Multi-Layer Laminated Thin Films for Inflatable Structures

Special-purpose balloons and other inflatable structures would be constructed as flexible laminates of multiple thin polymeric films interspersed with layers of adhesive, according to a proposal. In the original intended application, the laminate would serve as the envelope of the Titan Aerobot a proposed robotic airship for exploring Titan (one of the moons of Saturn). Potential terrestrial applications for such flexible laminates could include blimps and sails. In the original application, the multi-layered laminate would contain six layers of 0.14-mil (0.0036-mm)-thick Mylar (or equivalent) polyethylene terephthalate film with a layer of adhesive between each layer of Mylar . The overall thickness and areal density of this laminate would be nearly the same as those of 1-mil (0.0254-mm)-thick monolayer polyethylene terephthalate sheet. However, the laminate would offer several advantages over the monolayer sheet, especially with respect to interrelated considerations of flexing properties, formation of pinholes, and difficulty or ease of handling, as discussed next. Most of the damage during flexing of the laminate would be localized in the outermost layers, where the radii of bending in a given bend would be the largest and, hence, the bending stress would be the greatest. The adverse effects of formation of pinholes would be nearly completely mitigated in the laminate because a pinhole in a given layer would not propagate to adjacent layers. Hence, the laminate would tend to remain effective as a barrier to retain gas. Similar arguments can be made regarding cracks: While a crack could form as a result of stress or a defect in the film material, a crack would not propagate into adjacent layers, and the adjacent layer(s) would even arrest propagation of the crack. In the case of the monolayer sheet, surface damage (scratches, dents, permanent folds, pinholes, and the like) caused by handling would constitute or give rise to defects that could propagate through the thickness as cracks or pinholes that would render the sheet less effective or ineffective as a barrier. In contrast, because damage incurred during handling of the laminate would ordinarily be limited to the outermost layers, the barrier properties of the laminate would be less likely to be adversely affected. Therefore, handling of the laminate would be easier because there would be less of a need to exercise care to ensure against surface damage.

Yavrouian, Andre↗

Morphology of PET, part II

Morphology of polyethylene terephthalate studied, emphasizing morphology of glass and effect of strain induced crystallization of polymer

POLYETHYLENE TEREPHTHALATE↗

Infrared radiation of thin plastic films.

A combined analytical and experimental study is presented for infrared radiation characteristics of thin plastic films with and without a metal substrate. On the basis of the thin-film analysis, a simple analytical technique is developed for determining band-averaged optical constants of thin plastic films from spectral normal transmittance data for two different film thicknesses. Specifically, the band-averaged optical constants of polyethylene terephthalate and polyimide were obtained from transmittance measurements of films with thicknesses in the range of 0.25 to 3 mil. The spectral normal reflectance and total normal emittance of the film side of singly aluminized films are calculated by use of optical constants; the results compare favorably with measured values.

Tien, C. L.↗

Testing of flat conductor cable to Underwriters Laboratory standards UL719 and UL83

The flat conductor cable (FCC) which was tested consisted of three AWG No. 12 flat copper conductors laminated between two films of polyethylene terephthalate (Mylar) insulation with a self-extinguishing polyester adhesive. Results of the tests conducted on this cable, according to specifications, warrants the use of this FCC for electrical interconnections in a surface nonmetallic protective covering.

Loggins, R. W.↗

Testing flat-conductor cable

Report describes characteristics of type of FCC which consists of three AWG No. 12 flat copper conductors laminated between two films of polyethylene terephthalate (Mylar) insulation with self-extinguishing polyester adhesive.

Loggins, R. W.↗