Search NASA⌕ Search

SEARCH · Search NASA

Results for “Na2SO4”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Deposition of Na2SO4 from salt-seeded combustion gases of a high velocity burner rig

With a view to developing simulation criteria for the laboratory testing of high-temperature materials for gas turbine engines, the deposition rates of sodium sulfate from sodium salt-seeded combustion gases were determined experimentally using a well instrumented high-velocity burner. In the experiments, Na2SO4, NaCl, NaNO3, and simulated sea salt solutions were injected into the combustor of the Mach 0.3 burner rig operating at constant fuel/air ratios. The deposits formed on an inert rotating collector were then weighed and analyzed. The experimental results are compared to Rosner's vapor diffusion theory. Some additional test results, including droplet size distribution of an atomized salt spray, are used in interpreting the deposition rate data.

Santoro, G. J.↗

A microstructural investigation of a Na2SO4 activated cement-slag blend

The reactivity and early strength of cement:slag binders is usefully enhanced by the addition of sodium sulfate though the underlying mechanisms of the relationship between the enhanced hydration reactions and the structural aspects of the strength behavior remain unclear. In this study, microstructural development in the presence of Na{sub 2}SO{sub 4} was investigated utilizing mercury intrusion porosimetry (MIP), NMR relaxometry, and XRD. Increased rates of early strength development and decreased rates of late strength development due to the presence of added Na{sub 2}SO{sub 4} were linked to effects on capillary porosity refinement. While degree of hydration at later age was shown to have been lower in the presence of Na{sub 2}SO{sub 4}, and may have been responsible for the higher capillary porosity, a clear alteration in the pathway of microstructural development had occurred with inhibition to hydration of the slag component due to earlier microstructural development proposed.

36 MATERIALS SCIENCE↗

Na2SO4 induced corrosion of nickel at high temperature

Sodium sulfate-induced corrosion of nickel was studied at 900 C as a function of oxygen partial pressure. For high O2 partial pressures, accelerated corrosion during the first few minutes occurred by rapid penetration of the melt along the metal grain boundaries. A mechanism is proposed to explain this phenomenon. Repetitive scale metal detachment was observed for corrosion in lower O2 partial pressures and during the later period of corrosion in higher O2 partial pressures. The effect of preoxidation on the hot corrosion has also been studied. An induction period is observed before the onset of rapid corrosion for the preoxidized samples; the onset of rapid corrosion is associated with sudden cracking of the scale. The length of the induction period for the preoxidized samples is a function of the length of preoxidation, and appears to be related to the structure of the oxide scale after the preoxidation treatment.

Misra, A. K.↗

CMI Winter Meeting 2025 Presentation

Lanthanides are important to many technologies including magnets used in high efficiency traction motors. While common in the environment and industrial waste streams, lanthanides are often present at very low concentrations. This work demonstrates synergistic lanthanide recovery from an aqueous magnet leachate to single ppm concentrations using Na2SO4 addition and subsequent DME-FC treatment. It was found that combining DME-FC with low concentrations of Na2SO4 (~0.1 M) results in synergistic isolation of lanthanides while making use of Na2SO4, an excessive byproduct of hydrometallurgical metal production. Combined Na2SO4 + DME reduced lanthanide metal ion's (Pr, Nd, Sm, Gd, Dy, and Ho) solubilities by 1,000 - 25,000x with final concentrations ranging from 2 ppm to 200 ppm. This can be compared to 0.1 M Na2SO4 alone providing a 10 - 200x reduction and DME providing a 100 - 1,500x reduction in lanthanide solubilities. Final solution concentrations of lanthanides were 99.8% lower than what could not be achieved with either individual process. The results also reveal different periodic trends in the solubility reduction for DME and Na2SO4.

37 - INORGANIC, ORGANIC, PHYSICAL AND ANALYTICAL C↗

Sodium sulfate - Deposition and dissolution of silica

The hot-corrosion process for SiO2-protected materials involves deposition of Na2SO4 and dissolution of the protective SiO2 scale. Dew points for Na2SO4 deposition are calculated as a function of pressure, sodium content, and sulfur content. Expected dissolution regimes for SiO2 are calculated as a function of Na2SO4 basicity. Controlled-condition burner-rig tests on quartz verify some of these predicted dissolution regimes. The basicity of Na2SO4 is not always a simple function of P(SO3). Electrochemical measurements of an (Na2O) show that carbon creates basic conditions in Na2SO4, which explains the extensive corrosion of SiO2-protected materials containing carbon, such as SiC.

Jacobson, Nathan S.↗

Sodium sulfate: Vaporization thermodynamics and role in corrosive flames

Gaseous species over liquid Na2SO4 were identified by the technique of molecular beam mass spectrometry. The heat and entropy of vaporization of the Na2SO4 molecule were measured directly. Comparisons of the experimental entropy with values calculated using various molecular parameters were used to estimate the molecular structure and vibrational frequencies. The thermodynamic properties of gaseous and condensed phase Na2SO4, along with additional pertinent species, were used in a computer program to calculate equilibrium flame compositions and temperatures for representative turbine engine and burner rig flames. Compositions were calculated at various fuel-to-oxidant ratios with additions of sulfur to the fuel and the components of sea salt to the intake air. Temperatures for condensation of Na2SO4 were obtained as a function of sulfur and sea salt concentrations.

Kohl, F. J.↗

The role of NaCl in flame chemistry, in the deposition process, and in its reactions with protective oxides as related to hot corrosion

Sodium chloride is believed to be the primary source of turbine engine contamination that contributes to hot corrosion. The behavior of NaCl-containing aerosols ingested with turbine intake air is very complex; some of the NaCl may vaporize during combustion while some may remain as particulates. The NaCl can lead to Na2SO4 formation by several possible routes or it can contribute to corrosion directly. Hydrogen or oxygen atom reaction with NaCl(c) was shown to result in the release of Na(g). Gaseous NaCl in flames can be partially converted to gaseous Na2SO4 by homogeneous reactions. The remaining gaseous NaCl and other Na-containing molecules can act as sodium carriers for condensate deposition of Na2SO4 on cool surfaces. A frozen boundary layer theory was developed to predict the rates of deposition. The condensed phase NaCl can be converted directly to condensed Na2SO4 by reaction with sulfur oxides and O2. Reaction of gaseous NaCl with Cr2O3 results in the vapor phase transport of chromium by the formation of complex Cr-containing gaseous molecules. Similar gaseous complexes are formed with molybdenum. The presence of gaseous NaCl was shown to affect the oxidation kinetics of Ni-Cr alloys. It also causes changes in the surface morphology of Al2O3 scales formed on Al-containing alloys.

Kohl, F. J.↗

Investigation into the role of NaCl deposited on oxide and metal substrates in the initiation of hot corrosion

Morphological aspects of the conversion to Na2SO4 of NaCl deposits over the temperature range 500-700 C, in air with added SO2 and H2O. Progress of the reaction was observed by withdrawing samples at various times and examining them under the scanning electron microscope using EDAX to assess the extent of chloride to sulfate conversion. These initial results show that the conversion to Na2SO4 proceeds directly on the sodium chloride surface as well as on the surrounding substrate due to evaporation of NaCl from the solid particle. The mechanism of this reaction could involve reaction in the vapor to produce Na2SO4 which then deposits, alternatively Na2SO4 could form directly on the substrate surface due to direct reaction there between the vapors NaCl, SO2 and O2.

Birks, N.↗

Corrosion of metals and alloys in sulfate melts at 750 C

The corrosion of Ni, Co, Ni-10Cr, Co-21Cr, and IN738 was studied at 750 C in the presence of molten sulfate mixtures (Na2SO4-Li2SO4 and Na2SO4-CoSO4) and in an atmosphere consisting of O2 + 0.12 percent SO2-SO3. The corrosion was observed to be similar for both Na2SO4-Li2SO4 and Na2SO4-CoSO4 melts. The corrosion of Ni and Co took place by the formation of a mixed oxide plus sulfide scale, very similar to the corrosion in SO2 or SO3 alone. The initial stage for the corrosion of Ni-10Cr involved the formation of a thick NiO + Ni3S2 duplex scale, and Cr sulfide was formed during the later stages. A pitting type of morphology was observed for both Co-21Cr and IN738. The pit was Cr sulfide at the beginning, and subsequently the sulfides oxidized to Cr2O3. A base-metal oxide layer was present above the pit, and this was observed to be formed very early in the corrosion process. A mechanism is proposed to explain this. In general, the formation of sulfides appears to be the primary mode of degradation in mixed sulfide melts.

Misra, A. K.↗

Reactions occurring during the sulfation of sodium chloride deposited on alumina substrates

The reaction between solid NaCl and air containing 1 pct SO2 has been studied between 500 and 700 C. The reaction product, Na2SO4, forms not only on the surface of the NaCl but also on surrounding areas of the substrate due to the volatility of the NaCl at these temperatures. At the higher temperatures, the vapor pressure of NaCl is so high that the majority of the reaction product is distributed on the substrate. Above 625 C, the reaction product is a liquid solution of NaCl and Na2SO4 that exists only so long as NaCl is supplied from the original crystal source. Eventually, the liquid solidifies by constitutional solidification as the NaCl is converted to Na2SO4. While it exists, the liquid NaCl-Na2SO4 solution is shown to be highly corrosive to Al2O3 and, on a scale of Al2O3 growing on alloy HOS 875, particularly attacks the grain boundaries of the scale at preferred sites where chromium and iron oxides and sulfides rapidly develop. This is proposed as one mechanism by which NaCl deposition contributes to the initiation of low temperature hot corrosion.

Wu, C. S.↗

Gaseous sodium sulfate formation in flames and flowing gas environments

Formation of Na2SO4(g) in flames and hot flowing gas systems was studied by high pressure, free-jet expansion, modulated molecular beam mass spectrometric sampling. Fuel-lean CH4-O2 flames doped with SO2, H2O and NaCl yielded the gaseous Na2SO4 molecule in residence times of less than one millisecond. Intermediate species NaSO2(g) and NaSO3(g) were also observed and measured. Composition profiles were obtained for all reaction products. Nonflame flowing gas experiments showed that Na2SO4 and NaSO3 gaseous molecules were formed at 1140 C in mixtures of O2, H2O(g), SO2 and NaCl(g). Experimental results are compared with calculated equilibrium thermodynamic predictions.

Stearns, C. A.↗

Gaseous sodium sulfate formation in flames and flowing gas environments

Formation of Na2SO4(g) in flames and hot flowing gas systems was studied by high pressure, free-jet expansion, modulated molecular beam mass spectrometric sampling. Fuel-lean CH4-O2 flames doped with SO2, H2O and NaCl yielded the gaseous Na2SO4 molecule in residence times of less than one millisecond. Intermediate species NaSO2(g) and NaSO3(g) were also observed and measured. Composition profiles were obtained for all reaction products. Non-flame flowing gas experiments showed that Na2SO4 and NaSO3 gaseous molecules were formed at 1140 C in mixtures of O2, H2O(g), SO2 and and NaCl(g). Experimental results are compared with calculated equilibrium thermodynamic predictions.

Stearns, C. A.↗