Search NASA⌕ Search

SEARCH · Search NASA

Results for “back surface passivation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Electrical Analysis of Pulsed Laser Annealed Poly-Si:Ga/SiOx Passivating Contacts

High-efficiency single crystalline silicon (c-Si) solar cells require precise control of dopant diffusion profiles and highly active doping concentrations through thermal annealing. Conventional furnace annealing has been successfully employed for dopant diffusion in aluminum back-surface field (Al-BSF), passivated emitter and rear contact (PERC), and Topcon cells. However, furnace annealing limits some next-generation polycrystalline silicon (poly-Si) on SiOx passivating contacts. This limitation largely affects p-type passivating contacts by not being able to: 1) control the dopant diffusion accurately to prevent B segregation at the SiOx and c-Si interface; and 2) provide highly activated doping concentrations for low contact resistivity. In this contribution, we use a nanosecond excimer laser to examine the passivation quality and electrical performance of both B- and Ga-doped poly-Si/SiOx passivating contacts. The core of this method is to take advantage of the nonequilibrium nature of the anneal through rapid melting and recrystallizing the poly-Si in a short timescale and to achieve doping concentrations above the solid solubility limit. Simulations were performed on polished surfaces to visualize the doping diffusion profiles under different laser conditions, and secondary ion mass spectrometry (SIMS) was used to verify the experimental diffusion profiles post pulsed laser melting (PLM). The results show the dopant diffusion profiles can be tuned precisely through PLM. The electrical analysis using VdP-Hall measurements reveals that the active doping concentration reached 10^21 cm-3 for B and ~2×10^21 cm-3 for Ga in poly-Si, far exceeding their solid solubility limit in Si, with a nearly 100% dopant activation achieved for B, and 20% for Ga. This highly activated dopant profile results in a low contact resistivity of <15 mO·cm^2 for B-doped contacts and <40 mO·cm^2 for Ga-doped contacts. We demonstrate that the passivation quality of the laser annealed contacts shows a linear dependency with the laser energy density and the number of pulses. PLM was also performed on random pyramid textured samples, and we found that preferential melting exists for the tips of pyramids, which can be pursued further for selective pinhole opening. Additionally, we perform thermal stability tests of these hyperdoped passivating contacts and show that under certain laser conditions, the B-doped samples exhibit good thermal stability with near full activation for temperatures up to 800°C. Lastly, we transfer this technique to a larger area by overlapping laser spots and show uniform passivation quality and electrical performance. We are currently implementing this PLM annealed p-type passivating contacts into double-side back-junction poly-Si/SiOx passivating contact devices. Our results show that PLM can not only enable the next generation of high-efficiency c-Si photovoltaics technology but can also benefit the c-Si integrated circuit industry through hyperdoping other semiconductors with atoms that may otherwise have a low solubility.

doping diffusion profile↗

Sputtered Aluminum Oxide and p+ Amorphous Silicon Back-Contact for Improved Hole Extraction in Polycrystalline CdSexTe1-x and CdTe Photovoltaics

A thin layer of Al 2 O 3 at the back of CdSe x T e1-x /CdTe devices is shown to passivate the back interface and drastically improve surface recombination lifetimes and photoluminescent response. Despite this, such devices do not show an improvement in open-circuit voltage (VOC.) Adding a p + amorphous silicon layer behind the Al 2 O 3 bends the conduction band upward, reducing the barrier to hole extraction and improving collection. Further optimization of the Al 2 O 3 , amorphous silicon (a-Si), and indium-doped tin oxide (ITO) layers, as well as their interaction with the CdCl 2 passivation process, are necessary to translate these electro-optical improvements into gains in voltage.

14 SOLAR ENERGY↗

Improved performance of a near-field thermophotovoltaic device by a back gapped reflector

Various spectral control techniques can be applied to improve the performance of a thermophotovoltaic (TPV) device. For example, a back surface reflector (BSR) is a common structure to improve the performance of TPV devices. A conventional metal BSR structure enhances the photogeneration rate by increasing the absorption probability of photons via back surface reflections, affording a second chance for absorption. However, the effects of surface passivation and external luminescence introduced by BSR structures have been previously ignored, which potentially decreases the performance of TPV devices. Recently, a back gapped reflector (BGR) structure was proposed to greatly improve the performance of far-field TPV devices by reducing imperfect reflections at the semiconductor-metal interface. In the present work, the performance improvement on a thin-film, near-field InAs TPV device with a BGR is investigated, comparing its performance to that with a conventional metal BSR. Surface passivation conditions are also investigated to further improve the performance of TPV devices with back reflectors. Further, the output power and efficiency are calculated using an iterative model combining fluctuational electrodynamics and the full drift diffusion model. For the well-passivated condition, when the BSR is replaced by the BGR, the calculated conversion efficiency of the near-field TPV was improved from 16.4% to 21% and the output power was increased by 10%. Finally, the absorption of the back reflectors and external luminescence loss are analyzed to explain the performance improvement.

external luminescence↗

Photovoltaic cell and production thereof

An efficient photovoltaic cell, and its process of manufacture, is disclosed wherein the back surface p-n junction is removed from a doped substrate having an oppositely doped emitter layer. A front surface and edges and optionally the back surface periphery are masked and a back surface etch is performed. The mask is not removed and acts as an anti-reflective coating, a passivating agent, or both. The photovoltaic cell retains an untextured back surface whether or not the front is textured and the dopant layer on the back surface is removed to enhance the cell efficiency. Optionally, a back surface field is formed.

14 SOLAR ENERGY↗

PERC silicon PV infrared to ultraviolet optical model

Here, optical modeling of aluminum back surface field (Al-BSF) and passivated emitter and rear contact (PERC) silicon wafer solar cells are extended into the infrared wavelength range (300–2500 nm). The model incorporates ray tracing to account for pyramidal texture of the front silicon surface, free carrier absorption in the front emitter; bulk silicon wafer, BSF; and Lambertian scattering at the silicon back contact. Total reflectance of pyramidal textured cells with different contact geometries with and without encapsulation are simulated. Simulated reflectance and short circuit current density match well with experimental values. These physics-based optical models serve as input for evaluating optical and thermal management strategies for silicon wafer solar cells.

14 SOLAR ENERGY↗

Simulation of Device Parameters of High Efficiency Multicrystalline Silicon Solar Cells

The results of the simulation of the reported experimental results of high efficiency multicrystalline silicon (mc-Si) solar cells, using PC1D software, are reported in this study. Results obtained by various groups have been incorporated and compared in this study. The highest efficiency reported so far for mc-Si solar cells is 20{center_dot}4% and 17-18% by research laboratories and commercial houses, respectively. The efficiency can be further enhanced if passivation characteristics on both the front and back surface are improved. The role of back surface recombination has become more significant in light of the use of thin mc-Si wafers by the solar cell industry. Based on the passivation characteristics and considering the understanding of the past three decades of studies, the authors have proposed and simulated a structure for mc-Si solar cells to improve the performance of the same. The results of our modeled structure of mc-Si solar cell show an efficiency of 21{center_dot}88% with short-circuit current density, J{sub sc} = 39{center_dot}39 mA/cm2, and open circuit voltage, V{sub oc} = 0{center_dot}666 V.

14 SOLAR ENERGY↗

Enabling Efficiencies > 22.5% with Metal Oxide Passivating Contacts using Low-Cost Spatial Atomic Layer Deposition (Final Technical Report)

In this project, the University of Central Florida (UCF) worked to both increase module efficiency and reduce manufacturing cost by driving demonstrated lab-scale passivating contact technology using materials and processes compatible with high-volume manufacturing for crystalline silicon (c-Si) photovoltaic (PV) cells. Passivating contacts have garnered significant attention in recent years. They provide a means of suppressing contact recombination, a loss mechanism that limits the performance of industrially relevant cell architectures like Al back surface field (Al-BSF) cells and passivated emitter and rear cells (PERC). Most of the development of passivating contact technology has focused on the use of doped amorphous silicon or doped polysilicon contacts, but both suffer from parasitic optical absorption amongst other issues. Our team developed fully transparent hole-selective heterojunctions, deposited using atomic layer deposition (ALD), and showed how they could be incorporated into c-Si PV cells. The team conducted experiments to understand the process-structure-property relationship of hole-selective oxides, surface passivation oxide materials, and transparent conductive oxides deposited by ALD, and use that understanding to reduce contact recombination, contact resistivity, and parasitic optical absorption within c-Si PV cells. Before getting into the details of the report, we would like to note that COVID-19 has made it more challenging to conduct experimental research at UCF. UCF has a number of mandatory policies in place to ensure social distancing, testing, and contact tracing are all carried out in day-to-day operations. Despite these challenges, we worked diligently to make progress on this project in a manner that was as safe as possible. Over the course of the project, the UCF team and its collaborators have made the following discoveries and developments.

14 SOLAR ENERGY↗

Systematic Operating Temperature Differences Between Al-BSF, PERC, and PERT-With-Optimized-Rear-Reflector Solar Mini-Modules Due to Rear Reflectance

Reflecting sub-bandgap light from photovoltaic modules has the potential to improve lifetime energy generation of fielded systems by reducing operating temperature. In this article, the temperature of fielded aluminum back-surface field (Al-BSF) and passivated emitter and rear contact (PERC) mini-modules was monitored every 5 minutes for 75 days along with corresponding meteorological data. Additionally, passivated emitter rear totally diffused (PERT) mini-modules with high-performance sub-bandgap rear reflectors were tested and compared to the state-of-the-art industrial modules. These reflectors consisted of a >300-nm-thick silicon dioxide nanoparticle film with a low refractive index. The impact of reflectance on measured operating temperature was isolated with a previously developed thermal model and quantified as the reflectance-induced median temperature difference between each tested module at representative outdoor conditions (1000 W m -2 , 25 degrees C ambient temperature, and 1.43 m s -1 wind speed). We found that, because of their reflectance differences, PERC modules ran systematically cooler than Al-BSF modules by 1.0 degrees C, whereas the PERT-with-optimized-rear-reflector systematically operated 1.4 degrees C cooler than the Al-BSF module and 0.4 degrees C than the PERC module. We also found that the rear reflector provided the greatest temperature benefit during periods of highest irradiance.

14 SOLAR ENERGY↗

Optical Evaluation of PERC Cell Reflectance for Thermal Management

We discuss optical modeling of aluminum back surface field (Al-BSF) and passivated emitter rear contact (PERC) solar cells extending into the infrared wavelength range. Total reflectance of pyramidical textured cells with and without encapsulation is simulated. This approach focusing on the encapsulated and bare cell reflectance serve as input for evaluating thermal management strategies for solar cells.

14 SOLAR ENERGY↗

Chalcogen back surface field layer

Kesterite photovoltaic devices having a back surface field layer are provided. In one aspect, a method of forming a photovoltaic device includes: forming a complete photovoltaic device having a substrate, an electrically conductive layer on the substrate, an absorber layer on the electrically conductive layer, a buffer layer on the absorber layer, and a transparent front contact on the buffer layer; removing the substrate and the electrically conductive layer from the complete photovoltaic device to expose a backside surface of the absorber layer; forming a passivating layer on the backside surface of the absorber layer; and forming a high work function back contact on the passivating layer. A photovoltaic device having a passivating layer is also provided.

Antunez, Priscilla D.↗

Chalcogen back surface field layer

Kesterite photovoltaic devices having a back surface field layer are provided. In one aspect, a method of forming a photovoltaic device includes: forming a complete photovoltaic device having a substrate, an electrically conductive layer on the substrate, an absorber layer on the electrically conductive layer, a buffer layer on the absorber layer, and a transparent front contact on the buffer layer; removing the substrate and the electrically conductive layer from the complete photovoltaic device to expose a backside surface of the absorber layer; forming a passivating layer on the backside surface of the absorber layer; and forming a high work function back contact on the passivating layer. A photovoltaic device having a passivating layer is also provided.

14 SOLAR ENERGY↗

High Rate Laser Pitting Technique for Solar Cell Texturing

Efficiency of crystalline silicon solar cells can be improved by creating a texture on the surface to increase optical absorption. Different techniques have been developed for texturing, with the current state-of-the-art (SOA) being wet chemical etching. The process has poor optical performance, produces surfaces that are difficult to passivate or contact and is relatively expensive due to the use of hazardous chemicals. This project shall develop an alternative process for texturing mc-Si using laser micromachining. It will have the following features compared to the current SOA texturing process: (1) Superior optical surfaces for reduced front-surface reflection and enhanced optical absorption in thin mc-Si substrates (2) Improved surface passivation (3) More easily integrated into advanced back-contact cell concepts (4) Reduced use of hazardous chemicals and waste treatment (5) Similar or lower cost. The process is based on laser pitting. The objective is to develop and demonstrate a high rate laser pitting process which will exceed the rate of former laser texturing processes by a factor of ten. The laser and scanning technologies will be demonstrated on a laboratory scale, but will use inherently technologies that can easily be scaled to production rates. The drastic increase in process velocity is required for the process to be implemented as an in-line process in PV manufacturing. The project includes laser process development, development of advanced optical systems for beam manipulation and cell reflectivity and efficiency testing. An improvement of over 0.5% absolute in efficiency is anticipated after laser-based texturing. The surface textures will be characterized optically, and solar cells will be fabricated with the new laser texturing to ensure that the new process is compatible with high-efficiency cell processing. The result will be demonstration of a prototype process that is suitable for scale-up to a production tool and process. The developed technique will have an reducing impact on product pricing. As efficiency has a substantial impact on the economics of solar cell production due to the high material cost content; in essence, improved efficiency through cost-effective texturing reduces the material cost component since the product is priced in terms of $/W. The project is a collaboration between Fraunhofer USA, Inc. and a c-Si PV manufacturer.

14 SOLAR ENERGY↗

Electrochemical Deposition of Conformal Semiconductor Layers in Nanoporous Oxides for Sensitized Photoelectrodes

Nanoporous photoelectrodes with photoactive semiconductors have been investigated for various energy applications such as solar cells and photoelectrochemical cells, but the deposition of the semiconducting materials on the nanoporous electrodes has been very challenging due to pore clogging or complete pore filling. Here, we propose a band alignment model that explains the morphology of the electrochemically deposited semiconductor layer on the semiconducting nanoporous oxide electrode. Briefly, the coating material with a conduction band edge higher (i.e., more negative) than that of the electrode material forms a conformal coating, which maintains the initial nanoporous structure. As a result, a conformal CdSe layer can be electrodeposited onto TiO 2 nanotubes, which can be used as a photoelectrode of a sensitized solar cell. The electron dynamics studies revealed that the CdSe-sensitized TiO 2 nanotube electrode exhibited faster charge transport and slower charge recombination than its dye-sensitized counterpart, which has been ascribed to the passivation of surface traps and the physically blocked back-electron transfer by the CdSe layer as well as the higher conduction band of CdSe.

36 MATERIALS SCIENCE↗

Value Proposition of UV-Absorbers in PV Module Encapsulation

Various common crystalline silicon cell technologies were exposed to UVA radiation (1.24 Wm-2 nm-1 at 340 nm peak) on the front and back faces at 45 degrees Celsius for periods up to 3000 h, representing about 3 y of solar exposure in Phoenix, Arizona, USA. The resulting degradation of the open-circuit voltage and short-circuit current is presented. Of the various cell types examined, significant levels of degradation were seen in all cases. Less degradation was generally found after UV irradiation of cell fronts and older cell types, whereas a bifacial PERC type exposed on the rear showed about 25% degradation in short circuit current, attributable to lack of a diffused surface field. Selected cells were exposed to UV irradiation with the addition of long pass UV filters to replicate UV-absorbers in encapsulants. Modern cell designs are sensitive to UV-ID because of reduced or eliminated front and back surface field and increased dependence on high quality surface passivation. Single transformation of the independent variable (t, kW h/m^2) could be used to achieve a linear model of the data to extrapolate to 50 y. Solar Advisor Model (SAM) shows appropriate filtering of UV-irradiation can improve LCOE and net present value of plant. Some advanced cell types are seen to be UV-resistant (cell level solutions also exist). Solutions therefore exist on the cell, glass, and encapsulant level. Changes over time in each of these would also need to be considered (solarization, encapsulant browning...).

ENGINEERING,SOLAR ENERGY↗

UV-Induced Degradation of High-Efficiency Solar Cells with Different Architectures

The ultraviolet-induced degradation (UVID) of solar panels is associated with the deterioration of cell performance and reduced reliability of packaging materials. Here we examine the UV stability of different architectures of high-efficiency solar cells without any encapsulation. Identical UV exposure tests were performed at two different labs using UVA-340 fluorescent lamps under different electrical bias configurations (open- or short-circuit) and irradiated cell surfaces (for bifacial technologies). Cell technologies, including heterojunction (HJ), interdigitated back-contact cells (IBC), passivated emitter rear contact (PERC), passivated emitter rear totally-diffused (PERT), are found to be more susceptible to UVID, leading to significant Isc loss (up to 4%) and P max loss (up to 15%) as compared to the conventional back surface field (Al-BSF) cells after exposure to UV irradiation of 8.92 MJ-m -2 -nm -1 at 340 nm. Additionally, the bifacial cells when irradiated from the backside exhibited greater photocurrent loss compared to the front side exposure, indicating potential sensitivity of rear surface passivation to UV radiation.

crystalline silicon↗

“Top-Down” Li Deposition Pathway Enabled by an Asymmetric Design for Li Composite Electrode

Designing Li composite electrodes with host frameworks for accommodating Li metal has been considered to be an effective approach to suppress Li dendrites. Herein, an asymmetric design of a Mo net/Li metal film (MLF) composite electrode is developed by an inverted thermal infusion method. The asymmetric MLF electrode has a dense oxide passivated layer on the top side, a porous Mo net matrix on the back side, and active Li layer in between. The back side has a larger specific area and higher electric field than the top side, which contacts with the separator upon cycling, triggering the preferred Li deposition and stripping of the porous back side of the electrode far from the separator. The surface passivation layer on the top side of the electrode as an artificial solid electrolyte interphase ensures the stable contact with the electrolyte and separator. Meanwhile, the porous structure of the supporting Mo net provides enough space for accommodating the volume change during Li deposition and stripping. This asymmetry design enables a unique “top down” growth pathway for Li deposition in the MLF electrode, suppressing the dendrite growth effectively. In conclusion, the design strategy provides a new direction for high-energy dendrite-free Li metal anodes.

25 ENERGY STORAGE↗

In-situ hydrogen microstructural characterization of Si heterojunction passivation: Addressing V OC degradation and mitigation pathways

Si heterojunction (SHJ) solar cells have demonstrated record efficiency >27%, approaching the theoretical limit of ≈ 29%, primarily due to best surface/interface defect passivation provided by deposited thin layers of hydrogenated amorphous silicon (a-Si:H). Such excellent surface/interface passivation reduces recombination loss and result in >100 mV improvement of cell open circuit voltage (V OC ) to ≈ 750 mV, thus the cell efficiency. However, fielded SHJ modules exhibit loss of V OC and hence efficiency over time in years, presumably due to degradation related to a-Si:H layers. This adversely affects the technology’s market acceptance, and levelized cost of energy (LCOE). It is hypothesized that the origin of a-Si:H degradation is somehow related to the presence of weak Si–Si bonds and hydrogen in a-Si:H films. The objective of this project is to test this hypothesis by directly measuring chemical and structural changes occurring within SHJ component layers and solar cells. This is achieved by developing an innovative in-situ Fourier transform infrared (FTIR) spectrometry apparatus to monitor hydrogen microstructural changes occurring within amorphous silicon and decipher hydrogen evolution kinetics over time when samples are exposed to heat and/or light stress. These in-situ measured hydrogen microstructural changes are correlated to the changes in effective minority carrier lifetime (τ eff ), implied V OC (iV OC ), surface recombination velocity (S), and cell V OC . These mechanistic understandings will provide critical guidance to mitigate the V OC -driven degradation of SHJ solar cell performance. Passivation optimization and degradation analysis of individual SHJ component structures were achieved through systematic deposition of three symmetric structures and the completed SHJ solar cell structure. The three symmetric structures used were intrinsic a-Si:H [(i)a-Si:H] layers in a bilayer structure, intrinsic and p-type doped stacked layers [(i-p)a-Si:H] representing the front heterojunction in the SHJ cell, and intrinsic and n-typed doped stacked layers [(i-n)a-Si:H] representing the back-side back surface field (BSF) in the SHJ cell. State-of-the-art passivation qualities are demonstrated by a champion iV OC of 740 mV for the (i)a-Si:H layers, and the (i-n)a-Si:H symmetric structure. A 725 mV iV OC is observed for the (i-p)a-Si:H symmetric structure. These symmetric passivated SHJ component structures were subsequently subjected to different accelerated lifetime (ALT) stressors to identify which conditions contribute the most to iV OC degradation. Degradation of the thin (10 nm) (i)a-Si:H passivation layers without any additional overlying layers is minimal; complexity of this study arises due to unavoidable surface oxidation of (i)a-Si:H layer during most of the stress application, which is likely irrelevant for a full SHJ cell configuration with overlying protective layers. The iV OC degradation of symmetric structures is found to occur primarily at the (i-p)a-Si:H passivation stack under dark heat stress with associated hydrogen loss from the (p)a-Si:H layer. An activation energy for increase in S (defect creation) of 0.65 eV can be correlated to the activation energy of ≈ 0.4 eV for hydrogen loss from the (i-p)a-Si:H stack. This also suggests the presence of weakly bonded hydrogen in the (p)a-Si:H films, which effuses out of the film stack at such low activation energy. When light and heat stress are applied together, similar hydrogen loss from (i-p)a-Si:H stack is observed, however, does not appreciably degrade iV OC or increase S. This is an important result and departure from direct correlation between hydrogen loss and defect creation. This perhaps indicates additional defect chemistries or annealing that might be occurring in the presence of light requiring further detailed defect measurements. The full SHJ cell structure used for this project is depicted in Fig.1(d). SHJ cells with an initial V OC ≈ 700 mV were fabricated and subjected to similar ALT stress conditions. Cell V OC is found to degrade the most under dark heat stress and is confirmed by observed hydrogen migration out of the (i-p)a-Si:H stack. However, hydrogen cannot escape from the cell stack, it accumulates near the (p)a-Si:H/ITO contact interface, where ITO acts as a barrier preventing hydrogen loss. Furthermore, light-heat combined stress does not degrade V OC appreciably, confirming the occurrence of a defect annealing process.

14 SOLAR ENERGY↗

Laterally inherently thin amorphous-crystalline silicon heterojunction photovoltaic cell

This article reports on an amorphous-crystalline silicon heterojunction photovoltaic cell concept wherein the heterojunction regions are laterally narrow and distributed amidst a backdrop of well-passivated crystalline silicon surface. The localized amorphous-crystalline silicon heterojunctions consisting of the laterally thin emitter and back-surface field regions are precisely aligned under the metal grid-lines and bus-bars while the remaining crystalline silicon surface is passivated using the recently proposed facile grown native oxide–plasma enhanced chemical vapour deposited silicon nitride passivation scheme. The proposed cell concept mitigates parasitic optical absorption losses by relegating amorphous silicon to beneath the shadowed metallized regions and by using optically transparent passivation layer. A photovoltaic conversion efficiency of 13.6% is obtained for an untextured proof-of-concept cell illuminated under AM 1.5 global spectrum; the specific cell performance parameters are V{sub OC} of 666 mV, J{sub SC} of 29.5 mA-cm{sup −2}, and fill-factor of 69.3%. Reduced parasitic absorption, predominantly in the shorter wavelength range, is confirmed with external quantum efficiency measurement.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗