Search NASA⌕ Search

SEARCH · Search NASA

Results for “Nickel-based superalloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Design Methods, Tools, and Data for Ceramic Solar Receivers

This report presents the development of tools and methods for evaluating the reliability and performance of ceramic materials in high temperature solar receivers. As Concentrating Solar Power (CSP) technologies aim for higher operating temperatures to enhance efficiency and meet industrial process heat requirements, current high temperature metallic materials face challenges in maintaining structural integrity. This report explores advanced ceramics as a promising alternative, given their superior high temperature strength and lower thermal expansion, compared to metals. To address the need for effective ceramic receiver design tools, this report integrates statistical failure models of ceramics into the existing srlife tool: an open-source software package designed to estimate the life of high temperature CSP components. These failure models account for the inherent variability and flaw distribution in ceramics, as well as the impact of subcritical crack growth under high temperature cyclic loads. The report also presents experimental data collected for a commercially available ceramic material, SiC, and details the process of estimating reliability model parameters from these data. A comparative design analysis is then performed between ceramic (SiC) and metallic (current nickel-based superalloys A740H and A282) receiver. This comparison demonstrates that SiC receivers can achieve service life exceeding 30 years under high incident heat flux conditions, compared to just a few years for metallic receivers.

14 SOLAR ENERGY↗

Ab Initio Design of High-Entropy Thermal/ Environmental Barrier Coatings

Next generation thermal/environmental barrier coatings (TEBC) require carefully balancing various properties including phase stability, thermal conductivity, coefficient of thermal expansion (CTE), mechanical properties, and resistance against hot corrosion and water vapor recession. This work mainly focuses on rapid design of cost-effective high entropy rare-earth disilicates and aluminum garnets to protect SiC-based ceramic matrix composites and nickel-based superalloys in the hot section of gas turbine engines using density functional theory methods. Our calculations identify several low-cost high entropy TEBC exhibiting ultralow thermal conductivity at 1500 K and desirable CTE while maintaining good mechanical properties, including Er1/2Y3/4Yb3/4Si2O7, Gd1/4Er1/4Y3/4Yb3/4Si2O7, Eu1/4Er1/4Y3/4Yb3/4Si2O7, and (Y1/4Gd1/4Er1/4Yb1/4)3Al5O12. This work also aims to gain fundamental understanding of oxygen diffusion in model disilicates. Minimizing oxidizer (such as water vapor and oxygen) permeability through the EBC layer can significantly decrease the growth rate of thermally grown oxide and extend the service life of the coating system. Oxygen diffusion mechanisms including formation energy of defects under varying oxygen conditions and defect migration energy barriers will be presented.

coefficient of thermal expansion↗

Powder metallurgy hot isostatic pressing - workshop report

The findings of the powder metallurgy (PM) hot isostatic pressing (HIP) workshop confirmed that the accelerated adoption of this technology requires the following action items: 1. By 2035, the HIP infrastructure must be scaled to sizes larger than 4 .0 meters for manufacturing components relevant to energy and defense industries at large. 2. The community must develop cost-effective and agile standards, qualifications, and certification pathways for these HIP parts. 3. At the same time, domestic powder production should be expanded to a wide range of metallic alloys, including Cr-Mo steels, stainless steels, and titanium- and nickel-based superalloys, as well as to emerging alloy classes in the refractory space. 4. The above initiatives can be enhanced by implementing digital modeling and controls, including AI-driven simulations, in situ monitoring, and digital twins.

36 MATERIALS SCIENCE↗

A Computer Design Tool for Ceramic Receivers

Gen3 solar receivers and other components will experience a combination of high temperatures and high stress caused by thermal stress and internal pressure. Under these conditions metallic components, even those manufactured from nickel-based superalloys, have poor reliability. Engineering ceramics could be a solution, as these materials have excellent high temperature strength. However, accurately assessing the reliability of a ceramic component operating in these conditions requires an entirely different approach compared to metallic materials. This paper describes the implementation of statistical models for evaluating the reliability of high temperature ceramic components in srlife – an open-source software package for estimating the life of high temperature concentrating solar power equipment. This new capability allows users to make fair comparisons between competing metallic and ceramic component designs and to accurately assess the plant efficiency and economics of ceramic solar receivers and other components.

Messner, Mark (ORCID:0000000200404385)↗

Time-Dependent Failure Assessment of Ceramic Receivers

The outlet temperature targets for Gen 3 Concentrating Solar Power (CSP) systems pose a significant challenge to the structural reliability of high temperature metallic components, including those manufactured from nickel-based superalloys. Advanced ceramics present a potential solution due to their excellent high-temperature strength. However, accurate assessment of ceramic components requires an entirely different approach compared to metallic components. This paper describes the implementation of time-dependent reliability analysis of ceramic components in srlife – an open-source software package for estimating the life of high temperature CSP components. This new capability will allow high temperature CSP designers to make fair comparisons between competing metallic and ceramic designs and accurately assess the performance of different ceramic materials for CSP receivers and other components. The current version of the tool is available at https://github.com/Argonne-National-Laboratory/srlife.

Barua, Bipul (ORCID:0000000247184113)↗

Microstructural evolution and hardness changes in ion irradiated nickel-based Haynes 282 superalloy

This study investigated the crucial aspects of thermal and irradiation stability in precipitation hardened Haynes 282 Ni-based superalloy. The Haynes 282 Ni-based alloy was irradiated by 8 MeV Ni 3+ ions to assess its resistance to phase instabilities and mechanical property alterations. The mid-range doses (at a depth of ∼1 µm) were 1 and 10 displacements per atom (dpa) at temperatures of 600°C and 750°C. Nanoindentation tests provided insights into bulk equivalent hardness of the irradiated and pristine regions, while scanning transmission electron microscopy (STEM) and energy dispersive X-ray spectroscopy (EDS) were used to examine the microstructural evolution of irradiation-induced defects and γ′ -Ni 3 (Al, Ti) precipitates and defect structure under irradiation. These precipitates, with an average diameter of 29 nm and a number density of 5 x 10 21 /m 3 , acted as robust dispersion strengthening agents with high radiation point defect sink strength. Remarkably, irradiation did not significantly alter the size or number density of the γ′ precipitates, indicating exceptional thermal stability and radiation resistance of these precipitates at the examined conditions. Radiation-induced dislocation loops were observed at 600°C, albeit without a substantial impact on mechanical properties due to the dominance of γ′ precipitates on the overall alloy strength. The superior stability of γ′ precipitates observed in this study contrasts with several previous research findings on Ni-based alloys that reported poor precipitate stability. Plausible reasons for this difference are discussed. Moreover, this work explicitly outlines a physically grounded approach to ensure accurate microstructure-hardness correlations and clarifies the hardening model by addressing common misapplications of superposition in prior studies.

36 MATERIALS SCIENCE↗

Phase-field predictions of the influence of cooling rates during AM on the Evolution of Microstructures in Nickel-Based Single Crystal Superalloys

Additive manufacturing of single crystals made of Ni-based superalloys offers major cost savings for gas turbine engines with the inclusion of internal cooling channels. However, the lack of understanding of the effect of transient thermal conditions on solidification grain structure during additive manufacturing hinders the potential for process control to maintain the single crystal quality. The use of high-fidelity simulations through high performance computing to predict the evolution of the solidification microstructure will enhance the abilities to tailor the microstructures through process optimization. Phase field simulations are used to determine the effect local thermal conditions and defects on the stability of the solidification morphology, specifically with respect to the onset of columnar-to-equiaxed transition that results in the loss of the single crystal. The results are expected to be instrumental for developing future surrogate models to speed up the integration of design and manufacturing of turbine blades under the harsh in-service conditions.

36 MATERIALS SCIENCE↗

Heterogeneous fatigue damage in a nickel-based single-crystal superalloy unraveled using correlative 3D X-ray technology

Nickel-based single-crystal (Ni-SX) superalloys under cyclic stress are susceptible to cracking at stress-concentration sites, eventually leading to low-cycle fatigue (LCF) failure. LCF cracks typically originate from intrinsic defects (e.g., voids and carbides) within solidified dendrites. However, systematic quantitative experimental analyses of defect-mediated local damage remain limited. To thoroughly understand the microscopic origins and evolution of LCF damage, correlated 3D mapping of dendrites across various regions is essential. Here, in this study, macroscale micro-computed tomography (μ-CT) was initially used to capture internal interdendritic secondary cracks within bulk DD413 superalloy after LCF testing at 760 °C. Subsequently, a multimodal methodology combining synchrotron 3D microdiffraction (3D-μXRD), high-resolution μ-CT, and electron microscopy was established. This approach allowed precise localization of internal damage zones near interdendritic secondary cracks and detailed mapping of the 3D correlated distributions of dendrites, defects, and residual stress/strain fields within these zones at submicron spatial resolution. Finally, the same approach was applied to specimens subjected to interrupted loading at approximately 40 % of the fatigue life to uncover the early damage states of dendrites. The dendrite cores (DCs) and interdendritic regions (IDs) exhibit microscale heterogeneous mechanical responses: nearly defect-free DCs accumulate local irreversible slip along specific slip systems to generate slip bands, while the IDs containing various defects accommodate local microplasticity through the activation of multiple slip systems around these defects. The local tensile stress near defects in the IDs exceeds that in the DC slip band regions by more than threefold, leading to the generation of local damage zones within the IDs. Chain-like defect distributions facilitate the interconnection of these local zones into a continuous damage region, further elevating the overall tensile stress in the IDs. Additionally, geometrically necessary dislocations alone are insufficient as indicators of LCF damage; both the internal stress state and its magnitude must be considered. These experimental results provide critical data and insights for the development of multi-physics fatigue models.

Localized deformation↗

Dissolution zone model of the oxide structure in additively manufactured dispersion-strengthened alloys

The structural evolution of oxides in dispersion-strengthened superalloys during laser-powder bed fusion is considered in detail. Alloy chemistry and process parameter effects on oxide structure are assessed through a parameter study on the model alloy Ni-20Cr, doped with varying concentrations of Y 2 O 3 and Al. Small angle neutron scattering measurements of the dispersoid size distribution show the dispersoid size increases with higher laser power, slower scan speed, and increasing Y 2 O 3 and Al content. Complementary electron microscopy measurements reveal reactions between Y 2 O 3 and Al, even in nanoscale dispersoids, and the presence of micron-scale oxide slag inclusions in select specimens. A scaling analysis of mass and momentum transport within the melt pool, presented here, establishes that diffusional structural evolution mechanisms dominate for nanoscale dispersoids, while fluid forces and advection become significant for larger slag inclusions. These findings are developed into a theory of dispersoid structural evolution, integrating quantitative models of diffusional processes – dispersoid dissolution, nucleation, growth, coarsening – with a reduced order model of time-temperature trajectories of fluid parcels within the melt pool. Calculations of the dispersoid size in single-pass melting reveal a zone in the center of the melt track in which the oxide feedstock fully dissolves. Within this zone the final Y 2 O 3 size is independent of feedstock size and determined by nucleation and growth kinetics. If the dissolution zones of adjacent melt tracks overlap sufficiently with each other to dissolve large oxides, formed during printing or present in the powder feedstock, then the dispersoid structure throughout the build volume is homogeneous and matches that from a single pass within the dissolution zone. Gaps between adjacent dissolution zones result in oxide accumulation into larger slag inclusions. Predictions of final dispersoid size and slag formation using this dissolution zone model match the present experimental data and explain process-structure linkages speculated in the open literature.

36 MATERIALS SCIENCE↗

Synchrotron X-ray diffraction analysis of constituent phases in transition joint between nickel alloy 738LC and a MnFeCoNiCu alloy

Synchrotron x-ray diffraction (XRD) analysis was performed on transition joints between a single-phase MnFeCoNiCu alloy and Ni-base Alloy 738LC to efficiently identify the constituent phases across the interface, with different levels of material intermixing generated by laser-welding with variable power. Here, the intermixing extent was quantified by postmortem energy dispersive x-ray spectroscopy mapping. Diffraction-based analyses on complex composition spaces with limited prior data present significant challenges because elemental substitution in both disordered and ordered phases is more extensive than in conventional alloy spaces, which may effectuate relatively large shifts in the observed lattice parameters that convolute the analysis. Therefore, thermodynamic simulations and crystallographic literature data were employed to construct a system-specific diffraction library of twelve prospective phases for the composition space investigated. Subsequently, for predicted disordered cubic phases, statistical hard-sphere models were established to estimate the lattice parameters and predict diffraction peak positions for inclusion in the library. The library was then employed to analyze diffraction profiles measured from the variably intermixed transition joints, with focus on accounting for both high and low-intensity peaks. 99.0 % of diffraction peaks with relative intensity greater than 0.001 were assigned to phases from the system-specific library, exemplifying rigorous peak accounting and indicating that no unexpected phases were present. Up to six of the twelve library phases were experimentally found in the transition joints. The lattice parameters predicted by the statistical hard-sphere model based upon thermodynamic simulations agree reasonably well with the measured values for the disordered FCC matrix phase.

36 MATERIALS SCIENCE↗

Development of a high-temperature Inconel 625 heat exchanger by model design and binder jetting additive manufacturing

A nickel-based Inconel 625 superalloy heat exchanger for high-temperature applications was developed via binder jetting additive manufacturing. The material properties were characterized first on printed and sintered parts. Two sintering temperatures were used to investigate the effects of the temperature on densification and microstructure. For channel geometry design, the heat transfer capabilities of the heat exchanger were optimized for the cross-section geometry of fluid flow channels in a counterflow configuration, and a stress analysis was conducted to investigate the effects of channel geometry. After headers were incorporated into the heat exchanger as a one-piece component, a prototype was printed. A complete depowdering was achieved via compressed air blowing, and sintering was performed with the developed profile. Ultimately, a one-piece heat exchanger with a nearly full density was obtained. Heat transfer tests were performed on this unit, and the results were compared with those from the simulations. In this study, systematic processes were developed for an additively manufactured Inconel-based heat exchanger for high-pressure, high-temperature heat transfer applications.

36 MATERIALS SCIENCE↗

Design of Novel Hot Gas Path Component for Gas Turbine Engines Enabled by Materials and Additive Manufacturing Process Development

This report covers the activities associated with the development and evaluation of two high-γ’ superalloys that were designed by external partners on this project, namely Carpenter Technologies Corporation and the University of California-Santa Barbra. One alloy was GammaPrint-700, a cobalt-base superalloy, and the other a nickel-base (Ni-base) superalloy GammaPrint-1100. Both were found to be printable through laser powder bed fusion (LPBF) additive manufacturing, with optimal process parameter sets being identified for each alloy. Further, high temperature mechanical testing was conducted on each alloy that showed both materials performed better than the comparative baseline (LPBF Hastelloy X), with the Ni-base superalloy being down-selected for scaling and printing of the tip shoe components.

36 MATERIALS SCIENCE↗

Design of Novel Hot Gas Component for Gas Turbine Engines Enabled by Materials and Additive Manufacturing Process Development

This CRADA project was the result of a project award under FOA-DOE-0001980. The overarching FOA project team consisted of researchers from Carpenter Technology Corporation (CTC), Solar Turbines Incorporated (Solar), Pennsylvania State University (PSU), University of California-Santa Barbara (UCSB), and Oak Ridge National Laboratory (ORNL). Evaluations were conducted on two high-γ’ superalloys that were designed by CTC and the UCSB. One alloy named GammaPrint-700 (GP-700) is a cobalt-base superalloy. The other alloy named GammaPrint-1100 (GP-1100) is a nickel-base (Ni-base) superalloy. PSU provided expertise and experimental testing of the thermal performance of AM micro-cooling architectures. ORNL provided expertise with the AM superalloy materials characterization and AM processing science. Solar provided turbine component design expertise. The focus of this CRADA report is to document the efforts between ORNL and CTC towards the development of superalloys designed for AM. The project goal was to use an AM processable high-temperature superalloy and design for Additive Manufacturing (DfAM) techniques to design an efficient turbine component (i.e. a turbine tip shoe) with enhanced cooling features that can only be fabricated through additive manufacturing (AM). The efficiencies of existing combined heat and power (CHP) engines are capped by both component design and materials limitations. However, AM of a tip shoe component from a γ’strengthened superalloy offers the design flexibility to increase the efficiency and power of an industrial gas turbine. This project brought about advancements in the DfAM tip shoe design space and in the area of high temperature superalloys processable through laser powder bed fusion (LPBF) AM. State of art computation design tools were utilized to optimize unique cooling features into a tip shoe component design. A two-prong materials development approach was taken to support development of the AM tip shoe geometry. The first approach centered on investigating the processability and the appropriate process science for the industry standard high-γ’ nickel-base (Ni-base) superalloy Mar-M247. This superalloy is typically cast and considered non-weldable by traditional welding standards. In the course of this work, the alloy was not deemed feasible for process scale-up due to significant cracking issues during printing. The second approach focused on the development and evaluation of a novel cobalt-base superalloy, GammaPrint™-700 (GP-700 and a Ni-base superalloy, GammaPrint™-1100 (GP-1100) designed to mitigate the significant AM processing issues with Mar-M247. The processability of these two alloys were investigated through electron beam melting (EBM) binder-jet AM (BJAM), and LPBF as a risk mitigation for manufacturability. To be considered a candidate material for down-selection to proceed to full-scale AM tip shoe engine testing trials, the high temperature creep rupture strength was required to achieve at a minimum, a Larsen Miller Parameter (LMP) increase of 10.9% over the baseline material LPBF AM Hastelloy X.

99 GENERAL AND MISCELLANEOUS↗

Design of Novel Hot Gas Component for Gas Turbine Engines Enabled by Materials and Additive Manufacturing Process Development

This CRADA project was the result of a project award under FOA-DOE-0001980. The overarching FOA project team consisted of researchers from Carpenter Technology Corporation (CTC), Solar Turbines Incorporated (Solar), Pennsylvania State University (PSU), University of California-Santa Barbara (UCSB), and Oak Ridge National Laboratory (ORNL). Evaluations were conducted on two high-γ’ superalloys that were designed by CTC and the UCSB. One alloy named GammaPrint-700 (GP-700) is a cobalt-base superalloy. The other alloy named GammaPrint-1100 (GP-1100) is a nickel-base (Ni-base) superalloy. PSU provided expertise and experimental testing of the thermal performance of AM micro-cooling architectures. ORNL provided expertise with the AM superalloy materials characterization and AM processing science. Solar provided turbine component design expertise. The focus of this CRADA report is to document the efforts between ORNL and CTC towards the development of superalloys designed for AM. The project goal was to use an AM processable high-temperature superalloy and design for Additive Manufacturing (DfAM) techniques to design an efficient turbine component (i.e. a turbine tip shoe) with enhanced cooling features that can only be fabricated through additive manufacturing (AM). The efficiencies of existing combined heat and power (CHP) engines are capped by both component design and materials limitations. However, AM of a tip shoe component from a γ’strengthened superalloy offers the design flexibility to increase the efficiency and power of an industrial gas turbine. This project brought about advancements in the DfAM tip shoe design space and in the area of high temperature superalloys processable through laser powder bed fusion (LPBF) AM. State of art computation design tools were utilized to optimize unique cooling features into a tip shoe component design. A two-prong materials development approach was taken to support development of the AM tip shoe geometry. The first approach centered on investigating the processability and the appropriate process science for the industry standard high-γ’ nickel-base (Ni-base) superalloy Mar-M247. This superalloy is typically cast and considered non-weldable by traditional welding standards. In the course of this work, the alloy was not deemed feasible for process scale-up due to significant cracking issues during printing. The second approach focused on the development and evaluation of a novel cobalt-base superalloy, GammaPrint™-700 (GP-700 and a Ni-base superalloy, GammaPrint™-1100 (GP-1100) designed to mitigate the significant AM processing issues with Mar-M247. The processability of these two alloys were investigated through electron beam melting (EBM) binder-jet AM (BJAM), and LPBF as a risk mitigation for manufacturability. To be considered a candidate material for down-selection to proceed to fullscale AM tip shoe engine testing trials, the high temperature creep rupture strength was required to achieve at a minimum, a Larsen Miller Parameter (LMP) increase of 10.9% over the baseline material LPBF AM Hastelloy X.

36 MATERIALS SCIENCE↗

AMMT 2025 Milestone

Idaho National Laboratory initiated the examination of nickel-based alloys manufactured laser powder directed energy deposition additive manufacturing for potential applications in nuclear, high temperature structural components. With the rapid push towards additive manufacturing, codes do not exist that definitively define what is or is not tolerable for each process and application, such as with conventional, wrought products. This report contains the initial work to understand possible manufacturing methods for high temperature alloys, and specifically, void formation, microstructure evolution, and mechanical properties. To generate mechanical test data, specimens were tested irrespective of voids and microstructures were analyzed to better understand how to negate/improve these issues. The preliminary results showed major decreases in mechanical performance for material tested. Test specimens will continue to be produced to further improve additive manufacturing processes, quantify void acceptance, and better understand the most suitable high temperature alloys receptive to additive manufacturing and high temperature nuclear applications.

36 - MATERIALS SCIENCE↗

A macro-micro approach for identifying crystal plasticity parameters for necking and failure in nickel-based alloy haynes 282

Here, this work develops a two-scales macro-micro approach to address the challenge in calibrating crystal plasticity microstructural models when samples undergo necking prior to fracture. The crystal plasticity models are crucial for predicting the materials’ plastic deformation and failure at the microstructure level, identifying the materials’ intrinsic properties as well as investigating the microstructure-properties relationships. However, after necking occurs, the experimentally measured stress-strain curves fail to reflect the materials ‘true’ stress-strain behavior and cannot be directly fitted into crystal plasticity models. The proposed macro-micro approach employs a top-down strategy to address this challenge, which has been studied with experimental tests on precipitation-strengthened Ni-based superalloy Haynes® 282®. In this approach, a macro rate-dependent anisotropic plasticity model with Voce-type hardening and Rice-Tracey damage law is first utilized to model the deformation and failure of the tensile bar, and calibrated by matching the stress-strain curves, necking strain, and reduction of area. Especially, to match the testing results under different applied strain rates, the rate-sensitivity parameter m and saturation stress in the elasticity model are modified to incorporate dependence on the local strain rate. Then, the ‘true’ stress-strain behaviors are extracted from the necking zone of the macro-model, which are used to calibrate a micro-model with explicit microstructures and governed by an extended crystal plasticity law. The consistency between the micro-model and macro-model are enforced during calibration. The calibration outcomes from the crystal plasticity model elucidate the materials intrinsic properties for slip, hardening, and failure, which is vital for further investigations into the microstructure-properties relationship and for accurate prediction of the material behavior under various test and service conditions.

36 MATERIALS SCIENCE↗

Crystal plasticity modeling and analysis for the transition from intergranular to transgranular failure in nickel-based alloy Inconel 740H at elevated temperature

The precipitation-strengthened Nickel alloy Inconel® 740H® (IN740H) exhibits increased ductility at higher applied strain rates during quasi-static tensile tests at an elevated temperature of 760°C. The examination of fracture surfaces in this context reveals a noteworthy transition of underlying fracture mechanisms from transgranular to intergranular fracture as the applied strain rate decreases from 1×10 -3 / s to 0.83×10 -4 / s . To thoroughly understand the mechanical response of IN740H under these conditions, this study develops a crystal plasticity finite element (CPFE) model. Further, this model incorporates various deformation mechanisms including dislocation slips, climb, and grain boundary sliding, which are relevant to the test conditions. The model is calibrated using data from both tensile tests at different strain rates and creep tests across a broad stress range at 760°C, enabling the accurate determination of model parameters for each mechanism. Simulation results well captured the experimental observations of different failure modes. At higher strain rates, the model shows a dominance of dislocation slip leading to heterogeneous plastic deformation and formation of transgranular shear bands causing the failure, while at lower strain rates, an increased activity of grain boundary sliding causes grain boundaries crack leading to intergranular failure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Impacts of Superalloys on the Surface Quality of Additively Manufactured Channels

Abstract Gas turbines feature many components that require superalloys capable of handling extreme thermal environments. Increasing the selection of materials available for these components is important to their use in these extremely high-temperature environments. This study investigated two recently developed materials intended to be used for additive manufacturing (AM), with one superalloy based on cobalt and the other on nickel. Sets of four test coupons were built using the materials, in addition to the commonly used Inconel-718, on multiple laser powder bed fusion machines. Several build conditions were varied between coupon sets, including coupon orientation, contour settings, and upskin and downskin treatment. Each set of test coupons featured four unique cooling designs to explore how different cooling technologies would be impacted by the variations in build conditions. After being built, coupons were computed tomography (CT) scanned to determine accuracy to design intent and quantify the surface roughness. The CT scans indicated that horizontally built test coupons had a significantly higher deviation from design intent and higher surface roughness than those built vertically. Results also indicated that the cobalt-based alloy consistently had a smoother surface quality with lower surface roughness compared to the nickel-based alloy. After geometric characterization, the cooling performance of the test coupons was measured experimentally. Pressure losses were found to correlate with increases in surface roughness; however, in some cases, the convective heat transfer did not increase proportionally to the pressure loss as a result of surface features significantly blocking the flow without proportionally increasing convective heat transfer.

Engineering↗