Search NASA⌕ Search

SEARCH · Search NASA

Results for “acrylic plastics”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

34 records · Page 2

Spacecraft Lighting to Mitigate Microbial Growth

In this innovation project, we investigated the usage of narrow band violet light (408 nm) to attenuate the growth of bacteria typically found on ISS. Violet light is less hazardous than UV light and it can transmit through plastics, such as clear acrylics, making it possible to incorporate into large surface lamps and acrylic or polycarbonate based optical light guides. This study built a custom LED surface panel that was edge lit by an array of 408 nm violet LEDS. The optical light guide technology used in the lamp and the 408 nm violet LEDs are available on the market from multiple vendors. The application of the concept of using violet light driven LED panels and optical light guides is to integrate the paneling into spacecraft architectural surfaces for the automation of a light based microbial countermeasure that could enhance current cleaning methods used in areas on spacecraft prone to microbial growth.

Clark, Toni A.↗

Metabolic Cages for a Space Flight Model in the Rat

A variety of space flight models are available to mimic the physiologic changes seen in the rat during weightlessness. The model reported by Wronski and Morey-Holton has been widely used by many investigators, in musculoskeletal physiologic studies especially, resulting in accumulation of an extensive database that enables scientists to mimic space flight effects in the 1-g environment of Earth. However, information on nutrition or gastrointestinal and renal function in this space flight model is limited by the difficulty in acquiring uncontaminated metabolic specimens for analysis. In the Holton system, a traction tape harness is applied to the tail, and the rat's hindquarters are elevated by attaching the harness to a pulley system. Weight-bearing hind limbs are unloaded, and there is a headward fluid shift. The tail-suspended rats are able to move freely about their cages on their forelimbs and tolerate this procedure with minimal signs of stress. The cage used in Holton's model is basically a clear acrylic box set on a plastic grid floor with the pulley and tail harness system attached to the open top of the cage. Food is available from a square food cup recessed into a corner of the floor. In this system, urine, feces, and spilled food fall through the grid floor onto absorbent paper beneath the cage and cannot be separated and recovered quantitatively for analysis in metabolic balance studies. Commercially available metabolic cages are generally cylindrical and have been used with a centrally located suspension apparatus in other space flight models. The large living area, three times as large as most metabolic cages, and the free range of motion unique to Holton's model, essential for musculoskeletal investigations, were sacrificed. Holton's cages can accommodate animals ranging in weight from 70 to 600 g. Although an alternative construction of Holton's cage has been reported, it does not permit collection of separate urine and fecal samples. We describe the modifications to Holton's food delivery system, cage base, and the addition of a separator system for the collection of urine and fecal samples for metabolic and nutrition studies in the tail suspension model.

Harper, Jennifer S.↗

A Study of Transparent Plastics for use on Aircraft. Supplement

This supplement to a NACA study issued in May 1937 entitled "A Study of Transparent Plastics for Use on Aircraft", contains two tables. These tables contain data on bursting strengths of plastics, particularly at low temperatures. Table 1 contains the values reported in a table of the original memorandum, and additional values obtained at approximately 25 C, for three samples of Acrylate resin. The second table contains data obtained for the bursting strength when one surface of the plastic was cooled to approximately -35 C.

Axilrod, Benjamin M.↗

Optical Property Requirements for Glasses, Ceramics and Plastics in Spacecraft Window Systems

This is a preliminary draft of a standard published by the National Aeronautics and Space Administration (NASA) Johnson Space Center (JSC) that is intended to provide uniform window optical design requirements in support of the development of human-rated spaceflight hardware. The material covered in this standard is based on data from extensive testing by the Advanced Sensing and Optical Measurement Branch at NASA Langley Research Center, and compiled into requirements format by the NASA JSC Structural Engineering Division. At the time of this initial document release, a broader technical community has not reviewed this standard. The technical content of this standard is primarily based on the Constellation Program Orion Crew Exploration Vehicle Window Optical Properties Requirements, CxP 72407, Baseline. Unlike other optical requirements documents available for human rated spacecraft, this document includes requirements that ensure functionality for windows that contain glass/ceramic and/or plastic window substrate materials. These requirements were derived by measuring the optical properties of fused silica and aluminosilicate glass window assemblies and ensuring that the performance of any window assembly that includes a plastic pane or panes will meet the performance level of the all-glass assemblies. The resulting requirements are based upon the performance and parameter metrology testing of a variety of materials, including glass, transparent ceramics, acrylics, and polycarbonates. In general, these requirements are minimum specifications for each optical parameter in order to achieve the function specified for each functional category, A through D. Because acrylic materials perform at a higher level than polycarbonates in the optics regime, and CxP/Orion is planning to use acrylic in the Orion spacecraft, these requirements are based heavily on metrology from that material. As a result, two of the current Category D requirements for plastics are cited in such a way that will result in the screening out of polycarbonates. It is acknowledged that many polycarbonates can perform the functions of Category D, such as piloting and imagery with lens with apertures up to 25mm, without performance issues. Therefore, this forward warns users that certain requirements, such as birefringence and wavefront, for Category D plastics need to be revised to allow those polycarbonates that perform adequately in Category D to be accepted, while at the same time, screen out those materials that do not perform up to par. At the time of document release, the requirements in question have been identified by a TBD beside the proposed requirement criteria (which is based upon acrylic performance). Vehicles that are designed with acrylic materials for windowpanes are encouraged to use the values presented in this document for all requirements, in order to ensure adequate optical performance.

Lynda R Estes↗

Scribable coating for plastic films

Scribable opaque coating for transparent plastic film tape is not affected by aging, vacuum, and moderate temperature extremes. It consists of titanium dioxide, a water-compatible acrylic polymer emulsion, and a detergent. The coating mixture is readily dispersed in water before it is dried.

Clark, R. T.↗

Immunohistochemical myofiber typing and high-resolution myofibrillar lesion detection in LR white embedded muscle

We have developed a method of fixing, embedding, sectioning, and staining that allows high-resolution detection of myofibrillar structure and myosin immunocytochemical muscle fiber typing in serial semithin sections of LR White plastic embedded muscle at the light microscopic level. Traditional approaches, such as cryostat sections, permit fiber typing, but small myofibrillar lesions (1-3 sarcomeres) are difficult to detect because of section thickness. Semithin sections of hydrophobic resins do not stain well either histochemically or immunocytochemically. Electron microscopy can resolve lesions and discriminate fiber types based on morphology, but the sampling area is small. Our goal was to develop a rapid method for defining both fiber type and high-resolution primary myofibrillar lesion damage. Mild fixation (1-4% paraformaldehyde, 0. 05-0.1% glutaraldehyde) and embedment in a hydrophilic resin (LR White) were used. Myofibrillar structure was extremely well preserved at the light microscopic (LM) level, and lesions could be readily resolved in Toluidine blue stained 500-nm sections. Fiber type was defined by LM immunomyosin staining of serial plastic semithin sections, which demonstrated reciprocal staining patterns for "fast (Sigma M4276) and "total" (skeletal muscle) myosins (Sigma M7523). Copyright 2000 Wiley-Liss, Inc.

NASA Program Fundamental Space Biology↗

Ultrasonic Assessment of Impact-Induced Damage and Microcracking in Polymer Matrix Composites

The main objective of this NASA FAR project is to conduct ultrasonic assessment of impact-induced damage and microcracking in polymer matrix composites at various temperatures. It is believed that the proposed study of impact damage assessment on polymer matrix composites will benefit several NASA missions and current interests, such as ballistic impact testing of composite fan containment and high strain rate deformation modeling of polymer matrix composites. Impact-induced damage mechanisms in GLARE and ARALL fiber-metal laminates subject to instrumented drop-weight impacts at various temperatures were studied. GLARE and ARALL are hybrid composites made of alternating layers of aluminum and glass (for GLARE) and aramid- (for ARALL) fiber-reinforced epoxy. Damage in pure aluminum panels impacted by foreign objects was mainly characterized by large plastic deformation surrounding a deep penetration dent. On the other hand, plastic deformation in fiber-metal laminates was often not as severe although the penetration dent was still produced. The more stiff fiber-reinforced epoxy layers provided better bending rigidity; thus, enhancing impact damage tolerance. Severe cracking, however, occurred due to the use of these more brittle fiber-reinforced epoxy layers. Fracture patterns, e.g., crack length and delamination size, were greatly affected by the lay-up configuration rather than by the number of layers, which implies that thickness effect was not significant for the panels tested in this study. Immersion ultrasound techniques were then used to assess damages generated by instrumented drop-weight impacts onto these fiber-metal laminate panels as well as 6061-T6 aluminum/cast acrylic sandwich plates adhered by epoxy. Depending on several parameters, such as impact velocity, mass, temperature, laminate configuration, sandwich construction, etc., various types of impact damage were observed, including plastic deformation, radiating cracks emanating from the impact site, ring cracks surrounding the impact site, partial and full delamination, and combinations of these damages.

Liaw, Benjamin↗

Ultrasonic Assessment of Impact-Induced Damage and Microcracking in Polymer Matrix Composites

The main objective of this NASA Faculty Awards for Research (FAR) project is to conduct ultrasonic assessment of impact-induced damage and microcracking in fiber-metal laminated (FML) composites at various temperatures. It is believed that the proposed study of impact damage assessment on FML composites will benefit several NASA's missions and current interests, such as ballistic impact testing of composite fan containment and high strain rate deformation modeling of polymer matrix composites. Impact-induced damage mechanisms in GLARE and ARALL fiber-metal laminates subject to instrumented drop-weight impacts at various temperatures were studied. GLARE and ARALL are hybrid composites made of alternating layers of aluminum and glass- (for GLARE) and aramid- (for ARALL) fiber reinforced epoxy. Damage in pure aluminum panels impacted by foreign objects was mainly characterized by large plastic deformation surrounding a deep penetration dent. On the other hand, plastic deformation in fiber-metal laminates was often not as severe although the penetration dent was still produced. The more stiff fiber-reinforced epoxy layers provided better bending rigidity; thus, enhancing impact damage tolerance. Severe cracking, however, occurred due to the use of these more brittle fiber-reinforced epoxy layers. Fracture patterns, e.g., crack length and delamination size, were greatly affected by the lay-up configuration rather than by the number of layers, which implies that thickness effect was not significant for the panels tested in this study. Immersion ultrasound techniques were then used to assess damages generated by instrumented drop-weight impacts onto these fiber-metal laminate panels as well as 2024-T3 aluminum/cast acrylic sandwich plates adhered by epoxy. Depending on several parameters, such as impact velocity, mass, temperature, laminate configuration, sandwich construction, etc., various types of impact damage were observed, including plastic deformation, radiating cracks emanating from the impact site, ring cracks surrounding the impact site, partial and full delamination, and combinations of these damages.

Gyekanyesi, John↗

Ultrasonic Assessment of Impact-Induced Damage and Microcracking in Polymer Matrix Composites

The main objective of this NASA FAR project is to conduct ultrasonic assessment of impact-induced damage and microcracking in polymer matrix composites at various temperatures. It is believed that the proposed study of impact damage assessment on polymer matrix composites will benefit several NASA's missions and current interests, such as ballistic impact testing of composite fan containment and high strain rate deformation modeling of polymer matrix composites. Currently, impact-induced delamination and fracture in 6061-T6 aluminum/cast acrylic sandwich plates adhered by epoxy were generated in an instrumented drop-weight impact machine. Although only a small dent was produced on the aluminum side when a hemispherical penetrator tup was dropped onto it from a couple of inches, a large ring of delamination at the interface was observed. The delamination damage was often accompanied by severe shattering in the acrylic substratum. Damage patterns in the acrylic layer include radial and ring cracks and, together with delamination at the interface, may cause peeling-off of acrylic material from the sandwich plate. Theory of stress-wave propagation can be used to explain these damage patterns. The impact tests were conducted at various temperatures. The results also show clearly that temperature effect is very important in impact damage. For pure cast acrylic nil-ductile transition (NDT) occurs between 185-195 F Excessive impact energy was dissipated into fracture energy when tested at temperature below this range or through plastic deformation when tested at temperature above the NDT temperature. Results from this study will be used as baseline data for studying fiber-metal laminates, such as GLARE and ARALL for advanced aeronautical and astronautical applications.

Liaw, Benjamin↗

Impact Delamination and Fracture in Aluminum/Acrylic Sandwich Plates

Impact-induced delamination and fracture in 6061-T6 aluminum/cast acrylic sandwich plates adhered by epoxy were generated in an instrumented drop-weight impact machine. Although only a small dent was produced on the aluminum side when a hemispherical penetrator tup was dropped onto it from a couple of inches, a large ring of delamination at the interface was observed. The delamination damage was often accompanied by severe shattering in the acrylic substratum. Damage patterns in the acrylic layer include radial and ring cracks and, together with delamination at the interface, may cause peeling-off of acrylic material from the sandwich plate. Theory of stress-wave propagation can be used to explain these damage patterns. The impact tests were conducted at various temperatures. The results also show clearly that temperature effect is very important in impact damage. For pure cast acrylic nil-ductile transition (NDT) occurs between 185-195 F. Excessive impact energy was dissipated into fracture energy when tested at temperature below this range or through plastic deformation when tested at temperature above the NDT temperature. Results from this study will be used as baseline data for studying fiber-metal laminates, such as GLARE and ARALL for advanced aeronautical and astronautical applications.

Liaw, Benjamin↗

Clear Film Protects Against Ultraviolet Radiation

Acrylic film contains screeing agent filtering ultraviolet radiation up to 380 nanometers in wavelength but passes other components of Sunlight. Film used to protect such materials as rubber and plastics degraded by ultraviolet light. Used as protective cover on outdoor sheets or pipes made of such materials as polyethylene or polypropylene and on solar cells.

Gupta, A.↗

Modelling of polymer photodegradation for solar cell modules

A computer model including an integration routine was developed and demonstrated to simulate, in principle, the chemical changes which may occur in the photooxidation of hydrocarbons, using as input data a set of elementary reactions, corresponding rate constants and appropriate starting conditions. Application of this model to the photooxidation of pottant and plastic materials used in the LSA module designs provides a reliable predictive capability regarding the useful lifetime of these materials. An earlier mechanism consisting of 46 reactions was simplified considerably by reducing the number of formal termination steps since it became apparent that the major termination process goes via the peroxy radicals. In addition, new reactions of oxygen with acryl radicals (from Norrish type I) to form peracids, which then decompose to form carbon dioxide are included.

Somersall, A. C.↗

Real time outdoor exposure testing of solar cell modules and component materials

Plastic samples, solar cell modules, and sub-modules were exposed at test sites in Florida, Arizona, Puerto Rico, and Cleveland, Ohio, in order to determine materials suitable for use in solar cell modules with a proposed 20-year lifetime. Various environments were encountered including subtropical, subtropical with a sea air atmosphere, desert, rain forest, normal urban, and urban-polluted. The samples were exposed for periods up to six months. Materials found not suitable were polyurethane, polyester, Kapton, Mylar, and UV-stabilized Lexan. Suitable materials were acrylic, FEP-A, and glass. The results of exposure of polyvinylidene fluoride were dependent on the specific formulation, but several types appear suitable. RTV silicone rubber (clear) appears to pick up and hold dirt both as a free film and as a potting medium for modules. The results indicate that dirt accumulation and cleanability are important factors in the selection of solar cell module covers and encapsulants.

Anagnostou, E.↗

Preliminary results of accelerated exposure testing of solar cell system components

Plastic samples and solar cell sub modules were exposed to an accelerated outdoor environment in Arizona and an accelerated simulated environment in a cyclic ultraviolet exposure tester which included humidity exposure. These tests were for preliminary screening of materials suitable for use in the manufacture of solar cell modules which are to have a 20-year lifetime. The samples were exposed for various times up to six months, equivalent to a real time exposure of four years. Suitable materials were found to be FEP-A, FEP-C, PFA, acrylic, silicone compounds and adhesives and possibly parylene. The method of packaging the sub modules was also found to be important to their performance.

Anagnostou, E.↗

Development of Craze and Impact Resistance in Glazing Plastics by Multiaxial Stretching

The loss of strength of cast polymethyl methacrylate plastic as a result of crazing is of considerable importance to the aircraft industry. Because of the critical need for basic information on the nature of crazing and the effects of various treatments and environmental conditions on its incidence and magnitude, an investigation of this phenomenon was undertaken. The following factors were examined: (1) the effect of stress-solvent crazing on tensile strength of polymethyl methacrylate; (2) the critical stress and strain for onset of crazing at various temperatures; (3) the effect of molecular weight on crazing; and (4) the effect of multiaxial stretching on crazing of polymethyl methacrylate and other acrylic glazing materials.

Kline, G M↗

Water permeation and electrical properties of pottants, backings, and pottant/backing composites

It is reported that the interface between plastic film back covers and ethylene vinyl acetates (EVA) or polyvinyl butyral (PVB) in photovoltaic modules can influence water permeation, and electrial properties of the composites such as leakage current and dielectric constant. The interface can either be one of two dissimilar materials in physical contact with no intermixing, or the interface can constitute a thin zone which is an interphase of the two materials having a gradient composition from one material to the other. The former condition is described as a discrete interface. A discrete interface model was developed to predict water permeation, dielectric strength, and leakage current for EVA, ethylene methyl acrylate (EMA), and PVB coupled to Tedlar and mylar films. Experimental data was compared with predicted data.

Orehotsky, J.↗