Search NASA⌕ Search

SEARCH · Search NASA

Results for “Solids Formation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Interfacial Chemistry in Solid-State Batteries: Formation of Interphase and Its Consequences

Benefitting from extremely high shear modulus and high ionic transference number, solid electrolytes are promising candidates to address both the dendrite growth and electrolyte consumption problems inherent to the widely adopted liquid-phase electrolyte batteries. However, solid electrolyte/electrode interfaces present high resistance and complicated morphology, hampering the development of solid-state battery systems, while requiring advanced analysis for rational improvement. Here, we employ an ultra-sensitive three-dimensional (3D) chemical analysis to uncover the dynamic formation of interphases at the solid electrolyte/electrode interface. While the formation of interphases widens the electrochemical window, their electronic and ionic conductivities determine the electrochemical performance and has a large influence on dendrite growth. Our results suggest that, contrary to the general understanding, highly stable solid electrolytes with metal anodes in fact promote fast dendritic formation, as a result of less Li consumption and much larger curvature of dendrite tips that leads to an enhanced electric driving force. Detailed thermodynamic analysis shows an interphase with low electronic conductivity, high ionic conductivity, chemically stable yet having a dynamic thickness and uniform coverage is needed to prevent dendrite growth. Finally, this work provides a paradigm for interphase design to address the dendrite challenge, paving the way for the development of robust, fully operational solid-state batteries.

25 ENERGY STORAGE↗

{beta}-Ti(M) solid solution formation and its thermal stability in a NiAl-Cr(Mo)-(Hf,Ti) near eutectic alloy

The effects of combined additions of Ti and Hf to NiAl-Cr(Mo) eutectics on the as-cast microstructure and its thermal stability are investigated through SEM, EDS and TEM, with focus on the formation mechanism of {beta}-Ti(M, M = Hf,Cr,Ni) solid solution phase and its thermal stability after short-term heat treatment. The results show that, due to the presence of large concentrations of {beta}-phase forming and stabilizing elements dissolved into the Ti solid solution phase during solidification, the thermodynamically metastable {beta}-phase was preserved at room temperature. With respect to its thermal stability, within the experimental range examined, the {beta}-Ti(M) solid solution phase, is not influenced. From the practical application point of view, this {beta}-Ti(M) solid solution phase may offer application as a strengthening phase for the design of NiAl-Cr(Mo)-Hf based alloys.

36 MATERIALS SCIENCE↗

Direct Visualization of Solid Electrolyte Interphase Formation in Lithium-Ion Batteries with In Situ Electrochemical Transmission Electron Microscopy

Complex, electrochemically driven transport processes form the basis of electrochemical energy storage devices. The direct imaging of electrochemical processes at high spatial resolution and within their native liquid electrolyte would significantly enhance our understanding of device functionality, but has remained elusive. In this work we use a recently developed liquid cell for in situ electrochemical transmission electron microscopy to obtain insight into the electrolyte decomposition mechanisms and kinetics in lithium-ion (Li-ion) batteries by characterizing the dynamics of solid electrolyte interphase (SEI) formation and evolution. Here we are able to visualize the detailed structure of the SEI that forms locally at the electrode/electrolyte interface during lithium intercalation into natural graphite from an organic Li-ion battery electrolyte. We quantify the SEI growth kinetics and observe the dynamic self-healing nature of the SEI with changes in cell potential.

25 ENERGY STORAGE↗

Operando Infrared Nanospectroscopy of the Silicon/Electrolyte Interface during Initial Stages of Solid-Electrolyte-Interphase Layer Formation

The solid electrolyte interphase (SEI) is a critical component in Li-ion batteries; however, its nanoscale structure and composition and unstable nature make it difficult to characterize and ascertain primary functional mechanisms. We use operando nanoscale Fourier transform infrared spectroscopy (nano-FTIR) with a broadband synchrotron IR source to study the SEI formation on a thin-film Si electrode at nanometer-scale spatial resolution as a function of time and voltage. By probing the Si/carbonate electrolyte interface through a 25 nm-thick amorphous Si window/electrode, we detect molecular vibrational modes within a 10s of nanometers region adjacent to the Si surface and observe that PF6 – anions react to form LiF at 0.5 V. Spatially resolved nano-FTIR spectra showcase subtle nanoscale heterogeneities in the initial solid/liquid interface and the resulting deposited LiF. With its nanoscale resolution and high chemical specificity, operando nano-FTIR provides unique insights into the dynamics and heterogeneous formation of SEIs and opens opportunities for connecting nanoscale interfacial properties to bulk performance metrics.

Dopilka, Andrew↗

Development of a Thermophysical Properties Model for Flowsheet Simulation of Biomass Pyrolysis Processes

A properties model was developed for use in commercial process simulators to model pyrolysis of lignocellulosic biomass. The component list was chosen to enable process simulations based on a recently published lumped pyrolysis kinetics model. Since many of the compounds involved in pyrolysis are not found in simulator databanks, estimation based on available literature data was used to establish missing parameters. Standard solid enthalpy of formation, solid heat capacity, and solid density estimates calculated from the limited experimental data available were prepared for six biomass constituents and nine intermediate and end-products of their pyrolysis. Ideal gas enthalpy of formation and heat capacity, critical property, and vapor pressure estimates were prepared for another four pyrolysis end-products and one biomass component. The estimates were all validated against the closest available experimental data in the literature. The addition of these new components and properties allows thermodynamically rigorous simulation of lumped biomass pyrolysis reactions with accurate energy balances. Furthermore enthalpies of reaction calculated from the properties model were compared with reported reaction enthalpies for the same lumped biomass pyrolysis reactions and found to be in general agreement.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High electronic conductivity as the origin of lithium dendrite formation within solid electrolytes

Solid electrolytes (SEs) are widely considered as an ‘enabler’ of lithium anodes for high-energy batteries. However, recent reports demonstrate that the Li dendrite formation in Li 7 La 3 Zr 2 O 12 (LLZO) and Li 2 S–P 2 S 5 is actually much easier than that in liquid electrolytes of lithium batteries, by mechanisms that remain elusive. Here we illustrate the origin of the dendrite formation by monitoring the dynamic evolution of Li concentration profiles in three popular but representative SEs (LiPON, LLZO and amorphous Li 3 PS 4 ) during lithium plating using time-resolved operando neutron depth profiling. Although no apparent changes in the lithium concentration in LiPON can be observed, we visualize the direct deposition of Li inside the bulk LLZO and Li 3 PS 4 . Furthermore, our findings suggest the high electronic conductivity of LLZO and Li 3 PS 4 is mostly responsible for dendrite formation in these SEs. Lowering the electronic conductivity, rather than further increasing the ionic conductivity of SEs, is therefore critical for the success of all-solid-state Li batteries.

36 MATERIALS SCIENCE↗

Primary Radiation Damage Formation in Solids

The processes that give rise to changes in the microstructure and the physical and mechanical properties of solid metals and ceramics exposed to energetic particles are initiated by essentially elastic collisions between atoms in what has been called an atomic displacement cascade. These processes are similar in metals and ceramics, with some differences related to the ionic and covalent bonding in ceramics compared to metallic bonding. The formation and evolution of primary radiation damage mechanisms are described to provide an overview of how stable defects are formed by displacement cascades, as well as the nature and morphology of the defects themselves. The impact of the primary variables cascade energy and irradiation temperature are discussed, along with a range of secondary factors that can influence damage formation.

Zarkadoula, Eva↗

Formation of solid thorium monoxide at near-ambient conditions as observed by neutron reflectometry and interpreted by screened hybrid functional calculations

Oxidation of a ~1000 Å sputter-deposited thorium thin film at 150 °C in 100 ppm of flowing oxygen in argon produces the long-sought solid form of thorium monoxide. Changes in the scattering length density (SLD) distribution in the film over the 700-min experiment measured by in-situ, dynamic neutron reflectometry (NR) shows the densities, compositions and thickness of the various thorium oxides layers formed. Screened, hybrid density-functional theory calculations of potential thorium oxides aid interpretation, providing atomic-level picture and energetics for understanding oxygen migration. NR provided evidence of the formation of substoichiometric thorium oxide, ThO y (y < 1) at the interface between the unreacted thorium metal and its dioxide overcoat which grows inward, consuming the thorium at a rate of 2.1 Å/min while y increases until reaching 1:1 oxygen-to-thorium. Its presence indicates that kinetically-favored solid-phase ThO can be preferentially generated as a majority phase under the thermodynamically-favored ThO 2 top layer at conditions close to ambient.

36 MATERIALS SCIENCE↗

Insights into Spontaneous Solid Electrolyte Interphase Formation at Magnesium Metal Anode Surface from Ab Initio Molecular Dynamics Simulations

Spontaneous chemical reactivity at multivalent (Mg, Ca, Zn, Al) electrode surfaces is critical to solid electrolyte interphase (SEI) formation, and hence, directly affects the longevity of batteries. Here, we report an investigation of the reactivity of 0.5 M Mg(TFSI)2 in 1,2-dimethoxyethane (DME) solvent at a Mg(0001) surface using ab initio molecular dynamics (AIMD) simulations and detailed Bader charge analysis. Based on the simulations, the initial degradation reactions of the electrolyte strongly depend on the structure of the Mg(TFSI)2 species near the anode surface. At the surface, the dissociation of Mg(TFSI)2 species occurs via cleavage of the N-S bond for the solvent separated ion pair (SSIP) and via cleavage of the C-S bond for the contact ion pair (CIP) configuration. In the case of the CIP, both TFSI anions undergo spontaneous bond dissociation reactions to form atomic O, C, S, F, and N species adsorbed on the surface of the Mg anode. These products indicate that the initial SEI layer formed on the surface of the pristine Mg anode consists of a complex mixture of multiple components such as oxides, carbides, sulfides, fluorides, and nitrides. We believe that the atomic level insights gained from these simulations will lay the groundwork for the rational design of tailored and functional interphases that are critical for the success of multivalent battery technology.

Agarwal, Garvit↗

Solid–Electrolyte Interphase Formation and Electrolyte Reduction at Li-Ion Battery Graphite Anodes: Insights from First-Principles Molecular Dynamics

Understanding the nature and formation of the solid–electrolyte interphase (SEI) formed in electrochemical storage devices, such as Li-ion batteries, is most important for improving functionality. Few experiments exist that adequately probe the SEI, particularly in situ. We perform predictive ab initio molecular dynamics simulations of the anode–electrolyte interface for several electrolytes and interface functionalizations. These show strongly differing effects on the reducibility of the electrolyte. Electrolyte reduction occurs rapidly, on a picosecond time scale. Orientational ordering of electrolyte near the interface precedes reduction. The reduced species depend strongly on surface functionalization and presence of LiPF6 salt. While LiPF6 salt in ethylene carbonate is more stable at a hydrogen-terminated anode, oxygen/hydroxyl termination causes spontaneous dissociation to form LiF and other fluorophosphates. LiF migrates to the interface creating chainlike structures, consistent with experimental observations of LiF agglomeration. Inorganic products such as LiF and Li2CO3 migrate closer to the anode than purely organic components, consistent with their more ionic character. Significantly, we conclude that while the electrolyte reduction occurs at the molecular level near the interface, requiring specific alignments and proximity, the reducibility is governed by the average reduction potential barrier between the electrode (anode) and the electrolyte.

25 ENERGY STORAGE↗

Radiation-Induced Long-Lived Transients and Metal Particle Formation in Solid KCl–MgCl 2 Mixtures

Here, the electron paramagnetic resonance and diffuse reflectance-optical absorption spectra of room-temperature γ-irradiated KCl–MgCl 2 binary solid salt mixtures (98:2 mol % and 2:98 mol %) and the eutectic (68:32 mol %) are reported. Additionally, powder X-ray diffraction of the pristine salts and thermal annealing studies of the irradiated salts were performed to evaluate the radiolysis product stability, annihilation, and association in metallic particles. The main long-lived transient species detected in 98:2 mol % KCl–MgCl 2 salts were perturbed F-centers, that is, trapped electrons (e t – ) in the vicinity of Mg ions (λ max at 561 nm), and the radiolytic reduction of Mg 2+ to Mg + and Mg 0 . Thermal annealing promoted the diffusion of defects to yield polycations (Mg n + ). On the other hand, irradiation of 2:98 mol % KCl/MgCl 2 salts showed the formation of cationic and neutral Mg dimers (Mg 2 + and Mg 2 ) and trimers as well as centers with a rhombic powder pattern apparently consisting of an electron shared between three Mg 2+ nuclei associated with an anion vacancy (ν a + –Mg 3 5+ ). Trapped electrons (e t – ) (F-centers) were not observed in the irradiated eutectic mixture; instead, Mg 2 , Mg 0 , and Cl 3 – were observed. It was observed that the higher temperature for thermal ionization of radiation-reduced Mg species decreased the extent of electron recombination reactions and the disproportionation of Cl 3 – compared to the pure KCl but enhanced the aggregation of Mg into larger metallic microstructures (metallic particles).

36 MATERIALS SCIENCE↗

A Bottom-Up Formation Mechanism of Solid Electrolyte Interphase Revealed by Isotope-Assisted Time-of-Flight Secondary Ion Mass Spectrometry

Understanding the solid electrolyte interphase (SEI) formation mechanism is critically important for the performance and durability of lithium-ion batteries. However, the details of how SEI builds up into a nanometer-thick layer from molecular level reduction reactions on negative electrodes are missing. Here, isotope-assisted time-of-flight secondary ion mass spectrometry analyses were designed to answer this fundamental question. By investigating the isotope ratio profile in SEI during the initial SEI formation cycle, it is discovered that the topmost SEI near the electrolyte formed first and the SEI near the electrode formed later. Furthermore, this new “bottom-up” SEI growth mechanism was then correlated to the electrolyte one-electron and two-electron reduction reaction dynamics, which in turn explains the formation of the two-layered organic–inorganic SEI composite structure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗