Search NASA⌕ Search

SEARCH · Search NASA

Results for “cable aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Review of nuclear power plant safety cable aging studies with recommendations for improved approaches and for future work.

Many U. S. nuclear power plants are approaching 40 years of age and there is a desire to extend their life for up to 100 total years. Safety-related cables were originally qualified for nuclear power plant applications based on IEEE Standards that were published in 1974. The qualifications involved procedures to simulate 40 years of life under ambient power plant aging conditions followed by simulated loss of coolant accident (LOCA). Over the past 35 years or so, substantial efforts were devoted to determining whether the aging assumptions allowed by the original IEEE Standards could be improved upon. These studies led to better accelerated aging methods so that more confident 40-year lifetime predictions became available. Since there is now a desire to potentially extend the life of nuclear power plants way beyond the original 40 year life, there is an interest in reviewing and critiquing the current state-of-the-art in simulating cable aging. These are two of the goals of this report where the discussion is concentrated on the progress made over the past 15 years or so and highlights the most thorough and careful published studies. An additional goal of the report is to suggest work that might prove helpful in answering some of the questions and dealing with some of the issues that still remain with respect to simulating the aging and predicting the lifetimes of safety-related cable materials.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Summary Report of Cable Aging and Performance Data for Fiscal Year 2014

As part of the Light Water Reactor Sustainability Program, science - based engineering approaches were employed to address cable degradation behavior under a range of exposure environments. Experiments were conducted with the goal to provide best guidance for aged material states, remaining life and expected performance under specific conditions for a range of cable materials. Generic engineering tests, which focus on rapid accelerated aging and tensile elongation, were combined with complementary methods from polymer degradation science. Sandia's approach, building on previous years' efforts, enabled the generation of some of the necessary data supporting the development of improved lifetime predictions models, which incorporate known material behaviors and feedback from field - returned 'aged' cable materials. Oxidation rate measurements have provided access to material behavior under low dose rate thermal conditions, where slow degradation is not apparent in mechanical property changes. Such data have shown aging kinetics consistent with established radiation - thermal degradation models.

Celina, Mathias C.↗

Determining Remaining Useful Life of Aging Cables in Nuclear Power Plants – Interim Study FY13

The most important criterion for cable performance is its ability to withstand a design-basis accident. With nearly 1000 km of power, control, instrumentation, and other cables typically found in an NPP, it would be a significant undertaking to inspect all of the cables. Degradation of the cable jacket, electrical insulation, and other cable components is a key issue that is likely to affect the ability of the currently installed cables to operate safely and reliably for another 20 to 40 years beyond the initial operating life. The development of one or more nondestructive evaluation (NDE) techniques and supporting models that could assist in determining the remaining life expectancy of cables or their current degradation state would be of significant interest. The ability to nondestructively determine material and electrical properties of cable jackets and insulation without disturbing the cables or connections has been deemed essential. Currently, the only technique accepted by industry to measure cable elasticity (the gold standard for determining cable insulation degradation) is the indentation measurement. All other NDE techniques are used to find flaws in the cable and do not provide information to determine the current health or life expectancy. There is no single NDE technique that can satisfy all of the requirements needed for making a life-expectancy determination, but a wide range of methods have been evaluated for use in NPPs as part of a continuous evaluation program. The commonly used methods are indentation and visual inspection, but these are only suitable for easily accessible cables. Several NDE methodologies using electrical techniques are in use today for flaw detection but there are none that can predict the life of a cable. There are, however, several physical and chemical ptoperty changes in cable insulation as a result of thermal and radiation damage. In principle, these properties may be targets for advanced NDE methods to provide early warning of aging and degradation. Examples of such key indicators include changes in chemical structure, mechanical modulus, and dielectric permittivity. While some of these indicators are the basis of currently used technologies, there is a need to increase the volume of cable that may be inspected with a single measurement, and if possible, to develop techniques for in-situ inspection (i.e., while the cable is in operation). This is the focus of the present report.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

New Technologies for Repairing Aging Cables in Nuclear Power Plants: M3LW-14OR0404015 Cable Rejuvenation Report

The goal of this project is to conceptually demonstrate techniques to repair cables that have degraded through subjection to long-term thermal and radiation exposure in nuclear power plants. In fiscal year 2014 (FY14) we focused on commercially available ethylene-propylene rubber (EPR) as the relevant test material, isolated a high surface area form of the EPR material to facilitate chemical treatment screening and characterization, and measured chemical changes in the material due to aging and treatment using Fourier Transform Infrared (FTIR) spectroscopy.

42 ENGINEERING↗

Temperature Dependence of FDR Response for Thermally Aged Low-Voltage Cables

Frequency Domain Reflectometry (FDR) has attracted significant attention for use in nuclear power plants (NPPs) for non-destructive cable health monitoring. However, cable aging detection using FDR faces challenges due to its high sensitivity to environmental factors such as temperature, vibrations, proximity to other cables, and so on. This work aims to evaluate the influence of measurement temperature on the FDR reflected signal in a low voltage cable undergoing accelerated thermal aging. A 100 ft long multi-core low-voltage unshielded power cable insulated with flame retardant ethylene propylene rubber (FR-EPR) and covered by a chloro-polyethylene (CPE) jacket was selected for this study. The cable was energized during aging by a 480 VAC 3-phase motor, and a 30 ft mid-section of this cable was routed through an air circulating oven held at 140 °C for up to an effective aging time of 62 days. FDR measurements were taken periodically with the oven on (at 140 °C) and with the oven off (at 22 °C). A comparative analysis of data collected at both temperatures showed that the FDR response was strongly dependent on measurement temperature. FDR measurements at ambient temperature showed large peaks corresponding to impedance changes in the aged section of the cable after 3 days of aging. These peaks continued to rise steadily with increasing aging time. However, for measurements taken at 140 °C, slowly rising peaks in the oven region (aged section) were observed only after a lead time of 23 days of aging. This work highlights the importance of measurement temperature on the performance of FDR as a condition monitoring tool for aging cables.

Sriraman, Aishwarya↗

Simultaneous Thermal and Gamma Radiation Aging of Cable Polymers

Polymers used in nuclear power plant electrical cable systems experience aging and degradation over time due to environmental stress including heat and gamma irradiation. Prediction of long-term cable performance has been based on results of short-term accelerated laboratory aging studies, but questions remain regarding the correlation of accelerated aging to long-term, in-plant aging. This work seeks to increase understanding of the combined effects of heat and radiation on cable polymer material aging toward addressing these questions.

Cable Aging↗

Dielectric and Mechanical Behavior of Thermally Aged EPR/CPE Cable Materials

Power and instrumentation cables play a crucial role in the safe operation of Nuclear Power Plants (NPPs). Thermal and other stressors present in the reactor environment cause the cable materials to degrade. In this work, dielectric and mechanical properties of cable insulation and jacket materials are studied as they are thermally aged, supporting development of non-destructive evaluation sensors for monitoring cable aging. Materials selected for this study are found in certain types of single-core unshielded power cables. These utilize ethylene propylene rubber (EPR)-based insulation material and chlorinated polyethylene (CPE)-based jacket material. Flat mats of these materials were obtained from the cable manufacturer and thermally aged at 140 °C in an air-circulating oven. Elongation-at-break was measured on tensile specimens stamped from the aged mats, and dielectric properties were measured from 100 Hz to 100 kHz using a parallel plate capacitor and precision LCR meter. In the case of aged EPR-based materials, rapid decrease in elongation at break indicating end of useful life was accompanied by a significant increase in dissipation factor, D, measured at 100 kHz. Capacitive measurement of D shows promise, therefore, as a non-destructive indicator of corresponding mechanical property changes in thermally-aged EPR-based insulation materials.

cable aging, nuclear cables, material degradation,↗

Extension of Cable Electrical Assessment Techniques to Detect and Discriminate Radiation Aging on Cable Insulation Systems (Abstract)

The purpose of this study of the electrical responses of gamma radiation aged low voltage nuclear cables is to advance tools to determine cable condition (extent of damage) and identify degradation location along the cable length. The developed technology will provide nuclear plant operators with the options to focus cable repair, mitigation, or replacement efforts locally and avoid wholesale cable replacement.

42 ENGINEERING↗

Radiation Aging of Cable Insulation Systems to Support Extension of Cable Electrical Assessment Techniques - CRADA 562 (Final Report)

Radiation aging (primarily gamma radiation) affects a small subset of the LV cable population based on a 40-year operation. Increasing plant operating life to 60 or 80 years will result in additional cables experiencing degradation, either from radiation or from combined thermal and radiation effects. Previous research work done by EPRI and other researchers focuses on electrical diagnostics of thermal effects. However, the electrical diagnostic response of the cable system to radiation aging is minimally understood. In order to study the electrical responses from XLPE and EPR cabling and correlate these responses with radiation dose and level of thermal exposure, gamma radiation testing was performed at Pacific Northwest National Laboratory (PNNL). This report covers the radiation testing performed at PNNL, which involved irradiation of 30-foot long cables and short witness samples. The cabling was irradiated, at room temperature, using cobalt-60 gamma-rays to intervals of 10 million rads (10 Mrads), for a maximum of 70 Mrads. The results can be used to determine cable conditions (extent of damage) more accurately and localize where the degradation exists along the length of the cable (axial location). These insights can provide operators with the options to focus repair, mitigation, or replacement efforts locally.

36 MATERIALS SCIENCE↗