Search NASA⌕ Search

SEARCH · Search NASA

Results for “aluminide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Titanium Aluminide Applications in the High Speed Civil Transport

It is projected that within the next two decades, overseas air travel will increase to over 600,000 passengers per day. The High Speed Civil Transport (HSCT) is a second-generation supersonic commercial aircraft proposed to meet this demand. The expected fleet of 500 to 1500 aircraft is required to meet EPA environmental goals; the HSCT propulsion system requires advanced technologies to reduce exhaust and noise pollution. A part of the resultant strategy for noise attenuation is the use of an extremely large exhaust nozzle. In the nozzle, several critical components are fabricated from titanium aluminide: the divergent nap uses wrought gamma; the nozzle sidewall is a hybrid fabrication of both wrought gamma face sheet and cast gamma substructure. This paper describes the HSCT program and the use of titanium aluminide for its components.

Bartolotta, Paul A.↗

Effect of Hf Additions to Pt Aluminide Bond Coats on EB-PVD TBC Life

Small Hf additions were incorporated into a Pt aluminide coating during chemical vapor deposition (CVD) on single crystal RENE N5 substrates. Standard yttria-stabilized zirconia top coats were subsequently deposited onto the coated substrates by electron beam-physical vapor deposition (EB-PVD). The coated substrates underwent accelerated thermal cycle testing in a furnace at a temperature in excess of 1121 C (2050 F) (45 minute hot exposure, 15 minute cool to approximately 121 C (250 F)) until the thermal barrier coating (TBC) failed by spallation. Incorporating Hf in the bond coat increased the TBC life by slightly more than three times that of a baseline coating without added Hf. Scanning electron microscopy of the spalled surfaces indicated that the presence of the Hf increased the adherence of the thermally grown alumina to the Pt aluminide bond coat. The presence of oxide pegs growing into the coating from the thermally grown alumina may also partially account for the improved TBC life by creating a near-surface layer with a graded coefficient of thermal expansion.

Nesbitt, James↗

Evaluation of a Gamma Titanium Aluminide for Hypersonic Structural Applications

Titanium matrix composites (TMCs) have been extensively evaluated for their potential to replace conventional superalloys in high temperature structural applications, with significant weight-savings while maintaining comparable mechanical properties. New gamma titanium aluminide alloys and an appropriate fiber could offer an improved TMC for use in intermediate temperature applications (400-800 C). The purpose of this investigation is the evaluation of a gamma titanium aluminide alloy with nominal composition Ti-46.5Al-4(Cr,Nb,Ta,B)at.% as a structural material in future aerospace transportation systems, where very light-weight structures are necessary to meet the goals of advanced aerospace programs.

Johnson, W. Steven↗

Environmental Studies on Titanium Aluminide Alloys

Titanium aluminides are attractive alternatives to superalloys in moderate temperature applications (600 to 850 C) by virtue of their high strength-to-density ratio (high specific strength). These alloys are also more ductile than competing intermetallic systems. However, most Ti-based alloys tend to degrade through interstitial embrittlement and rapid oxidation during exposure to elevated temperatures. Therefore, their environmental behavior must be thoroughly investigated before they can be developed further. The goals of titanium aluminide environmental studies at the NASA Lewis Research Center are twofold: characterize the degradation mechanisms for advanced structural alloys and determine what means are available to minimize degradation. The studies to date have covered the alpha 2 (Ti3Al), orthorhombic (Ti2AlNb), and gamma (TiAl) classes of alloys.

Brindley, William J.↗

Very Long Term Oxidation of Titanium Aluminides Investigated

Titanium aluminides (TiAl) are of great interest for intermediate-temperature (600 to 850 C) aerospace and power-generation applications because they offer significant weight savings over today's nickel alloys. TiAl alloys are being investigated for low-pressure turbine blade applications, exhaust nozzle components, and compressor cases in advanced subsonic and supersonic engines. Significant progress has been made in understanding the fundamental aspects of the oxidation behavior of binary TiAl alloys. However, most of this work has concentrated on short term (<1000 hr), high-temperature (900 to 1000 C) exposures. Also, there is not much data available in the literature regarding the oxidation behavior of the quaternary and higher order engineering alloys. This is especially true for the very long term, low-temperature conditions likely to be experienced during aerospace applications. An investigation at the NASA Glenn Research Center at Lewis Field was undertaken to characterize the long-term oxidation behavior of various model and advanced titanium aluminides for periods up to 7000 hr at 704 C in air using a high-resolution field emission scanning electron microscope. Also, a unique surface treatment technique developed to improve the oxidation resistance of TiAl was evaluated. The alloys included in this investigation are listed in the table. The table also shows typical alloy compositions and the specific weight changes and scale thickness measured for each alloy after exposure to 700 C for 7000 hr in air.

Locci, Ivan E.↗

Dynamic Fracture Initiation Toughness at Elevated Temperatures With Application to the New Generation of Titanium Aluminide Alloys

Recently, a new generation of titanium aluminide alloy, named Gamma-Met PX, has been developed with better rolling and post-rolling characteristics. I'revious work on this alloy has shown the material to have higher strengths at room and elevated temperatures when compared with other gamma titanium aluminides. In particular, this new alloy has shown increased ductility at elevated temperatures under both quasi-static and high strain rate uniaxial compressive loading. However, its high strain rate tensile ductility at room and elevated temperatures is limited to approx. 1%. In the present chapter, results of a study to investigate the effects of loading rate and test temperature on the dynamic fracture initiation toughness in Gamma-Met PX are presented. Modified split Hopkinson pressure bar was used along with high-speed photography to determine the crack initiation time. Three-point bend dynamic fracture experiments were conducted at impact speeds of approx. 1 m/s and tests temperatures of up-to 1200 C. The results show that thc dynamic fracture initiation toughness decreases with increasing test temperatures beyond 600 C. Furthermore, thc effect of long time high temperature air exposure on the fracture toughness was investigated. The dynamic fracture initiation toughness was found to decrease with increasing exposure time. The reasons behind this drop are analyzed and discussed.

Shazly, Mostafa↗

Welding of gamma titanium aluminide alloys

An article made of a gamma titanium aluminide alloy is welded, as for example in the weld repair of surface cracks, by removing foreign matter from the area to be welded, first stress relieving the article, cooling the entire article to a welding temperature of from about 1000.degree. F. to about 1400.degree. F., welding a preselected region in an inert atmosphere at the welding temperature, and second stress relieving the article. Welding is preferably accomplished by striking an arc in the preselected region so as to locally melt the alloy in the preselected region, providing a filler metal having the same composition as the gamma titanium aluminide alloy of the article, and feeding the filler metal into the arc so that the filler metal is melted and fused with the article to form a weldment upon solidification.

Smashey, Russell W.↗

Enriched aluminide coatings for dispersion strengthened nickel materials

Improved aluminide/barrier coating combinations for dispersion strengthened nickel materials were investigated. The barrier materials involved alloys with refractory metal content to limit interdiffusion between the coating and the substrate, thereby minimizing void formation. Improved aluminide coatings involved the dispersion of aluminum-rich compounds. Coatings were tested in argon at 1533 K (2300 F) for 100 hours and in cyclic oxidation at 1422 K (2100 F). Two coatings on TDNiCr completed 300 hours of oxidation testing, none on TDNi. Selected coating combinations were evaluated in Mach 1 burner rig testing using JP-4 fuel and air at 1422 K (2100 F) and 1477 K (2200 F) for 350 and 100 hours, respectively. Static oxidation in 1-hour cycles was conducted at 1533 K (2300 F) for 100 hours. For comparison purposes a physical vapor deposition (PVD) NiCrAlY coating was tested concurrently. Only the NiCrA1Y coating survived the 1477 K (2200 F)/100-hour burner rig test and 275 hours of the 350-hour 1422 K (2100 F) test. Elevated temperature exposure reduced room temperature tensile properties but had little effect on elevated temperature properties.

Levinstein, M. A.↗

Thermodynamics and kinetics of pack aluminide coating formation on IN-100

An investigation of the effects of pack variables on the formation of aluminide coatings on nickel-base superalloy IN-100 was conducted. Also, the thermodynamics and kinetics of coating formation were analyzed. Observed coating weights were in good agreement with predictions made from the analysis. Pack temperature rather than pack aluminum activity controls the principal coating phase formed. In 1 weight percent aluminum packs, aluminum weight gains were related to the halide pack activator. Solid-state nickel diffusion controlled coating formation from sodium fluoride and chloride and ammonium fluoride activated packs. In other ammonium and sodium halide activated 1 weight percent aluminum packs, gaseous diffusion controlled coating formation.

Levine, S. R.↗