Characterization of Damp-Heat Degradation of CuInGaSe2 Solar Cell Components and Devices by (Electrochemical) Impedance Spectroscopy
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
This paper summarizes our work with more details and an emphasis on the DH-induced degradation of Al-doped ZnO and Zn1-xMgxO alloys. The other two TCOs, ITO and F:SnO2, are not included here.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Abstract not provided
Abstract not provided
The extent of potential-induced degradation of crystalline silicon modules in an environmental chamber is estimated using in-situ dark I-V measurements and applying superposition analysis. The dark I-V curves are shown to correctly give the module power performance at 200, 600 and 1,000 W/m 2 irradiance conditions, as verified with a solar simulator. The onset of degradation measured in low light in relation to that under one sun irradiance can be clearly seen in the module design examined; the time to 5% relative degradation measured in low light (200 W/m 2 ) was 28% less than that of full sun (1,000 W/m 2 irradiance). The power of modules undergoing potential-induced degradation can therefore be characterized in the chamber, facilitating statistical analyses and lifetime forecasting.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
The objectives are: (1) To achieve a high long-term performance reliability for the thin-film CIGS PV modules with more stable materials, device structure designs, and moisture-resistant encapsulation materials and schemes; (2) to evaluate the DH stability of various transparent conducting oxides (TCOs); (3) to identify the degradation mechanisms and quantify degradation rates; (4) to seek chemical and/or physical mitigation methods, and explore new materials. It's important to note that direct exposure to DH represents an extreme condition that a well-encapsulated thin film PV module may never experience.
Commercial PV modules have various packaging choices nowadays, which influence their long-term reliability. This study compared the degradation behaviors of sixteen module variants from two brands with varying encapsulant materials (EVA or POE), encapsulant types, module architectures (GB or DG), and cell types (monofacial or bifacial) using null hypothesis testing to determine statistical significant findings. The modules were exposed for 2,520 hours under two accelerated exposures: modified damp heat (mDH) and modified damp heat with full-spectrum light (mDH+FSL). For both brands, two DG module variants with UV-Cutoff rear encapsulant are found to have significantly lower average power loss than the module variants of EVA+GB with opaque rear encapsulant after each accelerated exposure. Metallization interconnect corrosion is identified as the primary degradation mechanism. Furthermore, unsupervised hierarchical clustering finds that the degradation behaviors of modules from one brand with a more strict manufacturing quality control depends on module architectures only.
We report that the backsheet in photovoltaic modules belongs to an important class of layered materials where the tearing behavior of the individual layers does not necessarily represent the tearing behavior of the entire backsheet. Such characteristic arises from the interaction between the individual layers during the tearing process, where one layer of the backsheet is mechanically constrained by its neighboring layers and the layers may debond from each other. The mechanical constraint and debonding change the amount of energy dissipated during tearing and affect the overall tearing energy. In this article, we exposed a wide selection of backsheets with polymers including ethylene-vinyl acetate (EVA), polyethylene terephthalate (PET), polyvinylidene fluoride (PVDF), and ethylene tetrafluoroethylene (ETFE) to damp heat (85°C/85%RH) for up to 2000 hours. We report on the effect of damp heat on the tearing energy as a function of damp heat exposure. We developed a model that describes the tearing energy of a layered structure by accounting for the tearing of the individual layers in the backsheet, the effect of mechanical constraint, and the adhesive debonding between the layers. Additionally, we explore the relationship between the microstructural change in the polymers which resulted from the damp heat exposure and the mechanical properties using modulated differential scanning calorimetry (MDSC), small and wide angle X-ray scattering (SAXS and WAXS), and tensile testing.
Heat conduction in metals is typically dominated by electron transport since electrons carry both charge and heat. In magnetic metals magnons, or spin waves, excitations of the magnetic order can be used to transport information. Heat conduction via magnons has been previously shown mostly for insulating magnets with low Gilbert damping and resulting long spin-wave lifetimes where conduction electrons cannot contribute. Here we show that thin films of properly optimized metallic ferromagnetic (FM) alloys show significant nonelectronic contributions to heat conduction, which furthermore depend on the direction of an applied magnetic field. These measurements are enabled by micromachined thermal isolation platforms optimized for thermal conductivity measurements of thin-film systems. Electrical conductivity measurements on exactly the same samples allow application of the Wiedemann-Franz relation, which shows large nonelectronic contributions to thermal conductivity for the cobalt-iron alloy with 25% Co. This composition has been shown to have exceptionally low damping for a metallic FM. The thermal conductivity of a 75-nm-thick film of the 25% Co alloy changes by more than 20% at some temperatures, while a reference sample with 50% cobalt that has much higher damping shows no field-direction dependence. Our measurements indicate that applied magnetic fields alter the magnon lifetimes in these films and that these magnons contribute to thermal conductivity in this metallic magnetic alloy with low Gilbert damping.
We report electrically conductive tape (ECT) was characterized and used to assemble shingled cell strings at low temperature to achieve high reliability Pb- and Ag-free interconnections. The volume resistivity for two considered ECTs are 0.13 ± 0.06 mΩ·cm and 0.47 ± 0.20 mΩ·cm and specific contact resistances, 6.85± 2.00 mΩ·cm 2 and 6.30 ± 0.37 mΩ·cm 2 using the emerging IEC 62788-8-1 Technical Specification for assessment of electrically conductive adhesives (ECA). Durability and performance of the technology in glass–glass mini modules were evaluated with temperature cycling, damp heat testing, and combined-accelerated stress testing (CAST). Through temperature cycling (-40°C to 85°C) applying five times the mini module short-circuit current in forward bias and in the multi climate CAST protocol, there was negligible degradation of fill factor after replacing connectors at the modules' cable leads; however, CAST resulted in short circuit current loss attributed to degradation in light collection by the cells, not the ECT. The IEC 61215-2 85°C, 85% relative humidity damp heat testing showed susceptibility of the HJT cells to effects of humidity in the electroluminescence intensity around the module perimeter that degraded power performance by 4% (relative). Contrasting the IEC 61215-2 qualification testing-based damp heat testing with CAST, factors such as the optical stress of CAST may precipitate the degradation of the modules whereas the humidity levels and duration of IEC 61215-2 damp heat testing may lead to excessive levels of humidity diffused into the modules, potentially resulting in degradation that is unrepresentative of the field.