Remaining Life Prediction of SNF Storage Canisters Exposed to CISCC Environments

• DOE Standardized SNF Storage Canisters o DOE designed standard spent nuclear fuel (SNF) storage canisters for storage of DOE SNF. o DOE canisters are significantly different from commercial MultiPurpose Canisters (MPC) in size. o MPC canisters are large, a height = 15.8 ft, OD = 68”, WT = 0.5”. o DOE canisters are small with 18” / 24” diameter, 10’ / 15’ length. • Integrity Evaluation of DOE versus MPC Canisters o Many investigations have been performed for MPC canisters. o Limit investigations were performed for DOE standard canisters. Most were done at Idaho National Lab (INL). o DOE has sponsored integrity studies to evaluate weld integrity using drop tests and FEA simulations. o No evaluation on CISCC/service life of DOE canister in literature. o MPC canister: 4 axial welds, 1 center girth weld, 2 closing welds.

ZHU, Xiankui↗

Flaw Tolerance Assessment for DOE Standard SNF Dry Storage Canisters - 26550

The U.S. DOE has designed four spent nuclear fuel (SNF) dry storage canisters for storing DOE standardized SNFs. The DOE standard canisters are cylindrical shells with a diameter of 24 inches (610 m) or 18 inches (457 m), a wall thickness of 0.5 inches (12.7 m) or 0.375 inches (9.53 m), and a length of 15 feet (4.57 m) or 10 feet (3.05 m). These DOE canister geometries are completely different from commercial canisters. The latter may experience chloride-induced stress cracking corrosion (CI-SCC) because they are stored near coastal regions. The former may not experience CI-SCC but face different challenges because they are stored in the SNF storage facilities. Because of large residual stresses, mechanical flaws may occur in the DOE canisters during long-distance transportation or lifting handling. To date, only limited structural integrity analyses were carried out through drop tests on the DOE canisters, but a more general flaw tolerance assessment has not been performed. Therefore, the failure assessment diagram (FAD)-based fracture mechanics method, as codified by the latest API 579-1/ASME FFS-1-2021 Edition, is adopted in this work to assess surface flaw tolerance for DOE canisters under operation loading and welding residual stresses (WRS), where the new code-recommended WRS distributions are used. To more adequately consider the transverse distribution of WRS, an equivalent WRS distribution is proposed to account for the WRS reduction with distance from the weld centerline. Moreover, the closed-form solutions of stress intensity factor K, which serves as the crack driving force during subcritical crack growth, are developed from the tabular data of the K factors provided in API 579-1/ASME FFS-1 and used to determine more accurate flaw sizes at flaw instability. Subsequently, the Level 2 assessment procedures with 12 assessment steps, as codified and detailed in API 579-1 and ASME FFS-1, are followed to assess the flaw tolerance for the surface flaws in the DOE standard canisters with consideration of normal or accident operation loads combined with WRS. The assessment results show that the four designs of DOE standard canisters can tolerate all surface flaws that meet the code permitted maximum sizes of a flaw length of 8 inches (i.e., 200 mm) and a flaw depth of 80% wall thickness. This demonstrates that all designs of DOE standard canisters are robust and reliable.

DOE standard canister↗

SNF Interim Storage Canister Corrosion and Surface Environment Investigations (FY2020 Status Report)

This progress report describes work performed during FY20 at Sandia National Laboratories (SNL) to assess the localized corrosion performance of container/cask materials used in the interim storage of spent nuclear fuel (SNF). Of particular concern is stress corrosion cracking (SCC), by which a through-wall crack could potentially form in a canister outer wall over time intervals that are shorter than possible dry storage times. Work in FY20 further defined our understanding of the potential chemical and physical environment present on canister surfaces, evaluated the relationship between the environment and the resultant corrosion that occurs, and initiated crack growth rate testing under relevant environmental conditions. In FY20, work to define dry storage canister surface environments included several tasks. First, collection of dust deposition specimens from independent spent fuel storage installation (ISFSI) site locations helped to establish a more complete understanding of the potential chemical environment formed on the canister. Second, the predicted evolution of canister surface relative humidity RH) values was estimated using ISFSI site weather data and the horizontal canister thermal model used by the SNL probabilistic SCC model. These calculations determined that for typical ISFSI weather conditions, seasalt deliquescence to produce MgCl2-rich brines could occur in less than 20 years at the coolest locations on the canister surface, and, even after nearly 300 years, conditions for NaCl deliquescence (75% RH) are not reached. This work illustrates the importance of understanding the stability of MgCl2-rich brines on the heated canister surface, and the potential impact of brine composition on corrosion processes, including pitting and stress corrosion cracking. In an additional study, the description of the canister surface environment was refined in order to define more realistic corrosion testing environments including diurnal cycles, soluble salt chemistries, and inert mineral particles. The potential impacts of these phenomena on canister corrosion are being evaluated experimentally. Finally, work over the past few years to evaluate the stability of magnesium chloride brines continued in FY20. MgCl2 degassing experiments were carried out, confirming that MgCl2 brines slowly degas HCl on heated surfaces, converting to less deliquescent magnesium hydroxychloride phases and potentially leading to brine dryout.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Radon-222 Charcoal Canister Steady State Model Calibrations Performed in a Highly Controlled Environmental Chamber and a Natural Indoor Environment

Charcoal canisters are a common method of 222 Rn screening. The calibrations of different batches of activated charcoal used in different canister designs are typically performed in large volume controlled environmental chambers with known and controlled radon concentration, temperature, and humidity. Radon screening could be facilitated in locations without ready access to environmental chambers if canisters could be accurately calibrated and undergo quality control in less controlled environments. This study compares charcoal canister calibrations from a highly controlled radon chamber with calibrations from a basement storage area experiencing temporally varying radon. In addition, the impacts of exposure time and spectral region of interest selection on calibration accuracy are investigated by comparing calibrations calculated using three different choices. Approximately 30 mo after calibrations were completed, groups of canisters were exposed for different durations of time to investigate measurement accuracy and calibration validity over an extended time. A digital simulation of charcoal canister kinetics was also performed to establish limits on how stable radon must be in a space for equilibrium-based calibration to be performed there. Overall, the accuracy of measurements using calibrations from each space differed by less than 10% after 2 d exposure time, showing that carefully controlled conditions are not necessary for the accurate calibration of charcoal canisters. Furthermore, measurement accuracy differed by less than 2% for different spectral region selections. Accuracy improved slightly with canister exposure duration. Simulations suggest that radon instability is most tolerable near the beginning of canister calibration exposures, but this merits further experimental study.

07 ISOTOPE AND RADIATION SOURCES↗

Acoustic sensing and autoencoder approach for abnormal gas detection in a spent nuclear fuel canister mock-up

Currently, spent nuclear fuel (SNF) from commercial nuclear power plants is stored in stainless-steel canisters for interim dry storage. To provide an inert environment, these canisters are backfilled with helium after vacuum drying. However, the helium environment may be contaminated during extended storage because of the material degradation. For example, the heavier fission gas xenon may be released from the fuel rods into the canister cavity should the fuel cladding be breached. Other gases such as air and water vapor may also be present as a result of leakage caused by chloride-induced stress corrosion cracking on the canister walls or by insufficient vacuum drying. Therefore, monitoring the gas composition can provide critical information about the health of SNF canisters. In this study, noninvasive testing was conducted on a 2/3-scaled SNF canister mock-up using acoustic sensing. Ultrasonic transducers were placed on the exterior surface of the canister to probe the gas composition. A dataset was collected by sealing the canister mock-up and introducing up to 1.53% argon or 1.29% air into the helium background gas. Three methods were used to detect changes in the gas composition: the time-of-flight (TOF) method, the differential method, and the autoencoder method. Results showed that the TOF method had sufficient resolution to detect abnormal gas concentrations of less than 1.0%. The differential method demonstrated a periodic in-phase and out-of-phase behavior between the benchmark (i.e., pure helium) and abnormal (i.e., with argon or air) state signals. The variational autoencoder (VAE) and the Wasserstein autoencoder (WAE) were trained on the benchmark data and were applied directly to the abnormal state data. It was found that both the unsupervised VAE and the WAE were able to distinguish the benchmark and abnormal states of the canister mock-up based on the reconstruction error.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Drop Analysis of Department of Energy Standard Canister with Fort Saint Vrain SNF

DOE manages over 300 types of SNF, most of which are located at the INL site. The Idaho Cleanup Project and INL are collaborating on the Road-Ready Capability Demonstration Project, which will develop and demonstrate the designs, technology, processes, and regulatory framework for packaging DOE-managed SNF at the INL site for ?road-ready dry storage?. ?Road-ready dry storage? is a SNF management concept where SNF is packaged into dry and sealed canisters, which are then placed in on-site storage in anticipation of later transportation. The forward-looking goal of the Demonstration is establishing the foundation for a large-scale road-ready dry storage program at the INL site. The Demonstration will first package Fort Saint Vrain SNF currently stored at INL into several DOE Standard Canisters. These Standard Canisters will then be loaded into another commercial transportation or storage containment system (e.g., storage cask or transportation package). The Standard Canister is a class of standardized canisters designed for containing the large variety of DOE-managed SNF during interim storage, transportation and/or disposal at a geological repository. One critical aspect of road-ready dry storage is the ability to license the DOE Standard Canisters and its associated transportation package to 10 CFR 71. Depending on the SNF and transportation strategy, the Standard Canisters may have to maintain structural integrity under normal conditions of transport and hypothetical accident scenarios (i.e., drop events). The Standard Canisters have been tested and analyzed under various SNF loading configurations and accident drop events in support of the Idaho Spent Fuel Facility and other DOE programs. However, no analysis has been completed to support the recent Demonstration. This analysis will consider the Ø0.5 m × 5.1 m Standard Canister under drop scenario(s) considered in previous INL tests and analyses, including the 9 m drop at 80 degree off vertical. However, this analysis will consider the more recent Fort Saint Vrain loading configurations proposed for the Demonstration. This analysis will performed using strain-based acceptance criteria established by the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Section III, Division 3. It will be compared to previous analyses and form the foundation of further formal calculations that will be used to support licensing efforts of the road-ready dry storage system at INL.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

An Assessment of Potential Dose Impacts from External Contamination on Naval Reactors Facility Waste Canisters (Special Analysis)

This Special Analysis (SA) was performed to address a request by Naval Reactors Facility (NRF) Waste Programs for a permanent exception to limits of removable surface contamination on the exterior of waste canisters shipped to the Remote-Handled Low-Level Waste (RHLLW) Disposal Facility as specified in the waste acceptance criteria (WAC) (PLN-5446). The purpose of this SA is to determine if the NRF-requested levels for removable surface contamination on the exterior of all NRF waste canisters is within the bounds of the current performance assessment (PA). This was done by calculating the groundwater all-pathways dose contribution from surface contamination on the exterior of NRF canisters for the following cases: (1) the exteriors of all NRF waste canisters are contaminated to the 10 CFR 835 Appendix D allowable limits in the current WAC, and (2) the exteriors of all NRF waste canisters are contaminated to the limits requested by NRF Waste Programs. Dose impacts for each case were compared to each other and to the all pathways dose for the PA base case. Dose impacts were also compared to the all pathways dose limit specified in DOE O 435.1. A simple assessment of the potential impacts of the increase in surface contamination using the NRF-requested limits on the biotic, air, and inadvertent intruder pathways was also performed. Based on the results of this SA, the increase in canister exterior contamination limits requested by NRF are well within the bounds of the current PA and will not result in a violation of performance objectives. The results also show the increased limits do not reflect or necessitate a fundamental change to the PA conceptual model, nor a change to the way exterior contamination is not included in PA dose calculations. Therefore, it is recommended the NRF request for an exception to the current limits for external surface contamination be accepted and the revised limits for NRF-generated waste canisters be added to the WAC. The monitoring plan will also be revised to identify external canister contamination as a potential mobile source term that may be detected by monitoring earlier than potential releases from waste. The PA, composite analysis (CA), closure plan, and PA/CA maintenance plan do not require revision. Recommendations are also included for inclusion of NRF procedures used to limit water pool radionuclide variability (and thus canister surface contamination variability) to the waste generator certification process.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Preliminary Modeling of Chloride Deposition on Spent Nuclear Fuel Canisters in Dry Storage Relevant to Stress Corrosion Cracking

This study presents a method that can be used to gain information relevant to determining the corrosion risk for spent nuclear fuel (SNF) canisters during extended dry storage. Currently, it is known that stainless steel canisters are susceptible to chloride-induced stress corrosion cracking (CISCC). However, the rate of CISCC degradation and the likelihood that it could lead to a through-wall crack is unknown. This study uses well-developed computational fluid dynamics and particle-tracking tools and applies them to SNF storage to determine the rate of deposition on canisters. The deposition rate is determined for a vertical canister system and a horizontal canister system, at various decay heat rates with a uniform particle size distribution, ranging from 0.25 to 25 µm, used as an input. In all cases, most of the dust entering the overpack passed through without depositing. Most of what was retained in the overpack was deposited on overpack surfaces (e.g., inlet and outlet vents); only a small fraction was deposited on the canister itself. These results are provided for generalized canister systems with a generalized input; as such, this paper is intended to demonstrate the technique. This study is a part of an ongoing effort funded by the U.S. Department of Energy, Nuclear Energy Office of Spent Fuel Waste Science and Technology, which is tasked with doing research relevant to developing a sound technical basis for ensuring the safe extended storage and subsequent transport of SNF. This work is being presented to demonstrate a potentially useful technique for SNF canister vendors, utilities, regulators, and stakeholders to utilize and further develop for their own designs and site-specific studies.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Analysis of spent nuclear fuel multipurpose canister dynamics during rail transportation

The primary mode of spent nuclear fuel transportation within the United States will be by railcar. One such system is the Atlas railcar, which is designed to transport 17 different spent nuclear fuel cask systems, including bare fuel systems and canister fuel systems. In the latter configuration, multipurpose canisters containing spent nuclear fuel may be placed within an overpack for storage, or within a cask for transportation. Compared to bare fuel systems, canister fuel systems have additional degrees of freedom for motion during transportation, because clearance between the cask and canister allows for some motion of the canister to occur relative to the cask. This work investigates the effect of canister motion on the shock and vibration imparted to the spent nuclear fuel within. Structural dynamic analyses have been conducted to identify the effects of canister to cask clearance, presence and type of dunnage, and loading direction and frequency. This modeling study calculates anticipated cask motion, canister motion, and spent nuclear fuel structural dynamic response to normal conditions of transportation railcar motion using finite element analysis methods that were developed to model the rail segment of the ENSA/DOE (Equipos Nucleares S.A., U.S. Department of Energy) multimodal transportation test of 2017.

SNF, UNF, LS-DYNA, dynamics, kinematics, shock, vi↗

Bounding Pressure and Flammability Evaluations of Aluminum-Clad Spent Nuclear Fuel Department of Energy Standard Canisters

This paper presents bounding pressure and flammability evaluations for DOE Standard Canister loaded with DOE-managed aluminum-clad spent nuclear fuel (ASNF). The objective of these evaluations is to gain confidence in the safety and feasibility of possible loading configurations for extended (>50 years) periods of dry storage, with particular focus on the dry storage canister pressures and potential for formation of a flammable atmosphere. The primary concern about the extended dry storage of ASNF is radiolytic gas generation. The aluminum cladding of these materials tends to corrode, and these corrosion products—typically aluminum oxides, such as boehmite, bayerite, or gibbsite—could carry water. This makes ASNF dry storage canisters difficult to dry. The gamma radiation field in dry storage environments could cause a radiolytic breakdown of residual water, forming chemical species such as molecular hydrogen (H2). The release of these species could increase the canister pressure and lead to the generation of a flammable canister atmosphere. The bounding evaluations presented within this study surmise conservative, but credible, conditions and processes. This includes the assumption of a full breakdown of a large quantity of free, physisorbed, and chemisorbed water (bound in a trihydrate, i.e., Al2O3 • 3H2O, layer). The considered dry storage configurations include a ~3 m (10 ft) long, ~46 cm (18 in) diameter (10 x 18) DOE Standard Canister loaded with 32 Advanced Test Reactor (ATR) ASNF elements, and a ~3 m (10 ft) long, ~61 cm (24 in) (10 x 24) diameter DOE Standard Canister loaded with 40 ATR ASNF elements. While the results of this study indicate the possibility of atmospheric hydrogen concentrations above the lower flammability limit, insufficient concentrations of oxygen will prevent the formation of flammable atmospheres. The maximum credible pressures remain well within the structural limits of the DOE Standard Canister.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Multiphysics modeling of a critical dual-purpose canister in a saturated geological repository

Dual purpose dry cask storage canisters for spent nuclear fuel are designed for storage and transportation, but are not licensed for permanent disposal in a geological repository. If dual purpose canisters were to be used to dispose of spent nuclear fuel in a geological repository, they would be expected to eventually breach and be flooded with groundwater, and it is shown that some fraction of these canisters will achieve criticality. In order to evaluate the consequences of canisters going critical in a repository, an initial capability has been developed for estimating the quasi-static power level of a critical canister using loosely coupled multiphysics simulations. The low power level in a critical canister enables coupling through precomputed physics proxies. This calculated power level is then used to compute the change in the critical canister’s isotopic inventory as a function of time. Three as-loaded canisters are evaluated and two were found to have power levels below 4 kW, with a modest effect on the radiological inventory over time. This effort also shows that although some DPCs will have extremely peaked power shapes, the relatively low power and long-time scales result in relatively homogenized thermohydraulic properties in the water within the DPC.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Sensitivity study of coupled chemical-CFD simulations for analyzing aluminum-clad spent nuclear fuel storage in sealed canisters

We report the United States Department of Energy (DOE) manages over 50 Metric Tons Heavy Metal (MTHM) of aluminum-clad spent nuclear fuel. One main source for DOE’s Aluminum-clad spent nuclear fuel (ASNF) inventory is the advanced test reactor (ATR) at the INL site, which makes this fuel of particular interest for storage scenarios. Road-ready and final disposition packaging configurations for the ATR fuel dictates storage within helium-backfilled, sealed DOE standard canisters. The conditions within these sealed canisters for extended (greater than50 year dry) storage is of interest. To further this goal, a three-dimensional (3D) multi-physics computational fluid dynamics (CFD) model is developed of the sealed DOE standard canisters. This 3D CFD model is one-way coupled with bulk gas radiolysis reactions considering sealed canisters with inert gas and possible trace amounts of air and water vapor. This study looks at the evolution of the thermal history of the canisters over a 50 year time period with a coupling to the chemical reactions occurring from radiolytic breakdown of residual water. A sensitivity study is then carried out over the parameters of the model including the fuel decay heat, residual water content, sealed pressure, canister external temperature, and canister emissivity. In pure helium, hydrogen generation rates are low, under 10 ppm, but hydrogen generation rates are affected greatly by the presence of even 1% residual air, increasing by 50-plus-fold, and nitric acid generation with residual air also occurs ranging from 500 to 4000 ppm after 50 years. The fuel decay heat and the residual water content show the most importance in the generation of hydrogen gas in pure air, and for nitric acid with a residual air condition. External temperature, canister emissivity and sealed pressure all show minor sensitivity effects to the generation of potentially harmful species.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of Residual Water on Storage Canister Internal Components

This report describes an evaluation of the spent nuclear fuel cladding and canister internal materials’ corrosion/oxidation due to (inadvertent) residual free water inside a dry storage canister post-dryout. Drying of spent nuclear fuel (SNF) and the impact of (inadvertent) residual water in a SNF canister is being addressed under the DOE-NE Spent Fuel and Waste Science and Technology (SFWST) program to ensure the safe extended dry storage and transportation of commercial SNF. A long-standing understanding has been that the amount of residual water in a storage canister after vacuum drying is not expected to be much more than trace amounts of 0.43 gram mole. However, recent findings from the High Burnup Demonstration project, and an Integrated Research Project show that residual free water well above the amount of approximately 0.43 gm-moles that had been assumed for a 3 torr rebound pressure, may remain within an SNF canister following prototypic drying. In fact, an NRC-NMSS sponsored study considered residual water amount as high as 55 moles. Considering the recent findings and the NRC-sponsored work, this present work was conducted to study the effects of unspecified amount of residual water on oxidation and corrosion of canister internals, i.e., it was assumed that the residual water amount is not limiting. It was assumed that the spent nuclear fuel content in the canister is not exposed to the internal environment, i.e., the packaged canister does not contain any damaged (breached) fuel.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Modeling DOE Standard Canister Configurations with Updated Surface Chemistry

Road-ready and final disposition packaging configurations for the advanced test reactor (ATR) fuel currently specifies storage within helium backfilled DOE sealed standard canisters. The aluminum cladding of the ATR fuel contains an oxyhydroxide layer of boehmite/bayerite that generates hydrogen when subjected to irradiation. Understanding the effect of this hydrogen buildup over time to important for long term storage considerations. Previous modeling efforts have built a coupled CFD-chemical model to simulate the temperature gas phase concentrations within the DOE sealed standard canisters. These models have coupled the temperature conditions to both the gas phase radiolysis chemistry and the surface chemistry associated with the oxyhydroxide layer. Continued experimental work has identified trends for aluminum surrogate samples with oxyhydroxide layers for tests done at higher dose rates. At low initial doses a fast generation rate of hydrogen occurs which starts to roll over to a lower generation rate as the total dose applied in increased. A previous study created a small-scale chemical model was built to replicate a mini-canister surrogate system at SRNL as well as for the smaller capsule tests performed at INL. The previous iteration of the model utilized step function for its G-values for the hydrogen generation over a 200-year period. This model makes an update to the surface chemistry to account for theorized surface chemistry reactions allowing for oxygen to remain bounded to the oxyhydroxide layer. As additional experiments continue, the kinetic fits may be adjusted to adapt to new data. Three canister configurations are modeled – the base 18-inch, 15-foot DOR standard canister with 30 ATR fuel elements, an 18-inch, 10-foot DOE standard canister with 32 ATR fuel elements and a 24-inch, 10-foot DOE standard canister with 40 ATR fuel elements. In previous reports, the primary sensitivity of the canister conditions was identified as the decay heat of the fuel and the dried condition of the fuel. Only these parameters are studied in the report. For the nominal case with dried fuel, the hydrogen generation is only about 2%, so it is even less than the flammability limit if it were exposed to oxygen. For the densely packed 18-inch case the total hydrogen concentration is only around 4% with the nominal decay heat. For the densely packed 24-inch case the total hydrogen concentration is only 2.5%, roughly 20% higher than the original packing design, and still under flammability conditions if exposed to oxygen.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

CISCC Countermeasures for Spent Fuel Canisters in Concrete Casks

Aging management of spent fuel is an important issue worldwide. Chloride-induced stress corrosion cracking (CISCC) of welded canisters is particularly important for concrete casks, where it occurs in response to a combination of environmental, material, and residual stress factors. In this paper, we introduce a countermeasure to prevent the occurrence of CISCC by adjusting the flow rate of the cooling air into the concrete cask so that the canister surface temperature does not decrease below 100°C, which is a conservative deliquesce temperature threshold for CISCC occurrence. The flow adjustment device was installed in a cask model, and two tests were conducted under the heat rate conditions corresponding to those of an actual canister. In the first test, the device was operated under a condition where the canister surface temperature was below 100°C to verify whether it could increase the canister surface temperature to above 100°C. In the second test, the heat rate was decreased from a state where the canister surface temperature was above 100°C, to verify whether the device could maintain the canister surface temperature above 100°C. Good results were obtained in both cases. However, in the case of a low decay heat rate of spent fuel after extended dry storage, the temperature of the canister surface may decrease below 100°C even if no air supply is provided. Therefore, in this case, it may be necessary to take measures such as blocking air outlets.

Takeda, Hirofumi↗

The Hanford Lead Canister Collaboration

The Hanford Site, Management of the Cesium and Strontium Capsules (MCSC) Project is preparing to place cesium and strontium material into dry storage using stainless steel canisters that are housed inside vertical concrete casks. Part of the site’s aging management program is to use a spare canister system as a leading indicator canister to provide advance warning for signs of chloride induced stress corrosion cracking (CISCC) or any other kind of canister degradation that might take place over the system’s 300-year design life. The Hanford Lead Canister (HLC) will use electric heaters to simulate the decay heat of cesium and strontium to ensure the HLC simulates the environment and conditions the capsule-loaded systems will experience. In addition to being part of the site’s aging management program, the HLC is being made available for research and development that advances the industry regarding canister mitigation and repair (M&R). The HLC system closely resembles current spent nuclear fuel (SNF) dry storage systems, making the HLC useful for demonstrating technologies or performing research that is relevant to SNF canisters . Several organizations are collaborating to prepare the HLC, along with technical strategy, to perform the needed research and development activities, to include the Pacific Northwest National Laboratory (PNNL), Central Plateau Cleanup Company (CPCCo), and the Electric Power Research Institute (EPRI). In one example of this collaborative research, EPRI is planning to use the HLC to demonstrate in-situ M&R technologies under controlled conditions before the HLC is deployed at Hanford. There is a period of several years when the HLC will be available for canister M&R activity before it is deployed. This paper describes the development of the HLC, its role in the Hanford site’s MCSC Project aging management program, and some of the research activities that are planned for the HLC.

Klymyshyn, Nicholas A.↗

Structural, Criticality, and Radiation Dose Calculations to Support SNF Loading into a DOE Standard Canister

The DOE Standard Canister Demonstration Project includes the development of an internal support structure (ISS) for the 4.6-m-long and 45.7-cm-diameter canister. This study presents structural evaluations, criticality safety assessments, and dose rate calculations conducted within the scope of the ISS design process to support smooth canister loading operations and to ensure safe storage, transportation, and disposal of Peach Bottom 1 Core II (PB2) and Fort St. Vrain (FSV) SNF, currently stored at INL’s CPP-603 facility. The ISS includes a 316L stainless-steel basket that holds 12 PB2 SNF rods. The PB2 basket rests on top of six individual, 78.7-cm-long, 316L stainless-steel columns that are equally spaced and welded to the inner canister wall at the lower end of the shell. These columns represent the FSV basket and can hold one FSV SNF element. An A92014 T6 aluminum spacer disc is bolted to the bottom plate of the PB2 basket to vertically restrain the FSV SNF element after the PB2 basket is placed inside the canister above the FSV basket. The structural evaluations of the ISS followed applicable ASME BPVC.III.3 guidelines and included finite element (FE) analyses of the PB2 basket structure; analyses of welds and bolds; buckling analyses of selected components, and acceptability assessments of the expected basket deformations under loading operations. The criticality safety assessments used the Monte Carlo N-Particle (MCNP) software architecture Version 6.2, including ENDF/B-V continuous-energy cross-section libraries, considering intact SNF in a single storage overpack or two multistorage overpack configurations and intact or failed SNF configured for disposal. The dose rate computations are based on source terms taken from the DOE Spent Fuel Database. The isotopic composition was decay corrected for the year 2022 using the ORIGEN module in the SCALE suite. A 19-group photon spectrum and a 27-group neutron-source spectrum were generated and used in MCNP to calculate estimated dose-equivalent rates, both on DOE Standard Canister contact and at a radial distance of 1 m from the canister surface. The results of this study indicate a structurally sound system that can uphold its criticality safety functions throughout its intended operational phases. Furthermore, this study provides confidence that sufficient radiological protection is technically achievable.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Structural, Criticality, and Radiation Dose Calculations to support SNF Loading into a DOE Standard Canister

The DOE Standard Canister Demonstration Project includes the development of an internal support structure (ISS) for the 4.6-m long and 45.7-cm diameter canister. This study presents structural evaluations, criticality safety assessments, and dose rate calculations conducted within the scope of the ISS design process to support smooth canister loading operations and to ensure safe storage, transportation, and disposal of Peach Bottom 1 Core II (PB2) and Fort St. Vrain (FSV) SNF, currently stored at the CPP-603 facility of the INL. The ISS includes a 316L stainless steel basket that holds twelve PB2 SNF rods. Further, six individual, 78.7-cm long, 316L stainless steel columns are equally spaced and welded to the inner canister wall at the lower end of the shell. These columns represent the FSV basket and can hold one FSV SNF element. An A92014 T6 aluminum spacer disc is bolted to the bottom plate of the PB2 basket to vertically restrain the FSV SNF element after the PB2 basket is placed inside the canister on top of the FSV basket. The structural evaluations of the ISS followed applicable ASME BPVC.III.3 guidelines and included finite element (FE) analyses of the PB2 basket structure; analyses of welds and bolds; buckling analyses of selected components, and acceptability assessments of the expected basket deformations under loading operations. The criticality safety assessments used the Monte Carlo N-Particle (MCNP) software architecture version 6.2 including ENDF/B-V continuous energy cross-section libraries, considering intact SNF in a single storage overpack or two multi-storage overpack configurations, and intact or failed SNF configured for disposal. The dose rate computations are based on source terms taken from the DOE Spent Fuel Database. The isotopic composition was decay corrected for the year 2022 using the ORIGEN module in the SCALE suite. A 19-group photon spectrum and 27-group neutron-source spectra were generated and used in MCNP to calculate estimated dose-equivalent rates, both on DOE Standard Canister contact and at a radial distance of from the canister surface. The results of this study indicate a structurally sound system that can uphold its criticality safety functions throughout its intended operational phases. Further, they increase confidence that sufficient radiological protection is technically achievable.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗