Atomic oxygen interactions with FEP Teflon and silicones on LDEF

The Long Duration Exposure Facility (LDEF) spacecraft represents the first controlled unidirectional exposure of high-fluence atomic oxygen on fluorinated ethylene propylene (FEP Teflon) and silicones. The atomic oxygen erosion yield for FEP Teflon was found to be significantly in excess of previous low fluence orbital data and is an order of magnitude below that of polyimide Kapton. LDEF FEP Teflon erosion yield data as a function of angle of attack is presented. Atomic oxygen interaction with silicon polymers results in crazing of the silicones as well as deposition of dark contaminant oxidation products on adjoining surfaces. Documentation of results and possible mechanistic explanations are presented.

Banks, Bruce A.↗

Atomic oxygen interactions with FEP Teflon and silicones on LDEF

The Long Duration Exposure Facility (LDEF) spacecraft has enabled the measurement of the effects of fixed orientation exposure of high fluence atomic oxygen on fluorinated ethylene propylene (FEP Teflon) and silicones. The atomic oxygen erosion yield for the FEP Teflon was found to be 3.64 x 10(exp -25) cm(exp 3)/atom. This erosion yield is significantly higher than that measured from previous low fluence orbital data. The FEP Teflon erosion yield was found to have the same dependence on oxygen arrival angle as Kapton and Mylar. Atomic oxygen interaction with silicon polymers results in the crazing of silicon. Released silicone contaminants were found to darken upon further atomic oxygen exposure.

Bruce A. Banks↗

The Effect of Polymer Char on Nitridation Kinetics of Silicon

Effects of polymer char on nitridation kinetics of attrition milled silicon powder have been investigated from 1200 to 1350 C. Results indicate that at and above 1250 C, the silicon compacts containing 3.5 wt percent polymer char were fully converted to Si3N4 after 24 hr exposure in nitrogen. In contrast, the silicon compacts without polymer char could not be fully converted to Si3N4 at 1350 C under similar exposure conditions. At 1250 and 1350 C, the silicon compacts with polymer char showed faster nitridation kinetics than those without the polymer char. As the polymer char content is increased, the amount of SiC in the nitrided material is also increased. By adding small amounts (approx. 2.5 wt percent) of NiO, the silicon compacts containing polymer char can be completely nitrided at 1200 C. The probable mechanism for the accelerated nitridation of silicon containing polymer char is discussed.

Chan, Rickmond C.↗

Investigation of environmental effects on coatings for thermal control of large space vehicles

The objective of significantly advancing the state-of-the-art of white, spacecraft-radiator coatings has been realized in a comprehensive goal-oriented, pigmented-coatings research program. Considered were inorganic pigments and coatings, silicone polymers and coatings, the design and construction of a combined ultraviolet-plus-proton irradiation facility, the development of zinc orthotitanate pigment and coatings, and the effects on several low alpha sub s/epsilon paints of combined ultraviolet and proton irradiation.

Zerlaunt, G. A.↗

Polyimide fiber-glass composite resists high temperatures

Composites synthesized from bismaleimide have superior strength and oxidation resistance at elevated temperatures when compared with similar composites prepared with epoxy or silicon polymers of similar cost. Polyimide synthesis technique and processing method yield essentially void-free fiber-glass reinforced composites.

Gilwee, W. J.↗

Fiber optics transmission of LV signal

The first use of a long optical fiber for transmitting megahertz frequencies in a laser velocimeter (LV) receiver system is reported. The fiber comprises a 600-micron diameter fused silica core, a silicon polymer cladding and a plastic jacket. The fiber numerical aperture is 0.22, corresponding to a maximum entrance half-angle of 0.22 rad. The 10-m length used results in a 5.6% attenuation loss. The fiber is found to transmit an 80-MHz signal with excellent resolution. It is established that an LV receiver using fiber optics sends a clean signal in electronically noisy and high-pressure environments and allows velocity measurements in places too small for a photomultiplier tube.

Young, A. D.↗

Video luminescent barometry - The induction period

Video monitoring of oxygen quenching of the photoluminescence of platinum octaethylporphyrin (PtOEP) in silicone polymer resin may be used to measure pressure distribution over an airfoil. A continuous increase of the luminescence intensity of PtOEP on exposure to the exciting light is known as the induction effect. The effect of several factors on PtOEP photoluminescence and the induction effect was investigated. The experimental apparatus is described and results are presented. It was observed that the relative induction amplitude and induction time increase at higher oxygen pressure and with thicker films. These observations may be explained if the singlet oxygen produced by oxygen quenching is consumed by the polymer and is therefore unavailable for further quenching. Researchers using this method for measuring pressure distribution on airfoil surfaces should be aware of the induction effect and its implications.

Uibel, Rory H.↗

MIR Solar Array Return Experiment: Power Performance Measurements and Molecular Contamination Analysis Results

A solar array segment was recently removed from the Mir core module and returned for ground-based analysis. The segment, which is similar to the ones the Russians have provided for the FGB and Service Modules, was microscopically examined and disassembled by US and Russian science teams. Laboratory analyses have shown the segment to he heavily contaminated by an organic silicone coating, which was converted to an organic silicate film by reactions with atomic oxygen within the. orbital flight environment. The source of the contaminant was a silicone polymer used by the Russians as an adhesive and bonding agent during segment construction. During its life cycle, the array experienced a reduction in power performance from approx. 12%, when it was new and first deployed, to approx. 5%, when it was taken out of service. However, current-voltage measurements of three contaminated cells and three pristine, Russian standard cells have shown that very little degradation in solar array performance was due to the silicate contaminants on the solar cell surfaces. The primary sources of performance degradation is attributed to "thermal hot-spotting" or electrical arcing; orbital debris and micrometeoroid impacts; and possibly to the degradation of the solar cells and interconnects caused by radiation damage from high energy protons and electrons.

Visentine, James↗

Lunar and Planetary Science XXXVI, Part 20

The topics include: 1) Virtual Reality Technology as a Tool to Enhance Collaboration Between Space Exploration and Public Outreach: The Case Using the Mars Exploration Rover Images; 2) Atmospheric Electron-induced X-Ray Spectrometer (AEXS) Instrument Development; 3) Impact of Low Thermal Conductivity Layers on the Bulk Conductivity of a Martian Crustal Column; 4) Impacting Classroom Teachers Through Long-Term Professional Development; 5) Oxygen, Ca, and Ti Isotopic Compositions of Hibonite-bearing Inclusions; 6) Phenomenological Excitation Functions of Xe Isotopes with Protons on Nuclei of Cs, La and Ce; 7) Double-Diffusive Convection and Other Modes of Salinity-modulated Heat and Material Transport in Europa s Ocean; 8) Slope Morphologies of the Hellas Mensae Constructs, Eastern Hellas Planitia, Mars; 9) Development of Polygonal Thermal Contraction Patterns in a South Polar Trough, Mars 3 Years of Observations; 10) Martian Relevance of Dehydration and Rehydration in the Mg-Sulfate System; 11) Formation of Martian Volcanic Provinces by Lower Mantle Flushing? 12) Can Glasses Help Us to Unravel the Origin of Barred Olivine Chondrules? 13) Loki Patera: A Magma Sea Story; 14) Compositions of Partly Altered Olivine and Replacement Serpentine in the CM2 Chondrite QUE93005; 15) Model of Light Scattering by Lunar Regolith at Moderate Phase Angles: New Results; 16) Radiation Resistance of a Silicone Polymer Grease Based Regolith Collector for the HERA Near-Earth Asteroid Sample Return Mission; 17) Analysis of the Tectonic Lineaments in the Ganiki Planitia (V14) Quadrangle, Venus; 18) Nanometer-sized Diamonds from AGB Stars; 19) Quantifying Exact Motions Along Lineaments on Europa; 20) Geometry of Thrust Faults Beneath Amenthes Rupes, Mars; 21) Mapping of the Physical Characteristics and Mineral Composition of a Superficial Layer of the Moon or Mars and Ultra-Violet Polarimetry from the Orbital Station; 22) Negative Searches for Evidence of Aqueous Alteration on Asteroid Surfaces; 23) What Processes Have Shaped Basalt Boulders on Earth and Mars? Studies of Feature Persistence Using Facet Mapping and Fractal Analysis; 24) The Popigai Fluidizites: Dense Water Inclusions in Lechatelierite; Evidence for Shock-generated Carbonate and Hydrous Silicate Melts; 25) Missing Xenon Problem and Climate of the Early Earth; and 26) More on Magnetic Spectra from Correlated Crustal Sources on Mars

Source record↗

Vacuum Ultraviolet Radiation Effects on DC93-500 Silicone Film Studied

A space-qualified silicone polymer, DC93-500 (Dow Corning, Midland, MI), has been used as a spacecraft solar cell adhesive and has been proposed for use in a Fresnel lens solar concentrator for space power applications. Applications of DC93-500 for exterior space system surfaces require an understanding of its overall space environmental durability. Vacuum ultraviolet (VUV) radiation is among the space environment elements that can be hazardous to the properties of DC93-500, causing degradation in optical and mechanical properties. For materials or components that have not been tested previously for long-duration performance in space, such as DC93-500 in freestanding film form, ground laboratory testing is an important tool for assuring durability. However, differences between the space environment and ground laboratory testing environments lead to complexities in interpreting the ground test results. Two important differences between space and laboratory vacuum ultraviolet exposure conditions are irradiance spectra and light intensity. These important differences were the basis for laboratory experiments conducted to examine VUV wavelength dependence and VUV intensity dependence of DC93-500 degradation. Testing conducted at the NASA Glenn Research Center along with additional data provided through a grant with the University of Nebraska-Lincoln, has advanced the understanding of VUV effects on DC93-500 and has provided important conclusions regarding the use of ground laboratory VUV testing to predict the space environment performance of DC93-500.

Dever, Joyce A.↗

Dust Solution Testing Initiative (DuSTI): Infusing Commercial Off the Shelf Dust Mitigation Technologies with NASA Practices

Dust is one of the most significant hazards to human lunar exploration. However, since the Apollo program concluded, limited research has been performed on lunar dust mitigation technologies. The safety of the crew members and sustainability of habitats, science, and supporting hardware depend on effective dust mitigation techniques and technologies. As NASA pursues a new generation of lunar missions with the Artemis program, the project team will pursue dust mitigation solutions with the Dust Solution Testing Initiative (DuSTI). DuSTI is a lunar dust mitigation effort that involves performing tests on commercial off the shelf (COTS) technologies over FY21. DuSTI will preform component and subsystem tests in dusty environments for up to five technologies with high potential. The specific technologies identified for study were selected based on several factors, including a market analysis of current terrestrial dust mitigation applications, availability of the technology, accessibility of various testing facilities, and cost of procurement. These technologies support the active and passive dust mitigation requirements of filtration systems, electro-mechanical systems, electro-static systems, surface coatings, textiles, and silicone polymers. Technology Readiness Level (TRL) will be increased by validating components in relevant environments. For example, if the COTS technology is at a TRL 9 for terrestrial use but at a 4-5 TRL for use in the lunar environment, we will test that technology in a lunar dust environment to increase the TRL for use on the Moon.

lunar dust↗

Silicon containing electroconductive polymers and structures made therefrom

An electropolymerized film comprised of polymers and copolymers of a monomer is formed on the surface of an anode. The finished structures have superior electrical and mechanical properties for use in applications such as electrostatic dissipation and for the reduction of the radar cross section of advanced aircraft.

Nagasubramanian, Ganesan↗