Effect of Si Content in Electrode and SiO2 Additions to the Slag during Electroslag Remelting

Evolution of Si concentration in 316 stainless steel electrodes was observed during a melting campaign consisting of recycling electroslag remelted (ESR) ingots to make new electrodes using vacuum induction melting (VIM). This campaign consisted of iterations of VIM + ESR operations to optimize melting parameters. The effect of Si content on the melt parameters and ingot quality was further evaluated and additions of SiO2 to the slag chemistry were studied using research-scale experiments, x-ray diffraction (XRF), combustion analysis, visual inspections, and computational tools. The Si concentration was found to decrease by approximately 600 ppm following ESR of 150 lb. research-scale electrodes. Eventually, this led to failure of the slag skin and direct ingot/crucible contact. Additions of SiO2 to the slag at levels matching the original calculated Si concentration in the electrode did not eliminate the slag skin failure and the current during steady state increased to maintain a constant melt rate. In this investigation, we propose a mechanism of slag skin failure consisting of local concentration of current density due to absence, or breakage, of the SiO2 layer around the molten metal drop during ESR. This theory was reinforced by additional experiments in which Nb was added to the electrode to change the structure of the oxide layer around the drops.

Jablonski, Paul↗

Multifunctional Properties of Cyanate Ester Composites with SiO2 Coated Fe3O4 Fillers

SiO2 coated Fe3O4 submicrometer spherical particles (a conducting core/insulating shell configuration) are fabricated using a hydrothermal method and are loaded at 10 and 20 vol % into a bisphenol E cyanate ester matrix for synthesis of multifunctional composites. The dielectric constant of the resulting composites is found to be enhanced over a wide frequency and temperature range while the low dielectric loss tangent of the neat cyanate ester polymer is largely preserved up to 160 ?C due to the insulating SiO2 coating on individual conductive Fe3O4 submicrometer spheres. These composites also demonstrate high dielectric breakdown strengths at room temperature. Dynamic mechanical analysis indicates that the storage modulus of the composite with a 20 vol % filler loading is twice as high as that of neat resin, but the glass transition temperature considerably decreases with increasing filler content. Magnetic measurements reveal a large saturation magnetization and negligibly low coercivity and remanent magnetization in these composites.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 crystallizes in the triclinic P-1 space group. The structure is one-dimensional and consists of one SiO2 ribbon oriented in the (0, 1, 0) direction. there are eight inequivalent Si4+ sites. In the first Si4+ site, Si4+ is bonded to four O2- atoms to form a mixture of corner and edge-sharing SiO4 tetrahedra. There is three shorter (1.66 Å) and one longer (1.68 Å) Si–O bond length. In the second Si4+ site, Si4+ is bonded to four O2- atoms to form a mixture of corner and edge-sharing SiO4 tetrahedra. There is three shorter (1.66 Å) and one longer (1.68 Å) Si–O bond length. In the third Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. All Si–O bond lengths are 1.65 Å. In the fourth Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. All Si–O bond lengths are 1.65 Å. In the fifth Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. All Si–O bond lengths are 1.65 Å. In the sixth Si4+ site, Si4+ is bonded to four O2- atoms to form a mixture of corner and edge-sharing SiO4 tetrahedra. There is three shorter (1.66 Å) and one longer (1.68 Å) Si–O bond length. In the seventh Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. All Si–O bond lengths are 1.65 Å. In the eighth Si4+ site, Si4+ is bonded to four O2- atoms to form a mixture of corner and edge-sharing SiO4 tetrahedra. There is three shorter (1.66 Å) and one longer (1.68 Å) Si–O bond length. There are sixteen inequivalent O2- sites. In the first O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the second O2- site, O2- is bonded in an L-shaped geometry to two Si4+ atoms. In the third O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the fourth O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the fifth O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the sixth O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the seventh O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the eighth O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the ninth O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the tenth O2- site, O2- is bonded in an L-shaped geometry to two Si4+ atoms. In the eleventh O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the twelfth O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the thirteenth O2- site, O2- is bonded in an L-shaped geometry to two Si4+ atoms. In the fourteenth O2- site, O2- is bonded in an L-shaped geometry to two Si4+ atoms. In the fifteenth O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms. In the sixteenth O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 crystallizes in the triclinic P1 space group. The structure is two-dimensional and consists of one SiO2 sheet oriented in the (0, 0, 1) direction. there are four inequivalent Si4+ sites. In the first Si4+ site, Si4+ is bonded in a distorted single-bond geometry to two O2- atoms. There is one shorter (1.10 Å) and one longer (1.43 Å) Si–O bond length. In the second Si4+ site, Si4+ is bonded in a distorted single-bond geometry to three O2- atoms. There are a spread of Si–O bond distances ranging from 1.20–1.82 Å. In the third Si4+ site, Si4+ is bonded in a 4-coordinate geometry to four O2- atoms. There are a spread of Si–O bond distances ranging from 1.41–2.36 Å. In the fourth Si4+ site, Si4+ is bonded in a 3-coordinate geometry to four O2- atoms. There are a spread of Si–O bond distances ranging from 1.45–2.49 Å. There are eight inequivalent O2- sites. In the first O2- site, O2- is bonded in a 2-coordinate geometry to two Si4+ atoms. In the second O2- site, O2- is bonded in a water-like geometry to two Si4+ atoms. In the third O2- site, O2- is bonded in a distorted single-bond geometry to one Si4+ atom. In the fourth O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the fifth O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the sixth O2- site, O2- is bonded in a distorted single-bond geometry to one Si4+ atom. In the seventh O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the eighth O2- site, O2- is bonded in a single-bond geometry to one Si4+ atom.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 crystallizes in the monoclinic C2 space group. The structure is two-dimensional and consists of one SiO2 sheet oriented in the (0, 0, 1) direction. there are two inequivalent Si4+ sites. In the first Si4+ site, Si4+ is bonded in a trigonal planar geometry to three O2- atoms. There are a spread of Si–O bond distances ranging from 1.53–1.64 Å. In the second Si4+ site, Si4+ is bonded in a tetrahedral geometry to four O2- atoms. There is two shorter (1.63 Å) and two longer (1.64 Å) Si–O bond length. There are three inequivalent O2- sites. In the first O2- site, O2- is bonded in a single-bond geometry to one Si4+ atom. In the second O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the third O2- site, O2- is bonded in a bent 120 degrees geometry to two Si4+ atoms.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 crystallizes in the triclinic P1 space group. The structure is one-dimensional and consists of one SiO2 ribbon oriented in the (1, 0, 0) direction. there are eight inequivalent Si4+ sites. In the first Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. There is two shorter (1.62 Å) and two longer (1.66 Å) Si–O bond length. In the second Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. There are a spread of Si–O bond distances ranging from 1.62–1.66 Å. In the third Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. There is two shorter (1.63 Å) and two longer (1.65 Å) Si–O bond length. In the fourth Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. There are a spread of Si–O bond distances ranging from 1.62–1.66 Å. In the fifth Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. There is two shorter (1.63 Å) and two longer (1.66 Å) Si–O bond length. In the sixth Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. There is two shorter (1.63 Å) and two longer (1.66 Å) Si–O bond length. In the seventh Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. There is two shorter (1.62 Å) and two longer (1.66 Å) Si–O bond length. In the eighth Si4+ site, Si4+ is bonded to four O2- atoms to form corner-sharing SiO4 tetrahedra. There is two shorter (1.62 Å) and two longer (1.66 Å) Si–O bond length. There are sixteen inequivalent O2- sites. In the first O2- site, O2- is bonded in a bent 120 degrees geometry to two equivalent Si4+ atoms. In the second O2- site, O2- is bonded in a bent 120 degrees geometry to two equivalent Si4+ atoms. In the third O2- site, O2- is bonded in a bent 120 degrees geometry to two equivalent Si4+ atoms. In the fourth O2- site, O2- is bonded in a bent 120 degrees geometry to two equivalent Si4+ atoms. In the fifth O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the sixth O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the seventh O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the eighth O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the ninth O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the tenth O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the eleventh O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the twelfth O2- site, O2- is bonded in a bent 150 degrees geometry to two Si4+ atoms. In the thirteenth O2- site, O2- is bonded in a bent 120 degrees geometry to two equivalent Si4+ atoms. In the fourteenth O2- site, O2- is bonded in a bent 120 degrees geometry to two equivalent Si4+ atoms. In the fifteenth O2- site, O2- is bonded in a bent 120 degrees geometry to two equivalent Si4+ atoms. In the sixteenth O2- site, O2- is bonded in a bent 120 degrees geometry to two equivalent Si4+ atoms.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 is Silicon Disuphide-like structured and crystallizes in the orthorhombic Ibam space group. The structure is one-dimensional and consists of two SiO2 ribbons oriented in the (1, 0, 0) direction. Si4+ is bonded to four equivalent O2- atoms to form distorted edge-sharing SiO4 tetrahedra. All Si–O bond lengths are 1.67 Å. O2- is bonded in an L-shaped geometry to two equivalent Si4+ atoms.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 is trigonal omega-like structured and crystallizes in the monoclinic C2 space group. The structure is two-dimensional and consists of three SiO2 sheets oriented in the (0, 0, 1) direction. Si4+ is bonded to six O2- atoms to form edge-sharing SiO6 octahedra. All Si–O bond lengths are 1.81 Å. There are two inequivalent O2- sites. In the first O2- site, O2- is bonded in a distorted T-shaped geometry to three equivalent Si4+ atoms. In the second O2- site, O2- is bonded in a distorted T-shaped geometry to three equivalent Si4+ atoms.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 is Silicon Disuphide structured and crystallizes in the orthorhombic Ibam space group. The structure is one-dimensional and consists of two SiO2 ribbons oriented in the (0, 1, 0) direction. Si4+ is bonded to four equivalent O2- atoms to form distorted edge-sharing SiO4 tetrahedra. All Si–O bond lengths are 1.67 Å. O2- is bonded in an L-shaped geometry to two equivalent Si4+ atoms.

36 MATERIALS SCIENCE↗

A VUV photoionization measurement and ab-initio calculation of the ionization energy of gas phase SiO2

In this work we report on the detection and vacuum-ultraviolet (VUV) photoionization of gas phase SiO2 generated in situ via laser ablation of silicon in a CO2 molecular beam. The resulting species are investigated by single photon ionization with tunable VUV synchrotron radiation and mass analyzed using reflectron mass spectrometry. Photoionization efficiency (PIE) curves are recorded for SiO and SiO2 and ionization energy estimates are revealed from such measurements. A state-to-state ionizationenergy of 12.60 (+-0.05) eV is recorded by fitting two prominent peaks in the PIE curve for the following process: 1SUM O-Si-O --> 2PRODg [O-Si-O]+. Electronic structure calculations aid in the interpretation of the photoionization process and allow for identification of the symmetric stretch of 2PRODg [O-Si-O]+ which is observed in the PIE spectrum to be 0.11 eV (890 cm-1) above the ground state of the cation and agrees with the 892 cm-1 symmetric stretch frequency calculated at the CCSD(T)/aug-cc-pVTZ level.

03 NATURAL GAS↗

Effects of Al2O3, B2O3, Li2O, Na2O, and SiO2 on Nepheline Crystallization in Hanford High Level Waste Glasses

Nepheline (nominally NaAlSiO4) formation during slow cooling of high-alumina (25.4 - 34.5 mass% Al2O3) Hanford high level waste glasses may significantly reduce product durability. To investigate the effects of composition on nepheline crystallization, 29 compositions were formulated by adjusting Al2O3, B2O3, Li2O, Na2O, and SiO2 around a baseline glass that precipitated 12 mass% nepheline. Thirteen of these compositions were generated by adjusting one-component-at-a-time, while two or three components were adjusted to produce the other 16 (with all remaining components staying in the same relative proportions). Quantitative X-ray diffraction was used to determine nepheline concentration in each sample. Twenty two glasses precipitated nepheline, two of which also precipitated eucryptite (nominally LiAlSiO4), and one glass formed only eucryptite upon slow cooling. Increasing Na2O and Li2O had the strongest effect in promoting nepheline formation. Increasing B2O3 inhibited nepheline formation. SiO2 and Al2O3 showed non-linear behavior related to nepheline formation. The composition effects on nepheline formation in these glasses are reported.

Kroll, Jared O.↗

Impedance spectroscopy study of SiO2-Li2O:Nd2O3 glasses

In the present study, neodymium-doped lithium silicate glasses have been prepared by the conventional melt-quenching technique. The dielectric properties, electric modulus and electrical conductivity of SiO2-Li2O (SiLi-0Nd) and SiO2-Li2O:Nd2O3 (SiLi-1.35Nd) have been studied from 1 Hz to 1 MHz in the 333 423 K temperature range. At a given temperature and frequency, we observe that the resistivity increases while the conductivity accordingly decreases when neodymium ions are added to the glass matrix. The activation energy of two distinct regions was evaluated from the ln( dc)=f(1/T) plot and was found to be E1(T<363K)=0.61(0.66)eV and E2(T>363K)=1.26(1.09)eV for SiLi-0Nd (SiLi-1,35Nd). The dielectric constant ( Re) decreases while the dielectric loss (tan ( )) increases under Nd2O3 doping. We also observe that for both glasses, Re and tan ( ) tend to increase with increasing temperature and decrease with increasing frequency.

dielectric properties↗

Ag@SiO2 Core-shell Nanoparticles for Probing Spatial Distribution of Electromagnetic Field Enhancement via Surface-Enhanced Raman Scattering

We show that the spatial distribution of the electromagnetic (EM) field enhancement can be probed directly via dynamic evolution of surface-enhanced Raman scattering (SERS) of Rhodamine 6G (R6G) molecules as they diffuse into Ag@SiO2 core-shell nanoparticles. The porous silica shell limits the diffusion of R6G molecules towards inner Ag cores, thereby allowing direct observation and quantification of the spatial distribution of SERS enhancement as molecules migrate from the low to high EM fields inside the dielectric silica shell. Our experimental evidence is validated by the generalized Mie theory, and the approach can potentially offer a novel platform for further investigating the site and spatial distribution of the EM fields and the EM versus chemical enhancement of SERS due to molecular confinement within the Ag@SiO2 nanoshell.

36 MATERIALS SCIENCE↗

Site-specific Pt Deposition and Etching on Electrically and Thermally Isolated SiO2 Micro-disk Surfaces

Electrically and thermally isolated surfaces are often crucial for improving the detection sensitivity of microelectronic sensors. The site specific in-situ growth of Pt nano-rods on thermally and electrically isolated micro-fabricated SiO2 disks using wet chemical etching and focused ion/electron dual-beam (FIB-SEM) is demonstrated in this work. Fabrication of an array of micro-cavities on top of micro-disk is also demonstrated. FIB source is also utilized to fabricate through-holes in the micro-disks. The nature of Ga Gaussian distribution in the Ga-implanted region using a FIB source can naturally create more conducting layer on the sidewalls of through-holes on the micro-disks. Some sensor design concepts based on micro-fabrication of SiO2 micro-disks utilizing thermally and electrically isolated surfaces are discussed from the viewpoint of applications in photonics and bio-sensing.

Saraf, Laxmikant V↗

Carbon Clusters as Possible Defects in the SiC-SiO2 Interface

High state densities in the band gap of the SiC-SiO2 interface significantly reduce the channel mobilities in SiC-based high-temperature/high-power microelectronics. Investigations of the nature of the interface defects are thus of great importance. While several possible defects including very small carbon clusters with up to four carbon atoms have been identified by first-principles theory, larger carbon clusters as possible defects have attracted less attention. Here, we report first-principles quantum-mechanical calculations for two larger carbon clusters, the C10 ring and the C20 fullerence, in the SiC-SiO2 interface. We find that both carbon clusters introduce significant states in the band gap. The states extend over the entire band gap with higher densities in the upper half of the gap, thus accounting for some of the interface trap densities observed experimentally

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Water adsorption, solvation and deliquescence of alkali halide thin films on SiO2 studied by ambient pressure X-ray photoelectron spectroscopy

The adsorption of water on KBr thin films evaporated onto SiO2 was investigated as a function of relative humidity (RH) by ambient pressure X-ray photoelectron spectroscopy. At 30percent RH adsorbed water reaches a coverage of approximately one monolayer. As the humidity continues to increase, the coverage of water remains constant or increases very slowly until 60percent RH, followed by a rapid increase up to 100percent RH. At low RH a significant number of the Br atoms are lost due to irradiation damage. With increasing humidity solvation increases ion mobility and gives rise to a partial recovery of the Br/K ratio. Above 60percent RH the increase of the Br/K ratio accelerates. Above the deliquescence point (85percent RH), the thickness of the water layer continues to increase and reaches more than three layers near saturation. The enhancement of the Br/K ratio at this stage is roughly a factor 2.3 on a 0.5 nm KBr film, indicating a strong preferential segregation of Br ions to the surface of the thin saline solution on SiO2.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 is Rutile structured and crystallizes in the tetragonal P4_2/mnm space group. The structure is three-dimensional. Si4+ is bonded to six equivalent O2- atoms to form a mixture of corner and edge-sharing SiO6 octahedra. The corner-sharing octahedral tilt angles are 49°. There is four shorter (1.78 Å) and two longer (1.84 Å) Si–O bond length. O2- is bonded in a distorted trigonal planar geometry to three equivalent Si4+ atoms.

36 MATERIALS SCIENCE↗

Materials Data on SiO2 by Materials Project

SiO2 is Fluorite structured and crystallizes in the cubic Fm-3m space group. The structure is three-dimensional. Si4+ is bonded in a body-centered cubic geometry to eight equivalent O2- atoms. All Si–O bond lengths are 1.98 Å. O2- is bonded to four equivalent Si4+ atoms to form a mixture of corner and edge-sharing OSi4 tetrahedra.

36 MATERIALS SCIENCE↗