Light polarization characteristics of m-plane Al{sub x}Ga{sub 1-x}N films suffering from in-plane anisotropic tensile stresses

Polarization characteristics of the near-band-edge optical transitions in m-plane Al{sub x}Ga{sub 1-x}N epilayers suffering from anisotropic stresses were quantified. The epilayers were grown by both ammonia-source molecular beam epitaxy and metalorganic vapor phase epitaxy methods on an m-plane freestanding GaN substrate. The light polarization direction altered from E perpendicular c to E || c at the AlN molar fraction, x, between 0.25 and 0.32, where E is the electric field component of the light and perpendicular and || represent perpendicular and parallel, respectively. To give a quantitative explanation for the result, energies and oscillator strengths of the exciton transitions involving three separate valence bands were calculated as functions of strains using the Bir-Pikus Hamiltonian. The calculation predicted that the lowest energy transition (E{sub 1}) is polarized to the m-axis normal to the surface (X{sub 3}) for 0<x{<=}1, meaning that E{sub 1} emission is principally undetectable from the surface normal for any in-plane tensile strained Al{sub x}Ga{sub 1-x}N. The polarization direction of observable surface emission was predicted to alter from c-axis normal (X{sub 1}) to c-axis parallel (X{sub 2}) for the middle energy transition (E{sub 2}) and X{sub 2} to X{sub 1} for the highest energy transition (E{sub 3}) between x=0.25 and 0.32. The experimental results were consistently reproduced by the calculation.

36 MATERIALS SCIENCE↗

Dynamic fracture of tantalum under extreme tensile stress

The understanding of fracture phenomena of a material at extremely high strain rates is a key issue for a wide variety of scientific research ranging from applied science and technological developments to fundamental science such as laser-matter interaction and geology. Despite its interest, its study relies on a fine multiscale description, in between the atomic scale and macroscopic processes, so far only achievable by large-scale atomic simulations. Direct ultrafast real-time monitoring of dynamic fracture (spallation) at the atomic lattice scale with picosecond time resolution was beyond the reach of experimental techniques. We show that the coupling between a high-power optical laser pump pulse and a femtosecond x-ray probe pulse generated by an x-ray free electron laser allows detection of the lattice dynamics in a tantalum foil at an ultrahigh strain rate of Embedded Image ~2 × 10 8 to 3.5 × 10 8 s -1 . A maximal density drop of 8 to 10%, associated with the onset of spallation at a spall strength of ~17 GPa, was directly measured using x-ray diffraction. The experimental results of density evolution agree well with large-scale atomistic simulations of shock wave propagation and fracture of the sample. Our experimental technique opens a new pathway to the investigation of ultrahigh strain-rate phenomena in materials at the atomic scale, including high-speed crack dynamics and stress-induced solid-solid phase transitions.

36 MATERIALS SCIENCE↗

Finite Element Analysis (FEA) for Water-Foam Fracturing of Granite Rock

In addition to the foam data that were obtained from literature and that were collected from the current study, simulation data was also generated from finite element analysis (FEA) conducted in this study using COMSOL Multiphysics software. The FEA models were built to simulate the experiments conducted at Oak Ridge National Laboratory (ORNL) on cement and granite samples. In these FEA models, temperature was kept at ambient while the pressure profile resembled the loading conditions during the ORNL experiments, where pressure was either monotonically increased or applied cyclically. The cement material was used as a model material and was used to study Von Mises stress and tensile stress distribution for different bore hole length geometry using a parametric sweep with water as fracturing fluid using solid-fluid interaction module. For the granite material, FEA models were developed for stress analysis of cylindrical samples with water or foam fluids. The solid mechanics module in COMSOL was implemented to solve for Von Mises stress and tensile stress. The fluid-structure interaction module was implemented to solve for water-foam interaction on granite cylinder with addition of fluid-loading on structure, i.e., large deformation in solid mechanics with no impact on fluid deformation. Foam was considered as a pseudo single-phase compressible fluid for which material properties were calculated from water and gas (nitrogen) phases. The density of foam is calculated as a function of the densities of water and nitrogen, while viscosity is a function of temperature. Four types of FEA analyses were modelled: 1. Monotonic injection with water 2. Monotonic injection with foam 3. Cyclic injection with water 4. Cyclic injection with foam All the COMSOL files are converted to a zip file which is save in .mph.

15 GEOTHERMAL ENERGY↗

Hoop Tensile Failure Stress of 500 µm-Diameter Ceramic Spheres

The tensile failure stress of a brittle-material sphere is important to the survival of the sphere itself but is particularly relevant to systems that employ such spheres for applications in which the sphere exterior is subjected to tension during system fabrication or operation. That maximum hoop or tangential stress can be measured by diametrally compressing a C-sphere specimen directly machined from such spheres. This combination of specimen geometry and test method was conceived at Oak Ridge National Laboratory around 20 years ago. Although the C-sphere geometry has been tested with larger spheres, the ease and efficacy of its testing are unknown for submillimeter sphere diameters. To consider this, C-sphere specimens were machined from yttria-stabilized zirconia (YSZ) spheres of ∼500 µm diameter. The maximum (hoop or tangential) tensile stress was determined as a function of compressive failure force and specimen dimensions using finite element analysis. Companion effective area and volume as a function of Weibull modulus were computed. Hoop tensile failure stresses were then measured and fractography conducted to examine flaw type and location and to estimate the mirror constant of this YSZ grade. This novel study demonstrates that hoop tensile failure stress can be determined with sub-millimeter brittle-material spheres.

Delia, Daniel [ORNL] (ORCID:0000000209023239)↗

Oxide growth stress measurements and relaxation mechanisms for alumina scales grown on FeCrAlY: Oxide growth stress measurements and relaxation mechanisms

Early-stage tensile stress evolution in α-Al 2 O 3 scales during oxidation of FeCrAlY at 1000, 1050, 1100, and 1200 °C was monitored in situ by use of synchrotron radiation. Tensile stress development as a function of oxidation temperature indicated a dynamic interplay between stress generation and relaxation. An analysis of the time dependence of the data indicated that the observed relaxation of the initial tensile stress in the oxide scales at 1100 and 1200°C is dominated by creep in the α-Al 2 O 3 . A thin layer of a (Fe,Cr,Al) oxide was observed at the oxide-gas interface, consistent with a mechanism whereby the conversion of (Fe,Cr,Al) 2 O 3 to α-Al 2 O 3 produces an initial tensile stress in the alumina scale.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Edge-Controlled Mechanical Failure of Si and SiC Semiconductor Chips

Silicon (Si) and silicon carbide (SiC) semiconductor chips are subjected to thermal gradients during service, have coefficient of thermal expansion mismatches with the constituents they are attached to, and are therefore subjected to thermomechanical tensile stresses that can initiate their fracture. Because of inherent brittleness, their probabilistic (Weibull) tensile failure strength was examined to understand sustainable tensile stresses and any exhibition of strength-size-scaling. Failure stress testing of entire (10-mm-square) chips was conducted using uniaxial flexure (3-point-bending) and biaxial flexure (anticlastic bending). The advantage of the anticlastic bend test is all eight primary edges are subjected to identical sinusoidal stress distribution so tensile failure stress is concurrently sensitive to edge-state quality, surface-state quality, crystallographic orientation, and any strength anisotropies of any of those. Tensile stress tolerance of both Si and SiC chips was limited by extrinsic strength-limiting flaws located at their edges and on lapped surfaces too in the case of the Si. Both materials exhibited strength-size scaling; namely, a larger chip is likely to fail at a lower tensile stress. The anticlastic bend test method was effective for evaluating edge failure stress provided surface-type strength-limiting flaws were not dominant. Edge-strength anisotropy (i.e., crystallographic orientation dependence) was observed with both the Si and SiC chips. Surface-strength anisotropy also occurred with Si chips because one side was lapped and the other polished. Lastly, the SiC chips failed at much higher tensile stresses than Si chips; however, that strength difference could be a ramification of differences in edge-slicing quality and not necessarily from intrinsic material differences.

36 MATERIALS SCIENCE↗

Examination of Hybrid Metal Coatings for Mitigation of Fission Product Release and Corrosion Protection of LWR SiC/SiC

There is a need to increase the safety margins of current and future light water reactors (LWRs) due to the unfortunate events at Fukushima Daiichi Nuclear Plant. Safety is crucial to restore public confidence in nuclear energy, acknowledged as an economical, high-­density energy solution to climate change. The development of accident-­tolerant fuel (ATF) concepts is crucial to this endeavor. The objective of ATF is to delay the consequences of accident progression, being inset in high temperature steam and maintaining high thermomechanical strength for radionuclide retention. The use of advanced SiCf-­SiC composite as a substitute for zircaloy-­based cladding is being considered. However, at normal operations, SiC is vulnerable to the reactor coolant and may corrode at an unacceptable rate. As a ceramic-­matrix composite material, it is likely to undergo microcracking operation, which may compromise the ability to contain gaseous fission products. A proposed solution to both issues is the application of mitigation coatings for use in normal operations. At Oak Ridge National Laboratory (ORNL), three coating technologies have been investigated with industry collaborators and vendors. These are electrochemical deposition, cathodic arc physical vapor deposition (PVD hereafter) and vacuum plasma spray (VPS). The objective of this document is to summarize these processing technologies, the resultant as-­processed microstructures and properties of the coatings. In all processes, substrate constraint resulted in substantial tensile stresses within the coating layer. Each technology must mitigate this tensile stress. Electrochemical coatings use chromium as the coolant facing material, and are deposited on a nickel or carbon “bond coat”. This is economical but suffers microcracking in the chromium layer. PVD-­based coatings use chromium and titanium in both metallic form and nitrides, and can be deposited defense-­in-­depth as multilayers. This vapor method eliminated tensile stress during processing and coatings were up to ~30 μm thick without microcracking. VPS produced coatings based on Zircaloy-2, which has a proven reactor-­compatibility. The tensile stresses appearred to be partially mitigated by annealing. Analysis showed that VPS coatings required further optimizations to prevent adverse reactions with the substrate and need a minimum thickness of ~50 μm. In addition, development of coatings are constrained by neutronic depletion analysis, which clearly indicated enrichment as an issue if the coating is too thick. Based on the present work, the cathodic arc PVD technology was considered ready for the extensive testing and evaluation on cladding materials due to their ability to mitigate the excessive tensile stresses and the reasonable coating quality achieved. The VPS Zircaloy-­2 coating technology required additional development toward mitigation of issues related to the substrate reaction and porosity. In the future, PVD and VPS will have be scaled upon successful development and demonstration. Electrochemical coatings, which are proven scalability, currently require development to mitigate issues related to the tensile stress after deposition.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Assessment of InSb infrared detector arrays assembly procedure employing ANSYS

Local failure in the InSb infrared detector arrays (InSb IDAs) is chiefly triggered by the local shear stress, the peeling stress, and the tensile stress in the InSb IDAs. Thus, these three stress components are utilized to assess the rationality of the current assembly procedure of the InSb IDAs in this paper, which is described as follows: firstly, performing liquid nitrogen shocking tests on the fabricated InSb IDAs, provided that no local failure phenomena occur in the InSb IDAs, then the balanced composite structure (BCS) is glued with the bottom surface of the InSb IDAs to accomplish the fabrication of the InSb IDAs assembly. We ascertain that the tensile stress in the center region of the InSb substrate declines slightly with the attached BCS, at the same time, both the interfacial shear stress and the peeling stress maintain unchanged at the locations where the local delamination most likely appears. These non-increased stress distribution characteristics with the added BCS confirmed that the current assembly procedure of the InSb IDAs is reasonable, and the glued BCS does not increase the failure probability of the InSb IDAs assembly.

36 MATERIALS SCIENCE↗

Pressure-dependent transition from atoms to nanoparticles in magnetron sputtering: Effect on WSi{sub 2} film roughness and stress

We report on the transition between two regimes from several-atom clusters to much larger nanoparticles in Ar magnetron sputter deposition of WSi{sub 2}, and the effect of nanoparticles on the properties of amorphous thin films and multilayers. Sputter deposition of thin films is monitored by in situ x-ray scattering, including x-ray reflectivity and grazing incidence small-angle x-ray scattering. The results show an abrupt transition at an Ar background pressure P{sub c}; the transition is associated with the threshold for energetic particle thermalization, which is known to scale as the product of the Ar pressure and the working distance between the magnetron source and the substrate surface. Below P{sub c} smooth films are produced while above P{sub c} roughness increases abruptly, consistent with a model in which particles aggregate in the deposition flux before reaching the growth surface. The results from WSi{sub 2} films are correlated with in situ measurement of stress in WSi{sub 2}/Si multilayers, which exhibits a corresponding transition from compressive to tensile stress at P{sub c}. The tensile stress is attributed to coalescence of nanoparticles and the elimination of nanovoids.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Stress evolution in platinum thin films during low-energy ion irradiation

Stress evolution of Pt thin films during low-energy ion irradiation is investigated by using wafer bending measurements and molecular dynamics simulations. Noble gas ions ranging in mass from He to Xe and energy from 0.5 to 5 keV are used. Depending on the type and energy of the ion, the change in stress can either be tensile or compressive. Heavier or higher-energy ions tend to create tensile stress, while lighter ions such as He always induce compressive stress. The stress evolution also depends on the initial state of stress in the thin films. The results are explained by a competition between the tensile stress induced by local melting along the ion track and the compressive stress induced by the accumulation of ion-induced interstitials in defect clusters or grain boundaries, often beyond the calculated ion penetration depth. Anisotropic diffusion of interstitials under an external stress field also plays an important role in the stress evolution. Molecular dynamics simulation is employed to evaluate the importance of each of these microscopic mechanisms.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Size Scaling of Tensile Failure Stress in a Soda-Lime-Silicate Float Glass

The (tensile) strength-size scaling of a float soda-lime silicate glass was studied using biaxial flexure and Hertzian ring crack initiation testing. The examined Weibull effective areas spanned ~ 0.4 to 48,000 mm2. Both the air- and tin-sides were tested. The air side was stronger than the tin side as others have observed; however, the differences in their characteristic strengths decreased with decreasing effective area, and their strengths converged for effective areas smaller than ~ 100 mm2. The failure stress at the smallest effective area examined for the tin-side was ~ 500% greater than that at the largest effective area while that difference was ~ 250% for the air- side. A Weibull modulus change at ~ 100 mm2 suggests different strength-limiting flaw types were dominant below and above that effective area. These results reinforce the importance to interpret and use tensile strength of glass in context to how much of its area is being tensile stressed.

36 MATERIALS SCIENCE↗

Evolution of Microstructure, Residual Stress, and Tensile Properties of Additively Manufactured Stainless Steel Under Heat Treatments

This study investigated the microstructure, residual stress and tensile properties of the directed energy deposited stainless steel 316L (SS316L) under thermal annealing. Microstructure characterization shows the as-printed sample has laser-generated patterns where dendritic structure is observed at the edge of the patterns and cellular structure dominates the interior region. Here, the thermal annealing at 983 and 1093°C effectively removes the dendritic/cellular structures. Synchrotron X-ray diffraction reveals that the as-fabricated SS316L exhibits compressive residual stress of -197.4 MPa. The stress is greatly relieved to -53.8 MPa after annealing at 1093°C. The room temperature tensile testing indicates that the yield strength and ultimate tensile strength drop from 378 and 502 MPa in the as-printed sample to 258 and 446 MPa in the annealed samples (1093°C), respectively. Our study provides insights into the relationship between microstructure, residual stress, and tensile properties of laser additive manufactured SS316L.

36 MATERIALS SCIENCE↗

Structure disorder degree of polysilicon thin films grown by different processing: Constant C from Raman spectroscopy

Flat, low-stress, boron-doped polysilicon thin films were prepared on single crystalline silicon substrates by low pressure chemical vapor deposition. It was found that the polysilicon films with different deposition processing have different microstructure properties. The confinement effect, tensile stresses, defects, and the Fano effect all have a great influence on the line shape of Raman scattering peak. But the effect results are different. The microstructure and the surface layer are two important mechanisms dominating the internal stress in three types of polysilicon thin films. For low-stress polysilicon thin film, the tensile stresses are mainly due to the change of microstructure after thermal annealing. But the tensile stresses in flat polysilicon thin film are induced by the silicon carbide layer at surface. After the thin film doped with boron atoms, the phenomenon of the tensile stresses increasing can be explained by the change of microstructure and the increase in the content of silicon carbide. We also investigated the disorder degree states for three polysilicon thin films by analyzing a constant C. It was found that the disorder degree of low-stress polysilicon thin film larger than that of flat and boron-doped polysilicon thin films due to the phase transformation after annealing. After the flat polysilicon thin film doped with boron atoms, there is no obvious change in the disorder degree and the disorder degree in some regions even decreases.

36 MATERIALS SCIENCE↗

The effect of a prior short-term ageing on mechanical and creep properties of P92 steel

Highlights: • The results of simulated ageing at 650°C allows to estimate degradation of P92 steam pipes due to accidental overheating. • Simulated ageing has only a slight effect on ambient tensile properties and hardness. • A sudden decrease in impact properties occurred after ageing for 2000h. The FATT of about 25°C was determined. • The creep results show a clear detrimental influence of tempering ageing on the creep strength. • No Z-phase precipitation occurred due to the ageing process. - Abstract: We have investigated the effect of prior short-term ageing on the mechanical and creep properties of tungsten and boron modified 9%Cr ferritic steel (ASTM Grade P92 steel), to provide material data base for the estimation of material degradation due to occurrence of accidental overheating in the early stage of service loading. The steel was aged at 650 °C for up to 100, 200, 500, 1000, 2000 and 5000 h prior to mechanical and creep testing. Changes in the microstructure during ageing had a slight effect on the reduction of room temperature tensile properties. A sudden decrease on impact properties occurred after ageing for 2000 h, but the occurred impact energy of about 70 J is in accordance with the specified minimum value of 68 J at room temperature for the virgin condition. The creep behaviour of P92 steel in the as-received condition and after different isothermal ageing exposures prior to creep was investigated at 600 and 650 °C in the power-law creep regime. The initial applied tensile stress ranged from 90 to 200 MPa. The results clearly show a detrimental influence of isothermal ageing on creep properties even after a few hundred hours. Based on microstructure analysis, which was done mostly in a qualitative way, a significant decrease in the creep life after ageing resulted from changes of the dislocation substructure and instability of Laves phase and M{sub 23}C{sub 6} particles.

36 MATERIALS SCIENCE↗