Study on effects of powder and flake chemistry and morphology on the properties of Al-Cu-Mg-X-X-X powder metallurgy advanced aluminum alloys

A study was conducted: (1) to develop rapid solidification processed (RSP) dispersoid-containing Al-3Cu-2Li-1Mg-0.2Zr alloys as substitutes for titanium alloys and commercial 2XXX aluminum alloys for service to at least 150 C; and (2) to develop RSP Al-4Li-Cu-Mg-Zr alloys as substitutes for high-strength commercial 7XXX alloys in ambient-temperature applications. RSP Al-3Cu-2Li-1Mg-0.2Zr alloys have density-normalized yield stresses at 150 C up to 52% larger than that of 2124-T851 and up to 30% larger than that of Ti-6Al-4V. Strength at 150 C in these alloys is provided by thermally stable delta' (Al3Li), T1 (Al2LiCu), and S' (Al2CuMg) precipitates. Density-normalized yield stresses of RSP Al-3Cu-2Li-1Mg-0.2Zr alloys are up to 100% larger than that of 2124-T851 and equivalent to that of Al-8Fe-4Ce at 260 C. Strength in the RSP alloys at 260 C is provided by incoherent dispersoids and subboundary constituent particles such as T1 and S. The RSP alloys are attractive substitutes in less than or = 100-h exposures for 2xxx and Al-4Fe-Ce alloys up to 260 C and for titanium alloys up to 150 C. RSP Al-4Li-Cu-Mg-Zr alloys have ambient-temperature yield and ultimate tensile stresses similar to that of 7050-T7651, and are 14% less dense. RSP Al-4Li-0.5Cu-1.5Mg-0.2Zr has a 20% higher specific yield stress, 40% higher specific elastic modulus, and superior corrosion resistance compared to the properties of 7050-T7651. Strength in the Al-4Li-Cu-Mg-Zr alloy class is primarily provided by the substructure and delta' precipitates and is independent of Cu:Mg ratio. Improvements in fracture toughness and transverse-orientation properties in both alloy classes depend on improved melt practices to eliminate oxide inclusions which are incorporated into the consolidated forms.

Meschter, P. J.↗

Metallurgy and properties of plasma spray formed materials

Understanding the fundamental metallurgy of vacuum plasma spray formed materials is the key to enhancing and developing full material properties. Investigations have shown that the microstructure of plasma sprayed materials must evolve from a powder splat morphology to a recrystallized grain structure to assure high strength and ductility. A fully, or near fully, dense material that exhibits a powder splat morphology will perform as a brittle material compared to a recrystallized grain structure for the same amount of porosity. Metallurgy and material properties of nickel, iron, and copper base alloys will be presented and correlated to microstructure.

Mckechnie, T. N.↗

Investigation of Mechanical Properties of Parts Fabricated with Gas- and Water-Atomized 304L Stainless Steel Powder in the Laser Powder Bed Fusion Process

In this report the use of gas-atomized powder as the feedstock material for the Laser Powder Bed Fusion (L-PBF) process is common in the Additive Manufacturing (AM) community. Although gas-atomization produces powder with high sphericity, its relatively expensive production cost is a downside for application in AM processes. Water atomization of powder may overcome this limitation due to its low cost relative to the gas-atomization process. In this work, gas- and water-atomized 304L stainless steel powders were morphologically characterized through Scanning Electron Microscopy (SEM). The water-atomized powder had a wider particle size distribution and exhibited less sphericity. Measuring powder flowability using the Revolution Powder Analyzer (RPA) indicated that the water-atomized powder had less flowablility than the gas-atomized powder. Through examining the mechanical properties of L-PBF fabricated parts using tensile tests, the gas-atomized powder had significantly higher yield tensile strength and elongation than the water-atomized powder, however, their ultimate tensile strengths were not significantly different.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Laser Additive Manufacturing Process Development for Bismuth Telluride Thermoelectric Material

Thermoelectric generators have strong potential for aerospace and aircraft applications. However, traditional manufacturing methods for thermoelectric devices severely limit device adaptability and consequently marketability. Laser powder bed fusion is an additive manufacturing method which shows promising potential for producing thermoelectric devices. Thermoelectric materials pose unique challenges compared to metals because of low thermal conductivity, brittle fracture characteristics, and irregular powder particle morphologies. Herein, we communicate processing procedures to fabricate thermoelectric parts of Bi 2 Te 3 through laser powder bed fusion. In this study, we identify the successful combination of key process parameters—laser power, scan speed, hatch distance, and powder layer thickness—to achieve high-quality parts in terms of density and physical properties, and we demonstrate the impact of process parameter variation on built part quality. While it cannot exclusively determine part quality, the volumetric energy density is a useful guide in deciding process parameters for thermoelectric materials, and the optimal value is between 9 and 11 J/mm 3 for Bi 2 Te 3 . We demonstrate successful fabrication of different freeform geometries of Bi 2 Te 3 powders. The results suggest it is possible to extend this method more broadly to other semiconductor materials, including thermoelectric power generation materials applicable for space applications.

36 MATERIALS SCIENCE↗

Manufacturing Bulk Nanocrystalline Al-3Mg Components Using Cryomilling and Spark Plasma Sintering

In the current study, pure aluminum (Al) powders were cryomilled with and without 3 wt.% pure magnesium (Mg) dopant for varying durations followed by spark plasma sintering (SPS) of powders to prepare bulk components with superior mechanical properties. The crystallite sizes were determined for powders and the bulk components by analyzing the X-ray diffraction (XRD) spectrum. The calculations indicated a reduction in crystallite size with the increase in the cryomilling duration. The results also showed a more significant decrease in the crystallite sizes for Al-3Mg samples than that of pure Al. The changes in the surface morphology of powders were characterized using scanning electron microscopy (SEM). The elemental mapping analysis at nanoscale was carried out using Energy-dispersive X-ray spectroscopy (EDX) in Scanning transmission electron microscopy (STEM). The mechanical properties of the bulk components were assessed using a Vickers Microhardness tester. The test results demonstrated an improvement in the hardness of Mg-doped components. Higher hardness values were also reported with an increase in the cryomilling duration. This article discusses the mechanisms for the reduction in crystallite size for pure Al and Al-3Mg and its subsequent impact on improving mechanical properties.

36 MATERIALS SCIENCE↗

Particle Morphology Effects on Flow Characteristics of PS304 Plasma Spray Coating Feedstock Powder Blend

The effects of BaF2-CaF 2 particle morphology on PS304 feedstock powder flow ability have been investigated. BaF2-CaF2 eutectic powders were fabricated by comminution (angular) and by gas atomization (spherical). The fluoride powders were added incrementally to the other powder constituents of the PS304 feedstock: nichrome, chromia, and silver powders. A linear relationship between flow time and concentration of BaF2-CaF2 powder was found. Flow of the powder blend with spherical BaF2-CaF2 was better than the angular BaF2-CaF2. Flow ability of the powder blend with angular fluorides decreased linearly with increasing fluoride concentration. Flow of the powder blend with spherical fluorides was independent of fluoride concentration. Results suggest that for this material blend, particle morphology plays a significant role in powder blend flow behavior, offering potential methods to improve powder flow ability and enhance the commercial potential. These findings may have applicability to other difficult-to-flow powders such as cohesive ceramics.

Stanford, Malcolm K.↗

Elucidating the effect of preheating temperature on melt pool morphology variation in Inconel 718 laser powder bed fusion via simulation and experiment

In laser powder bed fusion (L-PBF) additive manufacturing, the mechanical performance, microstructure and defects of fabricated parts are closely associated with the melt pool morphology, e.g., its dimension and shape through the building process. Past studies have largely focused on how the process parameters such as laser power and scan speed affect melt pool characteristics. In this study, the melt pool morphology variation as a function of preheating temperature in the conduction, transition, and keyhole regimes and the underlying mechanisms in each regime are investigated through ex-situ sample characterization and computation thermal fluid dynamics (CtFD) simulation. Single tracks with different combinations of laser power and scan speed are deposited on an Inconel 718 bare plate preheated to a temperature range of 100–500 °C in the experiment. Significant changes are observed in melt pool morphology as a function of preheating temperature from optical measurements of melt track cross sections. The depth of melt pool in the three regimes increases monotonically with preheating temperature, e.g., at 500 °C, the experimental melt pool depth is increased by 49% in conduction regime, 34% in transition regime and 33% in keyhole regime, respectively, while the variation of melt pool width in each regime does not all follow an increasing trend but depends on the melt pool regimes. Melt pool width variation in the conduction and transition regimes is found to depend on the enhanced heat conduction directly related to temperature dependent thermal properties. Through validated CtFD simulations, it is found that in the keyhole regime the evaporation mass, recoil pressure, and laser drilling effect is enhanced with higher preheating temperature, which gives rise to a deeper melt pool. The simulations also reveal that preheating temperature significantly elongates the melt track length due to the increased flow rate and strong recoil pressure that accelerates the backward flow.

36 MATERIALS SCIENCE↗

A Simulated Evaluation of Powder Flowability Through a Partially Obstructed Consumable in Blown Powder Directed Energy Deposition Systems

Abstract In the interest of continued industrialization of metal additive manufacturing in modern production environments, cost is often referenced as a primary deterrent to new adopters. Conventional economic models for additive systems, processes, and supply chains often focus on specific process applications with little generalizability, or they neglect significant costs associated with production such as machine maintenance and consumable part replacement. Compounding the latter issue are substantial knowledge gaps in consumable part wear characterization for additive and other convergent manufacturing systems. In coaxial blown powder directed energy deposition systems, gas atomized metal powder is wasted during material deposition at a rate that is partly dependent on present wear phenomena in a consumable nozzle housed in the cladding head assembly. The price and lead time required to replace the nozzle incentivizes its reuse even when visibly worn. Often this initiates a process quality decline in the form of underbuilt geometry and internal defects due to losses in powder catchment efficiency. While depositing H13 steel using a hybrid manufacturing machine tool equipped with such a deposition system, a unique partial clog with a bridge-like structure formed at the consumable nozzle exit when supporting argon gas flows failed mid-process. To further understand coaxial multi-phase powder flow in the event of support gas failure, a computational fluid dynamics simulation is tailored to relevant process parameters, H13 powder material profile, and machine operator observations collected after the incident. The resulting differences in powder flow compared to control gas flow parameters is presented and discussed. The powder flowability and performance of the clogged nozzle is then assessed by using an optical profilometer to extract the profile of the clog and recreate the clog geometry within the simulation environment. In past work this simulation has been experimentally validated for a 316L steel powder material profile and used specifically for analyzing powder stream geometry and catchment efficiency. After the initial powder flow characterization, the clog is removed, and the nozzle is reprofiled. After removing the obstructing clog, the newly unobstructed nozzle geometry, the original off the shelf nozzle geometry, and additional nozzle profiles exploring different consumable refurbishment strategies are reevaluated in the simulation. Powder catchment efficiency for all variant nozzle geometries and relevant flow variables are compared and discussed, along with potential mitigation strategies for optimizing powder flowability with worn consumables. This work expands on the known morphology of blown powder obstructions and wear defects present in consumable coaxial nozzles while discussing pragmatic simulation driven responses to unanticipated subsystem failure in hybrid manufacturing machining platforms.

DeWitte, Lisa↗

Combustion Synthesis of Sm0.5Sr0.5CoO3-x and La0.6Sr0.4CoO3-x Nanopowders for Solid Oxide Fuel Cell Cathodes

Nanopowders of Sm0.5Sr0.5CoO(3-x) (SSC) and La0.6Sr0.4CoO(3-x) (LSC) compositions, which are being investigated as cathode materials for intermediate temperature solid oxide fuel cells, were synthesized by a solution-combustion method using metal nitrates and glycine as fuel. Development of crystalline phases in the as-synthesized powders after heat treatments at various temperatures was monitored by x-ray diffraction. Perovskite phase in LSC formed more readily than in SSC. Single phase perovskites were obtained after heat treatment of the combustion synthesized LSC and SSC powders at 1000 and 1200 C, respectively. The as-synthesized powders had an average particle size of ~12 nm as determined from x-ray line broadening analysis using the Scherrer equation. Average grain size of the powders increased with increase in calcination temperature. Morphological analysis of the powders calcined at various temperatures was done by scanning electron microscopy.

Bansal, Narottam P.↗

Novel structured Sm 0.5 Sr 0.5 CoO 3-δ cathode for intermediate and low temperature solid oxide fuel cells

The performance of solid oxide fuel cell (SOFC) can be significantly enhanced using nanostructured cathode obtained by infiltration/impregnation method. However, this method has been limited due to multi-step preparation process and instability of the obtained nanoscale catalyst under long-term operation. We report here a simple, cost-effective and reproducible approach to fabricate nanostructured Sm 0.5 Sr 0.5 CoO 3-δ (SSC) cathode with enhanced performance and stability. The SSC powders were prepared by a freeze-drying method through a combustion route using Pluronic F-127 as the template. The SSC freeze-drying powders have unique morphology and a significant phase change at 750 °C. The oxygen non-stoichiometry (δ) of the SSC powders is 0.18 at room temperature, while the δ values are 0.66, 0.75 and 0.90 at 600 °C, 700 °C and 800 °C, respectively. The novel structured SSC cathode was prepared by screen-printing and one-step sintering process using the freeze-drying SSC powders. Maximum cell power densities of 0.83 and 1.13 W cm -2 are achieved at 550 °C and 600 °C, respectively for single cells with the novel structured SSC cathode. Moreover, single cells show excellent stability at 600 °C under a current density of 600 mA cm -2 over 250 h. This work expands opportunities to exploit nanotechnology in a wide range of intermediate and low temperature energy conversion devices.

25 ENERGY STORAGE↗

Variations in GARS powder microstructure as a function of powder chemistry and particle size

The properties of metal produced through powder metallurgy depends on the feedstock used. Powders produced via gas atomization reaction synthesis (GARS) are used to produce oxide dispersion strengthened alloys. The desired powder size range can vary for each consolidation technique. However, powder microstructure also can vary with powder particle size, which in turn can impact the microstructure and properties of the consolidated parts. In this study, GARS powders are characterized via inductively coupled plasma mass spectroscopy, inert gas fusion, and high-resolution x-ray diffraction to determine variations in elemental and phase compositions. Transmission electron microscopy was used to understand microstructure variations as a function of chemistry and size. Across the three batches tested intermetallic content was 0.73–1.35 wt% in the 0-20 μm powder batch and increased to 2.46–3.80 wt% in the coarse 45-106 μm batch. Across all batches, volume percent of surface oxidation decreased with powder diameter, with volume percents within the range of 0.75–1.2 % across 10 μm powder particles, and below 0.4 % across coarse powder particles approximately 100 μm in diameter. These observations were supported by inert gas fusion measurements. However, the oxide layer was thicker in coarse powder particles due to a slower cooling rate. Increasing oxygen content in atomization gas to 2000 ppm and adding yttrium increased both the surface oxidation content and yttrium intermetallic content. Lastly, intermetallic phases within the powder coarsened with powder size. Intermetallic morphology changed from fine spherical intermetallic and columnar dendritic growth to a cellular structure with finer spherical intermetallic, to coarse irregular intermetallic and intermetallic along grain boundaries as a result of slower cooling rate and solidification rate in coarse powder particles. Furthermore, the addition of zirconium does not appear to significantly change intermetallic morphology, but the composition changed from a Y-Fe rich intermetallic to a Y-Zr-Fe intermetallic.

42 ENGINEERING↗

Laser pre-sintering for denudation reduction in the laser powder bed fusion additive manufacturing of Ti-6Al-4V alloy

As a fundamentally different process for creation of complex parts, laser powder bed fusion (LPBF) additive manufacturing exhibits complex behavior at the melt pool that has a direct influence on the macroscopic properties of the final material. Powder denudation, a previously studied deleterious phenomenon, is the displacement of powder due to entrainment in a jet of rapidly vaporized metal created by the process laser. To minimize the effect of denudation and inspired by methods in adjacent fields, a laser pre-sintering (LPS) method was studied in an effort to reduce denudation. LPS was found to be most effective in the 1–4 J/mm3 volumetric energy density processing regimes, minimizing the common experimentally observed problems with the LPBF process. Scanning electron microscopy of the LPS-treated powder bed revealed insight into the accelerating effect morphological irregularities along the powder particle surface have in the pre-sintering process. To further understand the process, an estimation of the sintered neck sizes necessary to eliminate denudation in LPS is made, qualitatively affirming the low energy densities needed to prevent denudation. Here, the results presented in this work represent an initial step towards understanding and implementing LPS as a quality-enhancing step in LPBF.

36 MATERIALS SCIENCE↗

Experimental shock lithification of water-bearing rock powders

The geology and morphology of the terrestrial planets and their moons have been profoundly affected by impact cratering. Some of these bodies contain substantial quantities of water or ice in their regoliths. It is pointed out that the effects of impacts into water-bearing target rocks are not well understood, and may be significantly different from those produced by identical impacts on a desiccated surface. The present investigation has the objective to determine the effects of water on targets of powdered rock and to seek evidence of impact-induced hydration or clay formation. Samples of andesitic basalt were crushed and sieved, and experiments were conducted on the material smaller than 150 micrometers. These experiments show that the water content of a powdered rock target can strongly affect its physical condition following an impact. A relatively small component (5-15 wt %) of water or ice in planetary surface material could inhibit or prevent lithification throughout much of the shocked volume at an impact site.

Allen, C. C.↗

Rapid Solidification Effects in Additively Manufactured Si and SiGe Compositions

SiGe alloys have a proven track record as robust high-temperature thermoelectric materials, powering NASA missions like SNAP-10A, LES-9, and Voyager 1 and 2. Enhancing thermoelectric efficiency hinges on minimizing thermal conductivity while preserving electrical conductivity. Rapid solidification via LPBF can generate microstructural features such as subgrain cellular boundaries and twinning, which may help reduce thermal conductivity while preserving semiconducting behavior. Here, this study investigates the potential of laser powder bed fusion (LPBF) additive manufacturing to fabricate nanostructured Si and SiGe thermoelectric materials. High cooling rates (10 5 to 10 7 K/s) rates inherent to the LPBF process are conducive to forming such nanostructures. Moreover, this fabrication technique could also be suitable for fabricating complex geometries needed to achieve improved device level performance. Process mapping of commercial Si powder with irregular morphology was first performed to understand the LPBF processing behavior of this semiconductor material. Subsequent studies included in-house synthesized B-doped (p-type) Si7 8 Ge 22 spherical powder that was produced via ultrasonic atomization. Scan strategies involved multiple laser exposures to mitigate solidification cracking: a high density of >98% was achieved, but solidification cracking could not be fully eliminated. Subsequently, a high electrical resistivity (i.e., low conductivity) was observed, but the measured Seebeck coefficient, ∼230 μV/K @ 500 °C, proved that good semiconductor material was being fabricated. A subgrain cellular structure (5–10 μm) was observed as defined by Ge segregation to the intercellular boundaries. The remelting strategies helped lower the cooling rates in processing SiGe, but this still resulted in high residual stresses, which induced a remarkably high density of twins (78–95%) to accommodate the deformation. This unique grain structure offers an avenue for phonon scattering and potential improvements in thermoelectric performance.

figure of merit↗

Sol-Gel Synthesis of La(0.6)Sr(0.4)CoO(3-x) and Sm(0.5)Sr(0.5)CoO(3-x) Cathode Nanopowders for Solid Oxide Fuel Cells

Nanopowders of La(0.6)Sr(0.4)CoO(3-x) (LSC) and Sm(0.5)Sr(0.5)CoO(3-x) (SSC) compositions, which are being investigated as cathode materials for intermediate temperature solid oxide fuel cells (IT-SOFC) with La(Sr)Ga(Mg)O(3-x) (LSGM) as the electrolyte, were synthesized by low-temperature sol-gel method using metal nitrates and citric acid. Thermal decomposition of the citrate gels was followed by simultaneous DSC/TGA methods. Development of phases in the gels, on heat treatments at various temperatures, was monitored by x-ray diffraction. Solgel powders calcined at 550 to 1000 C consisted of a number of phases. Single perovskite phase La(0.6)Sr(0.4)CoO(3-x) or Sm(0.5)Sr(0.5)CoO(3-x) powders were obtained at 1200 and 1300 C, respectively. Morphological analysis of the powders calcined at various temperatures was done by scanning electron microscopy. The average particle size of the powders was approx.15 nm after 700 C calcinations and slowly increased to 70 to 100 nm after heat treatments at 1300 to 1400 C.

Bansal, Narottam P.↗

Developing tools and process controls to manufacture energy-efficient powders for additive manufacturing feedstocks: Computational analysis of metal powder manufacturing via machining

Traditionally, metal powders have been produced through methods such as grinding, atomization, and electrolysis. In contrast to these techniques, Metal Powder Works, Inc. has pioneered a methodology based on metal cutting. This innovative approach utilizes a vibrating cutting tool to machine metal particles, in the form of chips, from a workpiece. This technique allows for control of powder particle size, morphology, and avoids any thermally induced material changes. This collaboration aims to elucidate metal cutting characteristics and assess performance on tough materials like Inconel alloys. Computational models, using FEA and SPH techniques, will be developed initially, focusing on aluminum alloy (Al 7075-T6) for studying mesh sensitivity, cutting forces, and chip morphology.

99 GENERAL AND MISCELLANEOUS↗

Developing tools and process controls to manufacture energy-efficient powders for additive manufacturing feedstocks

Traditionally, metal powders have been produced through methods such as grinding, atomization, and electrolysis. In contrast to these techniques, Metal Powder Works, Inc. has pioneered a methodology based on metal cutting. This innovative approach utilizes a vibrating cutting tool to machine metal particles, in the form of chips, from a workpiece. This technique allows for control of powder particle size, morphology, and avoids any thermally induced material changes. This collaboration aims to elucidate metal cutting characteristics and assess performance on tough materials like Inconel alloys. Computational models, using FEA and SPH techniques, will be developed initially, focusing on aluminum alloy (Al 7075- T6) for studying mesh sensitivity, cutting forces, and chip morphology.

36 MATERIALS SCIENCE↗