At least 37 records · Page 2

Highly porous ZnS microspheres for superior photoactivity after Au and Pt deposition and thermal treatment

Graphical abstract: Highly porous ZnS microsphere of size 2–5 μm having large surface area ca. 173.14 m{sup 2} g{sup −1} exhibits superior photocatalytic activity for the oxidation of 4-nitrophenol under UV light irradiation. The rate of photooxidation has been significantly improved by Au and Pt deposition and after sintering, respectively, due to rapid electron acceptance by metal from photoexcited ZnS and growth of crystalline ZnS phase. - Highlights: • Photoactive ZnS microsphere of size 2–5 μm was prepared by hydrothermal route. • Highly porous cubic spherical ZnS crystals possess a large surface area, 173 m{sup 2} g{sup −1}. • 1 wt% Au and Pt photodeposition highly quenched the photoluminescence at 437 nm. • Sintering and metal loading notably improve the photooxidation rate of 4-nitrophenol. • Pt co-catalyst always exhibits superior photoactivity of ZnS microsphere than Au. - Abstract: This work highlights the enhanced photocatalytic activity of porous ZnS microspheres after Au and Pt deposition and heat treatment at 500 °C for 2 h. Microporous ZnS particles of size 2–5 μm with large surface area 173.14 m{sup 2} g{sup −1} and pore volume 0.0212 cm{sup 3} g{sup −1} were prepared by refluxing under an alkaline medium. Photoluminescence of ZnS at 437 nm attributed to sulfur or zinc vacancies were quenched to 30% and 49%, respectively, after 1 wt% Au and Pt loading. SEM images revealed that each ZnS microparticle consist of several smaller ZnS spheres of size 2.13 nm as calculated by Scherrer's equation. The rate of photooxidation of 4-nitrophenol (10 μM) under UV (125 W Hg arc–10.4 mW/cm{sup 2}) irradiation has been significantly improved by Au and Pt deposition followed by sintering due to better electron capturing capacity of deposited metals and growth of crystalline ZnS phase with less surface defects.

36 MATERIALS SCIENCE↗

Low-temperature phase transition of ZnS: The critical role of ZnO

Wurtzite zinc sulfide (WZ-ZnS) is a valuable wide-band-gap semiconductor. However, it is difficult to synthesize due to its high transition temperature (1020 Degree-Sign C). This study investigates the formation of WZ-ZnS particles using a ZnO template. Various phase structures of ZnS with the same size but different levels of ZnO content are generated during the annealing process. The transition temperature can be lowered significantly to below 350 Degree-Sign C. Furthermore, when the powders of ZnO and zinc-blende ZnS are mixed, large ZnS particles are not induced by ZnO to transform into WZ-ZnS. The results strongly suggest that grain size is an essential but not sufficient factor in the formation of WZ-ZnS at lower temperatures. - Graphical abstract: By controlling pH of the precursor, wurtzite ZnS particles can be generated at {approx}350 Degree-Sign C. The ZnO-template mechanism was proposed and discussed. Highlights: Black-Right-Pointing-Pointer Wurtzite ZnS particles were prepared by using simple wet chemistry. Black-Right-Pointing-Pointer pH of the precursor solution was adjusted to decrease the phase transition temperature of ZnS. Black-Right-Pointing-Pointer ZnO-template-inducing mechanism of ZnS phase transition was proposed and discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Charge transfer and optical properties of wurtzite-type ZnS/(CdS/ZnS){sub n} (n = 2, 4, 8) superlattices

Graphical abstract: (a) Normalized temperature-dependent PL spectra of ZnS/(CdS/ZnS){sub 4} superlattices from 5 to 300 K and (b) schematic of charge transfer at CdS/ZnS interface. - Highlights: • Wurtzite ZnS/(CdS/ZnS){sub n} superlattices were prepared at 100 °C by pulsed laser deposition. • Surface phonon of ZnS and multiple phonons modes of ZnS and CdS were observed. • The charge transfer of electrons from CdS electron to ZnS holes by excitation energy was found. - Abstract: ZnS/(CdS/ZnS){sub n} (n = 2, 4, 8) superlattices were deposited on sapphire substrate by pulsed laser deposition (PLD) with alternate cadmium sulfide (CdS) and zinc sulfide (ZnS) crystals at 100 °C. The prepared samples with an average thickness of ∼30 nm for ZnS layer and ∼60 nm for CdS layer have a wurtzite-type structure. Surface phonon of ZnS and multiple phonons modes for ZnS and CdS were observed from Raman spectra. PL spectra show a strong green emission at ∼496 nm, two weak emission bands at ∼400 and ∼577 nm, where the emission band at 400 nm was attributed to the recombination of surface defects states to valence, the emission band at 577 nm as the recombination of Cd{sub i}–V{sub Cd} centers, and the strong emission at ∼496 nm is from the charge transfer of electrons from CdS electron to ZnS holes by excitation energy.

36 MATERIALS SCIENCE↗

Starch-assisted synthesis and optical properties of ZnS nanoparticles

Highlights: • ZnS spherical nanostructure was prepared via starch-assisted method. • The crystalline lattice structure, morphologies, chemical and optical properties of ZnS nanoparticles. • The forming mechanism of ZnS nanoparticles. • ZnS spherical nano-structure can show blue emission at 460–500 nm. - Abstract: ZnS nanoparticles are fabricated via starch-assisted method. The effects of different starch amounts on structure and properties of samples are investigated, and the forming mechanism of ZnS nanoparticles is discussed. By X-ray diffraction (XRD), high resolution transmission electron microscopy (HRTEM) and selected area electron diffraction (SAED), scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR), ultraviolet–visible (UV–vis) spectroscopy and fluorescence (FL) spectrometer, their phases, crystalline lattice structure, morphologies, chemical and optical properties are characterized. The results show that ZnS has polycrystalline spherical structure with the mean diameter of 130 nm. Sample without starch reveals irregular aggregates with particle size distribution of 0.5–2 μm. The band gap value of ZnS is 3.97 eV. The chemical interaction exists between starch molecules and ZnS nanoparticles by hydrogen bonds. The stronger FL emission peaks of ZnS synthesized with starch, indicate a larger content of sulfur vacancies or defects than ZnS synthesized without starch.

36 MATERIALS SCIENCE↗

On the Luminescence Enhancement of Mn2+ By Co-doping of Eu2+ in ZnS:Mn,Eu

The photoluminescence and X-ray luminescence of ZnS:Mn, ZnS:Mn,Eu and ZnS:Eu were investigated and it was found that the luminescence intensity of Mn2+ in ZnS:Mn,Eu co-doped phosphors is highly dependent on the doping concentration of Eu2+. At the optimized Eu2+concentration (0.2%), the photoluminescence of Mn2+ shows about a 5.5 times enhancement and its X-ray luminescence is enhanced by a factor of 2.5. Both wurtzite and zinc blend phases are present in the samples with wurtzite phase dominant. Co-doping of Eu2+ into ZnS:Mn does not change appreciably the ratio of the two phases or the Mn2+ emission luminescence lifetime; however, the doping of Eu2+ into ZnS:Mn does change the phonon activity. Furthermore, it was found that the defect-related blue emission of ZnS:Eu overlaps with the excitation bands of Mn2+ in ZnS:Mn and there is likely energy transfer from these defect states to Mn2+ in ZnS:Mn,Eu. This energy transfer and the phonon modification are considered to be the two main reasons for the luminescence enhancement and the intensity dependence of Mn2+ emission on Eu2+ doping concentration in ZnS:Mn,Eu.

decay Lifetime↗

ZnS-Graphene nanocomposite: Synthesis, characterization and optical properties

A ZnS-Graphene nanocomposite was prepared by a facile one-step hydrothermal method using zinc nitrate hexahydrate, ethylenediamine and carbon disulfide as precursors, graphene oxide as a template. The composite was characterized by X-ray power diffraction, X-ray photoelectron spectroscopy, transmission electron microscopy, Fourier transform infrared, Raman spectra and fluorescence spectroscopy. The results show that graphene oxide was reduced to graphene in the hydrothermal reaction process. Simultaneously, the graphene sheets in the composite are exfoliated and decorated with ZnS nanoparticles. Furthermore, Raman and fluorescence properties of the composite were observed. ZnS-Graphene nanocomposite displays surface-enhanced Raman scattering activity for graphene oxide, and fluorescence enhancement property compared with pure ZnS sample. - Graphical abstract: Approach of reaction makes the reduction of grapheme oxide and the deposition of Zns on the grapheme sheets occur simultaneously and overcomes the aggregation of the grapheme sheets and Zns. Highlights: Black-Right-Pointing-Pointer Graphene oxide is reduced to graphene in the hydrothermal reaction process. Black-Right-Pointing-Pointer ZnS nanoparticles are attached onto the almost transparent graphene sheets. Black-Right-Pointing-Pointer ZnS-Graphene system shows surface-enhanced Raman scattering (SERS) activity. Black-Right-Pointing-Pointer ZnS-Graphene system displays relatively better fluorescence property than pure ZnS.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A simple one-step synthesis of ZnS nanoparticles via salt-alkali-composited-mediated method and investigation on their comparative photocatalytic activity

Graphical abstract: The TEM image shows that the as-synthesized ZnS particle size was estimated to be about 40 nm and this newly synthesized ZnS nanoparticles can be as a promising photocatalytic degradation material for the organic pollutant removal. Display Omitted Highlights: ► ZnS nanoparticles with cubic phase have been successfully synthesized via salt-alkali-composited-mediated method (SACM) for the first time and this method has not been found so far. ► Its band gap (E{sub g}) is a little bigger than commercial ZnS particle mainly due to quantum size effect. ► The as-synthesized ZnS nanoparticles show much more efficient photocatalytic degradation on methyl orange than commercial ZnS powder. -- Abstract: ZnS nanoparticles have been successfully synthesized via salt-alkali-composited-mediated method (SACM) for the first time, using a mixture of LiNO{sub 3} and LiOH (LiNO{sub 3}/LiOH = 60.7:39.3) as a reaction solvent, sodium sulfide and zinc nitrate as reactants at temperature of 210 °C for 24 h in the absence of organic dispersant or capping agents. X-ray diffraction, environment scanning electron microscopy (ESEM) and Transmission electron microscopy (TEM) indicated that the as-synthesized products were well crystallized and belonged to nano-scale. Their UV–vis absorption spectrum demonstrated a band gap of 3.6406 eV corresponding to the absorption edge of 340 nm. The experimental result of photocatalytic degradation on methyl orange by the nano-ZnS showed much better photocatalysis than that by the commercial ZnS powder under the irradiation of ultraviolet light and visible light, respectively.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of ZnS thin films synthesized through a non-toxic precursors chemical bath

Highlights: • High quality ZnS thin films have been deposited by chemical bath deposition technique from a non-toxic precursor’s solution. • Nanocrystalline ZnS thin films with large band gap energy were synthesized without using ammonia. • Evidence that the growing of the thin films is carried out by means of hydroxide mechanism was found. • The properties of these ZnS thin films are similar and in some cases better than the corresponding ones produced using toxic precursors such as ammonia. - Abstract: In solar cells, ZnS window layer deposited by chemical bath technique can reach the highest conversion efficiency; however, precursors used in the process normally are materials highly volatile, toxic and harmful to the environment and health (typically ammonia and hydrazine). In this work the characterization of ZnS thin films deposited by chemical bath in a non-toxic alkaline solution is reported. The effect of deposition technique (growth in several times) on the properties of the ZnS thin film was studied. The films exhibited a high percentage of optical transmission (greater than 80%); as the deposition time increased a decreasing in the band gap values from 3.83 eV to 3.71 eV was observed. From chemical analysis, the presence of ZnS and Zn(OH){sub 2} was identified and X-ray diffraction patterns exhibited a clear peak corresponding to ZnS hexagonal phase (1 0 3) plane, which was confirmed by electron diffraction patterns. From morphological studies, compact samples with well-defined particles, low roughness, homogeneous and pinhole-free in the surface were observed. From obtained results, it is evident that deposits of ZnS–CBD using a non-toxic solution are suitable as window layer for TFSC.

36 MATERIALS SCIENCE↗

Preparation and application of Mn-Doped Zn0.5Cd0.5S @ ZnS nanorods with high quantum yield as sensitive fluorescence probe for detection of glucose

Highlights: • Mn:ZCS@ZnS NRs are successfully synthesized by a facile thermal decomposition approach. • Mn:ZCS@ZnS NRs exhibit high photoluminescence with quantum yield reaching up to 85%. • Mn:ZCS@ZnS NRs with high quantum yield can be used as sensitive probe for glucose detection. - Abstract: Blood glucose level is a crucial clinical index of monitoring diabetes patients. Glucose sensors based on fluorescent quantum dots have received extensive attention. Herein, a highly photoluminescent Mn-doped Zn{sub 0.5}Cd{sub 0.5}S capped ZnS nanorods (Mn:ZCS@ZnS NRs) are successfully synthesized by a facile thermal decomposition approach. The maximum fluorescence quantum yield (QY) of as-prepared Mn:ZCS@ZnS NRs enable to reach 85% by optimizing Mn-doping level, temperature, time and ZnS coating. The results of probe experiments for glucose indicate that H{sub 2}O{sub 2} generated from the oxidation of glucose in presence of glucose oxidase (GOD) can lead to a pronounced decrease of fluorescence intensity of Mn:ZCS@ZnS NRs samples. Two distinct linear detections within the range from 50 μM to 300 μM and from 200 μM to 1000 μM are obtained and the limit of detection can reach to 100 nM. Preliminary study exhibits that Mn:ZCS@ZnS nanorods with high fluorescence quantum yield can be used as an efficient fluorescent probe for glucose detection.

60 APPLIED LIFE SCIENCES↗

Optimization of {sup 6}LiF:ZnS(Ag) Scintillator Light Yield Using Geant4

Neutrons provide an effective tool to probe materials structure. Neutron diffraction is a method to determine the atomic and magnetic structure of a material based on neutron scattering. By this method a collimated incident beam of thermal neutrons heat the examined sample and based on the obtained diffraction pattern information on the structure of the material is provided. Research for developing a novel cold neutron detector for Chromatic Analysis Neutron Diffractometer Or Reflectometer (CANDOR) is underway at the NIST center for neutron research. The system unique design is aimed to provide over ten times fold faster analysis of materials than conventional system. In order to achieve the fast analysis a large number of neutron detectors is required. A key design constraint for this detector is the thickness of the neutron sensitive element. This is met using {sup 6}LiF:ZnS(Ag) scintillation material with embedded wavelength shifting (WLS) fibers conducting scintillation light to silicon photomultiplier photo-sensors. The detector sensitivity is determined by both the neutron capture probability ({sup 6}Li density) and the detectable light output produced by the ZnS(Ag) ionization, the latter of which is hindered by the fluorescence absorption of the scintillation light by the ZnS. Tradeoffs between the neutron capture probability, stimulated light production and light attenuation for determining the optimal stoichiometry of the {sup 6}LiF and ZnS(Ag) as well as the volume ratio of scintillator and fiber. Simulations performed using the GEANT4 Monte Carlo package were made in order to optimize the detector design. GEANT4 enables the investigation of the neutron interaction with the detector, the ionization process and the light transfer process following the nuclear process. The series of conversions required for this detector were modelled: - A cold neutron enters the sensor and is captured by {sup 6}Li in the scintillator mixture ({sup 6}Li (n,α) {sup 3}H reaction). The study of investigating the capture process probability for neutron energy of 5.1 meV to 2.27 meV (4 - 6 A) is presented. - Alpha particles and tritons travel for a few microns in the scintillation material (α ∼0.007 mm, T ∼0.04 mm) losing energy and ionizing the ZnS. The mean free path of the two particles in each of the component materials and the complete compound was investigated. - The ionization of the ZnS(Ag) scintillation material produces blue light photons with luminescence wavelength of 450 nm. The amount of light output produced for different grain sizes of ZnS is discussed. - A large portion of the scintillation photons are reabsorbed during their passage through the scintillation material. - The blue photons that reach the WLS fibers are absorbed by fluorescent dye and are re-emitted as green photons, conducted by the fiber to the SiPM photo-sensor. This work presents the CANDOR unique design and its design constrains, the results measured by the ultra-thin {sup 6}LiF:ZnS(Ag)-based neutron detector versus the simulation results for several binder concentrations. The light measurement attenuation results along with the measured stopping power were utilized to predict the sensitivity results of configuration with different ZnS grain size, weight ratios and fibers geometry (number and location). The simulations enable to optimize the final sensor design. This design successfully achieved both the high gamma rejection with a sensitive and accurate neutron event detection of 80 percent. (authors)

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Field-assisted sintering and phase transition of ZnS-CaLa 2 S 4 composite ceramics

In the present study, zinc sulfide (ZnS) and calcium lanthanum sulfide (CaLa 2 S 4 , CLS) composite ceramics were consolidated via field-assisted sintering of 0.5ZnS-0.5CLS (volume ratio) composite powders at 800–1050 °C. Through sintering curve analyses and microstructural observations, it was determined that between 800 and 1000 °C, grain boundary diffusion was the main mechanism controlling grain growth for both the ZnS and CLS phases within the composite ceramics. The consolidated composite ceramics were determined to be composed of sphalerite ZnS, wurtzite ZnS and thorium phosphate CLS. The sphalerite-wurtzite phase transition of ZnS was further demonstrated to be accompanied by the formation of stacking faults and twins in the ceramics. Furthermore, it was also found that the addition of the CLS phase improved the indentation hardness of the ceramics relative to pure ZnS by homogeneous dispersion of ZnS and CLS small grains.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Benchmark Analysis on Magnetic and Photoluminescence Properties of Selective Metal Ions Doped ZnS Nanoparticles

The creation of diluted magnetic semiconductors (DMSs) at lower dimensions that exhibit room temperature ferromagnetism (RTFM) has been given immense significance for the fabrication of a new class of spintronic devices through utilizing spin degrees of freedom besides charge nature of electrons. In this view, nanocrystals of ZnS doped with 4% concentration of Fe, Co, Ni, Cr, Mn, Sr, Cu, and Ce have been synthesized at room temperature (RT) by chemical co-precipitation method. The samples were examined by various characterization techniques like energy dispersive spectroscopy (EDS), X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), vibrating sample magnetometer (VSM), and photoluminescence (PL). EDS spectra revealed the existence of parent elements in the prepared samples. XRD characterization disclosed hexagonal structures of nanocrystals, and no secondary phases were observed in all the samples except for Cu and Ni doped ZnS. FTIR data confirmed the proper substitution of dopants in the host lattice as all the graphs have almost same stretchings. The magnetic nature of each sample was evaluated from M-H graphs of VSM, and it corroborated the transition of magnetic properties due to doping. Pristine ZnS showed diamagnetic nature, while Fe and Sr doped ZnS evinced strong ferromagnetic and anti-ferromagnetic properties, respectively. Photoluminescence studies on Ce, Sr and Mn doped ZnS samples revealed strong emission peaks with enhanced luminescence properties compared to bare ZnS. Cu, Cr and Mn doped ZnS exhibited a red shift in emission wavelengths, whereas Co doped ZnS showed emission peak shifted towards the blue region as compared to the host lattice.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of Reaction Parameters on Morphology and Photoluminescence of Intrinsic and Mn-doped ZnS Microspheres Synthesized by Hydrothermal Method

Intrinsic and Manganese (Mn)-doped ZnS microspheres have been synthesized by hydrothermal method. Thiourea and amino acid, and L-histidine have been used as sulfur source and capping agent, respectively. The synthesized materials have been characterized using x-ray diffraction, field emission scanning electron microscopy, photoluminescence (PL) and UV–Vis spectroscopy. The above-said characterizations conveyed the information regarding the crystallinity, existence of microspheres, size and optical properties of synthesized ZnS and Mn-doped ZnS samples. Formation of microspheres of intrinsic and Mn-doped ZnS has been observed when the reaction parameters are kept at 150 °C for 4 h, and similarly, the micropores have been noticed when reaction parameters are kept at 150 °C for 8 h. The PL of ZnS microspheres shows multiple defect emissions. The nature of PL for pure ZnS has been regulated based on reaction parameters. Doping of Mn in the ZnS enhances the PL emission. This study reveals the role of reaction parameters and effect of Mn doping on tuning the morphology and emission behavior of ZnS microspheres.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Phase transformation and optical properties of Cu-doped ZnS nanorods

ZnS nanorods doped with 0-15 mol% of Cu have been prepared by simple solvothermal process. With gradual increase in the Cu concentration, phase transformation of the doped ZnS nanorods from wurtzite to cubic was observed. Twins and stacking faults were developed due to atomic rearrangement in the heavily doped ZnS nanorods during phase transformation. UV-vis-NIR absorbance spectroscopy ruled out the presence of any impure Cu-S phase. The doped ZnS nanorods showed luminescence over a wide range from UV to near IR with peaks at 370, 492-498, 565 and 730 nm. The UV region peak is due to the near-band-edge transition, whereas, the green peak can be related to emission from elementary sulfur species on the surfaces of the nanorods. The orange emission at 565 nm may be linked to the recombination of electrons at deep defect levels and the Cu(t{sub 2}) states present near the valence band of ZnS. The near IR emission possibly originated from transitions due to deep-level defects. - Graphical abstract: ZnS nanorods doped with 0-15 mol% of Cu has been prepared by simple solvothermal route. Interestingly, phase transformation of the doped ZnS nanorods from wurtzite to cubic was observed with gradual increase in the Cu concentration. Doped ZnS nanorods showed luminescence over a wide range from UV to near IR, which is also a rare observation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synthesis and different property of yttrium doped ZnS nanoparticles

Yttrium doped ZnS samples Zn{sub 1-x}Y{sub x}S with nominal compositions (x = 0.00, 0.04 and 0.06) were synthesized by a chemical co - precipitation route at room temperature. The synthesized Zn{sub 1-x}Y{sub x}S nanoparticles were characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR) and UV–VIS spectrometer. XRD patterns revealed that entire peaks corresponding to the various planes of cubic zinc blend structure with no segregation of Y. The lattice parameters were calculated for the Y doped ZnS using XRD data and it found to be slightly smaller than pure ZnS, which indicate substitution of Y in to ZnS lattice. The average crystallite size was calculated using Debye - Scherrer’s formula for pure and Y doped ZnS samples. It is observed that grain size is in the range 30 to 12 nm. Band gap of Y doped ZnS nanoparticles has been calculated using UV-Vis spectrometer. It is found that the band gap decreases as content of Y increases, It may be due the smaller average grain size or ionic radii. The functional groups and chemical interactions of Y substituted Zinc sulfide samples were detected peaks using FTIR spectra and observed the presence of functional groups in the samples. It outlines the formation of ZnS with the stretching vibrational mode around at 511 cm{sup −1}. It is evidently confirmed from FTIR spectra that yttrium substitutes into ZnS lattice.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Density Functional Theory Study on Electronic Structures and Magnetism for Nitrogen-Doped ZnS

Using the full-potential linearized augmented plane wave method, together with the generalized gradient approximation and modified Becke-Johnson as correlation potential, the electronic structures and magnetism for nitrogen-doped ZnS are investigated. Based on the generalized gradient approximation, calculations show nitrogen-substituting sulfur (N{sub S}) would induce the ZnS to be paramagnetic metal. As the band gap increasing to the experimental results (obtained by the modified Becke-Johnson potential), the N{sub S} defects would induce the ZnS to be a ferromagnetic metal. The total magnetic moment for ZnS supercell with single N{sub S} defect is 0.85 μ{sub B}. Positive chemical pair interactions imply that N{sub S} defects would form homogeneous distribution in ZnS host. Sulfur vacancies would give rise to the ZnS with N{sub S} defects system losing the magnetism. Moderate formation energy (0.71 eV) indicates ZnS with N{sub S} defects could be fabricated experimentally.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Highly-defective nanocrystals of ZnS formed via dissimilatory bacterial sulfate reduction: A comparative study with their abiogenic analogues

The physicochemical properties of a (nano)mineral are strongly affected by its formation processes, and thus, may indicate the (nano)mineral’s formation environment and mechanism. This correlation, although relevant to a myriad of geological, environmental, and material-science processes, has not yet been fully appreciated and systematically explored. In this study, using the Zn–S system, we demonstrate that biological and abiotic processes at similar experimental conditions can produce distinctive particle size, morphology, and crystal structure in the formed ZnS. Specifically, bacterial sulfate reduction led to the formation of highly-defective nanocrystals of mixed sphalerite and wurtzite in a range of ~4–12 nm. By comparison, the abiotic procedures of titration- or diffusion-controlled precipitation resulted in the formation of polycrystalline aggregates that contained randomly-oriented, ultrafine crystals below ~2–3 nm. The poor crystallinity in the abiogenic samples, regardless of the sulfide addition rates, reveals an overall nucleation-dominated, crystal growth-restricted pathway for the formation of ZnS from low-temperature aqueous solutions. The difficulty in the ZnS crystallization likely stems from the intrinsic surface instability of the ZnS growth units (i.e., in the form of nanoclusters) resulting from the dipole–dipole interactions of the unit with surrounding water molecules. In the biogenic samples, the ZnS crystallinity was significantly improved, indicating that the presence of bacterial metabolites somehow promoted the crystallization process. With evidence for the enlarged {1 1 1} planes in the biogenic nanocrystals, we attribute this enhancement mainly to the selective interaction of the bacterial metabolites with polar faces of the ZnS growth units, which might have effectively screened the dipole moments in the growth units and enabled their crystallographic assembly. By revealing the intrinsic difficulty and specific pathways for the ZnS crystallization, we also present viable explanations for the exclusive occurrence of structural defects in {1 1 1} planes of the biogenic nanocrystals. The findings of our study provide insight into the origin and fate of metal sulfide nanoparticles in the environment, and have implications for biomineralization, bioremediation of metal-contaminated sites, and bacterial production of functional nanomaterials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Infrared, visible and ultraviolet absorptions of transition metal doped ZnS crystals with spin-polarized bands

The formation energies, electronic structures and optical properties of TM:ZnS systems (TM=Cr{sup 2+}, Mn{sup 2+}, Fe{sup 2+}, Co{sup 2+} and Ni{sup 2+}) are investigated by using the first principles method. It is found that the wurtzite and zinc-blende structures have about the same stability, and thus can coexist in the TM:ZnS system. From the wurtzite TM:ZnS, especially, a partially filled intermediate band (IB) is obtained at TM=Cr{sup 2+}, Ni{sup 2+} and Fe{sup 2+}, while it is absent at TM=Mn{sup 2+} and Co{sup 2+}. The additional absorptions are obtained in infrared, visible and ultraviolet (UV) regions, due to the completely spin-polarized IB at Fermi level. The results are very helpful for both the designs and applications of TM:ZnS opto-electronics devices, such as solar-cell prototype. -- Graphical abstract: Absorption coefficients of w-TM{sub x}Zn{sub 1-x}S crystals (TM=Cr{sup 2+}, Mn{sup 2+}, Fe{sup 2+}, Co{sup 2+} and Ni{sup 2+}) at x=0.028. The results may be helpful for the design and applications of TM:ZnS devices, especially for the new high efficiency solar-cell prototype, UV detector and UV LEDs. Display Omitted Research highlights: > It is found that the wurtzite and zinc-blende structures can coexist in TM:ZnS. > An intermediate band is obtained in TM:ZnS at TM=Cr{sup 2+}, Ni{sup 2+} and Fe{sup 2+}. > The absorption coefficients are obtained in infrared, visible and ultraviolet regions.