Novel Corrosion and Erosion Protective Amorphous Alloys Coatings
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Amorphous iron and titanium-based alloys containing various amounts of chromium, phosphorus, and boron exhibit high corrosion resistance. Some physical properties of Fe and Ti-based metallic alloy films deposited on a glass substrate by a dc-magnetron sputtering technique are reported. The films were characterized using differential scanning calorimetry, stress analysis, SEM, XRD, SIMS, electron microprobe, and potentiodynamic polarization techniques.
Recently, solid-state amorphization through temperature-induced martensitic transition has been reported. The stability of the amorphous martensite phase, which co-exists with a crystalline counterpart, is intriguing but remains ill-defined. In this work, we studied the structural stability of a Ti 59.1 Zr 37 Cu 2.3 Fe 1.6 amorphous martensite alloy by combining in situ high-pressure synchrotron x-ray diffraction with ex situ transmission electron microscopy. During compression at room temperature, an irreversible pressure-induced crystallization of the amorphous martensite phase into a β-Ti phase is revealed. Qualitative analysis reveals the important role of the local atomic strain in stabilizing/destabilizing amorphous martensite alloys and its high tunability of the local atomic strain under high pressure.
Amorphous complexions in nanocrystalline metals have the potential to improve mechanical properties and radiation tolerance, as well as resistance to grain growth. In this study, the stability of amorphous complexions in binary and ternary Cu-based alloys is investigated by observing the effect of cooling rate from high temperature on the occurrence of amorphous-to-ordered complexion transitions. Bulk Cu-Zr and Cu-Zr-Hf alloy samples were annealed to induce boundary premelting and then quenched through a procedure that induces a gradient of local cooling rate through the sample height. Amorphous complexion thickness distributions were found to be invariant to local cooling rate in the Cu-Zr-Hf alloy, demonstrating enhanced stability of the amorphous complexion structure compared to the Cu-Zr alloy, which had thinner amorphous complexions in the regions that were slowly cooled. The experimental results are used to construct time-temperature-transformation diagrams for the amorphous-to-ordered complexion transition in both the binary and ternary alloys, enabling a deeper understanding of the influence of cooling rate and grain boundary chemistry on complexion transitions. In conclusion, the critical cooling rate necessary to avoid complexion transitions in the ternary alloy is found to be at least three orders of magnitude slower than that for the binary alloy.
The radiation resistance of commercial solar cells fabricated from hydrogenated amorphous silicon alloys is reported. A number of different device structures were irradiated with 1.0 MeV protons. The cells were annealing at 200 C. The annealing time was dependent on proton fluence. Annealing devices for one hour restores cell parameters or fluences below 1(exp 14) cm(exp -2); fluences above 1(exp 14) cm(exp -2) require longer annealing times. A parametric fitting model was used to characterize current mechanisms observed in dark I-V measurements. The current mechanisms were explored with irradiation fluence, and voltage and light soaking times. The thermal generation current density and quality factor increased with proton fluence. Device simulation shows the degradation in cell characteristics may be explained by the reduction of the electric field in the intrinsic layer.
The radiation resistance of commercial solar cells fabricated from hydrogenated amorphous silicon alloys was investigated. A number of different device structures were irradiated with 1.0 MeV protons. The cells were insensitive to proton fluences below 1E12 sq cm. The parameters of the irradiated cells were restored with annealing at 200 C. The annealing time was dependent on proton fluence. Annealing devices for one hour restores cell parameters for fluences below lE14 sq cm require longer annealing times. A parametric fitting model was used to characterize current mechanisms observed in dark I-V measurements. The current mechanisms were explored with irradiation fluence, and voltage and light soaking times. The thermal generation current density and quality factor increased with proton fluence. Device simulation shows the degradation in cell characteristics may be explained by the reduction of the electric field in the intrinsic layer.
The radiation resistance of commercial solar cells fabricated from hydrogenated amorphous silicon alloys is reported. A number of different device structures were irradiated with 1.0 MeV protons. The cells were insensitive to proton fluences below 1E12 sq cm. The parameters of the irradiated cells were restored with annealing at 200 C. The annealing time was dependent on proton fluence. Annealing devices for one hour restores cell parameters for fluences below 1E14 sq cm fluences above 1E14 sq cm require longer annealing times. A parametric fitting model was used to characterize current mechanisms observed In dark I-V measurements. The current mechanism were explored with irradiation fluence, and voltage and light soaking times. The thermal generation current density and quality factor increased with proton fluence. Device simulation shows the degradation in cell characteristics may be explained by the reduction of the electric field in the intrinsic layer.
Method produces large amorphous alloys. Spheres of amorphous metal alloys formed and collected after molten samples coated and cooled in drop tube. Coated spheres cooled acoustically and cryogenically. Amorphous specimens 5mm in diameter or larger possible.
Ultralight and ultrathin, flexible, rollup monolithic PV modules have been developed consisting of multijunction, amorphous silicon alloys for either terrestrial or aerospace applications. The rate of progress in increasing conversion efficiency of stable multijunction and multigap PV cells indicates that arrays of these modules can be available for NASA's high power systems in the 1990's. Because of the extremely light module weight and the highly automated process of manufacture, the monolithic a-Si alloy arrays are expected to be strongly competitive with other systems for use in NASA's space station or in other large aerospace applications.
Although nanocrystalline alloys regularly exhibit high strengths, their use in structural applications often face challenges due to sample size limitations, unstable microstructures, and the limited ability to plastically deform. The incorporation of amorphous grain boundary complexions has been proposed to address these issues, by simultaneously stabilizing nanocrystalline grain structures for scale-up processing and improving alloy toughness. In the present study, the mechanical behavior of bulk nanocrystalline Al–Mg–Y is examined with macroscale compression testing, probing a length scale that is relevant to real-world structural applications. Bulk samples were fabricated via a simple powder metallurgy approach, with different hot-pressing temperatures and durations employed for consolidation in order to investigate microstructural and property evolution. All of the specimens contained primary face-centered cubic Al and secondary Al 4 C 3 and Al 3 Y phases, with the Al 3 Y particles exhibiting two populations of small equiaxed and larger elongated particles. Appreciable plasticity was measured along with high ultimate stresses over 800 MPa due to the presence of amorphous grain boundary complexions. Microstructural characterization of fracture surfaces revealed that the area fraction of dimpled regions increased with longer hot-pressing time. Most importantly, the elongated Al 3 Y particles formed regular cellular patterns with increasing hot-pressing time, delaying shear localization and significantly enhancing plasticity. The hierarchy present in the microstructure of the Al–Mg–Y alloy, from amorphous grain boundary complexions to secondary phases, gives rise to excellent bulk mechanical properties, which are attractive for structural applications.
The development of the first commercial, ultralight, flexible, deployable, PV array for aerospace applications is discussed. It is based on thin-film, amorphous silicon alloy, multijunction, solar cells deposited on a thin metal or polymer by a proprietary, roll-to-roll process. The array generates over 200 W at AM0 and is made of 20 giant cells, each 54 cm x 29 cm (1566 sq cm in area). Each cell is protected with bypass diodes. Fully encapsulated array blanket and the deployment mechanism weigh about 800 and 500 g, respectively. These data yield power per area ratio of over 60 W/sq m specific power of over 250 W/kg (4 kg/kW) for the blanket and 154 W/kg (6.5 kg/kW) for the power system. When stowed, the array is rolled up to a diameter of 7 cm and a length of 1.11 m. It is deployed quickly to its full area of 2.92 m x 1.11 m, for instant power. Potential applications include power for lightweight space vehicles, high altitude balloons, remotely piloted and tethered vehicles. These developments signal the dawning of a new age of lightweight, deployable, low-cost space arrays in the range from tens to tens of thousands of watts for near-term applications and the feasibility of multi-100 kW to MW arrays for future needs.
Amorphous Si:H and amorphous Si sub x, Ge sub (1-x):H solar cells were irradiated with 1.00 MeV proton fluences in the range of 1.00E14 to 1.25E15 cm (exp -2). Annealing of the short circuit current density was studied at 0, 22, 50, 100, and 150 C. Annealing times ranged from an hour to several days. The measurements confirmed that annealing occurs at 0 C and the initial characteristics of the cells are restored by annealing at 200 C. The rate of annealing does not appear to follow a simple nth order reaction rate model. Calculations of the short-circuit current density using quantum efficiency measurements and the standard AM1.5 global spectrum compare favorably with measured values. It is proposed that the degradation in J sub sc with irradiation is due to carrier recombination through the fraction of D (o) states bounded by the quasi-Fermi energies. The time dependence of the rate of annealing of J sub sc does appear to be consistent with the interpretation that there is a thermally activated dispersive transport mechanism which leads to the passivation of the irradiation induced defects.
Thin-film, tandem-junction, amorphous silicon (a-Si) photovoltaic modules were constructed in which a part of the a-Si alloy cell material is used to form bypass protection diodes. This integral design circumvents the need for incorporating external, conventional diodes, thus simplifying the manufacturing process and reducing module weight.
The range of topics covered by the papers includes: rapid quenching (and specifically splat quenching) of metals, spin quenching, levitation melting, rapid quenching from liquid state; amorphous metal phases and metastable phases, metallic glasses, ribbons, splats, films, metal ribbon reinforced resins; crystallization of metallic glasses, and ferromagnetic amorphous alloys. Structural models for amorphous metals, splat-quenching equipment, and measurements of the properties of amorphous and noncrystalline metals and metallic glasses are also discussed, in addition to: fatigue events (crack propagation) in amorphous metals, fracture behavior in rapidly quenched metals, ductile superconducting Cu-Nb-Sn alloys, and semiconducting amorphous V205 alloy. Individual items are announced in this issue.
Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.
Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.
Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.
The microstructure and corrosion behavior of magnetron sputter deposited amorphous metallic films of (Mo6ORu40)82B18 under varying sputtering atmospheres have been investigated. The microstructural details and topology of the films have been studied by scanning electron microscopy and correlated with the deposition conditions. By reducing the pressure of pure argon gas, the characteristic features of rough surface and columnar growth full of vertical voids can be converted into a mirror-smooth finish with very dense deposits. Films deposited in the presence of O2 or N2 exhibit columnar structure with vertical voids. Film deposited in pure argon at low pressure show remarkably high corrosion resistance due to the formation of a uniform passive surface layer. The influence of the microstructure and surface texture on the corrosion behavior is discussed.