphite/NMC811: Influence of Particle Morphology, Electrolyte, and Charge Voltage

LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) is an important Li-ion battery cathode material; however, there is a tradeoff between delivered capacity and capacity retention. As the charge potential increases the capacity rises but at the expense of capacity retention. The decrease in capacity retention has been ascribed to several factors including particle cracking, surface reconstruction, transition metal dissolution, and electrolyte reactivity. The present study compares 4.1 and 4.3 V charging limits in commercially relevant graphite/NMC811 pouch cells for single crystal (SC) and polycrystalline (PC) NMC811 with ethylene carbonate (EC)-containing or EC-free electrolytes. The electrochemistry is rationalized through analysis of electrochemical impedance spectroscopy, positive electrode X-ray photoelectron spectroscopy, soft X-ray absorption spectroscopy, X-ray diffraction, and negative electrode mapping by X-ray fluorescence. Graphite/SC-NMC811 cells show high-capacity retention at 4.1 V but exhibit degradation at 4.3 V charging potentials. The EC-free electrolyte cells led to higher capacity fade, especially when charged to 4.3 V. Cathode dissolution and deposition on the negative electrode from PC-NMC811 cells was higher than for samples from SC-NMC811 cells. This study reveals the impact of material type, charge voltage, and electrolyte composition on the reactions at the positive electrode, their influence on the negative electrode, and evolution with cycle number.

36 MATERIALS SCIENCE↗

Simultaneous Single Crystal Growth and Segregation of Ni-Rich Cathode Enabled by Nanoscale Phase Separation for Advanced Lithium-Ion Batteries

Here, a novel nanoscale phase separation process has been discovered to promote the growth and segregation of single-crystal LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811). This process occurs directly during high-temperature calcination without significant agglomeration. The key lies in converting transition metal hydroxide (TM(OH) 2 ) precursors with well-controlled morphology into transition metal oxide (TMO) intermediates before reacting them with lithium salt. The nanoscale redistribution of Ni in TMO, resulting from the concurrent formation of spinel and rock salt phases, helps to deagglomerate the clusters of later-formed NMC811 crystals. The as-prepared single-crystal NMC811 is further validated in a 2Ah pouch cell, demonstrating 1,000 stable cycles. The fundamentally new reaction mechanism of single-crystal growth and segregation provides a new direction for large-scale synthesis of a broad range of single crystals for advanced energy storage.

25 ENERGY STORAGE↗

Lattice-Oxygen-Driven Selective Oxidation Strategy for Stable Argyrodite Solid-State Lithium Metal Batteries

All-solid-state lithium metal batteries (ASSLMBs) with Li6PS5Cl argyrodite electrolytes and high-voltage LiNi0.8Mn0.1Co0.1O2 (NMC811) cathodes offer high energy density but suffer from rapid capacity fading due to the layered-to-rock-salt transition of NMC811 and structural degradation of Li6PS5Cl from parasitic interfacial reactions. Here, we demonstrate a catholyte engineering strategy using a Li2S scavenging additive to suppress interfacial reactivity and preserve the structural and electrochemical stability of both NMC811 and Li6PS5Cl. Incorporating 0.10 wt.% Li2S enables exceptional cycling stability, achieving 76% capacity retention after 550 cycles at C/10 and 88% retention after 800 cycles at C/3 at 60 degrees C, compared with rapid failure in pristine cells. Spectroscopic, electrochemical, and morphological analyses confirm that Li2S maintains electrode integrity by sustaining particle contact and suppressing phase decomposition. This work elucidates interfacial degradation pathways in NMC811/argyrodite systems and introduces a low-cost, scalable strategy to stabilize nickel-rich oxide cathodes in ASSLMBs, advancing their practical viability.

25 ENERGY STORAGE↗

Resolving Chemical and Spatial Heterogeneities at Complex Electrochemical Interfaces in Li-Ion Batteries

The high specific capacities of Ni-rich transition metal oxides have garnered immense interest for improving the energy density of Li-ion batteries (LIBs). Despite the potential of these materials, Ni-rich cathodes suffer from interfacial instabilities that lead to crystallographic rearrangement of the active material surface as well as the formation of a cathode electrolyte interphase (CEI) layer on the composite during electrochemical cycling. While changes in crystallographic structure can be detected with diffraction-based methods, probing the chemistry of the disordered, heterogeneous CEI layer is challenging. In this work, we use a combination of ex situ solid-state nuclear magnetic resonance (SSNMR) spectroscopy and X-ray photoemission electron microscopy (XPEEM) to provide chemical and spatial information, on the nanometer length scale, on the CEI deposited on LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) composite cathode films. XPEEM elemental maps offer insight into the lateral arrangement of the electrolyte decomposition products that comprise the CEI and paramagnetic interactions (assessed with electron paramagnetic resonance (EPR) and relaxation measurements) in 13 C SSNMR provide information on the radial arrangement of the CEI from the NMC811 particles outward. Using this approach, here we find that LiF, Li 2 CO 3 , and carboxy-containing structures are directly appended to NMC811 active particles, whereas soluble species detected during in situ 1 H and 19 F solution NMR experiments (e.g., alkyl carbonates, HF, and vinyl compounds) are randomly deposited on the composite surface. We show that the combined approach of ex situ SSNMR and XPEEM, in conjunction with in situ solution NMR, allows spatially-resolved, molecular-level characterization of paramagnetic surfaces and new insights into electrolyte oxidation mechanisms in porous electrode films.

36 MATERIALS SCIENCE↗

Formation of Surface Impurities on Lithium–Nickel–Manganese–Cobalt Oxides in the Presence of CO 2 and H 2 O

Surface impurities involving parasitic reactions and gas evolution contribute to the degradation of high Ni content LiNi x Mn y Co z O 2 (NMC) cathode materials. The transient kinetic technique of Temporal Analysis of Products (TAP), density functional theory, and infrared spectroscopy have been used to study the formation of surface impurities on varying nickel content NMC materials (NMC811, NMC622, NMC532, NMC433, NMC111) in the presence of CO 2 and H 2 O. CO 2 reactivity on a clean surface as characterized by CO 2 conversion rate in the TAP reactor follows the order: NMC811 > NMC622 > NMC532 > NMC433 > NMC111. The capacity of CO 2 uptake follows a different order: NMC532 > NMC433 > NMC622 > NMC811 > NMC111. Moisture pretreatment slows down the direct CO 2 adsorption process and creates additional active sites for CO 2 adsorption. Electronic structure calculations predict that the (012) surface is more reactive than the ($10\bar{1}4$) surface for CO 2 and H 2 O adsorption. CO 2 adsorption leading to carbonate formation is exothermic with formation of ion pairs. The average CO 2 binding energies on the different materials follow the CO 2 reactivity order. Water hydroxylates the (012) surface and surface OH groups favor bicarbonate formation. Water creates more active sites for CO 2 adsorption on the ($10\bar{1}4$) surface due to hydrogen bonding. The composition of surface impurities formed in ambient air exposure is dependent on water concentration and the percentage of different crystal planes. Different surface reactivities suggest that battery performance degradation due to surface impurities can be mitigated by precise control of the dominant surfaces in NMC materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Unraveling the convoluted and dynamic interphasial mechanisms on Li metal anode

Accurate understanding of the chemistry of solid-electrolyte interphase (SEI) is key to developing new electrolytes for high-energy batteries using lithium metal (Li-0) anodes(1). SEI is generally believed to be formed by the reactions between Li-0 and electrolyte(2,3). However, our new study shows this is not the whole story. Through synchrotron-based X-ray diffraction and pair distribution function analysis, we reveal a much more convoluted formation mechanism of SEI, which receives considerable contributions from electrolyte, cathode, moisture and native surface species on Li-0, with highly dynamic nature during cycling. Using isotope labelling, we traced the origin of LiH to electrolyte solvent, moisture and a new source: the native surface species (LiOH) on pristine Li-0. When lithium accessibility is very limited as in the case of anode-free cells, LiOH develops into plate-shaped large crystals during cycling. Alternatively, when the lithium source is abundant, as in the case of Li||NMC811 cells, LiOH reacts with Li-0 to form LiH and Li2O. While the desired anion-derived LiF-rich SEI is typically found in the concentrated electrolytes or their derivatives, we found it can also be formed in low-concentration electrolyte via the crosstalk effect, emphasizing the importance of formation cycle protocol and opening up opportunities for low-cost electrolyte development.