Search NASASearch

SEARCH · Search NASA

Results for “Solids”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

169 records · Page 2

Reliability Assessment of Solid-State Circuit Breakers (CRADA CRD-21-21469, Project 4 Final Report)

Growth in power requirements and the complexity of emerging distribution systems are creating the need for new solid-state products for many applications. The qualification requirements, testing standards and life-cycle management practices of solid-state devices used in protection applications is not established. The project will leverage newly developed accelerated testing capabilities design specifically for protection applications to generate large data sets that will enable advanced digital techniques for data analysis and embedded health monitoring.

14 SOLAR ENERGY

Metal–Organic Framework-derived Atomic Metal Sites Promoting Sulfur Cathode for All-Solid-State Lithium–Sulfur Batteries

All-solid-state lithium–sulfur batteries (ASSLSBs) offer high energy density and intrinsic safety; however, they still face major challenges, including sluggish redox kinetics and poor sulfur utilization. Incorporating conductive materials into sulfur cathodes is an effective strategy to mitigate these limitations. Here, a highly conductive cobalt–nitrogen–doped carbon (Co–NC) derived from a metal–organic framework (MOF) is introduced to accelerate charge transfer and promote reversible sulfur conversion. Co−NC provides atomically dispersed Co–N sites and conductive carbon pathways that correlate with improved charge transfer, sulfur utilization, and rate capability. Co–NC@S cathode delivers 1499 mAh g–1 at C/20 with a high sulfur loading (5 mg cm–2) and retains 1292 mAh g–1 after five cycles (vs 443 mAh g–1 without Co–NC). Moreover, Co–NC derived ASSLSB achieves 903 mAh g–1 at 5C at 60 °C. This work provides a practical and effective approach to develop high energy, high-rate ASSLSBs.

25 ENERGY STORAGE

Lagrange-Remap strategy for multi-material fluid-solid simulations using compressive limiters

In the present work, the Lagrange-Remap strategy proposed in [1] is extended to multi-material fluid-solid simulations. Both hypo-elastic and hyper-elastic material models are considered to describe the mechanical behavior of the solids. In practice, the deviatoric stress tensor (for hypo-elastic materials) and the left Cauchy-Green tensor (for isotropic hyper-elastic materials) are remapped, while the use of compressive limiters effectively reduces numerical diffusion during the remapping step. The simplicity of this diffuse interface approach is emphasized in the context of multi-material fluid-solid simulations. A series of Lagrange-Remap test cases, involving both solids and fluids, are conducted and compared with reference Lagrangian simulations, demonstrating the robustness and accuracy of the overall numerical strategy.

Compressive limiters

Revealing the Roles of CuF 2 /NiF 2 Incorporation in the Electrochemical Performance of FeF 3 Cathodes in Solid‐State Batteries

Mixed metal fluorides have been considered as a promising candidate to lower the voltage hysteresis of conversion-type iron fluoride cathodes, but their cycling stability is limited due to transition metal dissolution and interphase growth in liquid electrolyte batteries. Here, we study the role of incorporating CuF 2 and NiF 2 in the electrochemical performance of FeF 3 cathode in halide-based solid-state batteries to test whether we can transfer the kinetic benefit of low voltage hysteresis to solid-state batteries while using solid electrolyte to eliminate transition metal dissolution and stabilize the interphase. Synchrotron X-ray absorption spectroscopy results indicated the redox reactions are attributed to Cu 0 /Cu + and Fe 0 /Fe 2+ in 25CuF 2 -75FeF 3 and Ni 0 /Ni 2+ and Fe 0 /Fe 3+ in 10NiF 2 -90FeF 3 . While no apparent improvement in electrode kinetics can be observed, the incorporation of CuF 2 and NiF 2 can largely improve the cycling stability of FeF 3 cathodes. In conclusion, the results demonstrate the advantages of using solid-state concept to improve the cycling stability of conversion-type cathodes.

25 ENERGY STORAGE

Enhancing cathode composites with conductive alignment synergy for solid-state batteries

Enhancing transport and chemomechanical properties in cathode composites is crucial for the performance of solid-state batteries. Our study introduces the filler-aligned structured thick (FAST) electrode, which notably improves mechanical strength and ionic/electronic conductivity in solid composite cathodes. The FAST electrode incorporates vertically aligned nanoconducting carbon nanotubes within an ion-conducting polymer electrolyte, creating a low-tortuosity electron/ion transport path while strengthening the electrode’s structure. This design not only mitigates recrystallization of the polymer electrolyte but also establishes a densified local electric field distribution and accelerates the migration of lithium ions. The FAST electrode showcases outstanding electrochemical performance with lithium iron phosphate as the active material, achieving a high capacity of 148.2 milliampere hours per gram at 0.2 C over 100 cycles with substantial material loading (49.3 milligrams per square centimeter). This innovative electrode design marks a remarkable stride in addressing the challenges of solid-state lithium metal batteries.

Science & Technology - Other Topics

Design and Synthesis of Cubic K 3−2 x Ba x SbSe 4 Solid Electrolytes for K–O 2 Batteries

Developing K-ion conducting solid-state electrolytes (SSEs) plays a critical role in the safe implementation of potassium batteries. In this work, a chalcogenide-based potassium ion SSE is reported, K 3 SbSe 4 , which adopts a trigonal structure at room temperature. Single-crystal structural analysis reveals a trigonal-to-cubic phase transition at the low temperature of 50 °C, which is the lowest among similar compounds and thus provides easy access to the cubic phase. The substitution of barium for potassium in K 3 SbSe 4 leads to the creation of potassium vacancies, expansion of lattice parameters, and a transformation from a trigonal phase to a cubic phase. As a result, the maximum conductivity of K 3−2x Ba x SbSe 4 reaches around 0.1 mS cm −1 at 40 °C for K 2.2 Ba 0.4 SbSe 4 , which is over two orders of magnitude higher than that of undoped K 3 SbSe 4 . This novel SSE is successfully employed in a K–O 2 battery operating at room temperature where a polymer-laminated K 2.2 Ba 0.4 SbSe 4 pellet serves as a separator between the oxygen cathode and the potassium metal anode. Effective protection of the K metal anode against corrosion caused by O 2 is demonstrated.

25 ENERGY STORAGE

Kondo effect in ferromagnetic quantum critical CeRh 6 ⁢Ge 4

The mechanism of a pressure-induced quantum critical point in the heavy fermion ferromagnet CeRh 6 ⁢Ge 4 has attracted interest, as ferromagnetic quantum criticality in a clean itinerant Ce compound is typically avoided. The localized versus itinerant character of the 4⁢𝑓 electrons is a key aspect for understanding this behavior. We investigated the electronic structure of the 4⁢𝑓 shell in CeRh 6 ⁢Ge 4 using core-level photoelectron and x-ray absorption spectroscopy, demonstrating the hybridization of Ce 4⁢𝑓 with the conduction electrons. Linearly polarized x-ray absorption reveals a temperature-dependent linear dichroism consistent with the crystal-electric-field sequence as inferred from the static susceptibility. This dichroism cannot be described by an ionic full-multiplet model alone, but is reproduced by including the Kondo effect within a single-impurity Anderson model in the noncrossing approximation. The Kondo effect mixes higher-lying crystal-field states into a resulting multiorbital ground state with 4⁢𝑓 occupancy, 𝑛 𝑓 ∼ 0.9. Deviations at low temperatures between the measured linear dichroism and calculated dichroism suggest an orbital-dependent Kondo effect. A scenario in which there is a multiorbital ground state and orbital-dependent Kondo hybridization should be a starting point for a model of pressure-induced criticality in CeRh 6 ⁢Ge 4 .

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Solid polymer electrolytes based on plastic crystals are promising for solid-state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 -electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, in this study, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non-uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive-embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile-plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome-like Na 0 with thin, amorphous, and fluorine-rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

25 ENERGY STORAGE

A stable high-humidity bubbler design to supply steam for solid oxide electrolysis cells

A stable steam supply is required for the operation of solid oxide electrolysis cells. Heated water bubblers are the most common method due to the simplicity and inherent safety of the method, however, several design challenges hinder effective implementation. Here, a stable and validated bubbler design is presented, capable of achieving very high steam concentrations, relatively high flow rates, and continuous operation. A piping and instrumentation diagram and bill of materials are provided to enable easy duplication. Critical design parameters are discussed, including safety considerations and materials requirements, which are applicable to any bubbler design. The practical implementation of bubblers is also presented, including methods to prevent condensation instability and reduce backpressure to achieve a stable steam supply. The 3″ x 6″ (7.6 cm × 15.2 cm) bubbler achieves up to 98% steam balance hydrogen at 200 sccm and up to 1 slpm at 96% steam.

08 - HYDROGEN

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE

Dissecting Disorder: Defect-Driven Structural Complexity in Layered Li3InCl6 Solid Electrolyte

Halide solid electrolytes have emerged as promising candidates for solid-state batteries owing to their high oxidative stability and ionic conductivity. Among them, Li3InCl6 (LIC) has attracted significant attention. However, diffraction patterns of LIC synthesized via different methods exhibit distinct differences particularly at low-angle reflectionsindicative of underlying structural disorder. These variations are attributed to deviations from ideal crystallographic order, especially stacking faults, whose impact on structure and ion transport remains poorly understood. Here, we identify and quantify stacking faults in LIC samples prepared under different synthetic conditions. Using X-ray diffraction and time-of-flight neutron diffraction, we construct and refine stacking fault models that accurately reproduce the experimental diffraction features. LIC samples with higher degrees of stacking faults exhibit only negligible differences in ionic conductivities and activation energies. This indicates that stacking faults have a limited impact on altering the Li+ diffusion pathway along the c-axis, likely due to the high concentration of vacancies in the In layers, while Li+ diffusion remains nearly unchanged in the ab-plane. Our results account for the observed differences in diffraction patterns across samples and provide a quantitative assessment of faulting probabilities and stacking sequences. The insights gained from this study are expected to be broadly applicable to other layered halide solid electrolytes and contribute to a deeper understanding of the role of structural disorder in ion transport.

Liu, Jue [ORNL] (ORCID:000000024453910X)

Salt‐Assisted Vapor–Liquid–Solid Growth of 1D van der Waals Materials

The method of salt-assisted vapor–liquid–solid (VLS) growth is introduced to synthesize 1D nanostructures of trichalcogenide van der Waals (vdW) materials, exemplified by niobium trisulfide (NbS 3 ). The method uses a unique catalyst consisting of an alloy of Au and an alkali metal halide (NaCl) to enable rapid and directional growth. High yields of two types of NbS 3 1D nanostructures, nanowires and nanoribbons, each with sub-ten nanometer diameter, tens of micrometers length, and distinct 1D morphology and growth orientation are demonstrated. Strategies to control the location, size, and morphology of growth, and extend the growth method to synthesize other transition metal trichalcogenides, NbSe 3 and TiS 3 , as nanowires are demonstrated. Finally, the role of the Au–NaCl alloy catalyst in guiding VLS synthesis is described and the growth mechanism based on the relationships measured between structure (growth orientation, morphology, and dimensions) and growth conditions (catalyst volume and growth time) is discussed. These results introduce opportunities to expand the library of emerging 1D vdW materials to make use of their unique properties through controlled growth at nanoscale dimensions.

1D van der Waals material

Liquified SO 2 induced solid/cathode electrolyte interphase for lithium ion batteries

Formation of robust solid/cathode electrolyte interphases (S/CEI) is vital for long-term stability and high-performance operation of lithium-ion batteries (LIBs), particularly under high voltage regimes. However, engineering electrochemically stable S/CEIs that effectively suppress interfacial side reactions remains a key challenge. Herein, we introduce a liquefied sulfur dioxide (SO 2 )– ionic liquid complex as a fluorine-free multifunctional electrolyte additive for the first time that significantly improves the formation of sulfate/sulfite-rich S/CEI layers at both graphite and NMC811 interfaces. The unique SO 2 -N coordination with a 1,2,4-triazolide-based ionic liquid enables homogeneous SO 2 dissolution, resulting in controlled SO 2 decomposition during the initial electrochemical cycle. This decomposition yields sulfur-rich interphase species that stabilize the electrolyte-electrode interface, reduce impedance growth, and lessen electrolyte decomposition. Electrochemical tests show significantly improved cycle life, reduced polarization, and increased Coulombic efficiency for both anodes and cathodes. XPS confirms the presence of SO 2 -derived surface species that contribute to interfacial stability. In conclusion, this approach highlights a new direction for interphase engineering using liquefied gas additives and opens pathways for sulfur-based S/CEI chemistry in advanced battery systems.

Graphite

Ionic Interdiffusion at Cathode|Solid-Electrolyte Interface: A Machine Learning–Assisted Multiscale Investigation and Mitigation Strategies

Future lithium batteries are expected to use solid electrolytes to achieve higher energy density and fast charge capabilities. However, most solid electrolytes are thermodynamically unstable against layered oxide cathodes. In this study, the stability of LiCoO2 (LCO) cathode with Li10GeP2S12 (LGPS) solid electrolyte is investigated using ab initio molecular dynamics (AIMD) and machine learning molecular dynamics (MLMD). The propensity of ionic interdiffusion, formation of a passivating interphase layer, and corresponding decay in cell performance is addressed using a continuum model. Large-scale MLMD simulations confirm that the LCO|LGPS interface permits interdiffusion of cobalt (Co) and other ionic species, leading to the formation and growth of a resistive interphase and to dramatic capacity fade even in the first cycle. We examine the literature evidence that incorporating a thin layer of LiNb0.5Ta0.5O3 (LNTO) between LCO and LGPS prevents the interdiffusion of ions. Atomistic simulations suggest that substituting lithium (Li) in LNTO with Co is thermodynamically unfavorable, thereby inhibiting ionic interdiffusion. The stable Nb5+/Ta5+ states form a rigid metal-oxide framework, which consequently also prevents the substitution of niobium (Nb) or tantalum (Ta). However, continuum-level analysis suggests that the higher mechanical stiffness of LNTO can lead to interfacial delamination between the LCO and LNTO. This phenomenon reduces the effectiveness of the protective layer. This paper, therefore, highlights the need to develop novel interlayers that balance low ionic interdiffusion with low mechanical stiffness.

Ncube, Musawenkosi K.

Crack‐Free Single‐Crystalline LiNiO 2 for High Energy Density All‐Solid‐State Batteries

Abstract Single‐crystalline layered oxide (LiNi 1‐ x ‐ y Mn x Co y O 2 ) cathodes have been found to exhibit exceptional electrochemical properties when coupled with various inorganic solid electrolytes (ISEs) in all‐solid‐state batteries (ASSBs). Their advantages stem from the robust morphological integrity with the absence of grain boundaries and the high electrochemical oxidative stability. Here, ASSBs featuring single‐crystalline LiNiO 2 (LNO) with the highest Ni content are reported, offering a high theoretical specific capacity of 275 mAh g ‐1 alongside a high average discharge voltage (3.7 V vs Li + /Li). Through a careful investigation, it is demonstrated that micron‐sized single‐crystalline LNO (µSC‐LNO) composite cathodes with a halide ISE exhibit a high initial discharge capacity of 205 mAh g ‐1 with an outstanding cycle performance over 200 cycles in room‐temperature ASSBs. The significance of engineering parameters is emphasized, such as particle size and specific density, in promoting a homogeneous and fast Li + transport within the composite cathodes. Furthermore, the formation of undesirable interphase between the halide ISE in the cathode and sulfide ISE separator is elucidated, which may be a critical factor impeding long‐term cyclability of ASSBs. This work provides insights into the design of composite cathodes for high‐energy‐density ASSBs.

Chemistry

A Cross‐Linked Flexible Metaferroelectrolyte Regulated by 2D/2D Perovskite Heterostructures for High‐Performance Compact Solid‐State Sodium Batteries

Abstract To address the issues of limited ionic conductivity and poor interface stability at room and low temperatures in solid‐state electrolytes, a robust intrinsic ferroelectrolyte or nanoferroelectrolyte strategy for engineering solid‐state flexible ferroelectric composite electrolytes utilizing strongly coupled intrinsic ion conducting 2D/2D sodium‐rich anti‐perovskite (NaRAP)/ferroelectric perovskite heterostructures is introduced. Herein, highly scalable PVDF‐based metaferroelectrolytes with Na 2.99 Ba 0.005 OCl/Ca 2 Na 2 Nb 5 O 16 − (CNNO − ) nanosheets into a ferroelectric poly(vinylidene fluoride‐co‐hexafluoropropylene) (PVDF‐HFP) matrix, through an in situ cross‐linking and spontaneous bridging method, for compact solid‐state sodium batteries (SSBs), are reported. Benefiting from unique well‐dispersed 3D ferroelectric coupled network and the Na 2.99 Ba 0.005 OCl/CNNO − ‐induced PVDF‐HFP ferroelectric β phase, the Na + flux is regulated, thereby inhibiting Na dendrite growth at the interface. Notably, the optimized PH‐5% NC metaferroelectrolyte exhibits rapid ion transport (1.11 × 10 −4 S cm −1 at 25 °C), a wide electrochemical window (> 4.8V), superior conformal mechanical compatibility, improved flexibility, good elasticity and flame retardancy. The solid‐state Na 3 V 2 (PO 4 ) 3 /PH‐5% NC/Na batteries present a stable cycling performance (remaining 56.4 mAh g −1 after 500 cycles at 1 C) even at 0 °C, potential for cost‐effective, safe, stable and compact SSB energy storage over 600 Wh L −1 , vastly surpassing 365 Wh L −1 of the current commercial sodium‐ion liquid‐electrolyte batteries.

Chemistry

Chemical Bond Covalency in Superionic Halide Solid‐State Electrolytes

Abstract Halide solid‐state electrolytes (SSEs) are promising superionic conductors with high oxidative stability and ionic conductivity, making them attractive for all‐solid‐state lithium‐ion batteries. However, most studies have focused on ion‐stacking structures, overlooking the role of bond characteristics in ionic transport. Here, we investigate bond dynamics and the superionic transition (SIT) in bromide electrolyte, Li 3 InBr 6 , using synchrotron X‐ray techniques and ab initio molecular dynamics (AIMD) simulations. We demonstrate that the SIT in halide SSEs is driven by a thermally induced transition in bonding character (ionic to covalent) rather than a change in crystal phase. AIMD simulations further reveal enhanced Li⁺ diffusion and collective anion motion at elevated temperatures. Expanding our study to Li 3 LnBr 6 (Ln = Gd, Tb, Ho, Tm, and Lu), we confirm the widespread occurrence of SIT in this material class, with Li 3 GdBr 6 exhibiting the highest ionic conductivity (5.2 mS cm −1 at 298 K). More importantly, the ionic‐covalent transition is highly tunable through electrolyte modifications, such as cation/anion substitution and synthesis methods. Our findings provide a new perspective on ionic transport, highlighting the critical role of chemical bond characteristics in halide SSEs.

Chemistry

Interface Design for High‐Performance All‐Solid‐State Lithium Batteries

All‐solid‐state batteries suffer from high interface resistance and lithium dendrite growth leading to low Li plating/stripping Coulombic efficiency (CE) of <90% and low critical current density at high capacity. Here, in this work, both challenges are simultaneously addressed and the Li plating/stripping CE is significantly increased to 99.6% at 0.2 mA cm −2 /0.2 mAh cm −2 , and critical current density (CCD) of > 3.0 mA cm −2 /3.0 mAh cm −2 by inserting a mixed ionic‐electronic conductive (MIEC) and lithiophobic LiF‐C‐Li 3 N‐Bi nanocomposite interlayer between Li 6 PS 5 Cl electrolyte and Li anode. The highly lithiophobic LiF‐C‐Li 3 N‐Bi interlayer with high ionic conductivity (10 −5 S cm −1 ) and low electronic conductivity (3.4×10 −7 S cm −1 ) enables Li to plate on the current collector (CC) surface rather than on Li 6 PS 5 Cl surface avoiding Li 6 PS 5 Cl electrolyte reduction. During initial Li plating on CC, Li penetrates into porous LiF‐C‐Li 3 N‐Bi interlayer and lithiates Bi nanoparticles into Li 3 Bi. The lithiophilic Li 3 Bi and Li 3 N nanoparticles in LiF‐C‐Li 3 N‐Li 3 Bi sub‐interlayer will move to CC along with plated Li, forming LiF‐C/Li 3 N‐Li 3 Bi lithiophobic/lithiophilic sublayer during the following Li stripping. This interlayer enables Co 0.1 Fe 0.9 S 2 /Li 6 PS 5 Cl/Li cell with an areal capacity of 1.4 mAh cm −2 to achieve a cycle life of >850 cycles at 150 mA g −1 . The lithiophobic/lithiophilic interlayer enables solid‐state metal batteries to simultaneously achieve high energy and long cycle life.

25 ENERGY STORAGE