Search NASA⌕ Search

SEARCH · Search NASA

Results for “button cell”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Synthesis and characterization of novel Ce{sub 0.8}Sm{sub 0.2}Fe{sub 0.9}Ir{sub 0.03}Co{sub 0.07}O{sub 3−δ} perovskite material and possible application as a cathode for low–intermediate temperature SOFCs

Highlights: • Ce{sub 0.8}Sm{sub 0.2}Fe{sub 0.9}Ir{sub 0.03}Co{sub 0.07}O{sub 3−δ} was synthesized using sol–gel methods. • Material was thoroughly characterized using Raman, FTIR, XRD, HRTEM, SEM, and TGA. • Electrochemical performance showed the materials are a promising new cathode material for low temperature SOFC. - Abstract: A novel perovskite material, Ce{sub 0.8}Sm{sub 0.2}Fe{sub 0.9}Ir{sub 0.03}Co{sub 0.07}O{sub 3−δ} was synthesized using a sol–gel technique. The materials were calcined at temperatures of 800 °C, 900 °C, and 1000 °C and then characterized using X-ray diffraction, Raman and infrared spectroscopy, high resolution transmission electron microscopy and scanning electron microscopy (SEM). The particle sizes and crystallite sizes increased with increasing calcination temperature and formed perovskite type materials with some separate magnetite and iridium oxide. The powders were used to assemble button cells using samarium doped ceria as the electrolyte and NiO/SDC as the anode materials. The electrochemical properties were investigated using a Fiaxell open flanges test set-up and a Nuvant™ Powerstat-05 potentiostat/galvanostat. The Ce{sub 0.8}Sm{sub 0.2}Fe{sub 0.9}Ir{sub 0.03}Co{sub 0.07}O{sub 3−δ} cathode material calcined at 1000 °C exhibited the most promising performance, with a maximum power density of 0.400 W/cm{sup 2}, a current density of 0.8 A/cm{sup 2}, and a corresponding area specific resistance of 0.247 Ωcm{sup 2} at 500 °C. The button cells were reasonably stable over15 h.

36 MATERIALS SCIENCE↗

Advanced Anode for Internal Reforming and Thermal Management in Solid Oxide Fuel Cells

Solid oxide fuel cell (SOFC) is an efficient and clean electrical power generation system compared to conventional combustion based technologies with energy efficiency reaching as high as 85-90% in co-generation mode (electricity and heat). Other advantages of SOFCs are hybridization, modularity of construction, small CO 2 foot print per kWh of generated electricity and fuel flexibility. Hydrocarbons present in the gaseous fuel is utilized in SOFCs by internal or external reforming. There are two different internal reforming concepts: Direct Internal Reforming (DIR) and Indirect Internal Reforming (IIR). For DIR operation, the endothermic reforming reaction and the exothermic reaction from the oxidation reaction are operated together in the single unit eliminating the requirement for a separate fuel reformer. This configuration also simplifies the overall system design, making SOFC more attractive and efficient means of producing electrical power. The main advantage of the DIR type of operation is that the H 2 or CO consumption by the electrochemical reaction could directly promote the conversion of methane at the anode side of the fuel cell resulting in high conversion and high efficiency. The DIR operation, however, requires an anode material that has desired dual catalytic (hetero and electro) properties for reforming reaction and electrochemical reactions. The anode materials also need to remain resistant to carbon formation at the operating temperature and atmosphere with stable cell performance. Another requirement is to match the reforming reactions and electrochemical reactions to avoid local cooling or overheating, which can result in mechanical failure due to thermally induced stresses. Direct internal reforming (DIR) of hydrocarbon fuels simplifies the overall SOFC system design making it more attractive and efficient for producing electrical power. Low cost alloy anodes for distributed internal reforming of methane and other hydrocarbon fuels offer increased fuel-flexibility, reliability, and long term performance stability of solid oxide fuel cells (SOFC). The research program examined modification of the chemical compositions and microstructure of high entropy alloy (HEA) anode materials using thermochemical calculations and process simulation and modeling to achieve distributed reforming over the entire anode to eliminate hot zones. Cell fabrication and testing of the HEA anodes using button cell configuration has been performed to demonstrate the advantages of new anode over traditional Ni-YSZ anodes for distributed reforming and carbon free operation. Technical accomplishments include identification and synthesis of HEA carbon-resistant anode, demonstration of reduction in reforming rate confirmed by GC and modelling data validating effectiveness for thermal management in cell/stacks, electrochemical testing of HEA anode in single cell (HEA-GDC||YSZ||LSM-YSZ) and Characterization of pretest and posttest anode materials by TEM and SEM-EDS confirming carbon-free operation.

30 DIRECT ENERGY CONVERSION↗

DEGRADATION IN PERFORMANCE OF LANTHANUM STRONTIUM MANGANITE BASED SOLID OXIDE FUEL CELL CATHODES UNDER ACCELERATED TESTING

The performance of solid oxide fuel cells (SOFCs) with three different lanthanum strontium manganite (LSM) based cathode compositions were evaluated. All cells were yttria-stabilized zirconia (Zr0.92Y0.08O2-δ, 8YSZ) electrolyte-supported button cells, consisting of a nickel oxide – yttria-stabilized zirconia (NiO-8YSZ) anode and a cathode of 8YSZ and LSM. The three LSM compositions differed in the amount of excess Mn: Composition A was (La0.85Sr0.15)0.90MnO3±δ (10% excess Mn); Composition B was (La0.80Sr0.20)0.95MnO3±δ (5% excess Mn); and Composition C was (La0.80Sr0.20)0.98MnO3±δ (2% excess Mn). The cells were tested under conventional and accelerated conditions, where the accelerated conditions were meant to simulate the results of months of long-term testing in just 500 hours (approximately three weeks) of testing by using high operating temperature and current density. Accelerated tests showed lower degradation rates, lower continuous area specific resistance (ASR), and higher power output than conventional tests for all cathode compositions. Continuous measurements of the cells' output voltage versus time, together with periodic electrochemical impedance spectroscopy (EIS) measurements, were used to evaluate the performance of the cells in terms of ASR degradation rates (% ASR rise per kh) and power outputs. The EIS measurements also permitted a partial deconvolution of the cathode ASR from the anode ASR. Cathodes with 10% excess Mn tested under accelerated conditions had the lowest degradation rates, but the highest continuous ASR and lowest power outputs. Cathodes with 2% excess Mn tested under accelerated conditions had the lowest continuous ASR and highest power outputs; thus it was concluded that cells with the lowest amount of excess Mn cathodes performed the best.

08 HYDROGEN↗

Degradation Mechanisms of SOFC Anodes in Coal Gas Containing Phosphorus

The interaction of phosphorus in synthetic coal gas with the nickel-based anode of solid oxide fuel cells has been investigated. Tests with both anode-supported and electrolyte-supported button cells were performed at 700 to 800oC in synthetic coal gas containing 0.5 to 10 ppm phosphorus, introduced as phosphine. Two primary modes of degradation were observed. The most obvious was the formation of a series of bulk nickel phosphide phases, of which Ni3P, Ni5P2, Ni12P5 and Ni2P were identified. Phosphorus was essentially completely captured by the anode, forming a sharp boundary between converted and unconverted anode portions. These products partially coalesced into large grains, which eventually affected electronic percolation through the anode support. Thermodynamic calculations predict that formation of the first binary nickel phosphide phase is possible at sub-parts per billion concentrations in coal gas at temperatures relevant to fuel cell operation. A second mode of degradation is attributed to surface diffusion of phosphorus to the active anode/electrolyte interface to form an adsorption layer. Direct evidence for the presence of such an adsorption layer on nickel was obtained by surface spectroscopies on fracture surfaces. Further, cell performance losses were observed well before the entire anode was converted to bulk nickel phosphide. Impedance spectroscopy revealed that these losses were primarily due to growth in electrodic resistance, whereas large ohmic increases were visible when the entire anode was converted to nickel phosphide phases. The rate of resistance growth for anode-supported cells showed a very low dependence on phosphorus concentration, attributed to phosphorus activity control within the anode by bulk nickel phosphide products.

01 COAL, LIGNITE, AND PEAT↗

Electrochemical, Structural and Surface Characterization of Nickel/Zirconia Solid Oxide Fuel Cell Anodes in Coal Gas Containing Antimony

The interaction of antimony with the nickel-zirconia solid oxide fuel cell (SOFC) anode has been investigated. Tests with both anode-supported and electrolyte-supported button cells were performed at 700 and 800oC in synthetic coal gas containing 10 ppb to 9 ppm antimony. Minor performance loss was observed immediately after Sb introduction to coal gas resulting in ca. 5 % power output drop. While no further degradation was observed during the following several hundred hours of testing, cells abruptly and irreversibly failed after 800-1500 hours depending on Sb concentration and test temperature. Antimony was found to interact strongly with nickel and result in extensive alteration phase formation, consistent with expectations based on thermodynamic properties. Nickel antimonide phases, NiSb and Ni5Sb2, were partially coalesced into large grains and eventually affected electronic percolation through the anode support. Initial degradation was attributed to diffusion of antimony to the active anode/electrolyte interface to form an adsorption layer.

01 COAL, LIGNITE, AND PEAT↗

High Power Planar Sodium-Nickel Chloride Battery

Widespread penetration of renewable energy and increasing demands on reliability/security of the electrical grid require extensive advances in energy storage technologies. One most promising technology is the sodium-beta batteries (NBBs) based on a sodium-ion conducting β''-Al2O3 solid electrolyte (BASE) and operated at elevated temperatures (300-350oC). Current NBBs, constructed on a 1-3 mm thick tubular electrolyte, have high capital cost, performance/safety issues and relatively high operating temperature that limit market penetration of the technology. In this work we report a new generation NBB that utilizes a planar design, incorporating a thinner BASE that reduces the area of specific resistance and may be operated at reduced temperatures. The lower operating temperatures allows for use of more cost-effective cell materials and decreases adverse temperature effects that impact cycle life and overall cost. We here present recent progress generated from planar NBB button cells, including initial cell performance, cathode design and chemistry.

25 ENERGY STORAGE↗

Influence of electronic transport on electrochemical performance of (Cu,Mn) 3 O 4 solid oxide fuel cell cathodes

Alkaline Earth free spinel oxides provide a potential benefit over Sr-doped perovskite-based materials commonly used as electrodes in high-temperature electrochemical energy conversion devices, e.g., solid oxide fuel cells (SOFCs). Sr-segregation is a known issue leading to performance degradation. In this study, Cu x Mn 3-x O 4 (x = 1, 1.2, and 1.5) porous electrodes were examined as SOFC cathodes using electrochemical impedance spectroscopy to investigate the oxygen reduction reaction (ORR) kinetics in relation to the material's intrinsic conductivity, the extrinsic electrode structure, and the cell test design. Similar to the electronic conducting (La,Sr)MnO 3 SOFC cathodes, the ORR kinetics of Cu x Mn 3-x O 4 spinel electrodes was governed by the oxygen adsorption and diffusion at the particle surface as well as the charge transfer at the triple phase boundaries. The overall electrode polarization resistance was highly dependent on contact density with the metallic current collector, active material particle connectivity, electrode thickness, and the intrinsic electronic materials conductivity. Here, we describe the importance of effective electronic charge transport parallel to the electrode surface in maximizing the electrochemically active electrode volume and enhancing electrode performance. We discuss an approach to optimize cell and electrode design with respect to active materials properties. This aspect is critical to ensure reliable evaluation of new materials, since laboratory-scale button-cells typically exhibit a high degree of electrode microstructure (e.g. porosity, thickness) and electrical contact density variation from sample to sample.

(Cu,Mn)3O4↗

Evaluation of Cation Migration in Lanthanum Strontium Cobalt Ferrite Solid Oxide Fuel Cell Cathodes via In-Operando X-ray Diffraction

Anode-supported SOFC button cells with LSCF-6428 cathodes were operated at various temperatures under constant current conditions for hundreds of hours in dry or humid (~3% water) cathode air while continuously collecting 1 hour XRD scans throughout the test duration. Additionally, one cell in dry air was held at OCV, and 12% CO2 was added to the humid air for another cell. Long cumulative XRD count times allowed minor phases in concentrations of less than 0.1 wt% to be identified. In humid air, cell performance increased during the first couple of hundred hours. XRD measured a gradual shift of Fe-rich Fe,Co spinel peaks to lower angles while post-mortem SEM discovered nano-nodules on the LSCF surfaces. When 12% CO2 was added to humid air, performance degradation was observed after the initial conditioning response, unlike in tests without CO2, which were stable after conditioning. XRD also measured a shift in the peaks of the major LSCF phase in the test with CO2 indicative of some degree of gradual decomposition. Cells tested at constant current in dry air exhibited fast initial degradation that decelerated over time, while the cell held at OCV maintained a stable voltage. XRD of the cathodes held at OCV at 750 °C and operated at constant current at 700 °C in dry air measured a slower shift of the Fe-rich spinel peaks to lower angles than was seen in tests in humid air, along with a shift in the peaks of a Co-rich Fe,Co spinel to higher angles. Post-mortem SEM of cells exposed to dry air discovered smaller nano-nodules on the LSCF surfaces than had been present in cells tested in humid air. Cells tested at constant current in dry air at 750 °C and 800 °C did not exhibit any gradual changes in the XRD patterns nor were nano-nodules discovered.

Hardy, John S.↗

Optimization of metal-supported solid oxide fuel cells with a focus on mass transport

Performance of symmetric-architecture metal-supported solid oxide fuel cells was improved significantly by optimizing the catalyst infiltration process and metal support structure. Optimization of component structure and processing parameters was performed during tape-casting and fabrication of button cells. Mass transport of oxygen in the metal support was identified as a major limitation. To overcome this limitation, pore former loading and thickness of the metal support (130–250 μm) were optimized. The catalyst infiltration process was also improved by studying the impact of firing temperature (400 °C–900 °C) and infiltration cycle numbers (1–15). The maximum power density of the optimized cell was 0.9 W cm –2 at 700°C using hydrogen as a fuel, a three-fold increase over the baseline cell performance. The degradation rate of optimized cells at 550 °C, 600 °C, and 700 °C was 2%, 4.5%, and 5.5% per 100 h, respectively. Here, the phenomena of mass transport, catalyst coarsening, and chromium poisoning on the catalyst were analyzed by electrochemical impedance spectroscopy and scanning electron microscopy.

13 HYDRO ENERGY↗

Idaho National Laboratory Experimental Research In High Temperature Electrolysis For Hydrogen And Syngas Production

The Idaho National Laboratory (Idaho Falls, Idaho, USA), in collaboration with Ceramatec, Inc. (Salt Lake City, Utah, USA), is actively researching the application of solid oxide fuel cell technology as electrolyzers for large scale hydrogen and syngas production. This technology relies upon electricity and high temperature heat to chemically reduce a steam or steam / CO2 feedstock. Single button cell tests, multi-cell stack, as well as multi-stack testing has been conducted. Stack testing used 10 x 10 cm cells (8 x 8 cm active area) supplied by Ceramatec and ranged from 10 cell short stacks to 240 cell modules. Tests were conducted either in a bench-scale test apparatus or in a newly developed 5 kW Integrated Laboratory Scale (ILS) test facility. Gas composition, operating voltage, and operating temperature were varied during testing. The tests were heavily instrumented, and outlet gas compositions were monitored with a gas chromatograph. The ILS facility is currently being expanded to ~15 kW testing capacity (H2 production rate based upon lower heating value).

08 HYDROGEN↗

SYNGAS PRODUCTION VIA HIGH-TEMPERATURE COELECTROLYSIS OF STEAM AND CARBON DIOXIDE

This paper presents results of recent experiments on simultaneous high-temperature electrolysis (coelectrolysis) of steam and carbon dioxide using solid-oxide electrolysis cells. Coelectrolysis is complicated by the fact that the reverse shift reaction occurs concurrently with the electrolytic reduction reactions. All reactions must be properly accounted for when evaluating results. Electrochemical performance of the button cells and stacks were evaluated over a range of temperatures, compositions, and flow rates. The apparatus used for these tests is heavily instrumented, with precision mass-flow controllers, on-line dewpoint and CO2 sensors, and numerous pressure and temperature measurement stations. It also includes a gas chromatograph for analyzing outlet gas compositions. Comparisons of measured compositions to predictions obtained from a chemical equilibrium coelectrolysis model are presented, along with corresponding polarization curves. Results indicate excellent agreement between predicted and measured outlet compositions. Cell area-specific resistance values were found to be similar for steam electrolysis and coelectrolysis. Coelectrolysis significantly increases the yield of syngas over the reverse water gas shift reaction equilibrium composition. The process appears to be a promising technique for large-scale syngas production.

10 SYNTHETIC FUELS↗

Dynamic operation of metal-supported solid oxide electrolysis cells

Symmetric-structure metal-supported solid oxide fuel cells and electrolysis cells (MS-SOFCs, MS-SOECs) offer several advantages over conventional solid oxide cells, including the use of inexpensive materials, high mechanical strength, and rapid ramp-up ability. Aggressive operation of MS-SOCs in fuel cell mode is well-established, including extremely fast start-up, redox tolerance, and imbalanced pressure. Here, we extend dynamic operation to MS-SOCs in SOEC mode with high steam content for both small button cells and a large rectangular cell, including: steam cycling, thermal cycling, redox cycling and power cycling. Steam cycling entailed switching between 3:97 and 50:50 steam:hydrogen ratio. For thermal cycling, the temperature was rapidly varied between 150°C and 700°C for 50 cycles. Redox cycling involved switching the steam side gas between 50 % humidified H 2 and 50 % humidified N 2 for 5 cycles. Power cycling was performed by operating the cell under variable current density, resulting in cell voltage between 1.3V and 2.8V. Degradation rates for each testing strategy were compared to a baseline cell, and found to be similar. In conclusion, the excellent tolerance to dynamic operation increases confidence that MS-SOECs will be compatible with dynamic or intermittent renewable resources.

08 HYDROGEN↗

Multiphysics modeling of SOFC performance degradation caused by interface delamination and active layer cracking

In solid oxide device operation, delamination and cracking cause more catastrophic damage to cell life than other degradation mechanisms, leading to more rapid cell failure. The electrochemical performance degradation caused by electrode/electrolyte interface delamination and active layer cracking were investigated through in-house developed three-dimensional multiphysics simulations. Here the multiphysics simulations, fully calibrated against experimental datasets for button cells in a previous study, were extended to quantitatively investigate the effects of electrode/electrolyte interface delamination and active layer cracking. The simulated polarization curves and impedance behavior with various levels of delamination and cracking provided insights of the performance degradation. Furthermore, the local current distributions within the cell were analyzed for three different operating modes: constant voltage, constant current, and constant power. Finally, a practical strategy was proposed to mitigate the performance degradation in the realistic cell operations, extending overall cell lifetime.

08 HYDROGEN↗

Precautions of Using Three-Electrode Configuration to Measure Electrode Overpotential in Solid Oxide Electrochemical Cells: Insights from Finite Element Modeling

Accurate determination of electrode overpotentials is essential to assess the performance of the electrode and understand the rate-limiting steps involved. Three-electrode configuration with the use of a reference electrode at a fixed potential is a standard way to measure overpotential of a specific electrode in liquid electrochemical systems. However, application of such three-electrode configuration to solid electrochemical cells for overpotential determination is not straightforward and requires extra caution. Here we report a theoretical Finite Element Analysis on the geometrical requirements for which the reference electrode can be applied to anode- or electrolyte-supported solid oxide button cells. The modeling results suggest that the symmetry of the working and counter electrodes is the key factor determining if a reference electrode is suitable to use. For anode-supported fuel cells with asymmetrical working and counter electrodes, reference electrode cannot be used under all circumstances. To use reference electrode for overpotential measurements, electrolyte-supported cells with symmetrical semicircular-shaped electrodes are preferred. A data processing procedure has also been presented to obtain the electrode overpotential from the measured potential using the three-electrode scheme in solid oxide electrochemical cells.

25 ENERGY STORAGE↗

Effect of Nickel-Phosphorus Interactions on Structural Integrity of Anode-Supported Solid Oxide Fuel Cells

An integrated experimental/modeling approach was utilized to assess the structural integrity of Ni - yttria-stabilized zirconia (YSZ) porous anode supports followed the solid oxide fuel cell (SOFC) operation on coal gas containing trace amounts of phosphorus impurities. Phosphorus was chosen as a typical impurity exhibiting strong interactions with the nickel followed by second phase formation. Tests were performed using Ni-YSZ anode-supported button cells exposed to 0.5-10 ppm of phosphine in synthetic coal gas at 700-800oC. The extent of Ni-P interactions was determined by a post-test scanning electron microscopy (SEM) analysis. Severe damage to the anode support due to nickel phosphide phase formation and extensive crystal coalescence was revealed, resulting in electric percolation loss. The subsequent finite element stress analyses were conducted using the actual anode support microstructures to assist in degradation mechanism explanation. Volume expansion induced by the Ni phase alteration was found to produce high stress levels such that local failure of the Ni-YSZ anode became possible under the operating conditions. These results emphasize the need for extensive coal gas cleanup when used as a fuel for SOFCs.

coal gas impurity↗

Stable perovskite-fluorite dual-phase composites synthesized by one-pot solid-state reactive sintering for protonic ceramic fuel cells

We report that this work synthesized a series of oxide composites with nominal compositions of BaCe 05 Zr 0.4 Y 0.1 O 3-δ (BCZY)-Ce 0.5 Y 0.5 O 2-δ (YDC) based on the BCZY/YDC molar ratios of 0.5:1, 1:1, 2:1, and 4:1 (BCZY-YDC-0.5–1, BCZY-YDC-1-1, BCZY-YDC-2-1, and BCZY-YDC-4-1) using a one-pot solid state reactive sintering (SSRS) method. The X-ray diffraction (XRD) patterns and refinement proved that the one-pot SSRS at 1450 °C for 12 h could achieve the perovskite-fluorite dual-phase composites (DPCs) with the desired structure compositions. The scanning electron microscopy (SEM) images showed that the two DPCs of BCZY-YDC-1-1 and BCZY-YDC-2-1 formed excellent percolation for perovskite and fluorite phases. The conductivity measurement by electrochemical impedance spectroscopy (EIS) and the transference number measurement by the electromotive force (EMF) test proved that changing the BCZY/YDC molar ratio and operating condition could adjust the DPC's conduction property to make them suitable for electrolytes and electrode scaffolds for protonic ceramic fuel cells (PCFCs). The long-term conductivity testing and the crystal structure analysis after EMF testing under versatile conditions indicated that the DPCs of BCZY-YDC-2-1 and BCZY-YDC-1-1 were durable PCFC component materials. The PCFC button cells with the as-discovered BCZY-YDC-2-1 and BCZY-YDC-1-1 as an electrolyte and an anode scaffold, respectively, and the reported Ba–Ce–Fe–Co–O perovskite-perovskite composite as a cathode showed promising performance under H 2 /air gradient.

08 HYDROGEN↗

Solid oxide electrolysis cell and stack testing best practices

Solid oxide electrolyzer (SOE) technology is an emerging method for hydrogen production, noted for its superior electrical efficiency. Despite the significant progress made in recent years, the broad development of SOE technology is often constrained by the necessary and extensive "skill of the craft" required to successfully test simple single cell test articles. This may be linked to the dearth of practical and pragmatic guidance within the literature for safe, reliable, and performant test equipment and test procedures. Researchers at the Idaho National Laboratory (INL) have been actively testing SOEs ranging from button cells to stacks up to 500 kW, in collaboration with industry and other national laboratories. Based on operational experience, INL has developed system design procedures that ensure safe and reliable operation of SOE systems with the level of support required for each test. This paper presents key aspects of SOE stack and system testing, including safe design procedures, balance of plant components design, and specific implementations at INL. Practical design details of reactants, heat, and power management are presented along with lessons learned from the SOE test facility operations at INL.

08 HYDROGEN↗

Mechanical and electrochemical performance of composite cathode contact materials for solid oxide fuel cells

The feasibility of adding glass or inorganic binder to conventional SOFC cathode contact materials (CCM) in order to improve bonding to adjacent materials in the cell stack is assessed. Two glasses (SEM-COM SCZ-8 and Schott GM31107) and one inorganic binder (Aremco 644A) are mixed with LSM particles to produce composite CCM pastes. These are used to bond Mn1.5Co1.5O4-coated stainless steel mesh current collectors to anode-supported button cells. The cells are operated at 800 C for about 1000 h. The cell with SCZ-8 addition to the CCM displays quite stable operation (3.9%/1000 h degradation), whereas the other additives lead to somewhat higher degradation rate. Bonding of the CCM to coated stainless steel coupons is also assessed. Interfacial fracture toughness is determined using a four-point bend test. The fracture toughness for LSM Schott glass (12.3 N mm 1), LSM SCZ-8 glass (6.8 N mm 1) and LSM 644A binder (5.4 N mm 1) are significantly improved relative to pure LSM (1.7 N mm 1). Indeed, addition of binder or glass is found to improve bonding of the CCM layer without sacrificing cell performance.