Adsorption Processes during Electrochemical Atomic Layer Deposition of Gold

Electrochemical atomic layer deposition (e-ALD) technique offers a simple and effective "wet chemistry" approach enabling high-precision monolayer-by-monolayer deposition of metal films. The process of e-ALD of Au involves lead underpotential deposition (PbUPD) followed by its redox replacement by a Au monolayer. The time evolution of the deposit mass during "one-pot" Au e-ALD is known to exhibit a unique three-stage response that is presently not well understood. In this work, we probe this response using voltammetry, electrochemical quartz crystal microgravimetry (e-QCM), and chronoamperometry to unravel the underlying mechanistic events during Au e-ALD. Furthermore, the presence of adsorbed Au +3 -ligand complex(es) (Au-L) on the Au surface is established. In stage I of e-ALD, this Au-L adsorbed layer is reduced to Au while a Pb UPD adlayer is formed. In stage II, the Pb UPD adlayer undergoes spontaneous surface-limited redox replacement by nobler Au under open-circuit conditions. Finally, in stage III, re-adsorption of the Au-L occurs on the newly deposited Au. Quantitative analysis of the deposit mass transients obtained under a variety of conditions provides an estimate of the Au-L mass and its molecular weight.

36 MATERIALS SCIENCE↗

Electrocatalysts, and fuel cells containing them

Provided are electrocatalysts, fuel cells, methods of making fuel cells, and methods of generating an electric current, each featuring a platinum (Pt)-containing substrate in contact with an aqueous solution comprising Pb2+. Electrocatalysts of the invention are formed via underpotential deposition (UPD) when a trace amount of Pb2+ is present in the electrolyte of a half anodic cell for oxidizing formic acid using Pt as the anode. Surprisingly, the UPD process dramatically enhances the activity of formic acid oxidation, at least as much as 10-fold compared with palladium (Pd) black. In an embodiment, the electrocatalyst comprises a Pt-containing substrate, a submonolayer of lead (Pb) adsorbed onto the Pt-containing substrate, and an aqueous solution comprising Pb2+, wherein the concentration of Pb2+ in the aqueous solution is 10 to 500 μm.

30 DIRECT ENERGY CONVERSION↗

The Chemistry, Formation and Passivation of Solid-Electrolyte Interphase (SEI) from FSI- Breakdown at Li-metal Potential

LiFSI-based liquid electrolytes are promising for realizing high Coulombic efficiency (CE) and long cycle life of next-generation high-energy Li metal battery. Nevertheless, the fundamentals of both the chemistry and formation of solid-electrolyte interphase (SEI) in these electrolytes have remained elusive. Herein, we extensively combine electrochemistry and X-ray photoelectron spectroscopy (XPS) to illustrate the reaction pathways of electrolyte decomposition, especially FSI- breakdown, as well as the dissolution trend of various inorganic SEI components. The SEI-forming reactions at Cu/electrolyte interface manifest a potential (E) dependence, driven by direct electron-transfer (ET) and Li underpotential-deposition (Li UPD) at high and low E regions, respectively. By closely correlating the XPS data obtained with and without solvent washing, we demonstrate that not all the products derived from SEI reactions are incorporated into forming a passivating surface layer, with a notable portion dissolving into liquid electrolyte instead. Importantly, high-CE electrolyte dictated by the chemical identity of solvent, is found to exhibit minimized interfacial reactivity of SEI formation enabling more effective interphasial passivation, via preferential integration of passivating ingredients such as LiF. Overall, this work formulates a systematic understating of bridging the SEI chemistry, formation and passivation while identifying key characteristics of high-performance electrolyte for guiding future design.

Bao, Zhenan [SLAC National Accelerator Laboratory ↗

Constitutional under-potential plating (CUP) – New insights for predicting the morphological stability of deposited lithium anodes in lithium metal batteries

Lithium (Li) cycling in lithium metal batteries (LMBs) inevitably witnesses a non-planar Li/electrolyte interface (cellular/dendritic microstructure) affecting the performance, safety and reliability of LMBs. Herein, the “constitutional under-potential plating” (CUP) concept is presented for the first time to understand the evolution, formation and predict the morphological stability/instability of the Li/electrolyte interface. Here, the CUP condition, a measure of the driving force for interface perturbation, occurs when the true potential gradient at the interface is smaller than the equilibrium electrodeposition potential gradient at the Li/electrolyte interface resulting in the electrolyte ahead of the Li-electrolyte interface to be in an under-potential state. Detailed CUP criterion calculations conducted herein establishes the relationship of battery operating conditions (e.g. current density, potential gradient) with the electrolyte properties (e.g. Li-ion transference number and diffusion coefficient) predicting the morphological stability condition at the interface. In addition to the driving force for interface perturbation, the capillarity effect or the Gibbs Thomson effect, a measure of the resistance to perturbation of the perturbed interface is discussed for understanding the influence of interfacial energy/adhesion energy between the current collector and the deposited Li on the overall morphological stability of the Li/electrolyte interface, a critical criterion for the unwanted dendritic morphology.