At least 37 records · Page 2

Role of Dynamic Nucleation at Moving Boundaries in Phase and Microstructure Selection

Solidification microstructures that form under steady-state growth conditions (cells, dendrites, regular eutectics, etc.) are reasonably well understood in comparison to other, more complex microstructures, which form under intrinsically non-steady-state growth conditions due to the competition between the nucleation and growth of several phases. Some important practical examples in this latter class include microstructures forming in peritectic systems in highly undercooled droplets, and in strip cast stainless steels. Prediction of phase and microstructure selection in these systems has been traditionally based on (1) heterogeneous nucleation on a static interface, and (2) comparing the relative growth rate of different phase/microstructures under steady-state growth conditions. The formation of new phases, however, occurs via nucleation on, or ahead of, a moving boundary. In addition, the actual selection process is controlled by a complex interaction between the nucleation process and the growth competition between the nuclei and the pre-existing phase under non-steady-state conditions. As a result, it is often difficult to predict which microstructure will form and which phases will be selected under prescribed processing conditions. This research addresses this critical role of nucleation at moving boundaries in the selection of phases and solidification microstructures through quantitative experiments and numerical modeling in peritectic systems. In order to create a well characterized system in which to study this problem, we focus on the directional solidification of hypo- and hyper-peritectic alloys in the two-phase region, imposing a large enough ratio of temperature gradient/growth rate (G/V(sub p)) to suppress the morphological instability of both the parent (alpha) and peritectic (Beta) phases, i.e. each phase alone would grow as a planar front. Our combined experimental and theoretical results show that, already in this simplified case, the growth competition of these two phases leads to a rich variety of microstructures that depend sensitively upon the relative importance of nucleation, diffusion, and convection.

Karma, Alain↗

Adaptive-Grid Methods for Phase Field Models of Microstructure Development

Modeling solidification microstructures has become an area of intense study in recent years. The properties of large scale cast products, ranging from automobile engine blocks to aircraft components and other industrial applications, are strongly dependent on the physics that occur at the mesoscopic and microscopic length scales during solidification. The predominant morphology found in solidification microstructures is the dendrite, a tree-like pattern of solid around which solidification proceeds. The microscopic properties of cast products are determined by the length scales of these dendrites, and their associated segregation profiles. For this reason understanding the mechanisms for pattern selection in dendritic growth has attracted a great deal of interest from the experimental and theoretical communities. In particular, a great deal of research has been undertaken to understand such issues as dendrite morphology, shape and growth speed. Experiments on dendrite evolution in pure materials by Glicksman and coworkers on succinonitrile (SCN), and more recently pivalic acid (PVA), as well as other transparent analogs of metals, have provided tests of theories for dendritic growth, and have stimulated considerable theoretical progress. These experiments have clearly demonstrated that in certain parameter ranges the physics of the dendrite tip can be characterized by a steady value for the dendrite tip velocity, radius of curvature and shape. Away from the tip, the time-dependent dendrite exhibits a characteristic sidebranching as it propagates, which is not yet well understood. These experiments are performed by observing individual dendrites growing into an undercooled melt. The experiments are characterized by the dimensionless undercooling. Most experiments are performed at low undercooling.

Dantzig, Jonathan A.↗

Influence of the Composition on the Solidification Path, Microstructure Evolution and Mechanical Properties of Al-Cu-Mg Alloys

The influence of the initial composition on the solidification path, microstructure evolution, thermophysical properties and mechanical properties of Al-Cu-Mg alloys was investigated. The solidification paths of the investigated alloys were determined by analyzing the solidification structure, and then the experimentally determined paths were compared with those from the calculated results. Three of the investigated alloys experienced typical ternary eutectic solidification, and the other four alloys experienced quasiperitectic reactions. Due to differences in the initial compositions, different eutectic morphologies were formed during the solidification process. The binary eutectic phases, (α-Al + Al{sub 2}Cu) and (α-Al + Al{sub 6}CuMg{sub 4}), and the (α-Al + Al{sub 6}CuMg{sub 4} + Al{sub 8}Mg{sub 5}) ternary eutectic phase tended to exhibit divorced growth, and the (α-Al + Al{sub 2}CuMg), (α-Al + Al{sub 6}CuMg{sub 4}) and (α-Al + Al{sub 2}Cu + Al{sub 2}CuMg) eutectic phases tended to exhibit coupled growth. The results indicated that the initial composition, solidification path, microstructure and morphology could greatly affect the melting enthalpy, microhardness and compressive strength of the investigated Al-Cu-Mg alloys.

36 MATERIALS SCIENCE↗

Understanding the solidification and microstructure evolution during CSC-MIG welding of Fe–Cr–B-based alloy

The present is a study of the solidification and microstructure of Fe–28.2%Cr–3.8%B–1.5%Si–1.5%Mn (wt.%) alloy deposited onto a 1020 plain carbon steel substrate using the controlled short-circuit metal inert gas welding process. The as-solidified alloy was a metal matrix composite with a hypereutectic microstructure. Thermodynamic calculation based on the Scheil–Gulliver model showed that a primary (Cr,Fe){sub 2}B phase formed first during solidification, followed by an eutectic formation of the (Cr,Fe){sub 2}B phase and a body-centered cubic Fe-based solid solution matrix, which contained Cr, Mn and Si. Microstructure analysis confirmed the formation of these phases and showed that the shape of the (Cr,Fe){sub 2}B phase was irregular plate. As the welding heat input increased, the weld dilution increased and thus the volume fraction of the (Cr,Fe){sub 2}B plates decreased while other microstructural characteristics were similar. - Highlights: • We deposit Fe–Cr–B-based alloy onto plain carbon steel using the CSC-MIG process. • We model the solidification behavior using thermodynamic calculation. • As deposited alloy consists of (Cr,Fe){sub 2}B plates embedded in Fe-based matrix. • We study the effect of the welding heat input on the microstructure.

36 MATERIALS SCIENCE↗

Influence of geometry on columnar to equiaxed transition during electron beam powder bed fusion of IN718

Correlation between spot-melt scan parameters (linear spot-density aka areal energy density), build geometry, and solidification microstructure evolution (columnar vs equiaxed) in a powder bed fusion technology is investigated. It is shown that to maintain the equiaxed solidification microstructure evolution in electron beam powder bed additive manufacturing (AM), the areal energy density per layer needs to be scaled with respect to the 2D cross-sectional area of the layer being melted. Samples with two different cross-sectional areas (40 × 40 mm and 20 × 20 mm) have been fabricated with varying areal energy densities. For a given square cross-section (20 × 20 mm), increasing the areal energy density (4.8 MJ/sq.m to 14.7 MJ/sq.m) transitioned the solidification microstructure from columnar to equiaxed. The observed microstructure data (Electron Back Scattered Diffraction - EBSD) is quantified by calculating the principal component (PC) score using a spatial statistics methodology. The sample with equiaxed grains is found to have a low PC score while the sample with columnar grain had a high PC score. A semi-analytical model is used to simulate the heat transfer and the local solidification conditions as a function of processing parameters (linear spot-density). The result from the heat transfer model is correlated with previously quantified microstructure data. Space-Time analysis of the melt pattern is done and correlated with the observed microstructure. In addition, from the findings, appropriate parameters have been used to additively manufacture a turbine blade with site-specific or hybrid solidification microstructure (traditional fabrication possible via a patented method of localized cold working and heat treatment).

36 MATERIALS SCIENCE↗

Phase Selection During Solidification and Solid-State Phase Transformations in an Al-10Ce-8Mn (wt pct) Alloy

In multicomponent Al-Ce alloys, and especially after additive manufacturing (AM), complex and metastable solidification microstructures are frequently observed. Here, in this research, the relationship between solidification conditions and phase selection are explored for an Al-10Ce-8Mn (wt pct) alloy using a systematic study of laser melting conditions. Three solidification modes were observed: primary Al 10 Mn 2 Ce; primary Al 20 Mn 2 Ce; and eutectic FCC Al + Al 20 Mn 2 Ce. These solidification modes were correlated to specific liquid-solid interface velocities using a simple thermal model, showing the change in primary solidification phase for low (< 6.8 × 10 −4 m/s), moderate (between 8.2 × 10 −4 and 5.9 × 10 −2 m/s) and high solidification velocities (> 6.2 x 10 −2 m/s) for the above three solidification microstructures, respectively. These results were rationalized by using interface response function (IRF) theory to describe the solidification undercooling for the possible primary intermetallic phases. The implication of the local phase selection from differing solidification conditions is summarized by a comparison of hardness which demonstrates the potential variance of Vickers hardness from 101 to 242 (VHV) by changing the laser velocity from 1 to 83 mm/s. Interestingly, on heat treatment at 400°C, the decomposition pathways of the solidification microstructure and hardness were also found to be different, thereby opening multiple pathways for spatial microstructure and property control within AM components.

Sisco, Kevin↗

Solidification pattern, microstructure and texture development in Laser Powder Bed Fusion (LPBF) of Al10SiMg alloy

Highlights: • The complex solidification pattern during Laser Powder Bed Fusion of Al10SiMg alloy is explained. • The evolution of α-Al cellular network, grain structure and texture development is characterized. • The grain structure is shown to be columnar throughout the printed sample • The grains’ orientation align with that of the α-Al cells. • The size evolution of α-Al cells and grains within the scan tracks follow opposite patterns. • Utilizing of a 67° hatch angle enhances densification and promotes a more isotropically developed texture across the build. - Abstract: A comprehensive analysis of solidification patterns and microstructural development is presented for an Al10SiMg sample produced by Laser Powder Bed Fusion (LPBF). Utilizing a novel scanning strategy that involves counter-clockwise rotation of the scan vector by 67° upon completion of each layer, a relatively randomized cusp-like pattern of protruding/overlapping scan tracks has been produced along the build direction. We show that such a distribution of scan tracks, as well as enhancing densification during LPBF, reduces the overall crystallographic texture in the sample, as opposed to those normally achieved by commonly-used bidirectional or island-based scanning regimes with 90° rotation. It is shown that, under directional solidification conditions present in LPBF, the grain structure is strictly columnar throughout the sample and that the grains' orientation aligns well with that of the α-Al cells. The size evolution of cells and grains within the melt pools, however, is shown to follow opposite patterns. The cells'/grains' size distribution and texture in the sample are explained via use of analytical models of cellular solidification as well as the overall heat flow direction and local solidification conditions in relation to the LPBF processing conditions. Such a knowledge of the mechanisms upon which microstructural features evolve throughout a complex solidification process is critical for process optimization and control of mechanical properties in LPBF.

36 MATERIALS SCIENCE↗

On the Microstructure and Solidification Behavior of N-Bearing Ti-46Al-8Ta (at.%) Intermetallic Alloys

Ti-46Al-8Ta (at.%) intermetallic alloys exhibit acceptable strength at low and high temperatures with good oxidation resistance. Different alloying elements are usually added to TiAl-based alloys to develop required properties. In this work, effects of N addition up to 2 at.% on microstructural features and solidification behavior of the Ti-46Al-8Ta alloy is investigated. The achieved results showed that alloying with N causes dendrite refinement and reduction of the retained metastable B2 phase in the as-cast microstructure. The dendrite morphology is also changed from fourfold to fivefold and then sixfold symmetry by increasing N content. The effect of N on interlamellar spacing, amount of constituent phases, and lattice parameters was not uniform. Increasing N content resulted in an increase in both small punch maximum load and hardness up to 1.05 at.%, whereas further N alloying, despite increasing of hardness, led to a drop in the maximum load.

36 MATERIALS SCIENCE↗

Schmid factor crack propagation and tracking crystallographic texture markers of microstructural condition in direct energy deposition additive manufacturing of Ti-6Al-4V

Metallic additive manufacturing (AM) provides a customizable and tailorable manufacturing process for new engineering designs and technologies. The greatest challenge currently facing metallic AM is maintaining control of microstructural evolution during solidification and any solid state phase transformations during the build process. Ti-6Al-4V has been extensively surveyed in this regard, with the potential solid state and solidification microstructures explored at length. In this study, we evaluate the applicability of previously determined crystallo- graphic markers of microstructural condition observed in electron beam melting powder bed fusion (PBF-EB) builds of Ti-6Al-4V in a directed energy deposition (DED) build process. The aim of this effort is to elucidate whether or not these specific crystallographic textures are useful tools for indicating microstructural conditions in AM variants beyond PBF-EB. Parent β-Ti grain size was determined to be directly related to α-Ti textures in the DED build process, and the solid state microstructural condition could be inferred from the intensity of specific α-Ti orientations. Qualitative trends on the as-solidified β-Ti grain size were also determined to be related to the presence of a fiber texture, and proposed as a marker for as-solidified grain size in any cubic metal melted by AM. Analysis of the DED Ti-6Al-4V build also demonstrated a near complete fracture of the build volume, suspected to originate from accumulated thermal stresses in the solid state. Crack propagation was found to only appreciably occur in regions of slow cooling with large α +β colonies. Schmid factors for the basal and prismatic α-Ti systems explained the observed crack pathway, including slower bifurcation in colonies with lower Schmid factors of both slip systems. Colony morphologies and localized equiaxed β-Ti solidification were also found to originate from build pauses during production and uneven heating of the build edges during deposition. Tailoring of DED Ti-6Al-4V microstructures with the insight gained here is proposed, along with cautionary insight on preventing unplanned build pauses to maintain an informed and controlled thermal environment for microstructural control.

36 MATERIALS SCIENCE↗

Influence of Bridgman solidification on microstructures and magnetic behaviors of a non-equiatomic FeCoNiAlSi high-entropy alloy

The non-equiatomic FeCoNiAlSi alloy is prepared by the Bridgman solidification (BS) technique at different withdrawal velocities (V = 30, 100, and 200 μm/s). Various characterization techniques have been used to study the microstructure and crystal orientation. The morphological evolutions accompanying the crystal growth of the alloy prepared at different withdrawal velocities are nearly the same, from equiaxed grains to columnar crystals. The transition of coercivity is closely related to the local microstructure, while the saturation magnetization changes little at different sites. The coercivity can be significantly reduced from the equiaxed grain area to the columnar crystal area when the applied magnetic field direction is parallel to the crystal growth direction, no matter what is the withdrawal velocity. As a result, the alloy possesses magnetic anisotropy when the applied magnetic field is in different directions.

36 MATERIALS SCIENCE↗

Anomalous Annealing Response of Directed Energy Deposited Type 304L Austenitic Stainless Steel

Directed energy deposited (DED) and forged austenitic stainless steels possess dissimilar microstructures but can exhibit similar mechanical properties. In this study, annealing was used to evolve the microstructure of both conventional wrought and DED type 304L austenitic stainless steels, and significant differences were observed. In particular, the density of geometrically necessary dislocations and hardness were used to probe the evolution of the microstructure and properties. Forged type 304L exhibited the expected decrease in measured dislocation density and hardness as a function of annealing temperature. Here, the more complex microstructure–property relationship observed in the DED type 304L material is attributed to compositional heterogeneities in the solidification microstructure.

36 MATERIALS SCIENCE↗

Solidification characterization of a new rapidly solidified Ni-Cr-Co based superalloy

The solidification characterization of a new rapidly solidified Ni-Cr-Co based superalloy prepared by plasma rotating electrode process was investigated by means of optical microscope, scanning electron microscope, and transmission electron microscope. The results show that the solidification microstructure changes from dendrites to cellular and microcrystal structures with decreasing powder size. The elements of Co, Cr, W and Ni are enriched in the dendrites, while Mo, Nb and Ti are higher in the interdendritic regions. The relationships between powder size with the average solid-liquid interface moving rate, the average interface temperature gradient and the average cooling rate are established. Microsegregation is increased with larger powder size. The geometric integrity of MC Prime type carbides in the powders changes from regular to diverse with decreasing powder size. The morphology and quantity of carbides depend on the thermal parameters and non-equilibrium solute partition coefficients during rapid solidification. - Highlights: Black-Right-Pointing-Pointer The relations of solidification thermal parameters with powder size are established. Black-Right-Pointing-Pointer The relation of non-equilibrium solute partition with powder size is investigated. Black-Right-Pointing-Pointer The solidification microstructure is related to thermal parameters. Black-Right-Pointing-Pointer The segregation behavior is linked to non-equilibrium partition coefficients. Black-Right-Pointing-Pointer The morphology and quantity of carbides depend on the above combined factors.

36 MATERIALS SCIENCE↗

An additively manufactured near-eutectic Al-Ce-Ni-Mn-Zr alloy with high creep resistance

A new additively manufactured (AM) Al-7.5Ce-4.5Ni-0.4Mn-0.7Zr (wt.%) near-eutectic alloy is reported, which shows unprecedented creep resistance up to 400 °C (a homologous temperature of 0.72). The eutectic solidification microstructure comprises ~ 27 vol% of coarsening-resistant second phase network with an ultrafine (<100 nm) inter-phase spacing. Both Mn and Zr contribute to creep resistance of the alloy. Small amount of Mn addition promotes selection of coarsening resistant phases without compromising the alloy processability. Zr not only improves hot-tearing resistance, but further enhances the second phase coarsening resistance resulting in improved creep resistance. Neutron diffraction performed during creep deformation reveals that the underlying mechanism for creep resistance in this alloy is impedance to dislocation motion stemming from the ultrafine eutectic solidification microstructure, whereas load transfer strengthening becomes less effective as the creep temperature increases. The second phase forms a continuous network in the as-fabricated condition, which is maintained during long-term creep at 300 °C. However, this network is fragmented into fine dispersoids at higher temperatures. It is proposed that the rate-limiting deformation mechanism at 300–400 °C is (i) dislocation climb for the alloy with fragmented second phase dispersoids and (ii) Orowan looping for the alloy with a continuous second phase network. In conclusion, the present design of an AM-processable multicomponent eutectic alloy with high creep resistance can be applied to other metallic systems exhibiting eutectic reactions, with expected extreme creep resistance.

36 MATERIALS SCIENCE↗