Search NASA⌕ Search

SEARCH · Search NASA

Results for “cracking”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Determination of Constraint-Independent Crack Tip Opening Angle for Stable Crack Growth in High-Strength Ductile Steels

The crack tip opening angle (CTOA) is one of fracture toughness parameters that has been used for decades in describing large stable crack growth in thin-walled aerospace structures under the low-constraint conditions. Recently, the pipeline industry has developed a growing interest in using the CTOA parameter to serve as the minimum required fracture toughness to arrest dynamic crack propagation in modern gas transmission pipelines made of high-strength ductile steel. To meet this industrial need, the CTOA test standard ASTM E3039 was therefore developed for measuring the constant critical CTOA. ASTM E3039 recommends a drop weight tearing test (DWTT) specimen with a shallow crack for standard CTOA testing, but its CTOA may depend on the low constraint condition of the DWTT specimen at the crack tip. Verifying the constraint independence of the DWTT-measured CTOA thus becomes indispensable for applying CTOA toughness to the running fracture control in the pipeline design. For this purpose, the present paper evaluates critical CTOA values in a set of fracture toughness tests on single-edge notched bend (SENB) specimens with shallow and deep cracks, based on four CTOA estimation models. Among these, the Ln(P)-LLD linear fit model is similar to that recommended by ASTM E3039 for CTOA calculation. Fracture test data for X80 pipeline steel and HY80 structural steel were considered in the CTOA evaluation. The results showed that the four CTOA models were able to determine a constraint independent CTOA value for stable crack growth in the SENB specimens. As a result, a single, reliable, constant CTOA value could be determined regardless of the specimen geometry or the crack-tip constraint conditions. Therefore, the CTOA measured using ASTM E3039 is constraint-independent and transferable to use in cases of actual cracks propagating in gas transmission pipelines.

36 MATERIALS SCIENCE↗

Instability in dynamic fracture and the failure of the classical theory of cracks

Cracks, the major vehicle for material failure, undergo a micro-branching instability at ~40% of their sonic limiting velocity in three dimensions. Recent experiments showed that in thin systems cracks accelerate to nearly their limiting velocity without micro-branching, until undergoing an oscillatory instability. Despite their fundamental importance, these dynamic instabilities are not explained by the classical theory of cracks, which is based on linear elasticity and an extraneous local symmetry criterion to predict crack paths. We develop a two-dimensional theory for predicting arbitrary paths of ultrahigh-speed cracks, which incorporates elastic nonlinearity without extraneous criteria. We show that cracks undergo an oscillatory instability controlled by small-scale, near crack-tip, elastic nonlinearity. This instability occurs above an ultrahigh critical velocity and features an intrinsic wavelength proportional to the ratio of the fracture energy to the elastic modulus, in quantitative agreement with experiments. As a result, this ratio emerges as a fundamental scaling length assumed to play no role in the classical theory of cracks, but shown here to strongly influence crack dynamics.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

An Enhanced Virtual Crack Closure Technique for Stress Intensity Factor Calculation along Arbitrary Crack Fronts and the Application in Hydraulic Fracturing Simulation

The virtual crack closure technique (VCCT) is widely used for calculating energy release rates along crack fronts and modeling the propagation of cracks in solid materials. Although the VCCT formulation for smooth crack fronts has been sufficiently addressed in the literature, the application of VCCT to a nonsmoothed crack front with sharp corners warrants further investigation. In this study, we describe an enhanced VCCT to calculate energy release rates and stress intensity factors for cracks with arbitrary shapes in 3D domains discretized on structured grids. The formulations of the enhanced VCCT were developed and implemented into a multiphysics simulation environment capable of simulating crack propagation in the framework of linear elastic fracture mechanics. Comparisons with existing analytical/numerical solutions and other VCCT approaches were performed to verify the enhanced VCCT in terms of SIF calculation along nonsmoothed crack fronts. We then applied the enhanced VCCT to a hydraulically driven penny-shaped fracture problem to further demonstrate its capability to simulate nonsmoothed fracture propagation.

02 PETROLEUM↗

Stress corrosion crack initiation of alloy 600 in PWR primary water

Stress corrosion crack (SCC) initiation of three mill-annealed (MA) alloy 600 heats in simulated pressurized water reactor primary water has been investigated using constant load tests equipped with in-situ direct current potential drop (DCPD) measurement capabilities. SCC initiation times were greatly reduced by a small amount of cold work. Shallow intergranular (IG) attack and/or cracks were found on most high-energy grain boundaries intersecting the surface with only a small fraction evolving into larger cracks and IGSCC growth. Crack depth profiles were measured and related to DCPD-detected initiation response. Processes controlling the SCC initiation in MA alloy 600 are discussed. IN PRESS, CORRECTED PROOF, 05/02/2017 - mfl

alloy↗

A two-set order parameters phase-field modeling of crack deflection/penetration in a heterogeneous microstructure

Modeling of crack deflection/penetration or manifested as intergranular/transgranular fracture in polycrystals has long been a challenge in both fracture mechanics and materials science. A phase-field model formulated with two-set order parameters describing the crack field and the microstructure field respectively, is herein established to investigate the competition between crack penetration and deflection at an interface. The advantages of the proposed model are three-fold: (1) the fracture toughness of grain boundaries and/or interfaces, besides single crystal properties (e.g., Young’s modulus, Poisson ratio, and fracture toughness), can be automatically incorporated, (2) cohesive interfaces are treated in one phase-field framework in comparison with the integrated phase-field and cohesive zone model in which cohesive elements have to be manually placed at the interface, and (3) two-set order parameters enable to describe the concurrent crack propagation and microstructure evolution. The proposed model is validated by comparing the simulated critical deflection angles with the results from theoretical analysis of the linear elastic fracture mechanics and the experiments. The model is then applied to a heterogeneous Silicon Nitride polycrystal to determine the effect of interface fracture toughness on the intergranular/transgranular fracture transition and the effective toughness of the materials.

Chen, Hu↗

Crack Growth Rate and Large Plate Demonstration of Chloride-induced Stress Corrosion Cracking in Spent Nuclear Fuel Storage Canisters

This report describes the body of work involving testing and analyses performed in FY18 and FY19 at the Savannah River National Laboratory and at Korea University to determine chloride-induced stress corrosion crack (CISCC) growth rates in weldments of austenitic stainless steel plate material. The primary work involved: several separate crack growth rate test campaigns with new testing setups using laboratory-scale corrosion specimens; analyses to estimate the stress intensity factors for flaws postulated to be present in the residual stress fields of axial and circumferential weldments in a prototypic dry storage canister; and establishment of a “large plate” (approximately 51×46 cm with thickness 16 mm and weight about 30 kg) CISCC test that uses a plate with a circumferential weldment harvested from the Sandia National Laboratories’ full-size mockup dry storage canister. The tests for crack growth rate were conducted on ASTM E1861 bolt-load compact tension specimens in a setup designed to allow initially dried salt deposits to deliquesce and infuse the brine to the crack front under conditions relevant to the canister storage environments (e.g., temperature and humidity). The crack growth rate test results matched previous experimental data in the open literature. These literature data had been compiled by SNL and EPRI to develop a temperature-dependent (K-insensitive) crack growth rate model to support flaw disposition in the ASME Boiler and Pressure Vessel Section XI Code Case N-860, “Examination Requirements and Acceptance Standards for Spent Nuclear Fuel Storage and Transportation Containment Systems.” The knowledge of the salt, temperature, humidity conditions for CISCC including the threshold stress intensity factor, $K_{ISCC}$, were used to setup the large plate test in which a set of partthrough- wall and through-wall electrical discharge machined (EDM) defects were positioned in the weld residual stress field of the welded plate material from the mockup canister. A salt solution was applied to this plate specimen with an air-brush spray, then dried, and then exposed to a constant 75% RH condition at an ambient room temperature of 22 °C. The salt loading and environmental condition is expected to be aggressive to cause CISCC. The visual results at the surface of the plate show corrosion product staining (brown rust appearance) but with no CISCC emanating from the machined notches after approximately 5 months exposure to date. The plate test will continue in FY20 and phased-array ultrasonic testing and other NDE techniques will be applied to identify and characterize CISCC that may emanate from the machined defects. The notches and any CISCC from them will be sectioned at the conclusion of the test to verify NDE characterization, and to develop effective through-wall crack growth rates from cracks that would likely be branched.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of temperature on the fatigue cracking mechanisms in A356 Al alloy

This work builds on our previous investigation of the room temperature fatigue cracking mechanisms of an A356 Al alloy. Here, we analyze the elevated temperature fatigue cracking mechanisms in cast and friction stir processed (FSP) A356, and contrast them with the room temperature behavior. Two sets of FSP parameters were used to modify the microstructure of the cast alloy. After heat treatment, both the FSPed microstructures exhibited severe abnormal grain growth (AGG) leading to a very wide grain size distribution (from a few microns to a few millimeters). During room temperature fatigue tests, the FSP conditions exhibited significant improvements in fatigue lives, even up to an order of magnitude. However, with increasing temperature, the difference in the performance of the FSPed and Cast microstructures decreased until, at 200 °C, all three microstructural conditions exhibited similar fatigue response. Detailed electron back scattered diffraction (EBSD) imaging of failed fatigue specimens was used to study crack behavior. At room temperature, cracks initiated at defect sites or along persistent slip bands (PSBs) and propagated transgranularly. The grain boundaries acted as barriers to crack growth. At elevated temperatures, there was a complete role reversal of the grain boundaries. Cracks initiated along grain boundaries and propagated intergranularly in all microstructures. Below, we explore this transition of the cracking mechanism in detail.

Nelaturu, Plalgun↗

Mesoscale-architecture-based crack evolution dictating cycling stability of advanced lithium ion batteries

The cracking phenomenon of Ni-rich NMC (LiNixMnyCo1-x-yO2, x = 0.6) secondary particles is frequently discovered and believed to be one of critical reasons deteriorating the long-term cycling stability of NMC cathode in lithium ion batteries (LIBs). However, the initiation and evolution of those cracks is still controversial due to the limited quantification especially by in situ monitoring, leading to the challenge of identifying an efficient approach to inhibit the formation of the fractures during repeated cycling. Herein, the irreversible, anisotropic cycling lattice and mesoscale expansion/shrinkage of nano-grain during the first cycle, as revealed by in situ X-ray diffraction (XRD) and in situ atomic force microscopy (AFM), have been quantified and confirmed to be the dominant driving forces of microcracks initiation at the grain boundaries. These microcracks preferentially nucleates at the core region with random oriented nano-grains in early stage. The further growth and aggregation of microcracks into macrocrack eventually results in microfracture propagation radially outward to the periphery region with more uniform nano-grain orientation. This mesoscale nano-grain architecture controlled cracking process highlight the importance of predictive synthesis of cathode materials with controllable multiscale crystalline architecture for high-performance LIBs.

25 ENERGY STORAGE↗

Decoupling the role of stress and corrosion in the intergranular cracking of noble-metal alloys

Intergranular stress-corrosion cracking (IGSCC) is a form of environmentally induced crack propagation causing premature failure of elemental metals and alloys. It is believed to require the simultaneous presence of tensile stress and corrosion; however, the exact nature of this synergy has eluded experimental identification. For noble metal alloys such as Ag–Au, IGSCC is a consequence of dealloying corrosion, forming a nanoporous gold layer that is believed to have the ability to transmit cracks into grain boundaries in un-dealloyed parent phase via a pure mechanical process. Here using atomic-scale techniques and statistical characterizations for this alloy system, we show that the separate roles of stress and anodic dissolution can be decoupled and that the apparent synergy exists owing to rapid time-dependent morphology changes at the dealloyed layer/parent phase interface. We discuss the applicability of our findings to the IGSCC of important engineering Fe- and Ni-based alloys in critical applications.

36 MATERIALS SCIENCE↗

The Effects of Carburization on the Fatigue Crack Growth Behaviors of Local Surface Cracks in Cylindrical Bars

In this study, a series of fatigue tests were conducted on C45 steel specimens with local surface cracks. The effects of carburizing treatment with different case depths were discussed under cyclic tensile and torsional loading. Moreover, the surface crack extension paths and crack propagation rates were discussed. In addition, the effects of additional static torsion under cyclic tensile loading and additional static tension under cyclic torsional loading were analyzed, and comparisons were made between the results of the carburized materials and those of the uncarburized materials. Some conclusions show that carburization can effectively retard crack extension and improve fatigue life. However, the improvement provided by the case depth on the fatigue life is limited to a certain range, and extensive case depths might decrease the fatigue strengths of materials. For the studied material, carburization had a more direct influence on the crack growth under cyclic tensile loading than cyclic torsional loading.

36 MATERIALS SCIENCE↗

Characterization of stress corrosion cracks in Ni-based weld alloys 52, 52M and 152 grown in high-temperature water

Ni-based weld alloys 52, 52M and 152 are extensively used in repair and mitigation of primary water stress corrosion cracking (SCC) in nuclear power plants. In the present study, a series of microstructure and microchemistry at the SCC tips of these alloys were examined with scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM), energy-dispersive X-ray spectroscopy (EDS), scanning transmission electron microscopy (STEM) and energy filtered transmission electron microscopy (EFTEM). The specimens have similar chemical compositions and testing conditions. Intergranular (IG) and transgranular (TG) SCC was observed in all of them. The cracks were filled with nickel-oxides and partial precipitations of chrome carbides (CrCs), niobium carbides (NbCs), titanium nitrides (TiNs) and silicon carbides (SiCs), while iron (Fe) was largely dissolved into the solution. However, the crack densities, lengths and distributions were different for all three specimens. - Highlights: • Microstructure and microchemistry at the SCC tips of Ni-based weld alloys 52, 52M and 152 were examined. • The crack densities, lengths and distributions were found to be different for different alloys. • IGSCC and TGSCC were observed on alloy 52, only TGSCC was observed on alloy 52M and 152. • The cracks were filled by Ni-oxides and precipitated CrCs, NbCs, TiNs and SiCs.

36 MATERIALS SCIENCE↗