At least 37 records · Page 2

Deflection And Stress In Preloaded Square Membrane

Theoretical analysis yields equations for transverse deflection of, and stresses in, square membrane subject to both uniform transverse load and tension preloads applied uniformly along the edges. Follows energy/virtual-displacement approach. Basic equation expresses strain energy in membrane as double integral, over x and y coordinates of square, of function of longitudinal strains, shear strain, thickness of membrane, and Young's modulus and Poissons's ratio of membrane material.

Hermida, Alfonso↗

Computing Displacements And Strains From Video Images

Subpixel digital video image correlation (SDVIC) technique for measuring in-plane displacements on surfaces of objects under loads, without contact. Used for analyses of experimental research specimens or actual service structures of virtually any size or material. Only minimal preparation of test objects needed, and no need to isolate test objects from minor vibrations or fluctuating temperatures. Technique implemented by SDVIC software, producing color-graduated, full-field representations of in-plane displacements and partial derivatives with respect to position along both principal directions in each image plane. From representations, linear strains, shear strains, and rotation fields determined. Written in C language.

Russell, Samuel S.↗

Deformation analysis of boron/aluminum specimens by moire interferometry

Whole-field surface deformations were measured for two slotted tension specimens from multiply laminates, one with 0 deg fiber orientation in the surface ply and the other with 45 deg orientation. Macromechanical and micromechanical details were revealed using high-sensitivity moire interferometry. Although global deformations of all plies were essentially equal, numerous random or anomalous features were observed. Local deformations of adjacent 0 deg and 45 deg plies were very different, both near the slot and remote from it, requiring large interlaminar shear strains for continuity. Shear strains were concentrated in the aluminum matrix. For 45 deg plies, a major portion of the deformation was by shear; large plastic slip of matrix occurred at random locations in 45 deg plies, wherein groups of fibers slipped relative to other groups. Shear strains in the interior, between adjacent fibers, were larger than the measured surface strains.

Post, Daniel↗

Microgravity Foam Structure and Rheology

To exploit rheological and multiple-light scattering techniques, and ultimately microgravity conditions, in order to quantify and elucidate the unusual elastic character of foams in terms of their underlying microscopic structure and dynamics. Special interest is in determining how this elastic character vanishes, i.e. how the foam melts into a simple viscous liquid, as a function of both increasing liquid content and shear strain rate. The unusual elastic character of foams will be quantified macroscopically by measurement of the shear stress as a function of static shear strain, shear strain rate, and time following a step strain; such data will be analyzed in terms of a yield stress, a static shear modulus, and dynamical time scales. Microscopic information about bubble packing and rearrangement dynamics, from which these macroscopic non-Newtonian properties presumably arise, will be obtained non-invasively by novel multiple-light scattering diagnostics such as Diffusing-Wave Spectroscopy (DWS). Quantitative trends with materials parameters, such as average bubble size, and liquid content, will be sought in order to elucidate the fundamental connection between the microscopic structure and dynamics and the macroscopic rheology.

Durian, Douglas J.↗

The Application of Strain Range Partitioning Method to Torsional Creep-Fatigue Interaction

The method of strain range partitioning was applied to a series of torsional fatigue tests conducted on tubular 304 stainless steel specimens at 1200 F. Creep strain was superimposed on cycling strain, and the resulting strain range was partitioned into four components; completely reversed plastic shear strain, plastic shear strain followed by creep strain, creep strain followed by plastic strain and completely reversed creep strain. Each strain component was related to the cyclic life of the material. The damaging effects of the individual strain components were expressed by a linear life fraction rule. The plastic shear strain component showed the least detrimental factor when compared to creep strain reversed by plastic strain. In the latter case, a reduction of torsional fatigue life in the order of magnitude of 1.5 was observed.

Zamrik, S. Y.↗

Experimental study of a metal-matrix composite

A metal-matrix specimen was investigated using moire interferometry with 2400 lines/m (60,960 l/in.). The specimen was a 6-ply (0/ + or - 45)s boron-aluminum tensile coupon with a central slot. The unequal deformations in fibers and matrix were evident. Special attention was given to a plastic slip zone in the matrix. Normal and shear strains were calculated in the slip zone; the shear-strain concentration factor rose dramatically with the onset of plastic slip and continued to rise gradually with load to 95 percent of the failure load. The precipitous change from maximum tensile strain in one fiber to zero tensile strain in the neighboring fiber was accommodated by the very high shear strains of the matrix in the slip zone. Experimental considerations are discussed: shear strains are independent of rigid-body rotations; simplified strain calculations are justified; averaging across the narrow slip region and the influence of finite thickness of the specimen grating contribute to underestimation of peak strains.

Post, D.↗

Deformation of a metal-matrix tensile coupon with a central slot - An experimental study

A metal-matrix specimen was investigated using high-sensitivity moire interferometry. In-plane displacement fields were analyzed at various load levels from 15 to 95 percent of the failure load. Normal and shear strains were determined from displacement gradients. Highly localized plastic slip zones occured in the ductile aluminum matrix tangent to the ends of the slot. Shear strains in the slip zone were an order of magnitude greater than the largest normal strains in the specimen. The shear-strain concentration factor rose dramatically with the onset of plastic slip and continued to rise gradually with load to 95 percent of the failure load. Upon unloading, shear strains in the slip zone remained precariously high.

Post, Daniel↗

Moire interferometry, 1986

Current capabilities of moire interferometry are described. Several examples illustrate this whole-field optical technique for measurements of in-plane displacements. Sensitivity corresponds to moire measurements with gratings of 2400 lines/mm. The examples are taken from studies of composite members, material anomalies, plasticity, joints, micromechanics and strain concentrations. The abundance of high-sensitivity displacement information permits calculation of normal strains and shear strains in the field, including critical zones of very high gradients.

Post, D.↗

Geodetic measurement of deformation in the central Mojave Desert, California

Data from triangulation and trilateration surveys made during 1934-1982 are used to calculate shear strain rates in the central Mojave Desert of California. For the region between the Helendale and Camp Rock faults the shear strain rate was determined to be 0.16 + or - 0.03 microstrain/yr, with maximum right-lateral shear strain occurring on a plane oriented N41 deg W + or - 5 deg. If this deformation is due to right-lateral motion across the northwest trending local faults, the average shear straining corresponds to a relative displacement of 6.7 + or - 1.3 mm/yr across this portion of the network, accounting for about 12 percent of the predicted 56 mm/yr of relative motion between the North Atlantic and Pacific plates. From the Camp Rock fault eastward across the network there is a transition from significant to very low strain rates. Examination of nine focal mechanisms and their relation to the local geology and the strain data suggests that most of the long-term displacement occurs on the major northwest trending faults oriented nearly along the direction of relative motion between the North American and Pacific plates. Secondary faulting, controlled by a Coulomb-Anderson failure mechanism or by slip on preexisting faults can account for the occurrence of earthquakes on faults of other orientations.

Sauber, Jeanne↗

Free edge strain concentrations in real composite laminates: Experimental-theoretical correlation

The magnitude of the maximum shear strain at the free edge of axially loaded theta (2)/-theta(2)(s) and (+ or - theta(2) (s) composite laminates was investigated experimentally and numerically to ascertain the actual value of strain concentration in resin matrix laminates and to determine the accuracy of finite element results. Experimental results using moire interferometry show large, but finite, shear strain concentrations at the free edge of graphite-epoxy and graphite-polyimide laminates. Comparison of the experimental results with those obtained using several different finite element representations showed that a four node isoparametric finite element provided the best and most trouble free numerical results. The results indicate that the ratio of maxium shear strain at the free edge to applied axial strain varies with fiber orientation and does not exceed nine for the most critical angle which is 15 deg.

Herakovich, C. T.↗

Free edge strain concentrations in real composite laminates Experimental-theoretical correlation

The magnitude of the maximum shear strain at the free edge of axially loaded theta (2)/theta(2)(s) and (+ or - theta(2) (s) composite laminates was investigated experimentally and numerically to ascertain the actual value of strain concentration in resin matrix laminates and to determine the accuracy of finite element results. Experimental results using moire interferometry show large, but finite, shear strain concentrations at the free edge of graphite-epoxy and graphite-polyimide laminates. Comparison of the experimental results with those obtained using several different finite element representations showed that a four node isoparametric finite element provided the best and most trouble free numerical results. The results indicate that the ratio of maximum shear strain at the free edge to applied axial strain varies with fiber orientation and does not exceed nine for the most critical angle which is 15 deg.

Herakovich, C. T.↗

Deformation measurements of composite multi-span beam shear specimens by Moire interferometry

Experimental analyses were performed for determination of in plane deformations and shear strains in unidirectional and quasi-isotropic graphite-epoxy beams. Forty-eight ply beams were subjected to 5 point and 3 point flexure. Whole field measurements were recorded at load levels from about 20% to more than 90% of failure loads. Contour maps of U and W displacement fields were obtained by moire interferometry, using reference gratings of 2400 lines/mm. Clearly defined fringes with fringe orders exceeding 1000 were obtained. Whole field contour maps of shear strains were obtained by a method developed for these tests. Various anomalous effects were detected in the displacement fields. Their analysis indicated excess shear strains in resin rich zones in regions of shear tractions; free edge shear strains in quasi-isotropic specimens in regions of normal stresses; and shear stresses associated with cyclic shear compliances of quasi-isotropic plies in regions of shear tractions. Their contributions could occur independently or in superposition. Qualitative analyses addressed questions of relaxation; influence of contact stress distribution; specimen failure; effect of specimen overhang; nonlinearity; and qualities of 5 and 3 point flexure tests.

Post, D.↗

Viscoelastic Vibration Dampers for Turbomachine Blades

Simple viscoelastic dampers have been invented for use on the root attachments of turbomachine blades. These dampers suppress bending- and torsion-mode blade vibrations, which are excited by unsteady aerodynamic forces during operation. In suppressing vibrations, these dampers reduce fatigue (thereby prolonging blade lifetimes) while reducing noise. These dampers can be installed in new turbomachines or in previously constructed turbomachines, without need for structural modifications. Moreover, because these dampers are not exposed to flows, they do not affect the aerodynamic performances of turbomachines. Figure 1 depicts a basic turbomachine rotor, which includes multiple blades affixed to a hub by means of dovetail root attachments. Prior to mounting of the blades, thin layers of a viscoelastic material are applied to selected areas of the blade roots. Once the blades have been installed in the hub and the rotor is set into rotation, centrifugal force compresses these layers between the mating load-bearing surfaces of the hub and the blade root. The layers of viscoelastic material provide load paths through which the vibration energy of the blade can be dissipated. The viscoelasticity of the material converts mechanical vibration energy into shear strain energy and then from shear strain energy to heat. Of the viscoelastic materials that have been considered thus far for this application, the one of choice is a commercial polyurethane that is available in tape form, coated on one side with an adhesive that facilitates bonding to blade roots. The thickness of the tape can be chosen to suit the specific application. The typical thickness of 0.012 in. (.0.3 mm) is small enough that the tape can fit in the clearance between the mating blade-root and hub surfaces in a typical turbomachine. In an experiment, a blade was mounted in a test fixture designed to simulate the blade-end conditions that prevail in a turbocompressor. Vibrations were excited in the blade by use of an impact hammer, and damping of the vibrations was measured by use of a dynamic signal analyzer. Tests were performed without and with viscoelastic dampers installed in the dovetail root attachment. The results of the measurements, some of which are presented in Figure 2, show that the viscoelastic dampers greatly increased the rate of damping of vibrations. Accordingly, dynamic stresses on rotor blades were significantly reduced, as shown in Figure 2.

Nguyen, Nhan↗

The Application of Strainrange Partitioning Method to Multiaxial Creep-Fatigue Interaction

The method of strain range partitioning was applied to a series of torsional fatigue tests conducted on tubular 304 stainless steel specimens at 1200 F (649 C). Creep strain was superimposed on cycling strain, and the resulting strain range was partitioned into four components: (1) completely reversed plastic shear strain, (2) plastic shear strain followed by creep strain, (3) creep strain followed by plastic strain, and (4) completely reversed creep strain. Each strain component was related to the cyclic life of the material. The experimental procedure used to achieve strain partitioning is described, and the torsional test results are compared to those obtained from axial tests. The damaging effects of the individual strain components were expressed by a linear life fraction rule.

Zamrik, S. Y.↗

Fracture Behavior of a Stitched Warp-Knit Carbon Fabric Composite

Tests were conducted on several types of fracture specimens made from a carbon/epoxy composite. The composite material was stitched prior to introducing epoxy resin. Boeing, used this material to develop a composite wing box for a transport aircraft in the NASA Advanced Composites Transport Program. The specimens included compact, extended compact, and center notched tension specimens. The specimens were cut from panels with three orientations in order to explore the effects of anisotropy. The panels were made with various thicknesses to represent a wing, skin from tip to root. All fractures were not self-similar depending on specimen type and orientation. Unnotched tension specimens were also tested to measure elastic constants and strengths. The normal and shear strains were calculated on fracture planes using a series representation of strain fields for plane anisotropic crack problems. The fracture parameters were determined using a finite element method. Characteristic distances for critical tension and shear strains were calculated for each specimen and a failure criterion based on the interaction of tension and shear strains was proposed.

Poe, Clarence C., Jr.↗

Geodetic Measurement of Deformation East of the San Andreas Fault in Central California

Triangulation and trilateration data from two geodetic networks located between the western edge of the Great Valley and the San Andreas fault have been used to calculate shear strain rates in the Diablo Range and to estimate the slip rate along the Calaveras and Paicines faults in Central California. Within the Diablo Range the average shear strain rate was determined for the time period between 1962 and 1982 to be 0.15 + or - 0.08 microrad/yr, with the orientation of the most compressive strain at N 16 deg E + or - 14 deg. The orientation of the principal compressive strain predicted from the azimuth of the major structures in the region is N 25 deg E. It is inferred that the measured strain is due to compression across the folds of this area: the average shear straining corresponds to a relative shortening rate of 4.5 + or - 2.4 mm/yr. From an examination of wellbore breakout orientations and the azimuths of P-axes from earthquake focal mechanisms the inferred orientation of maximum compressive stress was found to be similar to the direction of maximum compressive strain implied by the trend of local fold structures. Results do not support the hypothesis of uniform fault-normal compression within the Coast Ranges. From trilateration measurements made between 1972 and 1987 on lines that are within 10 km of the San Andreas fault, a slip rate of 10 to 12 mm/yr was calculated for the Calaveras-Paicines fault south of Hollister. The slip rate of the Paicines fault decreases to 4 mm/yr near Bitter.

Sauber, Jeanne M.↗

Plastic deformation - Its role in fatigue crack propagation

Recognizing the fact that the effective driving force Delta-K(eff) determines the fatigue crack propagation (FCP) rate and that the shear strain, which is considered to develop due to an occurrence of crack closure, primarily contributes to the plastic deformation, an effort is made here to elucidate the role of plastic deformation in FCP by developing a correlation between the Delta-K(eff) and the applied driving force (Delta-K) with shear strain as variable. The disparity between Delta(K)eff) and Delta-K, which apparently increases with shear strain level, persists at lower values of Delta-K. This suggests a strong influence of the degree of localized deformation on the FCP rates in the near threshold level. Hence, an improvement of FCP rates in the near threshold level should follow an effort that promotes the plastic deformation near the crack tip to a greater degree. This approach could explain the effect of the grain size, microstructure, environment, R-ratio and crack size on the near-threshold FCP rates.

Mazumdar, P. K.↗

Elastic-plastic deformation of a metal-matrix composite coupon with a center slot

A comprehensive experimental analysis of deformations of the surface of a metal-matrix specimen is reported. The specimen is a 6-ply 0 + or - 45 sub s boron-aluminum tensile coupon with a central slot. Moire interferometry is used for high-sensitivity whole-field measurements of in-plane displacements. Normal and shear strains are calculated from displacement gradients. Displacement fields are analyzed at various load levels from 15% to 95% of the failure load. Deformations of the boron fibers could be distinguished from those of the matrix. Highly localized plastic slip zones occur tangent to the ends of the slot. Shear strains and concurrent transverse compressive strains in the slip zones reach approximately 10% and 1%, respectively. Upon unloading, elastic recovery in surrounding regions causes a reverse plastic shear strain in the slip zone of about 4%. Longitudinal normal strains on the unslotted ligament peak at the slot boundary at about 1% strain. The strain concentration factor at the end of the slot decreases with load level and the advance of plasticity.

Post, D.↗