Search NASA⌕ Search

SEARCH · Search NASA

Results for “POTASSIUM ALLOYS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

36 records · Page 2

Study of Cu-Ni-Fe Alloys as Inert Anodes for Al Production in Low-Temperature KF-AlF{sub 3} Electrolyte

Cu-Ni-Fe-based alloys are considered as promising O{sub 2}-evolving anode materials for CO{sub 2}-free Al production. In the present study, biphased (as-cast) and monophased (postcasting homogenized) Cu{sub 65}Ni{sub 20}Fe{sub 15}, alloys, and monophased Ni{sub 65}Fe{sub 25}Cu{sub 10} alloy (in wt pct) are evaluated as O{sub 2}-evolving anodes for Al production in potassium cryolite at 700 °C. The produced Al purity is 99.6 wt pct, and the erosion rate is estimated at 0.4 cm year{sup −1} for both Cu{sub 65}Ni{sub 20}Fe{sub 15} anodes compared to 95.2 wt pct and 3.2 cm year{sup −1} for the Ni{sub 65}Fe{sub 25}Cu{sub 10} anode. The compositions, and morphologies of the surface oxide layer and the metal fluoride layer present at the oxide/alloy interface are compared for the three anodes. The deleterious impact of electrolyte infiltration on the surface oxide building is highlighted.

36 MATERIALS SCIENCE↗

Structural, Electrochemical and Hydrogen Sorption Studies of Nanocrystalline Ti-V-Co and Ti-V-Ni-Co Alloys Synthesized by Mechanical Alloying Method

In this paper, Ti-V-Co and Ti-V-Ni-Co alloys are considered as the hydrogen storage systems and the negative electrodes in Ni-MH{sub x} secondary batteries. This work shows results of studies that have been made on Ti{sub 0.5}V{sub 1.5−x}Co{sub x} and Ti{sub 0.5}V{sub 1.4−x}Ni{sub 0.1}Co{sub x} nanocrystalline alloys (x = 0, 0.1 0.2, 0.3) synthesized by the mechanical alloying technique. The goal of this study is to determine an effect of partial replacement of V by Co atoms on hydrogen storage and electrochemical properties of Ti-V and Ti-V-Ni alloys. X-ray diffraction studies have proven that 14 h of the ball milling has resulted in crystallization of body-centered-cubic solid solution. Studies performed on high-resolution transmission electron microscope confirm creation of nanocrystalline materials. Hydrogen sorption/desorption measurements that have been performed at 303 K show that Co accelerates the hydrogen sorption process, diminishes hysteresis and ameliorates the hydrogen storage reversibility. Properties of Ti-V-Co alloys, described in this work, originate mainly from structure of these materials. Electrochemical measurements of Ti-V-Co alloys have shown these materials poorly absorb hydrogen in 6 M KOH solution. Ti{sub 0.5}V{sub 1.4−x}Ni{sub 0.1}Co{sub x} alloys are characterized by better activation properties and improved cyclability in comparison to Co-free Ti{sub 0.5}V{sub 1.4}Ni{sub 0.1} alloy.

36 MATERIALS SCIENCE↗

Electronic Structures of Newly Discovered Quasi-One-Dimensional Superconductors A{sub 2}Mo{sub 3}As{sub 3} (A=K,Rb,Cs)

Electronic structures of the newly discovered quasi-one-dimensional superconductors A{sub 2}Mo{sub 3}As{sub 3} (A=K, Rb and Cs) are studied through first-principles calculations. We find that the bond lengths within the [Mo{sub 6}As{sub 6}]{sup 4−} chains are robust against the replacement of alkali cations, leading to quite similar electronic structures among the three members. Three bands cross the Fermi level and form two quasi-one-dimensional Fermi surfaces as well as one three dimensional component. The obtained density of states near the Fermi level show great Mo-4d orbitals character, in particular the d{sub z{sup 2}}, d{sub xy} and d{sub x{sup 2}−y{sup 2}} orbitals. Our calculations show that A{sub 2}Mo{sub 3}As{sub 3} share great similarity in electron properties with extensively studied A{sub 2}Cr{sub 3}As{sub 3}, indicating that A{sub 2}Mo{sub 3}As{sub 3} are probably another family of unconventional quasi-one-dimensional superconductors.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Corrosion sensitivity of nickel-based Alloy Inconel 600 in pressurized water reactor water chemistry: Can KOH replace LiOH?

Lithium hydroxide (LiOH) has been used to balance water acidity against boric acid moderators in the primary water of Western pressurized water reactor (PWR) designs for decades. However, the demand and the cost of lithium-7 has grown significantly since 2015. Potassium hydroxide (KOH) has been identified as a suitable and cost-effective substitute for LiOH and has been used successfully in Russian PWR designs for more than 40 years. However, it is important to know if alloys and water conditions used in Western PWR’s (Alloy 600) are similarly compatible with KOH additions. This work is focused on the aqueous corrosion behaviors of Alloy 600 with LiOH versus KOH additions at normal operating concentrations and crevice water chemistry at simulated PWR primary water conditions. TEM was used to characterize the formed oxide through diffraction analysis; SIMS was used to probe the cation ingress into the material; Atom probe tomography was used to determine the 3D elemental distribution within the oxide/metal structures; finally electrochemical impedance spectroscopy was used to discuss the structure and corrosion resistance of the oxide films. These advanced characterization techniques complement the weight measurments which showed lower mass gain in KOH than LiOH crevice water due to less oxide formation. Overall, the use of KOH as a potential alternative to LiOH in PWR is discussed.

Alloy 600↗

The Structural, Electronic, and Magnetic Properties of Binary Heusler Alloys ZCl{sub 3} (Z = Li, Na, K, Rb) with DO{sub 3}-Type Structure from First Principle Calculations

The structural, electronic, and magnetic properties of binary Heusler alloys ZCl{sub 3} (Z = Li, Na, K, Rb) with DO{sub 3}-type structure have been studied by means of the first principle calculations. The calculated results reveal that all four alloys are half-metallic (HM) materials at the stable ferromagnetic ground state. The total magnetic moments (M{sub t}) of LiCl{sub 3}, NaCl{sub 3}, KCl{sub 3,} and RbCl{sub 3} alloys are all 2.000 μ{sub B}/f.u., following the Slater-Pauling rule M{sub t} = 24 − Z{sub t} for the former two alloys, while satisfying the Slater-Pauling rule M{sub t} = 30 − Z{sub t} for the latter two alloys. The spin-up band gaps of the binary Heusler alloys ZCl{sub 3} (Z = Li, Na, K, Rb) are 5.598, 5.687, 6.744, and 6.745 eV at equilibrium lattice constants 7.076, 7.237, 7.588, and 7.819 Å, respectively. The positive cohesion energy and negative formation energy indicate that they are thermodynamically stable. Moreover, wide HM regions for binary Heusler alloys ZCl{sub 3} (Z = Li, Na, K, Rb) show their HM characters are robust when the lattices are expanded or compressed under uniform and tetragonal strains. Finally, the total charge density, magnetic charge density, and charge density difference of the (110) plane for LiCl{sub 3} alloy are analyzed in detail.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Vertical and Lateral Etch Survey of Ferroelectric AlN/Al 1-x Sc x N in Aqueous KOH Solutions

Due to their favorable electromechanical properties, such as high sound velocity, low dielectric permittivity and high electromechanical coupling, Aluminum Nitride (AlN) and Aluminum Scandium Nitride (Al 1-x Sc x N) thin films have achieved widespread application in radio frequency (RF) acoustic devices. The resistance to etching at high scandium alloying, however, has inhibited the realization of devices able to exploit the highest electromechanical coupling coefficients. In this work, we investigated the vertical and lateral etch rates of sputtered AlN and Al 1-x Sc x N with Sc concentration x ranging from 0 to 0.42 in aqueous potassium hydroxide (KOH). Etch rates and the sidewall angles were reported at different temperatures and KOH concentrations. We found that the trends of the etch rate were unanimous: while the vertical etch rate decreases with increasing Sc alloying, the lateral etch rate exhibits a V-shaped transition with a minimum etch rate at x = 0.125. By performing an etch on an 800 nm thick Al 0.875 Sc 0.125 N film with 10 wt% KOH at 65 °C for 20 min, a vertical sidewall was formed by exploiting the ratio of the {$10\overline{11}$ planes and {$1\overline{1}00$ planes etch rates. This method does not require preliminary processing and is potentially beneficial for the fabrication of lamb wave resonators (LWRs) or other microelectromechanical systems (MEMS) structures, laser mirrors and Ultraviolet Light-Emitting Diodes (UV-LEDs). It was demonstrated that the sidewall angle tracks the trajectory that follows the {$\overline{1}2\overline{12}$ of the hexagonal crystal structure when different c/a ratios were considered for elevated Sc alloying levels, which may be used as a convenient tool for structure/composition analysis.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

H-Canyon Flowsheet for the Neutralization of Dissolved Fast Critical Assembly (FCA) Fuel

The H-Canyon facility will be dissolving unirradiated stainless-steel clad Fast Critical Assembly (FCA) fuel in HNO3 and neutralizing the resulting solution with 50 wt% NaOH with no recovery operations prior to transfer to the Concentration, Storage, and Transfer Facility (CSTF). There are two types of FCA fuel, including a Pu-Al metal alloy and a mixed U and Pu oxide. H-Canyon anticipates dissolving 16 batches of the metal fuel and two batches of the oxide fuel. Potassium fluoride will be added to the dissolver solution at 0.05 M to promote dissolution. Gadolinium will be added after the dissolution as a thermal neutron poison for criticality control. H-Canyon requested that SRNL evaluate Gd:239Pu equivalent (239PuEq) ratios of 1:1 and 10:1. The neutralization process precipitates metals including actinides, Gd, and cladding components resulting in a slurry. Caustic neutralization is a routine H-Canyon operation, but the FCA dissolver solution will be unique relative to solutions that are typically processed due to the stainless-steel components, high HNO3 concentration of ~8.5 M, and an initial Pu concentration of up to 4 g/L. Previous neutralization studies have been performed for Pu containing solutions but at less than half the initial Pu concentration and much lower initial HNO3 concentrations. Experimental neutralizations targeted a final free hydroxide (OH-) concentration of 0.6 M as this was anticipated to be the final endpoint, but H-Canyon now expects the endpoint to be 1.2 M OH-. The purpose of this study was to characterize the distribution of the actinide, Gd, and cladding components between the precipitate and supernate, determine if the slurry will back up in the header during the transfer to the CSTF, and determine if solids will settle in the pipeline during the transfer.

Mills, Matthew S.↗

Application of the Solute-Solvent EMF Cell to Measure Activity of NiF 2 in Molten FLiNaK

Electromotive force (emf) measurements made using a combination of solute- and solvent-based electrodes were used to determine the activity of NiF 2 in molten FLiNaK eutectic at 823 K across a concentration range of x NiF2 = 5.2 × 10 –4 –1.0 × 10 –2 . The solute emf values were measured using electrodes consisting of Ni wires immersed in FLiNaK with dissolved NiF 2 contained in graphite crucibles. The measured emf values were then converted to the FLiNaK Eutectic Potassium Electrode (FEKE) potential and used to quantify the activity of dissolved NiF 2 . This quantification was based upon comparative measurements of a reference solvent electrode consisting of a K-Bi alloy immersed in pure FLiNaK contained in a boron nitride crucible and a solute electrode. Short cell lives were characteristic of the measurements due to the corrosive nature of the fluoride salts. Quantifying the activity of NiF 2 will improve the utility of Ni 2+ /Ni reference electrodes in molten fluoride salts, which are notoriously difficult electrolytes to work with because of their reactivity. In conclusion, this work demonstrates the general nature of the solute-solvent approach as a repeatable, easily employed method for measuring the activity values of electroactive species in a variety of molten salts to improve understanding of the electroactive species behavior in these systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Challenges and Development of Tin-Based Anode with High Volumetric Capacity for Li-Ion Batteries

Abstract The ever-increasing energy density needs for the mass deployment of electric vehicles bring challenges to batteries. Graphitic carbon must be replaced with a higher-capacity material for any significant advancement in the energy storage capability. Sn-based materials are strong candidates as the anode for the next-generation lithium-ion batteries due to their higher volumetric capacity and relatively low working potential. However, the volume change of Sn upon the Li insertion and extraction process results in a rapid deterioration in the capacity on cycling. Substantial effort has been made in the development of Sn-based materials. A SnCo alloy has been used, but is not economically viable. To minimize the use of Co, a series of Sn–Fe–C, Sn y Fe, Sn–C composites with excellent capacity retention and rate capability has been investigated. They show the proof of principle that alloys can achieve Coulombic efficiency of over 99.95% after the first few cycles. However, the initial Coulombic efficiency needs improvement. The development and application of tin-based materials in LIBs also provide useful guidelines for sodium-ion batteries, potassium-ion batteries, magnesium-ion batteries and calcium-ion batteries. Graphic Abstract

25 ENERGY STORAGE↗

Lessons Learned—Lithium Silicide Hydration Fire

Alkali metals, such as lithium, sodium, potassium, etc., are highly reactive elements. While researchers generally handle these metals with caution, less caution is taken when these elements have been “reacted”. In this work, a recent incident is examined in which a pair of researchers ignited a lithium silicide alloy sample that was assumed to be fully hydrated to lithium hydroxide and, thereby, no longer water-reactive. However, variations in the original chemical composition of the lithium compounds examined resulted in select mixtures failing to hydrate and react completely to lithium hydroxide in the time frame allowed. This gave rise to residual unreacted, water-sensitive lithium silicide which resulted in a violent exothermic reaction with water and autoignition of the produced hydrogen gas. This Article describes this incident and improvements that can be implemented to prevent similar incidents from occurring.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Role of Cation Ordering on Device Performance in (Ag,Cu)InSe 2 Solar Cells with KF Post-Deposition Treatment

CuInSe 2 (CIS) has been proposed as an attractive bottom cell candidate in tandem solar cells. However, to justify the coupling with high-performance top cells (e.g., perovskites, GaAs), significant work on improving the efficiency is required. To this extent, several authors have demonstrated the benefits of alkali post-deposition treatments (PDT) to increase device open-circuit voltage (V oc ) in CIS and how Ag alloying - (Ag,Cu)InSe 2 (ACIS) - reduces defect density and enhances current collection in devices. Herein, we present a detailed study of the role that KF-PDT plays on CIS and ACIS absorber composition and structure, and propose an explanation for the decreased V oc observed when silver and potassium coexist in the system (ACIS + KF). Through a suite of synchrotron-based techniques, we investigate the nanoscale chemical distribution of the films and the formation of secondary phases. Through photoluminescence imaging, we observed a high degree of passivation with the addition of KF, and synchrotron-based X-ray diffraction confirmed the absence of a KInSe 2 surface layer usually considered to be a passivating agent. Raman spectroscopy and synchrotron X-ray fluorescence show the increased presence of Cu- and Se-poor clusters in ACIS + KF, which are correlated to significantly reduced X-ray beam-induced current (XBIC). An increase in the intensity of the E/B 2 stretching mode of CIS is attributed to cation ordering near the junction and is found to track inversely to bulk V oc measurements. The cation ordering is hypothesized to arise from the formation and redistribution of defects that normally occur near the surfaces of CIS as a consequence of its polar character. Here, these defects compensate each other, and the overall inhomogeneity of the charge distribution generates electrostatic potential fluctuations that greatly increase the saturation current and hence reduce the open-circuit voltage of the device.

36 MATERIALS SCIENCE↗

Large-Area (Ag,Cu)(In,Ga)Se 2 Thin-Film Solar Cells with Increased Bandgap and Reduced Voltage Losses Realized with Bulk Defect Reduction and Front-Grading of the Absorber Bandgap

The 1.24 eV bandgap, 18.8% power conversion efficiency Ag-alloyed chalcopyrite (Ag,Cu)(In,Ga)Se 2 (ACIGS) solar cells are characterized to relate voltage and efficiency improvements to electro-optical (EO) characteristics. Shockley-Read-Hall recombination center defect density, identified and characterized through deep level transient spectroscopy and time-resolved photoluminescence (TRPL), is reduced through potassium and copper treatment optimization. Concomitantly, longer minority carrier lifetimes are achieved, which increases open-circuit voltage (V OC ). Near-conduction band defects associated in earlier studies with light-induced current instability are also mitigated. Analysis of charge-carrier dynamics after single- and two-photon excitation is used to separate recombination at the front interface and in the absorber bulk. From TRPL decay simulations, the authors estimate ranges of key solar cell material characteristics: bulk carrier lifetime T bulk = 110-210 ns, charge-carrier mobility u = 110-160 cm 2 V -1 s -1 , and front interface recombination velocity S front = 700-1050 cm s -1 . This lowest-reported S front for ACIGS absorbers originates from the notched conduction band grading, which also makes the impact of the back interface recombination negligible. It is suggested in the results that solar cell performance enhancements can be made most readily with two distinct strategies: improving device architecture and reducing semiconductor defect densities. Using these approaches, power conversion efficiency in large-area solar cells is improved by 1.1% absolute.

14 SOLAR ENERGY↗

Design strategies for nonaqueous multivalent-ion and monovalent-ion battery anodes

The inability of current battery technologies to keep up with the performance requirements of industry is pushing forward developments in electrochemistry. Specifically, the battery's negative electrode, the anode, presents many unique chemical, physical and engineering challenges. Lithium-based battery technologies have dominated the past decade, but concerns about the limited supply of lithium in the Earth's crust have led researchers to look towards alternative metal-ion technologies. Furthermore, various alkali metals (such as sodium and potassium) and alkali earth metals (such as magnesium and calcium) have attracted significant research interest. In this Review, we analyse these technologies in a coherent manner, addressing the problems of each type of anode, rather than those of specific types of metal-ion batteries. Covering direct metal plating and stripping, intercalation-based, alloy-based and conversion-reaction-based anode technologies, this analysis will offer the reader a comprehensive understanding of the behaviour of different metal-ion anodes and of what can be learned by transferring knowledge between these different systems. Increasing demand for energy-storage systems will inevitably stress the Earth's lithium supply; thus, the research focus is shifting towards other alkali and alkali earth metals. In summary, this Review compares and connects strategies to enable different multivalent and monovalent metal-ion battery anodes, including metal anodes and intercalation-based, alloy-based and conversion-reaction-based anodes.

36 MATERIALS SCIENCE↗

Kinetics of Radiation-induced Cr( II ) and Cr( III ) Redox Chemistry in Molten LiCl-KCl Eutectic

Chromium (Cr) is a frequent constituent of the metal alloys proposed for molten salt nuclear reactor (MSR) applications, and is typically the least noble metal ion present. Consequently, chromium is preferentially corroded into molten salt solutions. Here, the redox poise and redox cycling of chromium ions in the salt can greatly influence its corrosivity towards structural alloys, ultimately impacting the longevity of MSR systems. Radiation-induced chemistry is expected to play a significant role in determining the chromium oxidation state distribution during MSR operations. In the present research, electron pulse radiolysis techniques were employed to characterize the reactivity of Cr(II) and Cr(III) ions with primary radiolysis products in molten lithium chloride–potassium chloride (LiCl–KCl) eutectic over a temperature range of 400–600 °C. Both chromium oxidation states were found to rapidly react with the primary products of molten chloride salt radiolysis, i.e., the solvated electron (e S - ) and the dichlorine radical anion (Cl 2 ˙ - ). For reactions with the e S - , second-order rate coefficients (k) of k = (4.1 ± 0.2) and (6.1 ± 0.3) × 10 10 M -1 s -1 at 400 °C for Cr(II) and Cr(III), respectively, were determined. Temperature-dependent measurements allowed for the derivation of activation parameters for electron capture by Cr(II) and Cr(III). Both chromium ions also react with Cl 2 ˙ - , k = (7.2 ± 0.3) and (1.4 ± 0.1) × 10 9 M -1 s -1 at 400 °C for Cr(II) and Cr(III), respectively.

37 - INORGANIC, ORGANIC, PHYSICAL AND ANALYTICAL C↗

Electrolytes and metal hydride batteries

Metal hydride batteries comprising an electrolyte composition which comprises an aqueous solution comprising potassium hydroxide (KOH) and one or more halide and/or oxyacid salts exhibit reduced degradation of the anode material during operation. The salts are for instance alkali metal salts. Anode materials exhibit for instance <100 % of the degradation of the same anode material in the same battery when replacing the electrolyte composition with 30 weight percent (wt %) aqueous KOH and the conductivity of the electrolyte composition is for instance ≥85 % of 30 wt % aqueous KOH. Anode materials are for example ABx high capacity hydrogen storage alloys comprising Mg where x is from about 0.5 to about 5 and which has a discharge capacity of ≥400 mAh/g.

25 ENERGY STORAGE↗

Cesium Removal from Surrogate Pyroprocessing Salt by Electrodeposition

Active metals in used nuclear fuel dissolve into the salt during pyroprocessing and are not removed by electrorefining or drawdown operations. The buildup of 137 Cs over time increases the heat load and ionizing radiation level of the salt such that it must be replaced frequently, resulting in a significant amount of salt waste. An effective means of managing cesium in the molten salt electrolyte would increase the efficiency of pyroprocessing and decrease the volume of salt waste requiring disposal. A previous report summarized issues that must be addressed when developing a removal strategy and assessed the suitability of existing methods and remaining technological gaps to their application (Rose and Thomas 2023). Cesium is extremely stable in molten salt as a chloride—even more stable than the LiCl-KCl eutectic base salt used for pyroprocessing fuel—which makes removing cesium a challenge. However, sufficiently strong atomic interactions occur between active metal species and liquid metals that make the electrodeposition of active metal fission products into liquid metal electrodes energetically favorable. The feasibility of recovering cesium from LiCl-KCl pyroprocessing salt through electrodeposition into liquid metals is eing assessed by identifying potentially effective liquid metals and performing tests to determine the effectiveness of electrodepositing cesium from a LiCl/KCl salt into these liquid metals. Previous studies investigating the electrodeposition of Sr 2+ , and Ba 2+ into zinc, cadmium, bismuth, lead, tin and antimony have shown that alkali and alkaline earth metals can be electrodeposited at liquid metal cathodes (Kim et al., 2018). The removal of Ba 2+ and Sr 2+ was measured to be more efficient than the removal of monovalent cations due to the greater thermochemical driving force for alloying those elements with the liquid metal (Jang et al. 2022). Because the equilibrium potentials are dependent on the interactions of the active metal in the liquid metal, it is likely that the other alkali metals Li + , and K + , will deposit from LiCl/KCl salt with the Cs + . Therefore, application of this method to recover active metals from pyroprocessing salt will benefit from the use of a liquid metal and set of operating conditions that sufficiently increase the reduction potential of cesium to remove cesium from the waste salt with an acceptable amount of co-deposited lithium and potassium.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Quantifying the reaction mechanisms of a high-capacity CuP 2 /C composite anode for potassium ion batteries

Introducing metals into phosphorus to form metal phosphide materials as anodes for potassium ion batteries (PIBs) is an effective strategy to improve the electronic conductivity and alleviate the volume change during cycling, although with a compromise of capacity. Here in this paper, we explore a CuP 2 /C composite as a novel anode for PIBs, which delivers a high reversible capacity of >450 mA h g -1 . Unexpectedly, our results reveal that the POx components existing in the prepared composite are reversible, through a quantitative analysis via high-resolution solid-state 31 P NMR and synchrotron X-ray diffraction tests. Their potassiation products K 3 PO 4 and K 4 P 2 O 7 can react with K–P alloys and turn back to PO x during depotassiation, which probably accounts for the high capacity of the prepared material. The results also illustrate a crystallization–amorphization evolution process during cycling involving nanocrystalline α-K 4 P 6 , K 4 P 3 and KP, and amorphous K 4 P 6 , KP and K 3 P phases, among which, the amorphous phases are identified for the first time.

25 ENERGY STORAGE↗

Accelerated Testing of Selected Filler Compositions

The fillers R&D program, mostly experimental, is part of a broader R&D program that includes new process modeling and performance assessment of criticality effects and the overall importance of criticality to repository performance (consequence screening). A literature research and consultation effort with experts by Hardin and Brady (2018) identified several potentially effective and workable filler materials including cements (primarily phosphate based), molten-metal alloys, and low-temperature glasses. Filler attributes were defined and the preliminary lists were compared qualitatively. Further comparative analysis will be done (e.g., cost estimates) after experimental screening has narrowed the list of alternatives. The following cement filler compositions were selected for experimental development work and accelerated testing in FY19: Aluminum phosphate cements (APCs); more specifically aluminum oxide / aluminum phosphate (Al 2 O 3 / AlPO 4 ) cements in which Al 2 O 3 serves as the filler material bound by an AlPO 4 binder formed by the reaction of Al 2 O 3 with H 3 PO 4 ; Calcium phosphate cements (CPCs); more specifically composed of pure or nearly pure hydroxyapatite (Ca 5 (PO 4 ) 3 (OH)); Magnesium potassium phosphate cements (MKPs) composed of magnesium oxide / magnesium potassium phosphate (MgO / MgKPO 4 ) cements in which MgO serves as the filler and MgKPO 4 serves as the binder formed by the reaction of MgO with monopotassium phosphate (KH 2 PO 4 ) and tricalcium phosphate ((Ca 3 (PO 4 ) 2 ); Two additional potential cement materials were explored preliminarily as the result of: (1) continued literature investigations into other filler candidates (wollastonite-based phosphate ceramic) and (2) the experimental discovery of a well-consolidated fly ash phosphate cement during the evaluation of fly ash as a potential filler material with Al 2 O 3 in APCs. Fly ash phosphate cements, more specifically in which a fly ash material composed primarily of mullite and quartz serves as the filler and is reacted with H 3 PO 4 to form amorphous phosphate phase(s) as the binder; Wollastonite aluminum phosphate cements (WAPC), specifically wollastonite / aluminum phosphate (CaSiO 3 / AlPO 4 ) in which CaSiO 3 serves as the filler material and AlPO 4 serves as the binder formed by Al(OH) 3 or metakaolin as Al sources and H 3 PO 4 or ammonium dihydrogen phosphate (ADP) (NH 4 H 2 PO 4 ) as phosphate sources. The FY19 effort focused on the optimization of compositions and subsequent processing of these five materials to achieve dense and well-consolidated monolithic samples with relatively low porosity. Once these goals were met basic material properties screening evaluations were performed including an assessment of dissolution resistance in water at elevated temperature (200 °C) and mechanical testing including unconfined compressive strength (UCS) testing. To date, the aluminum phosphate cements (APCs) appear to show the most promise for continued development. They are easily prepared and form smooth pourable slurries that remain stable for days with relatively low viscosities of several thousand centipoise (cP). They are then set at elevated temperatures (e.g., 170 °C) under ambient (0.1 MPa) or elevated pressure (~1MPa). Overall, they demonstrate the best dissolution resistance in water at elevated temperature (200 °C) and good compressive strengths. However, additional effort is required to optimize the APC slurry formulations and the process used for thermal curing these materials. The calcium phosphate cements (CPCs) can be formed at room temperature to produce a well-consolidated body. However, their slurry viscosities are very high (and difficult to measure) and they exhibit relatively short cure times of 2 to 3 hours. Also, dissolution resistance is very poor, the poorest of all the cements examined The same is the case for the small number of MKP cements fabricated; they cure very quickly (10 minutes or less) and disintegrate within a few hours upon immersion in distilled water. Surprisingly, fly ash reacts with phosphoric acid to form dense and well-consolidated cements but the mixture rapidly sets at room temperature (less than 30 minutes) and the subsequent conversion of the binder to an amorphous phosphate phase(s) as a function of temperature is complicated. Finally, the wollastonite aluminum phosphate cements (WAPC) are easily prepared and form smooth pourable slurries that remain stable for several hours. They are then set at 130 °C. A WAPC sample exhibited the highest compressive strengths of all the materials we evaluated but in general their dissolution resistance to water is poor.

36 MATERIALS SCIENCE↗