Electroluminescence Analysis and Grading of Hail Damaged Solar Panels

We analyzed more than 4000 electroluminescence images of hail damaged solar panels from a cluster of houses in Texas. We enhanced the images for ease of analysis and classified the defects within each solar cell into categories of glass breakage, installer damage, inactive substrings, crack severity, interconnect wire problems, and whether the damage was likely caused by hail. From these statistics, we quantified each panel into five levels of hail damage for insurance claims, and four levels of overall quality for potential resale pricing. Here, we share here some statistics regarding the defects with the hope that the data is useful to others attempting to predict the invisible damage to systems based just on the easily observable glass breakage statistics.

14 SOLAR ENERGY↗

Evidence of Polarization‐Type Potential‐Induced Degradation (PID‐p) in the Field and Investigation of the Recovery Mechanism on Bifacial p ‐PERC Modules

This study investigates the polarization-type potential-induced degradation (PID-p) of bifacial glass/glass p-type passivated emitter rear contact (p-PERC) modules in the field and their recovery behavior. Modules were installed with three mounting configurations providing different albedo conditions. System voltage (–600, –1500, and +1500 V) was applied to the cell circuits, with respect to the grounded module frames. No degradation was observed for positively biased modules, but PID-p was identified on the rear side when cells are negatively biased, with maximum power dropping during the first days and stabilizing at values up to 8% loss. Electroluminescence images revealed a variation of the cells' PID-p susceptibility within a module. Three parameters were shown to impact the degradation rate: rear albedo light, voltage, and wetness conditions. Degraded modules were recovered either by (1) a positive bias (+1500 V), (2) outdoor illumination with the front side facing sun, (3) outdoor illumination with the rear side facing sun, or (4) dark storage. A recovery pattern was identified with I–V parameters decreasing to a local minimum before increasing to full recovery. The proposed mechanism is based on the band bending at the rear p-type Si/AlO x/SiN x interface, going from inversion to depletion and accumulation states. Full recovery was achieved in 2–7 h for the modules recovered with the rear side facing sun, four to eight nights for the modules positively biased at night, and 10–20 days for the modules with the front side facing sun. Dark storage showed slower recovery rates as I–V parameters were not improving even after 1 month. Here, the recovery rates were correlated with the net Coulombs transferred during the preceding PID stress: When more Coulombs are transferred during the degradation, the extent of degradation is greater, leading to slower recovery rates.

14 SOLAR ENERGY↗

Multiscale Characterization of Photovoltaic Modules—Case Studies of Contact and Interconnect Degradation

The current popularity of photovoltaic (PV) systems is due in large part to their exceptional reliability and significantly lower cost than other energy sources. Studying cell and module degradation is key to promote further development in the state of the art. Fielded or accelerated aged modules exhibit different failure modes, of which metallization degradation (contacts and interconnections) is prevalent. In this work, we discuss how multiscale characterization methods can be applied to a variety of module technologies that have been field exposed and have undergone accelerated age testing. These methods include performing characterization on the module level, cell level, and finally the materials level. The observed performance losses from the module- and cell-level characterization can be correlated with materials properties to find out the root cause of degradation. We recommend an initial nondestructive characterization suite, including module- and cell-level current-voltage ( I--V ), Suns-V OC , photoluminescence and electroluminescence imaging, quantum efficiency, ultraviolet fluorescence imaging, and thermal infrared imaging. Samples are then extracted from particularly degraded regions of the module and prepared for materials characterization techniques, such as top-down and cross-sectional scanning electron microscopy, energy-dispersive X-ray spectroscopy, X-ray photoelectron spectroscopy, secondary ion mass spectrometry, Raman spectroscopy, and transmission electron microscopy, allowing a deeper look into the mechanism behind the metallization degradation. This article serves as an instructional review to introduce the different multiscale characterization methods and how they can be effectively applied to perform PV degradation studies. Furthermore, we also share some of our examples and discuss the strengths, limitations, and best practices for each of the characterization techniques.

14 SOLAR ENERGY↗

Characterization of Field-Exposed Photovoltaic Modules Featuring Signs of Contact Degradation

Here, this work investigates several photovoltaic (PV) modules that have shown signs of metal contact corrosion due to field exposure in a hot and humid climate. This includes two multicrystalline silicon aluminum back surface field systems with 10 and 14 years of exposure and one monocrystalline silicon passivated emitter and rear cell system with four years of exposure. A comprehensive, multiscale characterization process is used to evaluate these PV modules in great detail. Current–voltage (I−V), Suns-V OC measurements, electroluminescence imaging, infrared imaging, and ultraviolet fluorescence imaging were performed, and locations of interest were cored and analyzed using cross-sectional scanning electron microscopy (SEM). A rigorous, quantitative analysis procedure for the cross-sectional SEM images is proposed and implemented. Careful characterization does reveal that some of these PV modules do indeed exhibit the same classic signs of acetic-acid-based corrosion of the glass frit that is present at the silver/silicon interface, which have been observed previously in PV modules exposed to damp heat in an environmental chamber.

14 SOLAR ENERGY↗

A New UV Spot Test for Quality Control

Here, we present a fast, low-cost ultraviolet (UV) spot test to screen photovoltaic modules for UV-induced degradation (UVID). The measurement is based on a fiber-coupled arc lamp that delivers a highly accelerated local UV dose-approximately five years of equivalent field exposure in less than a day. Spot-exposed areas are evaluated using electroluminescence imaging. We test a “known bad” product, which was observed to experience UVID in the field, and a “known good” product which did not exhibit UVID in the field. Results indicate that the method may be useful as a quick and relatively inexpensive quality control screening tool for customers and manufacturers.

14 SOLAR ENERGY↗

Extended Accelerated Stress Testing of Lamination-Free Edge-Sealed Photovoltaic Minimodules

Lamination-free minimodules are constructed with silicon solar cells between glass sheets and an edge seal of polyisobutylene and silicone. These samples are stressed using a repeated sequential testing sequence including ultraviolet-containing simulated solar spectrum light exposure at elevated temperature, damp heat, humidity freeze, and thermal cycling adapted from the International Electrotechnical Commission (IEC) TS 63209-2:2022. The minimodule performance throughout the stressing is characterized by flash testing and electroluminescence imaging. Results are compared to conventional laminated minimodules using the same type of solar cells. The lamination-free minimodules experience up to 8% power loss compared to roughly 3% for the laminated versions. However, those losses, dominated by current and fill factor, are caused by glass soiling and busbar ribbon separation on the cells. When glass is replaced and the stressed cells are contacted with probes bypassing the delaminated ribbons, the initial performance is recovered, and overall losses of the lamination-free samples become negligible.

14 SOLAR ENERGY↗

Different Damp-Heat-Induced Series Resistance Degradation Behaviors in Fielded Crystalline Silicon Photovoltaic Modules Due to Difference in Bill of Materials

This case study investigates mono-crystalline silicon modules from underperforming portions of a utility-scale photovoltaic power plant. Field-collected I-V curves and electroluminescence imaging suggested that increased series resistance was a primary factor driving module degradation. Selected modules were removed from the field for further analysis, including incremental damp heat accelerated testing, which confirmed a progression in series resistance degradation. Two distinct cell degradation behaviors became apparent during the investigation. Cross-sectional scanning electron microscopy (with elemental analysis) and scanning spreading resistance microscopy identified key differences between the two degradation mechanisms, primarily grid finger width and contact resistance. Additionally, the study highlights the reliability implications of retest requirements in International Electrotechnical Commission 61215 for material changes and how they may have mitigated the degradation observed at this site.

14 SOLAR ENERGY↗

Capacitance Transients, Photoconductive Decay, and Impedance Spectroscopy on 19% to 22% Efficient Silicon Solar Cells

High efficiency silicon solar cells are characterized using current-voltage curves, electroluminescence imaging, impedance spectroscopy, capacitance transients, microwave photoconductive decay, and time-resolved photoluminescence imaging. The sample set is composed of cells from different manufacturers and includes an n-type silicon heterojunction (SHJ), an n-type passivated emitter rear totally diffused (PERT), and five different p-type passivated emitter rear contact (PERC) cells. Carrier lifetimes, both photoconductivity and photoluminescence, are measured co-located with the light excitation pulse and within the cell but away from the light spot. Luminescence intensity and excess carrier lifetimes correlate to cell voltage. The capacitance transient time constants correlate to the capacitance values extracted from impedance spectroscopy.

capacitance↗

Novel Solar Panel Defect Detection Hardware and Defect Analysis Software (CRADA Final Report)

The CRADA work involved 1) the development of a machine learning software architecture to automatically detect defects within Electroluminescence images of solar panels, and 2) demonstrations of the usefulness of UV Fluorescence (UVF) defect detection for a wide variety of defect types across many different solar panel technologies with different field or environmental chamber histories.

14 SOLAR ENERGY↗

Comparative Analysis of Hotspot Stress Endurance in Pristine and Thermal Cycled Prestressed Glass–Glass Photovoltaic Modules

Hotspots pose a significant long-term reliability challenge in photovoltaic (PV) modules that can have a detrimental impact on the efficiency, safety, and financial viability of a PV system. This paper aims to evaluate the endurance of hotspot stress in pristine and prestressed glass–glass (GG) modules. The accelerated prestressing was conducted for 600 thermal cycles (TC600) to represent decades of field exposure. GG modules are quickly becoming an alternative to the traditional glass–backsheet (GB) modules that have been the industry standard. Unlike other conventional studies that subject only pristine modules to hotspot stress, this paper evaluates the performance of an accelerated/simulated field-aged GG module (using TC600) and a pristine GG module. Pre- and post-characterizations were performed before and after each test to determine changes in electrical performance and observe any defects in GG modules. During the hotspot test, an approximately 200 °C maximum cell temperature was observed with a cell shading of 25% (the worst-case shading ratio). After the hotspot test, electroluminescence imaging indicated that most cells in the prestressed GG module exhibited severe damage whereas no significant defects were evident in the pristine GG module where the prestressed GG module degraded 8.2% and the pristine GG module degraded 1.5% in maximum power. These findings are critical for the industry, considering that GG bifacial modules will dominate the market.

14 SOLAR ENERGY↗

Capacitance Transients, Photoconductive Decay, and Impedance Spectroscopy on 19% to 22% Efficient Silicon Solar Cells

High efficiency silicon solar cells are characterized using current-voltage curves, electroluminescence imaging, impedance spectroscopy, capacitance transients, microwave photoconductive decay, and time-resolved photoluminescence imaging. The sample set is composed of cells from different manufacturers and includes an n-type silicon heterojunction (SHJ), an n-type passivated emitter rear totally diffused (PERT), and five different p-type passivated emitter rear contact (PERC) cells. Carrier lifetimes, both photoconductivity and photoluminescence, are measured co-located with the light excitation pulse and within the cell but away from the light spot. Luminescence intensity and excess carrier lifetimes correlate to cell voltage. The capacitance transient time constants correlate to the capacitance values extracted from impedance spectroscopy.

capacitance↗

Bifacial Photovoltaic Module Degradation Dynamics

In a comprehensive study conducted at NREL's 75 kW bifacial single-axis-tracked field, accelerated degradation was observed in four out of five bifacial silicon photovoltaic (PV) module technologies when compared to their monofacial counterparts. Root cause analysis of accelerated bifacial degradation involved various analytical tools and techniques. This included employing RdTools to identify rates of power loss, conducting measurements on fielded and control modules using infrared imaging, electroluminescence (EL) and photoluminescence (PL), quantum efficiency (QE) analysis, IV-curves assessment, as well as utilizing handheld Raman and reflectance measurement targeted at anti-reflective coating. Most cases pointed to carrier lifetime degradation causing Voc loss and simultaneous Isc loss. In some cases, Isc further decreases likely due to optical effects from encapsulant degradation. The outcomes and methodologies employed in this investigation are documented in this publication. This study's significance is further emphasized by placing the findings within the broader context of the performance and degradation of various bifacial systems, as identified in the PV Fleets data.

bifacial↗

Fill Factor Loss in Fielded Photovoltaic Modules Due to Metallization Failures, Characterized by Luminescence and Thermal Imaging

Understanding the causes of photovoltaic module failure in the field can be achieved using spatially-resolved imaging tools in combination with current-voltage (IV) characterization. We evaluate 23 field-degraded modules by comparing their IV characteristics with module images obtained by electroluminescence, photoluminescence, UV-fluorescence, and dark lock-in thermography. We identify primarily metallization failures (metallization series resistance, solder point heating, broken fingers, disrupted interconnects) in these modules that has led to a severe drop in the fill factor and up to 35% power loss over only 2 years of deployment.

14 SOLAR ENERGY↗

Voltage mapping and local defects identification in solar cells using non-contact method

Electroluminescence, infrared imaging, and current–voltage curve techniques are used to detect and map underperforming cells in a photovoltaic module or the modules in a photovoltaic string. In this work, we present a non-contact electrostatic voltmeter technique to detect and map the underperforming spots in a cell and the cells in a module. This non-contact technique directly maps the charged surface voltage (671mV) of the superstrate glass, and it had an 11-mV difference with the voltmeter values (660mV). Another data set of voltage values obtained by electroluminescence images conversion into a voltage map showed a difference of 7mV with the non-contact voltmeter values. Further, the direct voltage values obtained at various good and poor-performing spots of the cells using this technique are 3.69V and 3.79V and are validated using the voltage values obtained in electroluminescence analysis and the difference in voltage obtained by the two techniques is determined to be less than 2%. In this work, we combine the strengths of two complementary techniques of the electrostatic voltmeter (strength: quantitative) and electroluminescence (strength: spatial mapping) to obtain a quantitative spatial mapping of defects. Furthermore, this work is extendable to detect the poor-performing modules in solar PV power plants.

14 SOLAR ENERGY↗

Exploring Capability of Multimodal Foundation Model for Image-based Fault Detection of Photovoltaic Modules

Multimodal Foundation Model (MFM), like ChatGPT and Gemini, have emerged as powerful tools for their exceptional natural language processing capabilities and their emerging potential in image analysis. This paper investigates the application of MFMs for photovoltaic (PV) fault detection through image analysis, focusing on ChatGPT 4.0 and Gemini 1.5 Pro. Three types of PV images and the corresponding common PV faults are detected: bird droppings using visible images, cell cracks via electroluminescence (EL) images, and hotspots using infrared (IR) images. Among the two models, Gemini 1.5 Pro demonstrated superior performance, achieving near-perfect results with an average F1 score of 0.97, consistently outperforming ChatGPT 4.0 in accuracy and reliability. Unlike traditional machine learning (ML) models, MFMs can operate in a zero shot manner that does not require additional training by the user, and the input images are not limited by size, angle, scope, or PV technology. The strong adaptability and user-friendliness make MFM a promising tool for analyzing PV images and advancing health monitoring for PV modules.

Li, Baojie↗

Multiscale Characterization of Electrode-Induced Degradation in Perovskite Solar Cells

The stability of metal-halide-perovskite (MHP) solar cells must be understood and improved for the commercial viability of MHP technologies. Here, we apply multiscale characterization methods to study degradation modes, specifically electrode corrosion, for p-i-n MHP partial device stacks and full devices that are stored in the dark under an inert atmosphere. Our multiscale characterization approaches include full-device electro-optical performance using current-voltage (JV) curves and spatial imaging with electroluminescence (EL) and photoluminescence (PL). We further correlate interface properties using cross-sectional Kelvin probe force microscopy, which maps the nanoscale electric field properties, and electron microscopy, which demonstrates structural and chemical features. Devices stored as a full device stack degrade primarily by metal (Ag) electrode diffusion into the absorber, with formation of AgI byproducts and Ag accumulation near the indium tin oxide (ITO) contact. This causes decomposition of the perovskite absorber domains, loss of the potential drop at the electron transport layer (ETL)/perovskite interface near the metal contact, and increased equivalent resistance at the perovskite/hole transport layer (HTL) interface near the ITO contact. The devices stored without metal show a different degradation pathway dominated by corrosion of the ITO, creating voids at the ITO electrode surface with diffusion of In and Sn into the absorber. We conclude that metal electrode-induced degradation is the most severe degradation pathway under dark storage, but that ITO corrosion and absorber instability must also be mitigated. We further demonstrate mitigation of these degradation pathways by changes to the device stack, including a SnO x blocking layer at the ETL side and replacing ITO with FTO at the HTL side. These results provide a useful demonstration of specific dark degradation pathways at each electrode interface, as well as a unique multiscale example that links degradation of chemical, structural, and electrical interface properties to the full-device electro-optical characteristics.

14 SOLAR ENERGY↗

Mechanistic Insights to Degradation of PERC Minimodules with Differentiated Packaging Materials & Module Architectures

In this paper, we study the degradation behavior of glass-backsheet (GB) and double glass (DG) multicrystalline sil- icon monofacial PERC minimodules, fabricated using polyolefin elastomer (POE) and ethylene vinyl acetate (EVA) encapsulants, undergoing exposures of modified damp-heat (80 °C / 85% RH), with and without full spectrum light. The completed exposure time, at this time, is 1512 hours with each step of 504 hours. Step- wise measurements are conducted throughout exposures including current-voltage (I-V ) curves, Suns-V oc , electroluminescence (EL) images, and four-point proof loading with EL for tracking changes in mechanical properties in encapsulants by cell fracture probability. The results show that GB minimodules of both encapsulants, compared to DG minimodules, experience more changes in features of I-V and Suns-V oc measurements. There is no development of PV cell cracking during proof loading as seen from EL images and the load versus load line displacement plots currently.

14 SOLAR ENERGY↗