Analytical modeling of the evolution of the nonlinearity parameter of sensitized stainless steel

Austenitic stainless steels are subject to the precipitation of chromium carbides (M 23 C 6 ) during exposure to high temperatures, causing these alloys to be susceptible to intergranular corrosion due to chromium depletion along grain boundaries. The acoustic nonlinearity parameter, β, shows sensitivity to the formation of carbides in these alloys. The Thermo-Calc TC-PRISMA module was used to model the nucleation and growth of grain boundary M 23 C 6 carbides. The model was verified with scanning transmission electron microscopy analysis that allowed measurements of the grain boundary precipitates. The paper introduces a reduced-order model of the acoustic nonlinearity based on the formation of misfit dislocations at the interface of the grain boundary precipitate and matrix to explain the change in β during isothermal aging. Furthermore, a direct relationship between the radius of the M 23 C 6 grain boundary carbides and β was observed and verified with nonlinear ultrasound measurements on 304L and 316L stainless steels.

36 MATERIALS SCIENCE↗

Technical Note: Characterization of Corrosion Films Formed on Austenitic Stainless Steel in Supercritical CO 2 Containing H 2 O and O 2

Future technologies require structural alloys resistant to corrosion in supercritical CO 2 (sCO 2 ) fluids containing impurities such as H 2 O and O 2 . Traditional pipeline steels are potentially unsuitable for these environments and more corrosion resistant alloys such as stainless steels might be required. Little is known about the corrosion products formed on, and hence the processes which control corrosion of, stainless steels in impure sCO 2 environments. In this study, austenitic stainless steel 347H (UNS S34709) was exposed to sCO 2 containing H 2 O and O 2 at 8 MPa and 50°C or 250°C, and separately to the aqueous phase in equilibrium with the sCO 2 at 50°C, to simulate conditions expected in sCO 2 -based power cycles and carbon capture and storage pipelines. Only thin (< 20 nm) surface films formed after 500 h resulting in small mass changes and corrosion rates < 10 –4 mm/y, suggesting the material resists significant degradation in these environments. X-ray photoelectron spectroscopy and transmission electron microscopy were used to characterize the corrosion films in detail. Here, the exposure to the aqueous phase resulted in a thin (< 5 nm) Cr-oxide and/or -hydroxide passive film, while exposure to sCO 2 phases resulted in a multilayer Fe-rich oxide structure characteristic of a gas-phase oxidation process.

36 MATERIALS SCIENCE↗

Characterization of Precipitation-Strengthening Heat-Resistant Austenitic Stainless Steels for Life-Prediction Modeling

In this study, the role of minor alloying additions in 347H stainless steels (UNS34709, ASTM A240/240M) on creep-rupture properties at 650-750°C and microstructure evolution during isothermal exposure at 750°C has been investigated, aiming to provide the experimental dataset as boundary conditions of physics-based modeling for material/component life prediction. Four different 347H heats containing various amounts of boron and nitrogen additions were prepared and evaluated. The combined additions of B and N are found to stabilize the strengthening secondary M23C6 carbides and retarding the transition from M23C6 to sigma phase precipitates during thermal exposure. The observed kinetics of microstructure evolution reasonably explains the improvement of creep-rupture properties of 347H stainless steels with the B and N additions.

Yamamoto, Yukinori↗

Effect of the Heat Treatment on the Corrosion Resistance of Duplex Stainless Steels

Duplex stainless steels (DSS) are biphasic austenitic-ferritic steels in which the best combination of mechanical and corrosion resistance properties is achieved for an almost equal volume fraction of the phases. In this work, the effect of secondary phases precipitation on the corrosion resistance of four DSS grades (2101, 2304, 2205 and 2507), after isothermal aging in the critical temperature range 750-900 °C, was studied. The corrosion resistance was investigated by potentiodynamic polarization tests in both 0.6 M NaCl solution (pH 7) and in an acid chlorinated solution (pH 3) at room temperature. Moreover, the critical pitting temperature was determined according to ASTM G150. The results showed that secondary phases precipitation mainly influenced the resistance to corrosion of the lean duplex grades.

36 MATERIALS SCIENCE↗

Micro-Abrasion Wear Resistance of Borided 316L Stainless Steel and AISI 1018 Steel

The 316L stainless steel has high corrosion resistance but low tribological performance. In different industrial sectors (biomedical, chemical, petrochemical, and nuclear engineering), improvement upon wear resistance of 316L stainless steel components using accessible and inexpensive methods is critical. The AISI 1018 steel is widely used in industry, but its tribological performance is not the best among steels. Therefore, in this study the behavior of the borided 316L stainless steel and 1018 steel is evaluated under micro-abrasion wear. The boriding was carried out at 1223 K over 6 h of exposure time, resulting in a biphase layer composed of FeB/Fe{sub 2}B phases. In order to evaluate Fe{sub 2}B phase with no influence from FeB phase, AISI 1018 steel samples were borided at 1273 K for over 20 min and then diffusion annealed at 1273 K over 2 h to obtain a Fe{sub 2}B mono-phase layer. Micro-abrasion wear resistance was evaluated by a commercial micro-abrasion testing rig using a mix of F-1200 SiC particles with deionized water as abrasive slurry. The obtained wear rates for FeB and Fe{sub 2}B phases and for the 316L stainless steel were compared. Wear resistance of 316L stainless steel increases after boriding. The wear mechanisms for both phases and for the stainless steel were identified. Also, transient conditions for rolling and grooving abrasion were determined for the FeB and Fe{sub 2}B phases.

36 MATERIALS SCIENCE↗

Mechanical property degradation and microstructural evolution of cast austenitic stainless steels under short-term thermal aging

Mechanical testing and microstructural characterization were performed on short-term thermally aged cast austenitic stainless steels (CASS) to understand the severity and mechanisms of thermal-aging degradation experienced during extended operation of light water reactor (LWR) coolant systems. Four CASS materials – CF3, CF3M, CF8, and CF8M – were thermally aged for 1500 hours at 290 °C, 330 °C, 360 °C, and 400 °C. All four alloys experienced insignificant change in strength and ductility properties but a significant reduction in absorbed impact energy. The primary microstructural and compositional changes during thermal aging were spinodal decomposition of the δ-ferrite into α/ α`, precipitation of G-phase in the δ-ferrite, segregation of solute to the austenite/ ferrite interphase boundary, and growth of M23C6 carbides on the austenite/ferrite interphase boundary. These changes were shown to be highly dependent on chemical composition, particularly the concentration of C and Mo, and aging temperature. A comprehensive model is being developed to correlate the microstructural evolution with mechanical behavior and simulation for predictive evaluations of LWR coolant system components.

36 MATERIALS SCIENCE↗

Three-Dimensional Morphological and Chemical Evolution of Nanoporous Stainless Steel by Liquid Metal Dealloying [3D Morphological and Chemical Evolution of Nanoporous Stainless Steel by Liquid Metal Dealloying]

Nanoporous materials, especially those fabricated by liquid metal dealloying processes, possess great potential in a wide range of applications due to their high surface area, bicontinuous structure with both open pores for transport and solid phase for conductivity or support, and low material cost. Here, we used X-ray nanotomography and X-ray fluorescence microscopy to reveal the three-dimensional (3D) morphology and elemental distribution within materials. Focusing on nanoporous stainless steel, we evaluated the 3D morphology of the dealloying front and established a quantitative processing-structure-property relationship at a later stage of dealloying. The morphological differences of samples created by liquid metal dealloying and aqueous dealloying methods were also discussed. Here, we concluded that it is particularly important to consider the dealloying, coarsening, and densification mechanisms in influencing the performance-determining, critical 3D parameters, such as tortuosity, pore size, porosity, curvature, and interfacial shape.

36 MATERIALS SCIENCE↗

Nonlinear resonant ultrasound spectroscopy of stress corrosion cracking in stainless steel rods

Stainless steel containers are susceptible to stress corrosion cracking (SCC) under certain stress and corrosion conditions. Nonlinear ultrasonic techniques are very sensitive to the early presence of damage, more so than linear techniques. Nonlinear Resonant Ultrasound Spectroscopy (NRUS) is used here to measure a nonlinear shift in the resonance frequency due to a cumulative amount of SCC. Steel rods are immersed in a heated magnesium chloride solution and removed after different exposure times. NRUS measurements are conducted using the fundamental longitudinal mode of vibration. Rods exposed longer generally have a larger resonance frequency shift and are therefore more nonlinear. Thus NRUS might offer a means of detecting a cumulative SCC damage in a sample.

36 MATERIALS SCIENCE↗

Towards directed energy deposition of metals using polymer-based supports: porosity of 316L stainless steel deposited on carbon-fiber-reinforced ABS

Directed energy deposition (DED) is increasingly valuable to many industries because of its high deposition rates relative to other metal additive manufacturing processes, but the design space of DED is limited. For instance, steep overhangs are difficult or impossible to manufacture. Polymer-based support structures could help address this challenge. The viability of DED on polymer composite substrates has begun to be explored, specifically with 316L stainless steel on carbon-fiber-reinforced ABS substrates. Monolithic metal components can be deposited on the polymer, but it was found that gas release during polymer degradation causes porosity due to gas entrapment in the metal. An interlayer cooling time was introduced to reduce polymer degradation and decrease the porosity due to gas entrapment, but this led to porosity from lack of fusion. The results of this work provide insight into process parameter selection and scan strategy development to enable the use of polymer support structures in blown-powder DED.

Kurfess, Rebecca↗

Microstructure, hardness and cavitation erosion resistance of different cold spray coatings on stainless steel 316 for hydropower applications

There is an urgent need for repair of hydropower components that have undergone damage due to cavitation. Conventional repair methods involve melting of materials and can deteriorate material properties and cause distortion. This study investigated the relevant properties of different materials using solid phase processing—cold spray technology. Stainless steel (SS) 316, Inconel 625 and CrC-NiCr materials were cold spray deposited onto base metal SS 316, respectively. Cold spray achieved dense uniform deposits with low level porosity, and intimate contact between the deposit and the base metal was observed. Severe plastic deformation imparted during the cold spray process resulted in significant grain size refinement, nanostructured regions were observed in the deposits across the interfacial area. Cold sprayed deposits exhibited elevated hardness in contrast to that of the base metal SS 316. The cavitation erosion resistance of the deposits was evaluated with a cavitation erosion jet adhering to ASTM G134. Both SS 316 and Inconel 625 achieved better cavitation erosion resistance when compared to that of the SS 316 base metal, with the former exhibiting close to a 4 times improvement.

Jiang, Xiujuan↗

Effects of long-term thermal aging on bulk and local mechanical behavior of ferritic-austenitic duplex stainless steels

Ferritic-austenitic duplex stainless steels (DSS) undergo significant thermal aging embrittlement in service in light water reactors. Specimens of cast CF–3 and CF–8 DSS have been laboratory aged for up to 17,200 h at four different temperatures (280, 320, 360, 400 °C) in order to characterize the aging evolution and mechanical properties. Standard Charpy V-Notch (CVN) impact testing and tensile testing are employed to measure the progression of embrittlement of the steels. Concurrently, nanoindentation measurements are performed to measure the hardening of the individual ferrite and austenite phases. Atom probe tomography (APT) analysis of the ferrite and austenite phases elucidates the relationship between spinodal decomposition of the ferrite and the mechanical effects of aging. The results are discussed to relate the effects of the local microstructure and property changes in the ferrite phase on the overall bulk mechanical evolution of these steels.

Schwarm, Samuel C.↗

Effects of Thermal Aging on the Fracture Toughness of Cast Stainless Steel CF8

Cast stainless steels are widely used in the primary coolant systems of nuclear power plants because of their high strength, toughness, and corrosion resistance. Mechanical property degradation in the steels, primarily due to a thermally-embrittled ferrite, is of major concern in an extended-term operation. To investigate the aging-induced loss of fracture resistance in cast stainless steels, static fracture resistance (J-R) testing was performed for three different CF8 cast stainless steels with significantly different d-ferrite contents. The materials were thermally-aged at 290-400°C for up to 10kh and fracture-tested at 25-400°C. It was found that the fracture toughness in high-ferrite materials generally decreased with thermal aging while the relationship between aging and fracture toughness in low-ferrite materials was rather complicated, showing non-monotonic variation with the degree of aging. While significant degradation was observed for the highly-aged high-ferrite materials, no material was observed having a K0.2mm less than 100 MPavm.

Collins, David A.↗

Evolution of {delta}ferrite in a CF3 cast stainless steel upon neutron irradiation to 3, 5, 10, 20, and 40 dpa

The microstructural evolution of delta ferrite in a CF3 cast stainless steel irradiated to 3, 5, 10, 20, and 40 dpa with two dose rates was studied with atom probe tomography (APT) and transmission electron mi-croscopy. Spinodal decomposition and G-phase precipitates induced by neutron irradiation and thermal aging were quantified systematically. The neutron irradiation significantly enhances the spinodal decom-position in delta ferrite as both the spinodal wavelength (i.e. a characteristic repeat distance) and am-plitude (i.e. magnitude of elemental concentration fluctuation) increase after irradiation. The wavelength only varies slightly when the dose increases from 5 to 40 dpa, while the amplitude increases dramatically from 10 to 20 dpa and starts to saturate before 20 dpa. The dose rate and irradiation temperature also have a notable effect on the spinodal wavelength and amplitude. The study shows that higher dose rate promotes a larger wavelength at given irradiation doses. Regarding the G-phase precipitates, a slightly lower irradiation temperature would result in a smaller mean size of G-phase precipitates, while a lower irradiation dose rate would lead to a larger G-phase precipitates at a given temperature and dose. Over-all, the spinodal decomposition and G-phase precipitates in the delta ferrite continue to evolve with the increasing dose beyond 10 dpa. This study confirms that the formation of G-phase precipitates at the in-terdomain region between alpha and alpha-prime is facilitated by the Si and Mo atoms rejected from Fe rich alpha phase and the Ni and Mn atoms rejected from Cr rich alpha-prime phase. Neutron irradiation plays a dominant role in the ferrite instability, and the effect of prior thermal aging at 400 degrees C for 10,000 hours is negligible as the dose is 3 dpa and above.

duplex stainless steel↗