29 records · Page 2

Bubble formation in helium-implanted nanostructured ferritic alloys at elevated temperatures

Helium bubble formation was examined by scanning/transmission electron microscopy (S/TEM) in Fe-9/10Cr binary alloys and two dispersion strengthened nanostructured alloys (CNA3 and 14YWT containing 5–10 nm diameter carbide and oxide particles, respectively) after ex-situ and in-situ He implantation to ~10,000 appm at 500 to 900 °C. The combination of high-resolution STEM images and electron energy loss spectroscopy (EELS) revealed that the Y-Ti-O nanoparticles in 14YWT were uniformly distributed and exhibited a one-to-one relationship for bubble attachment to the nanoclusters. In the in-situ experiment at 900 °C, grain boundary cracking was severe in the Fe-10Cr model alloy, but not in the nanostructured alloys. From 500 to 900 °C, the bubble size generally increased with increasing irradiation temperature, while the bubble density decreased with increasing temperature. At the same temperatures, the bubble size in the implanted materials was in the order of Fe-9/10Cr > CNA3 > 14YWT, while the bubble density showed the opposite order. The observed bubble number densities for the nanostructured alloys are comparable to the nanoparticle density, suggesting that the nanoparticles in both alloys were effective in trapping He. Overall, our results indicate that very high He concentrations can be managed in nanostructured alloys by sequestering the helium into smaller bubbles (which leads to a lower volume swelling value) and to shield He from the grain boundaries. This can be attributed to the much higher sink strength associated with the nanoclusters or the He trapping ability between different types of nanoclusters.

36 MATERIALS SCIENCE↗

Microstructures and mechanical properties of a modified 9Cr ferritic-martensitic steel in the as-built condition after additive manufacturing

A newly developed nano-structured high-Mn 9Cr ferritic-martensitic (FM) steel designed for additive manufacturing (Additive-manufactured Nanostructured Alloy, ANA) was fabricated via the direct energy deposition method. The as-printed ANA2 showed tensile properties (strength and elongation) and Charpy impact toughness (upper-shelf energy and ductile-brittle transition temperature) comparable to oxide-dispersion-strengthened (ODS) Eurofer and PM2000. Compared with wrought P91, the as-built ANA2 showed significantly higher yield strength but inferior Charpy impact toughness and ductility. Microstructural characterization revealed uniformly distributed sub-micron pores, an extremely high dislocation density, and a high density of ultrafine nano-structured precipitates in the matrix. The microstructures indicated the dislocations as the dominant strengthening element and the ultrafine precipitates as the primary contribution to estimated irradiation sink density. This work demonstrates the ability to exploit the unique consolidation properties of additive manufacturing to fabricate steels which marry the benefits of both ODS alloys and conventionally processed FM steels.

36 MATERIALS SCIENCE↗

Equilibrium distribution of point defects in Fe-Y-O as a typical representative of nanocluster-strengthened alloys

The statistical mechanic approach has been used to estimate the equilibrium defect distribution in a multiphase system by minimizing its free energy using microstructural characteristics and a finite set of defects obtained by first-principles calculations. Recently the approach was extended to take in consideration defects at the interface of the precipitate and matrix. Herein we apply the developed approach to the investigation of the stability of bcc Fe containing yttria, Y 2 O 3 , nanoclusters as a prototype of nanostructured ferritic alloys. It has been obtained that (100)Fe-O interface is unstable with respect to vacancies production. In a contrast to (100)Fe-O interface, the so called Klim interface is stable, i.e. local vacancy concentration at this interface at 600 K is below 10 -12 . It has been demonstrated that due to large defect formation energies the ODS particles are extremely stable and the main defect corresponds to Fe atoms substitute Y in Y 2 O 3 precipitate. Moreover, under thermodynamic equilibrium condition, the preexist vacancies in bulk Fe do not accumulate oxygen atom. The later observation not necessarily forbid the existence of a large amount of preexisting Fe vacancy - oxygen atom clusters at the initial stages of alloy formation far from equilibrium.

36 MATERIALS SCIENCE↗

Laser Powder Bed Fusion of ODS 14YWT from Gas Atomization Reaction Synthesis Precursor Powders

Abstract Laser powder bed fusion (LPBF) additive manufacturing (AM) is a promising route for the fabrication of oxide dispersion strengthened (ODS) steels. In this study, 14YWT ferritic steel powders were produced by gas atomization reaction synthesis (GARS). The rapid solidification resulted in the formation of stable, Y-containing intermetallic Y 2 Fe 17 on the interior of the powder and a stable Cr-rich oxide surface. The GARS powders were consolidated with LPBF. Process parameter maps identified a stable process window resulting in a relative density of 99.8%. Transmission electron microscopy and high-energy x-ray diffraction demonstrated that during LPBF, the stable phases in the powder dissociated in the liquid melt pool and reacted to form a high density (1.7 × 10 20 /m 3 ) of homogeneously distributed Ti 2 Y 2 O 7 pyrochlore dispersoids ranging from 17 to 57 nm. The use of GARS powder bypasses the mechanical alloying step typically required to produce ODS feedstock. Preliminary mechanical tests demonstrated an ultimate tensile and yield strength of 474 MPa and 312 MPa, respectively.

36 MATERIALS SCIENCE↗

Deuterium transport and retention properties of representative fusion blanket structural materials

Reduced activation ferritic-martensitic (RAFM) steels have been developed for decades for use as fusion blanket structural materials, and have advantages in both mechanical properties and irradiation resistance following careful engineering of the microstructure. However, the hydrogen isotope behavior in these proposed fusion structural materials is not well understood, but is important to assess since it impacts the fusion reactor safety and self-sufficient tritium fuel cycle. Here, we investigated deuterium transport and retention in representative advanced RAFM steels, including castable nanostructured alloys (CNAs), and oxide-dispersion-strengthened (ODS) steels. A gas-driven permeation (GDP) system was used to measure the permeability, diffusivity and solubility of the studied materials, covering the temperature range from 623 K to 873 K, and the loading pressures from 1.8 x 10 4 to 1.0 x 10 5 Pa. The results indicated that the deuterium permeability has little material dependence. In contrast, the deuterium diffusivity of the studied materials showed significant variation. The deuterium diffusivity in ODS steels is one order of magnitude lower than that in RAFM steels and CNAs, and correspondingly, have an effective solubility that is 2–10 times larger than RAFM steels and CNAs. In addition, thermal desorption spectroscopy (TDS) measurements were performed to assess the deuterium retention and desorption of these materials following a static thermal deuterium charging at 723 Kfor 1 hour under the deuterium pressure of 1.0 x 10 5 Pa. It was found that ODS steels exhibit the highest deuterium retention and have broader desorption peaks. Microstructural features contributing to deuterium retention and impacting deuterium transport are discussed to rationalize the observed deuterium behavior in the studied RAFM steels.

36 MATERIALS SCIENCE↗

Electric-field-assisted-sintering of rare-earth oxide dispersion strengthened Fe-Cr-Mo alloys

Oxide dispersion-strengthened (ODS) alloys are widely recognized for their exceptional high-temperature strength, creep resistance, and radiation tolerance, making them indispensable for advanced nuclear reactors, aerospace, and energy systems. Achieving a fine and stable dispersion of oxide nanoparticles is critical, as these particles act as strong barriers to dislocation motion and effective sinks for irradiation-induced defects, ensuring structural integrity under extreme conditions. Here, in this study, Fe–Cr–Mo-based ODS alloys were fabricated via mechanical alloying and consolidated using electric-field-assisted sintering (EFAS) with additions of Y 2 O 3 , La 2 O 3 , and CeO 2 . EFAS processing produced ultrafine-grained microstructures (average grain size <1 μm) with uniformly distributed oxide clusters (2–4 nm). Atom probe tomography revealed that La 2 O 3 -containing alloys exhibited the highest nanoparticle number density, resulting in superior tensile strength compared to yttria- and ceria-bearing counterparts. The combined effect of grain refinement and rare-earth oxide dispersion significantly enhanced mechanical performance, demonstrating the potential of EFAS for developing high-strength ferritic alloys for demanding environments such as nuclear systems.

36 - MATERIALS SCIENCE↗

Comparative Mechanical Properties Analysis of Triple Ion-Beam Irradiated and Neutron Irradiated Potential Plasma Facing Components

Abstract Several classes of materials are being proposed for use in fusion reactors including oxide dispersion strengthened (ODS) and reduced activation ferritic-martensitic (RAF/M) steels to withstand the severe and harsh conditions. In this work, the mechanical properties of a Fe-16Cr-4Al-2W-0.3Ti-0.3Y 2 O 3 (K3) (ODS) ferritic steel and a Fe-8.9Cr-1.1W-0.47Mn-0.2V-0.14Ta-0.11C (Eurofer 97) (RAF/M) steel) after triple ion beam irradiation were locally evaluated utilizing in-situ micro-pillar compression tests, and continuous stiffness/quasi-static nanoindentation. No change in mechanical properties was observed in the K3 ODS steel. However, the Eurofer 97 RAF/M steel exhibited radiation-induced effects via increases in yield strength. Micro-pillar techniques were expanded to neutron-irradiated materials via an in-situ testing technique employing lift-out methods on Fe-14Cr-0.9Ti-0.3Mo-0.25Y 2 O 3 (MA957) ODS ferritic steel. Both the non-irradiated and irradiated compressive yield stresses of the MA 957 micro-pillars were in good agreement with bulk yield stress values reported in the literature, suggesting that the lift-out micro-pillar compression testing technique is a promising method. The demonstration of these techniques on ion beam and neutron irradiated ODS steels and ion beam RAF/M steels gives information to inform models of the material degradation during use in a fusion device.

alloys↗

Enhancement of Nanostructured Ferritic Alloy 14YWT Properties via Heat Treatment for Post-Consolidation Processing

The nanostructured ferritic alloy 14YWT is a promising candidate for in-core use in generation IV nuclear reactors, due to a dense dispersion of insoluble, ultrafine-scale Y-Ti-O nano-oxides, which provide a high degree of irradiation tolerance and thermal stability. This work investigates the effects of heat treatment on the workability of 14YWT, along with the effect of processing history on abnormal grain structures and radial microstructural uniformity. In this study, a 14YWT rod consolidated at 850 °C was heat treated in argon at 1100 °C, 1150 °C, 1200 °C, or 1250 °C for 1 or 8 hours and changes in mechanical properties and microstructure were examined using microhardness and electron backscattered diffraction (EBSD). Two distinct types of large abnormal grains were observed, each with unique processing origins, including one with high and the other with low strain energy. Consolidation via direct extrusion resulted in radial microstructural gradients, where the center of the rod was softer with larger grain sizes and lower strain energies. These gradients persisted and intensified throughout heat treatment. Based upon this work, the recommended heat treatment for increased workability with minimal microstructural change is 1150 °C for 1 hours.

36 MATERIALS SCIENCE↗

Extensive nanoprecipitate morphology transformation in a nanostructured ferritic alloy due to extreme thermomechanical processing

Nano-oxide precipitates in a modern nanostructured ferritic alloy were investigated after extreme thermomechanical processing into a thin-walled tube geometry. It was found that the morphology of the precipitates changed from spherical to rod-shaped, with some increasing to aspect ratios of up to 9, despite the precipitate volume fraction (0.3%) and number density (> 10 23 m -3 ) of precipitates remaining unchanged. High-resolution electron microscopy showed that the precipitates likely remained coherent with the Fe-matrix, while atom probe tomography confirmed that the precipitate compositions remained unaffected by the transformation. The morphological change was attributed to the shearable nature of the (Y,Ti,O)-rich precipitates, indicating they should be considered as “soft” obstacles to dislocation motion. The elongation was most pronounced in larger (>5 nm) precipitates, which may be caused by preferential dissolution of the smallest (1–3 nm) precipitates followed by the competition between re-precipitation and solute diffusion to larger precipitates during recovery heat treatments.

36 MATERIALS SCIENCE↗

Microstructural and micro-mechanical analysis of 14YWT nanostructured Ferritic alloy after varying thermo-mechanical processing paths into tubing

Microstructural analyses and micro-pillar compression were conducted on 14YWT nanostructured ferritic alloy (NFA) to compare different processing pathways: hydrostatic extrusion and Pilger processing with varying annealing temperatures into thin walled tubing, and after hot extrusion and cross-rolling into a plate. Hydrostatic extrusion at 815 °C resulted in the smallest grain sizes and highest yield strength of 1.20 GPa. Pilger processing with annealing at 800 °C had fine grained regions and bands of coarse grains, leading to a large variation in yield strength of 0.9–1.40 GPa. Higher annealing temperatures of 1200 °C after pilger processing significantly increased the grain size and lowered the yield strength to 1.01 GPa. These tubes showed a stronger (111) crystallographic texture in the normal direction and elongated grains in the extrusion direction. Characterization of the nano-oxides using TEM reveals more numerous, smaller oxides present in tubing processed at lower temperatures. Overall, this work shows NFA tubing after hydrostatic extrusion and pilger processing can lead to fine grained microstructures and texturing leading to higher yield strengths at lower annealing temperatures (e.g. 800 °C).

14YWT↗