SEARCH · Search NASA
Results for “Selective Laser Melting”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Synthesis of precipitation-strengthened Al-Sc, Al-Zr and Al-Sc-Zr alloys via selective laser melting of elemental powder blends
Selective laser melting is used to create Al-1.5Sc, Al-1.5Zr and Al-0.75Sc-0.75Zr (at.%) alloys from blends of elemental Al, Sc, and Zr powders. This study investigates elemental alloying elements (Sc and Zr) which are high-melting and highly reactive, unlike previous work which focused on more concentrated elemental additions of lower-melting, lower-reactivity Cu and Si to aluminum. High-speed in situ synchrotron x-ray imaging and diffraction show that the 20–30 μm Al, Sc, and Zr powders fully melt and sufficiently mix in the molten state to create, on solidification, a homogeneous distribution of primary, micron-size L12 precipitates (Al 3 Sc, Al 3 Zr, and Al 3 (Sc,Zr), respectively) and nucleate micron-size Al matrix grains, as confirmed by SEM imaging of cross-sections. Here, a second laser pass, simulating a realistic additive-manufacturing build condition, fully remelts the initial volume which shows, after solidification, the same Al 3 (Sc,Zr) L1 2 primary micro-precipitates and very fine Al grains. After aging at 300–400°C, the alloys show large increases in hardness, consistent with an exceptionally high number density (1.4 × 10 24 m –3 ) and volume fraction (2.5%) of secondary Al 3 (Sc,Zr) nano-precipitates with a Sc-rich core and Zr-rich shell, as measured via atom-probe tomography.
Effect of processing parameters and build orientation on microstructure and performance of AISI stainless steel 304L made with selective laser melting under different strain rates
Selective laser melting (SLM) process brings diverse potentials on geometry flexibility; therefore, it is more and more widespread to be employed in fabrication metal alloys served for industries. Nonetheless, a material characterization study is desired to carry on for better understanding the correlation among process, structure, microstructure, and performance. In the current study, the SLM fabricated AISI stainless steel 304L was fabricated with different process parameters and built orientations (horizontal, inclined, and vertical. The tensile behavior was evaluated under different strain rates (0.0001 /s, 0.001 /s, 0.01 /s, and 0.1 /s) and compared to the commercial cold-rolled and annealed counterpart. Grain structures, tensile strength, elongation-to-failure, strain rate sensitivity, work hardening, and fractographic analysis were evaluated in terms of the effect of energy density, build orientation, and strain rate. The output indicates the tensile strength increases with increasing strain rates. On the contrary, the elongation-to-failure shows a decreasing trend with strain rates. Tensile properties of specimens built in the horizontal and inclined orientations are more sensitive to strain rates due to the smaller dimension of grain structures. Tensile anisotropy depends on the energy input, where a high energy density could yield a strong build orientation-dependent anisotropy. Hall-Petch relationship is validated to explain the mechanical anisotropy in different built orientations for SLM alloys. The strain hardening exponent and work hardening rate are demonstrated to be positively correlated, and they increase with smaller grain sizes. The fine dimple features indicate the ductile fracture mode regardless of strain rates. The size of the ductile dimples seems to depend on the strain rates and build orientations.
Laser Weldability of AlSi{sub 10}Mg Alloy Produced by Selective Laser Melting: Microstructure and Mechanical Behavior
Selective laser melting (SLM) allows 3D complex parts to be produced with integrated functionalities but does not permit to realize large dimension parts, as the building chamber volume of commercial SLM systems is limited. Therefore, the possibility of joining SLM-built parts by welding appears as extremely valuable. In this work, laser weldability of SLMed AlSi{sub 10}Mg parts has been investigated. The cooling rates induced by the welding process are lower than the ones of SLM; therefore, typical eutectic silicon network of SLM-built parts appears broken in both the melted zone and part of the heat-affected zone, as confirmed by calorimetric measurement. This microstructural evolution caused a local decrease of hardness from 132 HV to 73 HV and a reduction of ductility caused by porosity formation in the weld bead. Moreover, the thermal treatment, performed at 320°C, can limit the gap of tensile response among welded bead and base SLM material.
Particle Scale Melt Modeling of Selective Laser Melting with Uncertainty Quantification.
Abstract not provided.
Effect of Process Parameters on the Mechanical Properties of Hastelloy X Alloy Fabricated by Selective Laser Melting
Mechanical properties of Hastelloy X alloys fabricated by selective laser melting were investigated and compared with the wrought counterpart. Nano-inclusions (Mo-rich carbides) distributed at the sub-grain boundaries in the selective laser-melted (SLMed) Hastelloy X alloy, whereas micron-scale precipitations existed in the wrought counterpart. The molten pool boundaries widely existed in the SLMed substrate, which acted as an initial site for crack and led to poor plasticity. However, the ultimate tensile strength values of the SLMed Hastelloy X alloys were around 910 MPa and much higher than the wrought counterpart (~ 750 MPa), which was mainly ascribed to the high-density dislocations enriched at the sub-grain boundaries. Process parameter effects on the mechanical properties were also delineated in this work, and the volumetric energy density for the best mechanical properties of the SLMed Hastelloy X alloy was in the range from 140 to 170 J/mm{sup 3}.
High-speed X-ray investigation of melt dynamics during continuous-wave laser remelting of selective laser melted Co-Cr alloy
The objective of this study is to quantify the melt pool dynamics during continuous-wave laser remelting of a Co-Cr alloy manufactured using selective laser melting. This knowledge will inform process improvement and numerical modeling of laser remelting. A high-intensity x-ray beam imaged a 2 mm × 0.5 mm area of the surface with a 50 kHz framerate. Analysis of these videos quantified the melt pool surface wave movement and compared this to the initial surface features. Here, the results indicate that the keyhole and its characteristic oscillations can suppress large wavelength features on the initial surface.
Thermo-Fluid Modeling of Selective Laser Melting: Single-Track Formation Incorporating Metallic Powder
Selective laser melting (SLM) utilizes a laser source to melt and fuse metallic particles to form dense solid parts. Since molten metals have surface tension gradients, the thermo-capillary effect becomes a driving force of melt flow, which will subsequently determine the molten/solidified track as well as the build surface morphology. In this study, a 3D volume of fluid model has been developed to simulate heat transfer and fluid dynamic during single-track laser scanning. A sequential powder addition algorithm is applied to obtain random powder distribution over a thick substrate. Temperature-dependent thermo-physical properties of Ti-6Al-4V are used to define the material, and a volumetric heat source is included as an approximation to laser irradiation. As a result of continuous melting and solidifying, the thermal behavior, the molten metal flow and the free surface formation can be numerically analyzed. In addition, a two-layer simulation has been carried out to study the interlayer bonding. Simulations results are compared with SLM experiments using the single-track morphology acquired by white-light interferometry. The melt pool widths obtained from simulations are in good agreement with the measured single-track widths. On the other hand, it is observed that single tracks formed in SLM have an elevated bead height, which is not realized numerically.
Build Orientation Effects on Texture and Mechanical Properties of Selective Laser Melting Inconel 718
The production of components via selective laser melting (SLM) metal additive manufacturing results in microstructures unique to the process that are highly dependent on laser processing parameters and orientation of part geometry relative to the build direction. This study investigates the variation in tensile properties of SLM Inconel 718 at varying angles with respect to build direction. ASTM E8 tensile specimens were built in XY, Z, and B+45 from Z orientations to near-net shape, HIP and heat treated, and tensile tested at room temperature. Orientation dependence of mechanical properties was observed; Z samples had the lowest strength and highest elongation, while XY samples had the highest strength and lowest elongation. Optical, SEM, and EBSD analysis were conducted to probe for microstructure variation that could be the cause of the difference in mechanical properties. Analysis of pole figures and grain maps suggests a preferred grain texture and twinning orientation that aligns with the build direction, which may contribute to the anisotropic enhancement in ductility.
Microstructural Evolution and Properties of 24CrNiMoY Alloy Steel Fabricated by Selective Laser Melting
24CrNiMoY alloy steel samples were fabricated by selective laser melting (SLM), and a phase transformation model was established to study the alloy steel microstructural evolution. Meanwhile, microhardness and tensile properties of 24CrNiMoY alloy steel prepared by different laser energy densities (E{sub v}) were investigated. Results indicate that the microstructural evolution of 24CrNiMoY alloy steel is consistent with the phase transformation model. The main microstructure changed from martensite to bainite with the increase in thermal cycle numbers. In addition, a suitable E{sub v} plays an important role in refining the bainite structure and improving the alloy steel properties. When the E{sub v} decreases from 210 to 140 J/mm{sup 3}, the bainite lath width reduces from 1.7 to 0.6 μm. Simultaneously, the relative density, tensile strength and microhardness of the fabricated samples increase first and decrease later. 24CrNiMoY alloy steel sample prepared by 160 J/mm{sup 3} has fine mechanical properties: The tensile strength is 850 MPa and microhardness is 360 HV{sub 0.2}.
The Effect of Sulfuric Acid Anodization on the Electrochemical Properties of Aluminum Alloy AlSi 10 Mg Prepared by Selective Laser Melting
Aluminum alloy, AlSi 10 Mg, prepared by selective laser melt (SLM) fabrication was anodized in 9.8% sulfuric acid (Type II) at 15 V for a total of 23 min. Experiments were performed to study the potentiostatic anodization process and its effects on the oxide coating morphology, thickness, and electrochemical properties of the alloy. Prior to anodization, the alloy microstructure is composed of aluminum cells encapsulated in a silicon network. Anodizing the abraded and polished AlSi 10 Mg surface produced a porous oxide layer with a thickness of 5μm. The oxide coating weight was 698 ± 29 mg/ft 2 . The oxide coating forms in the aluminum cells that are isolated from one another by the silicon eutectic phase. In electrochemical tests, the anodic and cathodic potentiodynamic polarization currents were suppressed by factors of 15× and 215×, respectively, as compared to the unanodized controls. The data indicate the anodic oxide coating suppresses the cathodic more than the anodic reaction rate. Linear polarization resistance (R p ) values increased by 279× after anodization. The corrosion current density values (j corr ) decreased by 133× after anodization. Taken together, the electrochemical data indicate the anodic oxide coating (unsealed) increases the corrosion resistance of the SLM alloy by two orders of magnitude.
Size dependence of microstructure of AlSi10Mg alloy fabricated by selective laser melting
Highlights: • Plate-shaped samples with various widths were fabricated via selective laser melting. • The hardness of AlSi10Mg samples slightly decreased with decreasing sample width. • The alloy sample size had a slight effect on microstructure of the α-Al matrix. • Precipitation of Si phase in α-Al matrix was enhanced by reducing the sample size. • The softening by reducing sample size is likely due to their slower cooling rate. - Abstract: In order to investigate the size dependence of microstructure of the AlSi10Mg alloy fabricated by selective laser melting (SLM) combined with a powder bed technique, plate-shaped AlSi10Mg alloy samples with various widths (ranging from approximately 10 mm to 0.3 mm) were produced in this study. All the fabricated samples exhibited characteristic microstructural morphologies consisting of melt pools with columnar α-Al grains surrounded by fine eutectic Si particles, whereas their sample sizes had a relatively small effect on the texture and average grain size of the α-Al matrix. However, the formation of fine Si precipitates inside the columnar α-Al grains was observed more often for the smaller-sized samples, which could be a possible dominant contributor to the observed softening of the sample by reducing sample size. The obtained results were utilized for discussing the size dependence of the strength of the SLM-manufactured porous alloy samples.
Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment
The selective laser melting of high temperature alloys is of great interest to the aerospace industry as it offers the prospect of producing more complex geometries than can be achieved with other manufacturing methods. In this study, the microstructure of the nickel-based superalloy, CM247LC, has been characterised following selective laser melting and after a post deposition heat treatment below the γ′ solvus temperature. In the as-deposited state, scanning electron microscopy with electron backscatter diffraction revealed a fine, cellular microstructure with preferential alignment of 〈001〉 along the build direction. A high dislocation density was seen at the periphery of the cells, indicating substantial localised deformation of the material. Fine primary MC carbides were also observed in the inter-cellular regions. High-resolution transmission electron microscopy identified the occurrence of very fine γ′ precipitates, approximately 5 nm in diameter, dispersed within the gamma phase. After heat treatment, the elongated cell colonies were observed to partially coalesce, accompanied by a decrease in dislocation density, producing columnar grains along the build direction. Cuboidal γ′ precipitates approximately 500 nm in diameter were observed to form in the recrystallised grains, accompanied by larger γ′ precipitates on the grain boundaries.
Effect of Hot Isostatic Pressing and Powder Feedstock on Porosity, Microstructure, and Mechanical Properties of Selective Laser Melted AlSi10Mg
AlSi10Mg tensile bars were additively manufactured using the powder-bed selective laser melting process. Samples were subjected to stress relief annealing and hot isostatic pressing. Tensile samples built using fresh, stored, and reused powder feedstock were characterized for microstructure, porosity, and mechanical properties. Fresh powder exhibited the best mechanical properties and lowest porosity while stored and reused powder exhibited inferior mechanical properties and higher porosity. The microstructure of stress relieved samples was fine and exhibited (001) texture in the z-build direction. Microstructure for hot isostatic pressed samples was coarsened with fainter (001) texture. To investigate surface and interior defects, scanning electron microscopy, optical fractography, and laser scanning microscopy techniques were employed. Hot isostatic pressing eliminated internal pores and reduced the size of surface porosity associated with the selective laser melting process. Hot isostatic pressing tended to increase ductility at the expense of decreasing strength. Furthermore, scatter in ductility of hot isostatic pressed parts suggests that the presence of unclosed surface porosity facilitated fracture with crack propagation inward from the surface of the part.
Numerical Analysis of Molten Pool Behavior and Spatter Formation with Evaporation During Selective Laser Melting of 316L Stainless Steel
During the selective laser-melting process, material evaporation and resultant spatter are common phenomena that bring about many defects. However, the underlying physical phenomena such as molten pool behavior and spatter formation, as evaporation occurred, are sparsely understood and difficult to observe during the process. Thus, a three–dimensional powder-scale model was established to investigate the thermal and flow behavior of the molten pool, the morphology evolution of the molten pool and keyhole, and the spatter formation with evaporation in the selective laser-melting processing of 316L stainless steel. Phase transitions and variations in interfacial force were taken into account in this model. The modified phase-field method was applied to trace the melt–gas interface. The results showed that keyhole formed in molten pool under recoil pressure, and that there were some differences in the temperature distribution and flow behavior inside and outside the keyhole. In addition, the dimension and surface morphology of the molten pool and keyhole depth altered and gradually stabilized during the process. Moreover, droplet spatter formation at rear of molten pool proceeded roughly as follows: the backward ejection of melt vapor would induce a depression in molten pool and a bump on the molten pool surface, the bump moved backward and subsequently a liquid column formed, then the liquid column formed a neck and gradually pinched off, resulting in the droplet spatter. Furthermore, the characteristic morphology of the scan track and dimension of the molten pool were obtained through experiments, which showed good agreement with the simulation results.
Determination of Strain Rate Sensitivity of Micro-struts Manufactured Using the Selective Laser Melting Method
Micro-lattice structures manufactured using the selective laser melting (SLM) process provides the opportunity to realize optimal cellular materials for impact energy absorption. In this paper, strain rate-dependent material properties are measured for stainless steel 316L SLM micro-lattice struts in the strain rate range of 10{sup −3} to 6000 s{sup −1}. At high strain rates, a novel version of the split Hopkinson Bar has been developed. Strain rate-dependent materials data have been used in Cowper–Symonds material model, and the scope and limit of this model in the context of SLM struts have been discussed. Strain rate material data and the Cowper–Symonds model have been applied to the finite element analysis of a micro-lattice block subjected to drop weight impact loading. The model output has been compared to experimental results, and it has been shown that the increase in crush stress due to impact loading is mainly the result of strain rate material behavior. Hence, a systematic methodology has been developed to investigate the impact energy absorption of a micro-lattice structure manufactured using additive layer manufacture (SLM). This methodology can be extended to other micro-lattice materials and configurations, and to other impact conditions.
Effect of Heat Treatment on Microstructure Evolution and Mechanical Properties of Selective Laser Melted Inconel 718 Alloy
The microstructure characteristics of the selective laser melted Inconel 718 alloy under as-deposited, homogenization + solution + aging (HSA) and solution + aging (SA) conditions were studied. The anisotropy and heterogeneity of mechanical properties under different conditions were also investigated. Under the as-deposited condition, the morphology and size of the grains are heterogeneous. The dendrite structures which grow nearly perpendicular to the molten pool traces, accompanying interdendritic Laves phase, can be observed within the grains. The dendrite structure completely disappeared, and the Laves phases embedded in the interdendritic regions also dissolved into the matrix to precipitate γ′ and γ″ phases after heat treatments. Fully recrystallized grains were obtained under the HSA condition, while only incomplete recrystallized grains were obtained under the SA condition. However, the characteristics of γ′ and γ″ phases are very similar under the HSA and SA conditions. Significant improvement in strength after heat treatments was due to the dissolution of undesirable Laves phase and the precipitation of γ′ and γ″ phases. For all the three conditions, different tensile properties were observed depending on the orientation of the specimens. The scatter of mechanical properties is notable, and heat treatments increased the scatter of mechanical properties.
Uncertainties Induced by Processing Parameter Variation in Selective Laser Melting of Ti6Al4V Revealed by In-Situ X-ray Imaging
Selective laser melting (SLM) additive manufacturing (AM) exhibits uncertainties, where variations in build quality are present despite utilizing the same optimized processing parameters. In this work, we identify the sources of uncertainty in SLM process by in-situ characterization of SLM dynamics induced by small variations in processing parameters. We show that variations in the laser beam size, laser power, laser scan speed, and powder layer thickness result in significant variations in the depression zone, melt pool, and spatter behavior. On average, a small deviation of only ~5% from the optimized/reference laser processing parameter resulted in a ~10% or greater change in the depression zone and melt pool geometries. For spatter dynamics, small variation (10 μm, 11%) of the laser beam size could lead to over 40% change in the overall volume of the spatter generated. The responses of the SLM dynamics to small variations of processing parameters revealed in this work are useful for understanding the process uncertainties in the SLM process.