Fatigue and Fracture Behavior of Additively Manufactured Austenitic Stainless Steel

Additive manufacturing (AM) includes a diverse suite of innovative manufacturing processes for producing near-net shape components, typically from powder or wire feedstock. Reported mechanical properties of AM materials vary significantly depending on the details of the manufacturing process and the characteristics of the processing defects (namely, lack of fusion defects). However, an excellent combination of strength, ductility and fracture resistance can be achieved in AM type 304L and 316L austenitic stainless steels by minimizing processing defects. It is also important to recognize that localized solidification processing during AIVI produces microstructures more analogous to weld microstructures than wrought microstructures. Consequently, the mechanical behavior of AM austenitic stainless steels in harsh environments can diverge from the performance of wrought materials. This report gives an overview of the fracture and fatigue response of type 304L materials from both directed energy deposition (DED) and powder bed fusion (PBF) techniques. In particular, the mechanical performance of these materials is considered for high-pressure hydrogen applications by evaluating fatigue and fracture resistance after thermally precharging of test specimens in high-pressure gaseous hydrogen. The mechanical behaviors are considered with respect to previous reports on hydrogen-assisted fracture of austenitic stainless steel welds and the unique characteristics of the AM microstructures. Fatigue crack growth can be relatively insensitive to processing defects, displaying similar behavior as wrought materials. Fracture resistance of dense AM austenitic stainless steel, on the other hand, is more consistent with weld metal than with compositionally-similar wrought materials. Hydrogen effects in the AM materials are generally more severe than in wrought materials, but comparable to measurements on welded austenitic stainless steels in hydrogen environments. While hydrogenassisted fracture manifests differently in welded and AM austenitic stainless steel, the fracture process appears to have a common origin in the compositional microsegregation intrinsic to solidification processes.

additive manufacturing, austenitic stainless steel↗

Machine Learning Prediction of Fracture Toughness in Hydrogen-charged Stainless Steels

Austenitic stainless steels are structural materials utilized in tritium gas pressure boundaries since they are resistant to hydrogen isotope embrittlement [1-3]. However, exposure to tritium over long periods of time leads to tritium uptake which decays to result in helium ingrowth. This helium ingrowth results in further embrittlement effects which are synergistic with that from the hydrogen isotope [4]. Therefore, it is important for tritium facilities to understand the material limitations of stainless steel in this environment. The Savannah River National Laboratory (SRNL) has available a large experimental data set of austenitic stainless steels which have been exposed to tritium environments for various lengths of time. With the availability of this data set, machine learning (ML) algorithms provide an opportunity to model the embrittlement of stainless steel due to the algorithm’s ability to identify patterns in data sets that are difficult and costly to identify in other manners [5]. Ultimately, the amount and quality of the available data is one defining force in the ability of a ML model to accurately predict the desired outputs. The models developed herein will illustrate the ability for the various algorithms to predict the change in fracture toughness in stainless steels due to hydrogen-isotope embrittlement.

Hoar, Eric T.↗

2016 Accomplishments. Tritium aging studies on stainless steel. Forging process effects on the fracture toughness properties of tritium-precharged stainless steel

Forged austenitic stainless steels are used as the materials of construction for pressure vessels designed to contain tritium at high pressure. These steels are highly resistant to tritium-assisted fracture but their resistance can depend on the details of the forging microstructure. During FY16, the effects of forging strain rate and deformation temperature on the fracture toughness properties of tritium-exposed-and-aged Type 304L stainless steel were studied. Forgings were produced from a single heat of steel using four types of production forging equipment – hydraulic press, mechanical press, screw press, and high-energy-rate forging (HERF). Each machine imparted a different nominal strain rate during the deformation. The objective of the study was to characterize the J-Integral fracture toughness properties as a function of the industrial strain rate and temperature. The second objective was to measure the effects of tritium and decay helium on toughness. Tritium and decay helium effects were measured by thermally precharging the as-forged specimens with tritium gas at 34.5 MPa and 350°C and aging for up to five years at -80°C to build-in decay helium prior to testing. The results of this study show that the fracture toughness properties of the as-forged steels vary with forging strain rate and forging temperature. The effect is largely due to yield strength as the higher-strength forgings had the lower toughness values. For non-charged specimens, fracture toughness properties were improved by forging at 871°C versus 816°C and Screw-Press forgings tended to have lower fracture toughness values than the other forgings. Tritium exposures reduced the fracture toughness values remarkably to fracture toughness values averaging 10-20% of as-forged values. However, forging strain rate and temperature had little or no effect on the fracture toughness after tritium precharging and aging. The result was confirmed by fractography which indicated that fracture modes in the tritium-exposed specimens were similar for all forgings. Another FY16 objective was to prepare fracture toughness specimens from Types 304L and 21-6-9 stainless steel weldments and heat-affected zones (HAZ) for tritium charging.

36 MATERIALS SCIENCE↗

Effect of heat input on dissimilar welds of ultra high strength steel and duplex stainless steel: Microstructural and compositional analysis

The effect of heat input on the microstructure and compositional heterogeneity of welds of direct-quenched ultra high strength steel (Optim 960 QC) and duplex stainless steel (UNS S32205) was studied. The dissimilar welds were made using GMAW with a fully austenitic filler wire. In addition to grain coarsening in the heat affected zone (HAZ) of the ferritic side, it was found that an increase in heat input correlatively increased the proportional volume of bainitic to martensitic phases. Coarse ferritic grains were observed in the duplex HAZ. Higher heat input, however, had a beneficial effect on the nucleation of austenite in the HAZ. Heat input had a regulatory effect on grain growth within the austenitic weld and more favorable equiaxed austenite was obtained with higher heat input. On the ferritic side of the welds, macrosegregation in the form of a martensitic intermediate zone was observed for all the cooling rates studied. However, on the duplex side, macrosegregation in the fusion boundary was only noticed with higher cooling rates. Microstructural observations and compositional analysis suggest that higher heat input could be beneficial for the structural integrity of the weld despite higher heat input increasing the extent of adverse coarse grains in the HAZ, especially on the ferritic side. - Highlights: •The effect of heat input on dissimilar welds of UHSS and DSS was studied. •Transmutation of the microstructure was discussed in detail. •The influence of heat input on compositional heterogeneity of welds was described. •Higher heat input enhanced bainitic transformation on the ferritic side. •Macrosegregation was affected by the amount of heat input on the DSS side.

36 MATERIALS SCIENCE↗

HYDROGEN-ASSISTED FRACTURE IN FORGED TYPE 304L AUSTENITIC STAINLESS STEEL

Austenitic stainless steels generally have good resistance to hydrogen-assisted fracture; however, structural designs for high-pressure gaseous hydrogen are constrained by the low strength of this class of material. Forging is used to increase the low strength of austenitic stainless steels, thus improving the efficiency of structural designs. Hydrogen-assisted racture, however, depends on microstructural details associated with manufacturing. In this study, hydrogen-assisted fracture of forged type 304L austenitic stainless steel is investigated. Microstructural variation in multi-step forged 304L was achieved by forging at different rates and temperatures, and by process annealing. High internal hydrogen content in forged type 304L austenitic stainless steel is achieved by thermal precharging in gaseous hydrogen and results in as much as 50% reduction of tensile ductility.

36 MATERIALS SCIENCE↗

SA508 low alloy steel to 316L stainless steel dissimilar metal joint made by powder metallurgy hot isostatic pressing

Joining ferritic SA508 low alloy steel (LAS) and austenitic 316 L stainless steel (SS) via powder metallurgy hot isostatic pressing (PM-HIP) was evaluated as an alternative method to welding. This study investigated the mechanical and microstructural evolutions of the bimetallic interface under different joint designs and heat treatments. Here, the direct joining of dissimilar metal alloys by PM-HIP method resulted in two designs: 1) powder SA508 to solid bar 316 L (P508–B316L) and 2) powder 316 L solid bar SA508 (P316L-B508). In both cases, P508–B316L and P316L-demonstrated satisfactory tensile strength, however, high hardness and severe depreciation in toughness were located on the bimetallic interface. The mechanisms responsible for the detrimental mechanical properties were verified. Large oxides were observed in P508–B316L due to the prior powder boundary (PPB) oxides present in SA508 powder. The intense sensitization occurred from the formation of M 23 C 6 carbides, consequently from the slow cooling after PM-HIP in P316L-B508. Post-HIP heat treatments were explored to reduce the distance of carbide formation; however, the heat treatment could not eliminate the carbides. The experimental results were compared to the diffusion couple simulation as a function of carbide formation with distance. The analysis also showed the high hardness at the bimetallic interface was primarily contributed by solid solution strengthening. In conclusion, the direct joining of P316L-B508 and P508–B316L via PM-HIP was deemed to be unfeasible, and a transitional material is necessary to impede the diffusion of carbon.

316L stainless Steel↗

Effect of microstructural and environmental variables on ductility of austenitic stainless steels

Austenitic stainless steels are used extensively in harsh environments, including for high-pressure gaseous hydrogen service. However, the tensile ductility of this class of materials is very sensitive to materials and environmental variables. While tensile ductility is generally insufficient to qualify a material for hydrogen service, ductility is an effective tool to explore microstructural and environmental variables and their effects on hydrogen susceptibility, to inform understanding of the mechanisms of hydrogen effects in metals, and to provide insight to microstructural variables that may improve relative performance. In this study, hydrogen precharging was used to simulate high-pressure hydrogen environments to evaluate hydrogen effects on tensile properties. Several austenitic stainless steels were considered, including both metastable and stable alloys. Room temperature and subambient temperature tensile properties were evaluated with three different internal hydrogen contents for type 304L and 316L austenitic stainless steels and one hydrogen content for XM-11. Significant ductility loss was observed for both metastable and stable alloys, suggesting the stability of the austenitic phase is not sufficient to characterize the effects of hydrogen. Internal hydrogen does influence the character of deformation, which drives local damage accumulation and ultimately fracture for both metastable and stable alloys. While a quantitative description of hydrogen-assisted fracture in austenitic stainless steels remains elusive, these observations underscore the importance of the hydrogen-defect interactions and the accumulation of damage at deformation length scales.

36 MATERIALS SCIENCE↗

Characterization of carbon ion implantation induced graded microstructure and phase transformation in stainless steel

Austenitic stainless steel 316L is ion implanted by carbon with implantation fluences of 1.2 × 10{sup 17} ions-cm{sup −} {sup 2}, 2.4 × 10{sup 17} ions-cm{sup −} {sup 2}, and 4.8 × 10{sup 17} ions-cm{sup −} {sup 2}. The ion implantation induced graded microstructure and phase transformation in stainless steel is investigated by X-ray diffraction, X-ray photoelectron spectroscopy and high resolution transmission electron microscopy. The corrosion resistance is evaluated by potentiodynamic test. It is found that the initial phase is austenite with a small amount of ferrite. After low fluence carbon ion implantation, an amorphous layer and ferrite phase enriched region underneath are formed. Nanophase particles precipitate from the amorphous layer due to energy minimization and irradiation at larger ion implantation fluence. The morphology of the precipitated nanophase particles changes from circular to dumbbell-like with increasing implantation fluence. The corrosion resistance of stainless steel is enhanced by the formation of amorphous layer and graphitic solid state carbon after carbon ion implantation. - Highlights: • Carbon implantation leads to phase transformation from austenite to ferrite. • The passive film on SS316L becomes thinner after carbon ion implantation. • An amorphous layer is formed by carbon ion implantation. • Nanophase precipitate from amorphous layer at higher ion implantation fluence. • Corrosion resistance of SS316L is improved by carbon implantation.

36 MATERIALS SCIENCE↗

Quantification of stress history in type 304L stainless steel using positron annihilation spectroscopy

Five Type 304L stainless steel specimens were subjected to incrementally increasing values of plastic strain. At each value of strain, the associated static stress was recorded and the specimen was subjected to positron annihilation spectroscopy (PAS) using the Doppler Broadening method. A calibration curve for the 'S' parameter as a function of stress was developed based on the five specimens. Seven different specimens (blind specimens labeled B1-B7) of 304L stainless steel were subjected to values of stress inducing plastic deformation. The values of stress ranged from 310 to 517 MPa. The seven specimens were subjected to PAS post-loading using the Doppler Broadening method, and the results were compared against the developed curve from the previous five specimens. It was found that a strong correlation exists between the 'S' parameter, stress, and strain up to a strain value of 15%, corresponding to a stress value of 500 MPa, beyond which saturation of the 'S' parameter occurs. Research Highlights: {yields} Specimens were initially in an annealed/recrystallized condition. {yields} Calibration results indicate positron annihilation measurements yield correlation. {yields} Deformation produced by cold work was likely larger than the maximum strain.

36 MATERIALS SCIENCE↗

Time-Dependent 600 °C Post-Weld Heat Treatment Response of Laser-Wire-Directed Energy Deposited Austenitic Stainless Steel Claddings on Carbon Steel

Austenitic stainless steel overlay claddings are often used to protect nuclear reactor pressure vessels from corrosion. Arc welding processes are traditionally employed, which require a high heat input to bond the dissimilar metals, creating a large heat-affected zone and high residual stress that demands a lengthy stress-relieving post-weld heat treatment, up to 48 hours. High energy beam (e.g., laser, electron beam) directed energy deposition-based overlay cladding processes show promise for fabricating claddings with superior performance compared to arc welded ones because of their localized heat input; however, their necessity and time of post-weld heat treatment are currently unclear. In this research, we investigate the time dependence of a 600 C stress-relieving post-weld heat treatment of austenitic stainless steel clad on low carbon steel by laser-wire-directed energy deposition, comparing the microstructure and mechanical properties of the as-fabricated condition to 2-, 10-, and 48-hour heat treatment times. Diffusion simulations and microscopy show a gradual carburization of the stainless steel cladding and decarburization of the heat-affected zone/base metal. Nanoindentation testing shows up to a 1.8–2.69 embrittlement in the cladding and a 0.33 to 0.69 softening in the heat-affected zone after the 48-hour post-weld heat treatment. Tensile testing of the cladding composites reveals that increasing post-weld heat treatment time raises clad cracking susceptibility due to intergranular carbide formation and shows that laser-wire-directed energy deposition claddings may not require post-weld heat treatment.

Coating↗

Study on tempering behaviour of AISI 410 stainless steel

Martensitic stainless steels find extensive applications due to their optimum combination of strength, hardness and wear-resistance in tempered condition. However, this class of steels is susceptible to embrittlement during tempering if it is carried out in a specific temperature range resulting in significant reduction in toughness. Embrittlement of as-normalised AISI 410 martensitic stainless steel, subjected to tempering treatment in the temperature range of 673–923 K was studied using Charpy impact tests followed by metallurgical investigations using field emission scanning electron and transmission electron microscopes. Carbides precipitated during tempering were extracted by electrochemical dissolution of the matrix and identified by X-ray diffraction. Studies indicated that temper embrittlement is highest when the steel is tempered at 823 K. Mostly iron rich carbides are present in the steel subjected to tempering at low temperatures of around 723 K, whereas chromium rich carbides (M{sub 23}C{sub 6}) dominate precipitation at high temperature tempering. The range 773–823 K is the transition temperature range for the precipitates, with both Fe{sub 2}C and M{sub 23}C{sub 6} types of carbides coexisting in the material. The nucleation of Fe{sub 2}C within the martensite lath, during low temperature tempering, has a definite role in the embrittlement of this steel. Embrittlement is not observed at high temperature tempering because of precipitation of M{sub 23}C{sub 6} carbides, instead of Fe{sub 2}C, preferentially along the lath and prior austenite boundaries. Segregation of S and P, which is widely reported as one of the causes for temper embrittlement, could not be detected in the material even through Auger electron spectroscopy studies. - Highlights: • Tempering behaviour of AISI 410 steel is studied within 673–923 K temperature range. • Temperature regime of maximum embrittlement is identified as 773–848 K. • Results show that type of carbide precipitation varies with temperature of tempering. • Mostly iron rich Fe{sub 2}C carbides are present in the embrittlement temperature range. • With the precipitation of M{sub 23}C{sub 6} carbides, recovery from the embrittlement begins.

36 MATERIALS SCIENCE↗

Anomalous Annealing Response of Directed Energy Deposited Type 304L Austenitic Stainless Steel

Directed energy deposited (DED) and forged austenitic stainless steels possess dissimilar microstructures but can exhibit similar mechanical properties. In this study, annealing was used to evolve the microstructure of both conventional wrought and DED type 304L austenitic stainless steels, and significant differences were observed. In particular, the density of geometrically necessary dislocations and hardness were used to probe the evolution of the microstructure and properties. Forged type 304L exhibited the expected decrease in measured dislocation density and hardness as a function of annealing temperature. Here, the more complex microstructure–property relationship observed in the DED type 304L material is attributed to compositional heterogeneities in the solidification microstructure.

36 MATERIALS SCIENCE↗

Understanding Uranium Binding Mechanisms and Speciation on Stainless Steel - 17462

Stainless steels have been exposed to nitric acid solutions containing natural uranium under similar conditions to those found in reprocessing plants. Solution and solid analysis of the stainless steel samples has been undertaken to describe the contamination phenomenon. General corrosion of the surface was seen to take place over the month-long experiments. Contamination has been shown on all exposed surfaces. Solution analysis indicates that an equilibrium state is reached after 2 weeks exposure to the 12 M HNO{sub 3}. Surface analysis through autoradiography and X-ray absorption near edge structure (XANES) indicate that multiple mechanisms of uptake may occur and consequently concentrated regions of contamination may be produced. (authors)

36 MATERIALS SCIENCE↗

Development of Advanced 9Cr Ferritic-Martensitic Steels and Austenitic Stainless Steels for Sodium-Cooled Fast Reactor

Ferritic-martensitic (FM) steel Grade 92, with or without thermomechanical treatment (TMT), and austenitic stainless steels HT-UPS (high-temperature ultrafine precipitate strengthening) and NF709 were selected as potential candidate structural materials in the U.S. Sodium-cooled Fast Reactor (SFR) program. The objective is to develop advanced steels with improved properties as compared with reference materials such as Grade 91 and Type 316H steels that are currently in nuclear design codes. Composition modification and/or processing optimization (e.g., TMT and cold-work) were performed to improve properties such as resistance to thermal aging, creep, creep-fatigue, fracture, and sodium corrosion. Testings to characterize these properties for the advanced steels were conducted by the Idaho National Laboratory, the Argonne National Laboratory and the Oak Ridge National Laboratory under the U.S. SFR program. This paper focuses on the resistance to thermal aging and creep of the advanced steels. The advanced steels exhibited up to two orders of magnitude increase in creep life compared to the reference materials. Preliminary results on the weldment performance of the advanced steels are also presented. The superior performance of the advanced steels would improve reactor design flexibility, safety margins and economics.

Sham, Sam↗