Interdependence of Support Wettability ‐ Electrodeposition Rate‐ Sodium Metal Anode and SEI Microstructure

Abstract This study examines how current collector support chemistry (sodiophilic intermetallic Na 2 Te vs. sodiophobic baseline Cu) and electrodeposition rate affect microstructure of sodium metal and its solid electrolyte interphase (SEI). Capacity and current (6 mAh cm −2 , 0.5–3 mA cm −2 ) representative of commercially relevant mass loading in anode‐free sodium metal battery (AF‐SMBs) are analyzed. Synchrotron X‐ray nanotomography and grazing‐incidence wide‐angle X‐ray scattering (GIWAXS) are combined with cryogenic ion beam (cryo‐FIB) microscopy. Highlighted are major differences in film morphology, internal porosity, and crystallographic preferred orientation e.g. (110) vs. (100) and (211) with support and deposition rate. Within the SEI, sodium fluoride (NaF) is more prevalent with Te−Cu versus sodium hydride (NaH) and sodium hydroxide (NaOH) with baseline Cu. Due to competitive grain growth the preferred orientation of sodium crystallites depends on film thickness. Mesoscale modeling delineates the role of SEI (ionic conductivity, morphology) on electrodeposit growth and onset of electrochemical instability.

Lo, Chang‐An↗

Evolution of solid electrolyte interphase and active material in the silicon wafer model system

Alloying anode materials for lithium-ion batteries, such as silicon (Si), are an important focus of materials research due to the demand for increased energy density for electric vehicles and stationary grid storage. However, progress towards next generation anode materials has been hindered by poor capacity retention due to the instability of the Si active material and the solid electrolyte interphase (SEI). Herein, the evolution of the active Si material and the SEI are simultaneously investigated from the perspective of chemical, structural, morphological, and electronic evolution in the Si wafer model system through its cycling life, using time-of-flight secondary ion mass spectrometry (TOF-SIMS), scanning transmission electron microscopy (STEM), atomic force microscopy (AFM), and scanning spreading resistance microscopy (SSRM). The results illustrate a dynamic evolution of the SEI and active Si material through cycling. Through an improved understanding of evolution of SEI and Si active material within the Si wafer model system, mitigation strategies may be designed to extend the lifetime of Si anodes.

25 ENERGY STORAGE↗

xLi2MnO3 (1-x)LiMeO2 and Li4Ti5O12 Cell Chemistry for Behind-the-Meter Storage Applications

Li- and Mn-rich layered oxide material (xLi2MnO3 (1-x)LiMeO2, Me = Ni, Mn, and etc., LMR-NM) is paired with Li4Ti5O12 (LTO) in a full cell and evaluated for the Behind-the-Meter Storage (BTMS) applications. The LMR-NM/LTO full cell shows very high capacities and excellent long-term cycle life. It delivers 192 mAh g-1 after 500 cycles at C/2 and 45 degrees C with a capacity retention of 75% and coulombic efficiency higher than 99.95%. It also has impressive rate capabilities. A capacity of 220 mAh g-1 is achieved at 2C which is 88 % of the initial capacity at C/10. The high cycling temperature clearly enhances electrochemical kinetics and activates more Li2MnO3 component, which gives high capacities, low cell impedance, and better rate capabilities. Moreover, it helps to form a relatively thick cathode-electrolyte interphase (CEI) film to suppress transition metal dissolution from the cathode surface. The upper cut-off voltage (UCV) of 3.0 V keeps the structural integrity of the cathode during cycling. A higher UCV of 3.2 V accelerates structural instabilities of the cathode as well as growth of the solid-electrolyte interphase (SEI) via transition metal dissolution and deposition on the anode surface. It results in higher cell impedance, worse capacity retention and faster capacity fade.

behind-the-meter storage↗

Reactivity of Carbonate Solvent Electrolytes on Lithium Silicon Anodes

Silicon (Si) is promising for lithium-ion battery (LIB) anodes due to their high theoretical capacity and low electrochemical potential. However, significant challenges remain, including severe volumetric expansion during cycling and the electrochemical instability of electrolytes, which leads to the formation of a nonuniform solid electrolyte interphase (SEI). To investigate SEI formation mechanisms, computational molecular dynamics simulations offer valuable insights. In this work, we examine the trajectories and charge transfer behavior of lithium hexafluorophosphate (LiPF 6 ) salt with various solvent compositions using density functional theory (DFT) and ab initio molecular dynamics (AIMD). Among the tested electrolyte systems, LiPF 6 with vinylene carbonate (VC) added to ethyl methyl carbonate (EMC) exhibits the lowest reactivity with the Si anode. In contrast, the effects of fluoroethylene carbonate (FEC) and VC depend on whether the primary solvent is EMC alone or a mixture of ethylene carbonate (EC) and EMC. Moreover, we show that electrolyte reactivity varies with the degree of lithiation of the Si anode (LiSi vs Li 15 Si 4 ) and under different charge states. To decouple electrolyte reactivity from surface effects, we analyze the dissociation and formation energies of individual species from solvated configurations. Overall, these first-principles-based findings provide a strategic foundation for electrolyte design to improve cycling stability and extend calendar life in LIBs using Si anodes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Wet chemical synthesis and properties of argyrodite sulfide solid electrolytes for solid state lithium batteries

The commercialization of the lithium-ion battery (LIB) in 1991 was responsible for the explosion in portable electronic technologies that has been seen over the past 30 years. With the advent of electric vehicles and other high-powered technologies, there is tremendous demand for LIBs with higher energy density and high safety. To achieve this, new electrode materials must be explored. The obvious choice of anode material would be pure metal lithium, which has a theoretical specific capacity of 3860 mAh g-1 . Unfortunately, metal lithium anodes have not been widely commercialized due to their tendency to react violently with the flammable liquid electrolytes used in today’s batteries. Battery safety can best be achieved by adopting solid electrolytes in place of liquid electrolytes. Solid electrolytes are nonvolatile and nonflammable, safely allowing for the combination of high-capacity cathode materials with a Li metal anode. Argyrodite sulfide solid electrolytes such as halogen-doped Li6PS5X (X = Cl, Br, I) are noted for their high ionic conductivity. But before sulfides can be commercially adopted, they possess several disadvantages which must be addressed, including time- and energy-consuming synthesis processes, poor electrochemical stability, and intrinsically poor air stability. This dissertation seeks to address each of these challenges through materials design an synthesis strategies. In this work, we pioneer a solvent-based approach for the synthesis of argyrodite solid electrolytes Li7PS6 and Li6PS5Xinstead of a stringent solid-state synthesis. Nontoxic ethanol is employed as the solvent, enabling a rapid synthetic approach to produce argyrodite solid electrolytes with high phase purity and compositional flexibility. Compared with Li7PS6, halogen doping (i.e. X = F, Cl, Br, I) not only increases the ionic conductivity, but also enhances the electrochemical stability at the interface towards Li metal. Specifically, F-doped argyrodites produce a robust SEI layer containing LiF, contributing to enhanced interfacial stability. Finally, to address the air instability challenge, argyrodite-incorporated composite solid electrolytes (CSEs) are designed and prepared to produce stable and flexible membranes that are demonstrated in solid-state Li metal batteries. These advances push argyrodite sulfide solid electrolyte research further and pave the way for the proliferation of next generation lithium metal batteries.

25 ENERGY STORAGE↗

Mechanical Milling – Induced Microstructure Changes in Argyrodite LPSCl Solid-State Electrolyte Critically Affect Electrochemical Stability

Microstructure of argyrodite solid-state electrolyte (SSE) critically affects lithium metal electrodeposition/dissolution. While the stability of unmodified SSE is mediocre, once optimized state-of-the-art electrochemical performance is achieved (symmetric cells, full cells with NMC811) without secondary interlayers or functionalized current collectors. Planetary mechanical milling in wet media (m-xylene) is employed to alter commercial Li 6 PS 5 Cl (LPSCl) powder. Quantitative stereology demonstrates how milling progressively refines grain and pore size/distribution in the SSE compact, increases its density, and geometrically smoothens the SSE-Li interface. Mechanical indentation demonstrates that these changes lead to reduced site-to-site variation in the compact's hardness. Milled microstructures promote uniform early-stage electrodeposition on foil collectors and stabilize solid electrolyte interphase (SEI) reactivity. Analysis of half-cells with bilayer electrolytes demonstrates the importance of microstructure directly contacting current collector, with interface roughness due to pore and grain size distribution being key. For the first time, short-circuiting Li metal dendrite is directly identified, employing 1.5 mm diameter “mini” symmetrical cell and cryogenic focused ion beam (cryo-FIB) electron microscopy. The branching sheet-like dendrite traverses intergranularly, filling the interparticle voids and forming an SEI around it. Importantly, mesoscale modeling reveals the relationship between Li-SSE interface morphology and the onset of electrochemical instability, based on underlying reaction current distribution.

25 ENERGY STORAGE↗

Probing the Formation of Cathode-Electrolyte Interphase on Lithium Iron Phosphate Cathodes via Operando Mechanical Measurements

Interfacial instabilities in electrodes control the performance and lifetime of Li-ion batteries. While the formation of solid-electrolyte interface (SEI) on anodes has received much attention, there is still lack of understanding about the formation of cathode-electrolyte interface (CEI) on the cathodes. To fill this gap, we report on dynamic deformations on lithium iron phosphate, LiFePO 4 cathodes during charge / discharge by utilizing in-operando digital image correlation, impedance spectroscopy and Cryo X-ray photoelectron spectroscopy. LiFePO4 cathodes were cycled in either LiPF 6 , LiClO 4 or LiTFSI- containing organic liquid electrolytes. Beyond the first cycle, Li-ion intercalation results in a nearly linear correlation between electrochemical strains and the state of (dis)-charge, regardless of the electrolyte chemistry. However, during the first charge in LiPF 6 - containing electrolyte, there is a distinct irreversible positive strain evolution at the onset of anodic current rise as well as current decay at around 4.0V. Impedance studies show the increase in surface resistance in the same potential window, suggesting the formation of CEI layers on the cathode. The chemistry of the CEI layer was characterized by X-ray photoelectron spectroscopy. LiF is detected in CEI layer starting as early as 3.4 V and Li $x$ PO $y$ F $z$ appeared at voltages higher than 4.0 V during the first charge. In conclusion, our approach offers new insights into the formation mechanism of CEI layers on the cathode electrodes, which is crucial for the development of robust cathode and electrolyte chemistries for higher performance batteries.

25 ENERGY STORAGE↗

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Abstract Solid polymer electrolytes based on plastic crystals are promising for solid‐state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 ‐electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non‐uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive‐embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile‐plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome‐like Na 0 with thin, amorphous, and fluorine‐rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

Zou, Peichao↗

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Solid polymer electrolytes based on plastic crystals are promising for solid-state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 -electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, in this study, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non-uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive-embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile-plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome-like Na 0 with thin, amorphous, and fluorine-rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

25 ENERGY STORAGE↗

Non‐Linear Kinetics of The Lithium Metal Anode on Li 6 PS 5 Cl at High Current Density: Dendrite Growth and the Role of Lithium Microstructure on Creep

Abstract Interfacial instability, viz., pore formation in the lithium metal anode (LMA) during discharge leading to high impedance, current focusing induced solid–electrolyte (SE) fracture during charging, and formation/behaviour of the solid–electrolyte interphase (SEI), at the anode, is one of the major hurdles in the development of solid‐state batteries (SSBs). Also, understanding cell polarization behaviour at high current density is critical to achieving the goal of fast‐charging battery and electric vehicle. Herein, via in situ electrochemical scanning electron microscopy (SEM) measurements, performed with freshly deposited lithium microelectrodes on transgranularly fractured fresh Li6PS5Cl (LPSCl), the LiǀLPSCl interface kinetics are investigated beyond the linear regime. Even at relatively small overvoltages of a few mV, the LiǀLPSCl interface shows non‐linear kinetics. The interface kinetics possibly involve multiple rate‐limiting processes, i.e., ion transport across the SEI and SE|SEI interfaces, as well as charge transfer across the LiǀSEI interface. The total polarization resistance R P of the microelectrode interface is determined to be ≈ 0.8 Ω cm 2 . It is further shown that the nanocrystalline lithium microstructure can lead to a stable LiǀSE interface via Coble creep along with uniform stripping. Also, spatially resolved lithium deposition, i.e., at grain surface flaws, grain boundaries, and flaw‐free surfaces, indicates exceptionally high mechanical endurance of flaw‐free surfaces toward cathodic load (>150 mA cm −2 ). This highlights the prominent role of surface defects in dendrite growth.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electro-chemo-mechanical evolution of sulfide solid electrolyte/Li metal interfaces: operando analysis and ALD interlayer effects

Sulfide solid electrolytes (SE) show promise for high-performance solid-state batteries because of their high ionic conductivity and ease of processing. However, sulfide electrolytes have suffered from chemical and electrochemical instability against Li metal anodes. In this paper, we use a suite of in situ/operando microscopy and spectroscopy techniques to demonstrate that Al 2 O 3 interlayers deposited using atomic layer deposition (ALD) delay degradation at the Li/LGPS interface by modifying the solid electrolyte interphase (SEI) chemistry and morphology. Optical and scanning electron microscopy are used to rationalize the electrochemical response of the system, which is attributed to a delayed onset of mechanical degradation at the interface when ALD interlayers are used. Operando X-ray photoelectron spectroscopy demonstrates that the dynamic evolution of SEI chemistry is impacted by the presence of the ALD interlayer. In situ Auger spectroscopy and operando optical microscopy provide visual evidence of spatial heterogeneity of Li plating, which is attributed to the chemo-mechanical degradation of the ALD interphase. The implications of these observations provide valuable insights toward the development of robust interlayers for solid-state batteries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Stable Solid Electrolyte Interphase Layer Formed by Electrochemical Pretreatment of Gel Polymer Coating on Li Metal Anode for Lithium–Oxygen Batteries

Lithium (Li)-oxygen (O2) batteries (LOBs) exhibit the highest theoretical specific energy density among candidates of the next-generation energy storage systems, but the instability of Li metal anode (LMA), air electrode, and electrolyte largely limit the practical energy density of these batteries. Herein, we report an effective method to protect LMA against side reactions between LMA and crossover contaminants such as highly reactive oxygen moieties. A solid electrolyte interphase (SEI) layer rich in inorganic components was formed on a LMA coated with polyethylene oxide thin-film through an in-situ electrochemical pre-charging step under oxygen atmosphere. This uniformly distributed stiff SEI layer interacted with flexible polymer matrix and formed a submicron-sized gel-like polymer layer. This polymer supported SEI layer leads to much longer cycle life (130 vs. 65 cycles) as compared to those of pristine cell under the same testing conditions (1.0 mAh cm-2 at 0.2 mA cm-2 in the voltage range of 2 to 5 V without any catalysts). It is also very effective during low voltage (2 to 4.5 V) cycling with a redox mediator (0.1 and 0.15M (2,2,6,6-tetramethylpiperidin-1-yl) oxidanyl). Therefore, this approach can be used to stabilize LMA/electrolytes interphase and improve the cycle life of rechargeable LOBs.

lithium-oxygen batteries, lithium metal anodes, ar↗

Surface heterogeneity propagation and homogenization for pouch cell-scale Li metal anodes

Li metal anode is a promising candidate for next-generation energy storage systems and is widely explored in Li-ion and solid-state batteries. Despite its potential, Li metal anodes face instabilities during long-term cycling, especially when paired with NMC or sulfur-based cathodes, where Li is cycled at high capacities of 6-8 mAh/cm2, equivalent to a thickness of 30-40 µm. During such extensive utilization, degradation mechanisms such as excessive solid electrolyte interphase (SEI), dendrites, and dead Li emerge, and ultimately lead to sudden failure and reduced cycle life. The origin of the degradation mechanisms stem from surface heterogeneities introduced during Li foil manufacturing and storage [1, 2]. As cycling progresses, the local heterogeneities propagate, resulting in uneven Li utilization and degradation-prone regions across the electrode [3], which consequently induce performance variations at the cell level. This heterogeneity propagation is particularly pronounced in large-format pouch cells in practical applications, where the surface effects are magnified. Without a clear understanding of the multi-scale heterogeneities and the development of surface homogenization methods, the performance consistency will be compromised, hindering the commercialization of Li metal batteries. In this presentation, we investigate the evolution of surface heterogeneity propagation on commercially available Li foils. We discover that inhomogeneous Li utilization appears as early as the first half-cycle of formation, manifesting as localized clusters and pits. In pouch cell configurations, these features exhibit areal density variations across the electrode on a scale of millimeters. To improve Li utilization homogeneity, a scalable mechanical brushing method is introduced to remove the chemically heterogeneous surface passivation layer. Furtherore, the influence of utilization homogeneity on cell-to-cell consistency is evaluated using 32 Li-NMC811 pouch cells divided into as-received and brushed Li groups. On the brushed Li, clusters and pits are no longer observable, and the cells exhibit significantly improved consistency in discharge capacity trajectories and cycle lifetime. Overall, this study highlights the role of Li surface utilization homogeneity on long-term cycling performance. Our research provides a pathway for improving large-area electrode uniformity and establishing evaluation methods for cell-to-cell consistency, both are key steps toward the commercialization of Li metal batteries and beyond. [1] Otto, Svenja-K., et al. "In-depth characterization of lithium-metal surfaces with XPS and ToF-SIMS: toward better understanding of the passivation layer." Chemistry of Materials 33.3 (2021): 859-867. [2] Hatzell, Kelsey, et al. "Aligning lithium metal battery research and development across academia and industry." Joule (2024). [3] Kim, Sangwook, et al. "Calendar life of lithium metal batteries: Accelerated aging and failure analysis." Energy Storage Materials 65 (2024): 103147.

25 - ENERGY STORAGE↗

Salt‐in‐Salt Reinforced Carbonate Electrolyte for Li Metal Batteries

Abstract The instability of carbonate electrolyte with metallic Li greatly limits its application in high‐voltage Li metal batteries. Here, a “salt‐in‐salt” strategy is applied to boost the LiNO 3 solubility in the carbonate electrolyte with Mg(TFSI) 2 carrier, which enables the inorganic‐rich solid electrolyte interphase (SEI) for excellent Li metal anode performance and also maintains the cathode stability. In the designed electrolyte, both NO 3 − and PF 6 − anions participate in the Li + ‐solvent complexes, thus promoting the formation of inorganic‐rich SEI. Our designed electrolyte has achieved a superior Li CE of 99.7 %, enabling the high‐loading NCM811||Li (4.5 mAh cm −2 ) full cell with N/P ratio of 1.92 to achieve 84.6 % capacity retention after 200 cycles. The enhancement of LiNO 3 solubility by divalent salts is universal, which will also inspire the electrolyte design for other metal batteries.

Liu, Sufu↗

Salt‐in‐Salt Reinforced Carbonate Electrolyte for Li Metal Batteries

Abstract The instability of carbonate electrolyte with metallic Li greatly limits its application in high‐voltage Li metal batteries. Here, a “salt‐in‐salt” strategy is applied to boost the LiNO 3 solubility in the carbonate electrolyte with Mg(TFSI) 2 carrier, which enables the inorganic‐rich solid electrolyte interphase (SEI) for excellent Li metal anode performance and also maintains the cathode stability. In the designed electrolyte, both NO 3 − and PF 6 − anions participate in the Li + ‐solvent complexes, thus promoting the formation of inorganic‐rich SEI. Our designed electrolyte has achieved a superior Li CE of 99.7 %, enabling the high‐loading NCM811||Li (4.5 mAh cm −2 ) full cell with N/P ratio of 1.92 to achieve 84.6 % capacity retention after 200 cycles. The enhancement of LiNO 3 solubility by divalent salts is universal, which will also inspire the electrolyte design for other metal batteries.

25 ENERGY STORAGE↗

Review of Multifunctional Separators: Stabilizing the Cathode and the Anode for Alkali (Li, Na, and K) Metal–Sulfur and Selenium Batteries

Alkali metal batteries based on lithium, sodium, and potassium anodes and sulfur-based cathodes are regarded as key for next-generation energy storage due to their high theoretical energy and potential cost effectiveness. However, metal–sulfur batteries remain challenged by several factors, including polysulfides’ (PSs) dissolution, sluggish sulfur redox kinetics at the cathode, and metallic dendrite growth at the anode. Functional separators and interlayers are an innovative approach to remedying these drawbacks. Here we critically review the state-of-the-art in separators/interlayers for cathode and anode protection, covering the Li–S and the emerging Na–S and K–S systems. The approaches for improving electrochemical performance may be categorized as one or a combination of the following: Immobilization of polysulfides (cathode); catalyzing sulfur redox kinetics (cathode); introduction of protective layers to serve as an artificial solid electrolyte interphase (SEI) (anode); and combined improvement in electrolyte wetting and homogenization of ion flux (anode and cathode). It is demonstrated that while the advances in Li–S are relatively mature, less progress has been made with Na–S and K–S due to the more challenging redox chemistry at the cathode and increased electrochemical instability at the anode. Throughout these sections there is a complementary discussion of functional separators for emerging alkali metal systems based on metal–selenium and the metal–selenium sulfide. The focus then shifts to interlayers and artificial SEI/cathode electrolyte interphase (CEI) layers employed to stabilize solid-state electrolytes (SSEs) in metal–sulfur solid-state batteries (SSBs). The discussion of SSEs focuses on inorganic electrolytes based on Li- and Na-based oxides and sulfides but also touches on some hybrid systems with an inorganic matrix and a minority polymer phase. The review then moves to practical considerations for functional separators, including scaleup issues and Li–S technoeconomics. The review concludes with an outlook section, where we discuss emerging mechanics, spectroscopy, and advanced electron microscopy (e.g. cryo-transmission electron microscopy (cryo-TEM) and cryo-focused ion beam (cryo-FIB))-based approaches for analysis of functional separator structure–battery electrochemical performance interrelations. Finally, throughout the review we identify the outstanding open scientific and technological questions while providing recommendations for future research topics.

25 ENERGY STORAGE↗

Solvation Rule for Solid‐Electrolyte Interphase Enabler in Lithium‐Metal Batteries

Abstract Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium‐metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium‐metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. We unambiguously demonstrated the solvation rule for the solid‐electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

Su, Chi‐Cheung↗

Solvation Rule for Solid-Electrolyte Interphase Enabler in Lithium-Metal Batteries

Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium-metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium-metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. Here, we unambiguously demonstrated the solvation rule for the solid-electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥ 1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.