Low dielectric fluorinated poly(phenylene ether ketone) film and coating

The present invention relates to film and coating materials prepared from novel fluorinated poly(phenylene ether ketones). A fluorinated poly(phenylene ether ketone) is prepared by reacting a bisphenol with 1,1,1,3,3,3 hexafluoro-2,2-bis 4-(4-halobenzoyl) phenyl propane (wherein halo is fluoro or chloro), which is a novel monomer formed as the reaction product of halobenzene (wherein halo is fluoro or chloro) and 1,1,1,3,3,3 hexafluoro-2,2-bis (p-chloro formyl phenyl) propane. Especially beneficial results of this invention are that films and coating materials prepared from the novel fluorinated poly(phenylene ether ketone) are essentially optically transparent/colorless and have a lower dielectric constant than otherwise comparable, commercially available poly(phenylene ether ketones). Moreover, unlike the otherwise comparable commercially available materials, the novel fluorinated poly(phenylene ether ketones) of the present invention can be solution cast or sprayed to produce the films and coatings. Furthermore, the long term thermal stability of the polymers of the present invention is superior to that of the commercially available materials.

Cassidy, Patrick E.↗

Degradation of Perfluorinated Ether Lubricants on Pure Aluminum Surfaces: Semiempirical Quantum Chemical Modeling

The AM1 semiempirical quantum chemical method was used to model the interaction of perfluoroethers with aluminum surfaces. Perfluorodimethoxymethane and perfluorodimethyl ether were studied interacting with aluminum surfaces, which were modeled by a five-atom cluster and a nine-atom cluster. Interactions were studied for edge (high index) sites and top (low index) sites of the clusters. Both dissociative binding and nondissociative binding were found, with dissociative binding being stronger. The two different ethers bound and dissociated on the clusters in different ways: perfluorodimethoxymethane through its oxygen atoms, but perfluorodimethyl ether through its fluorine atoms. The acetal linkage of perfluorodimeth-oxymethane was the key structural feature of this molecule in its binding and dissociation on the aluminum surface models. The high-index sites of the clusters caused the dissociation of both ethers. These results are consistent with the experimental observation that perfluorinated ethers decompose in contact with sputtered aluminum surfaces.

Slaby, Scott M.↗

Infrared Band Strengths and Other Properties of Amorphous and Crystalline Dimethyl Ether

Laboratory astrochemists have generated infrared (IR) data for nearly all common classes of organic compounds, but ethers in the solid phase continued to be neglected despite detections of ethers in the interstellar medium by radio astronomers and uncertainty in how extraterrestrial ethers are formed. To address this paucity of data, here we present new mid-IR spectra of amorphous and crystalline dimethyl ether, (CH3)2O, the simplest member of its class. Spectral positions are tabulated and compared to previous results, but more importantly we also report IR band strengths and absorption coefficients, which we have not found in the literature and on which quantitative IR studies depend. Optical constants of amorphous and crystalline dimethyl ether also have been calculated. Some applications are described.

Hudson, Reggie L.↗

Mid-Infrared Spectra of Dipropargyl Ether Ices Revisited

The infrared (IR) spectrum of dipropargyl ether, (HCC-CH2)2O, has been reinvestigated for the compound's liquid, amorphous, and crystalline forms. The IR baseline changes and bandshape distortions seen in literature spectra have been considerably reduced by a different choice of conditions for preparing the crystalline solid, leading to the discovery of two crystalline phases of the ether. A spectrum of the liquid phase has been recorded and compared to that of the amorphous ether to check for possible procedural artifacts. To facilitate cross-laboratory comparisons, estimates are made for absorption coefficients of three IR peaks of the amorphous solid's spectrum. An interpretation is discussed for changes reported in spectral baselines and bandshapes on warming amorphous dipropargyl ether, and tests and predictions are described. The suggestion that the results from dipropargyl ether warming experiments might pose problems in applying Beer's Law to astronomical observations is addressed.

Hudson, Reggie L.↗

Improved boundary lubrication with formulated C-ethers

A comparison of five recently developed C-ether-formulated fluids with an advanced formulated MIL-L-27502 candidate ester is described. Steady state wear and friction measurements were made with a sliding pin on disk friction apparatus. Conditions included disk temperatures up to 260 C, dry air test atmosphere, 1 kilogram load, 50 rpm disk speed, and test times to 130 minutes. Based on wear rates and coefficients of friction, three of the C-ether formulations as well as the C-ether base fluid gave better boundary lubrication than the ester fluid under all test conditions. The susceptibility of C-ethers to selective additive treatment (phosphinic esters or acids and other antiwear additives) was demonstrated when two of the formulations gave somewhat improved lubrication over the base fluid. The increased operating potential for this fluid was shown in relationship to bulk oil temperature limits for MIL-L-23699 and MIL-L-27502 type esters.

Loomis, W. R.↗

Thermal and oxidative degradation studies of formulated C-ethers by gel-permeation chromatography

Gel-permeation chromatography was used to analyze C-ether lubricant formulations from high-temperature bearing tests and from micro-oxidation tests. Three mu-styragel columns (one 500 and two 100 A) and a tetrahydrofuran mobile phase were found to adequately separate the C-ether degradation products. The micro-oxidation tests yielded degradation results qualitatively similar to those observed from the bearing tests. Micro-oxidation tests conducted in air yielded more degradation than did tests in nitrogen. No great differences were observed between the thermal-oxidative stabilities of the two C-ether formulations or between the catalytic degradation activities of silver and M-50 steel. C-ether formulation I did yield more degradation than did formulation II in 111- and 25-hour bearing tests, respectively.

Jones, W. R., Jr.↗

Ketimine modifications as a route to novel amorphous and derived semicrystalline poly(arylene ether ketone) homo- and copolymers

A series of amine terminal amorphous poly(arylene ether ketone) oligomers of controlled molecular weights (2-15 K) were synthesized. These oligomers have been found to undergo 'self-crosslinking' reactions upon heating above 220 C, via the reaction of the terminal amine groups with the in-chain keto carbonyl functionalities. The resulting networks are ductile, chemically resistant, and nonporous. The networks obtained via generated ketimine functionality were characterized by solid state NMR. They have also been found to be remarkably stable toward hydrolysis. Ketimine functional bishalide monomers have also been synthesized. Such monomers have been utilized to synthesize a wide variety of amorphous poly(arylene ether) ketimine polymers. A high molecular weight hydroquinone functional poly(arylene ether) ketimine has been acid treated to regenerate a poly(arylene ether ketone) backbone in solution. This novel procedure thus allows for the synthesis of important matrix resins under relatively mild conditions.

Mohanty, D. K.↗

Tough poly(arylene ether) thermoplastics as modifiers for bismaleimides

Several aspects of research on thermoplastics as toughness modifiers are discussed, including the contribution of the backbone chemistry and the concentration of the poly(arylene ether) thermoplastic to fracture toughness, influence of the molecular weight of the poly(arylene ether) thermoplastic on neat resin fracture toughness, and the morphology of the thermoplastic modified networks. The results show that fracture toughness of brittle bismaleimide resins can be improved significantly with poly(arylene ether) thermoplastic levels of 20 percent by weight, and that high molecular weight poly(arylene ether) based on bisphenol A provides the highest degree of toughening. Preliminary composite evaluation shows that improvements in neat resin toughness translate into carbon fabric composite.

Stenzenberger, H. D.↗

LaRC-ITPI/arylene ether copolymers

As part of an effort to develop high performance structural resins for aerospace applications, work has continued on block copolymers containing imide and arylene ether segments. The arylene ether block used in this study contains a bulky fluorene group in the polymer backbone while the imide block contains an arylene ketone segment similar to that in the arylene ether block and has been named LaRC-ITPI. A series of imide/arylene ether block and segmented copolymers were prepared and characterized. Films were prepared from these copolymers and mechanical properties were measured.

Jensen, Brian J.↗

Structure-property study of keto-ether polyimides

As part of an on-going effort to develop an understanding of how changes in the chemical structure affect polymer properties, an empirical study was performed on polyimides containing only ether and/or carbonyl connecting groups in the polymer backbone. During the past two decades the structure-property relationships in linear aromatic polyimides have been extensively investigated. More recently, work has been performed to study the effect of isomeric attachment of keto-ether polyimides on properties such as glass transition temperature and solubility. However, little work has been reported on the relation of polyimide structure to mechanical properties. The purpose of this study was to determine the effect of structural changes in the backbone of keto-ether polyimides on their mechanical properties, specifically, unoriented thin film tensile properties. This study was conducted in two stages. The purpose of the initial stage was to examine the physical and mechanical properties of a representative group (four) of polyimide systems to determine the optimum solvent and cure cycle requirements. These optimum conditions were then utilized in the second stage to prepare films of keto-ether polyimides which were evaluated for mechanical and physical properties. All of the polyimides were prepared using isomers of oxydianiline (ODA) and diaminobenzophenone (DABP) in combination with 3,3',4,4'-benzophenonetetracarboxylic dianhydride (BTDA) and 4,4'-oxydiphthalic anhydride (ODPA).

Dezern, James F.↗

Matrix isolation studies of the interactions of BF3 with water and substituted diethyl ethers. Chemical ionization mass spectrometric determination of the proton affinity of (CF3CH2)2O

BF3 was co-condensed with H2O, D2O, (C2H5)2O, (CF3CH2)2O, and (C2F5)2O in excess argon at 15 K. Infrared spectra of BF3/water isolated in solid argon provided a more complete analysis of the BF3--H2O complex than previously published. Infrared spectra of the matrices showed a definite Lewis acid-base interaction between BF3 and diethyl ether; a weak but definite interaction with bis (2,2,2-trifluorodiethyl) ether, and no observable interaction with perfluorodiethyl ether. Thus, the ether data indicate a clear trend between strength of interaction with BF3 and the degree of F substitution. To support and explain the emerging relationship between interaction strength and the basicity of the oxygen-containing molecule, the proton affinity of (CF3CH2)2O was measured using chemical ionization mass spectrometry. The implications of the results for lubricant/metal oxide surface interactions are discussed.

Ball, David W.↗

Preparation and characterization of poly (arylene ether isoxazole)s by fluoride ion-mediated aromatic nucleophilic displacement reactions

As part of a continuing effort to prepare novel thermally stable high-performance polymers, poly(arylene ether isoxazole)s have been prepared by fluoride ion-catalyzed aromatic nucleophilic substitution reactions with bis(trimethylsiloxyphenyl) isoxazoles and activated bisarylhalides in diphenyl sulfone. Initial investigation involving the preparation of these materials with isoxazole bisphenols and activated bisarylhalides in the presence of potassium carbonate indicated that, under reaction conditions necessary to prepare high-molecular-weight materials, the isoxazole monomer was converted to an enamino ketone. This side reaction was avoided by using fluoride as a base. However, trimethylsilyl ether derivatives of the isoxazole bisphenols were required in these polymerizations for the preparation of high-molecular-weight materials. Moderate to high inherent viscosity eta(sub inh): 0.43-0.87 dl/g) materials with good thermal stability (air: 409-477 C, helium: 435-512 C) can be prepared by the silyl ether method. Glass transition temperatures ranged from 182 to 225 C for polymers with phenyl pendants and from 170 to 214 C for those without. Molecular weight control by 2% endcapping and the incorporation of a phenyl pendant at the 4 position of the isoxazole is necessary to yield polymers soluble in polar aprotic solvents at room temperature. There is evidence, however, indicating the existence of crosslinks between the polymer chains when the silyl ether approach is utilized.

Herbert, C. G.↗

Polyphenylene ethers with imide linking groups

Novel polyphenylene ethers with imide linking units are disclosed. These polymers incorporate the solvent and thermal resistance of polyimides and the processability of polyphenylene ethers. Improved physical properties over those of the prior art are obtained by incorporating meta linked ethers and/or polyphenylene oxides into the polymer backbone. A novel process for making polymers of this type is also disclosed. The process is unique in that the expected need of high process temperatures and/or special atmospheres are eliminated.

St.clair, T. L.↗

Thermal oxidative degradation reactions of linear perfluoroalkyl ethers

Thermal and thermal oxidative stability studies were performed on linear perfluoroalkyl ether fluids. The effect on degradation by metal catalysts and degradation inhibitors is reported. The linear perfluoroalkyl ethers are inherently unstable at 316 C in an oxidizing atmosphere. The metal catalysts greatly increased the rate of degradation in oxidizing atmospheres. In the presence of these metals in an oxidizing atmosphere, the degradation inhibitors were highly effective in arresting degradation at 288 C. However, the inhibitors had only limited effectiveness at 316 C. The metals promote degradation by chain scission. Based on elemental analysis and oxygen consumption data, the linear perfluoroalkyl ether fluids have a structural arrangement based on difluoroformyl and tetrafluoroethylene oxide units, with the former predominating. Previously announced in STAR as N82-26468

Jones, W. R., Jr.↗

Contact angle and surface tension measurements of a five-ring polyphenyl ether

Contact angle measurements were performed for a five-ring polyphenyl ether isomeric mixture on M-50 steel in a dry nitrogen atmosphere. Two different techniques were used: (1) a tilting plate apparatus, and (2) a sessile drop apparatus. Measurements were made for the temperature range 25 to 190 C. Surface tension was measured by a differential maximum bubble pressure technique over the range 23 to 220C in room air. The critical surface energy of spreading (gamma (sub c)) was determined for the polyphenyl ether by plotting the cosine of the contact angle (theta) versus the surface tension (gamma (sub LV)). The straight line intercept at cosine theta = 1 is defined as gamma (sub c). Gamma (sub c) was found to be 30.1 dyn/cm for the tilting plate technique and 31.3 dyn/cm for the sessile drop technique. These results indicate that the polyphenyl ether is inherently autophobic (i.e., it will not spread on its own surface film until its surface tension is less than gamma (sub c). This phenomenon is discussed in light of the wettability and wear problems encountered with this fluid.

Jones, W. R., Jr.↗

Polyarylene Ethers with Improved Properties

This invention relates to novel polyarylene ethers which possess the combination of high strength, toughness, and high use temperature with ease of extrusion and formation into complex objects. These polyarylene ethers are suitable for use in adhesives, coatings, films, membranes, and composite matrices. The polyarylene ethers of this invention are the polycondensation products from the reaction of either 1,3-bis (4-chloro or fluorobenzoyl) benzene with any one of the following bisphenolic compounds: bis (3-hydroxyphenyl) methane; bis (4-hydroxyphenyl) methane; 1,1-dimethyl-bis (4-hydroxyphenyl)methane, or 9,9-bis (4-hydroxyphenyl) fluorene. Random and block copolymers are also comprehended.

Hergenrother, P. M.↗

Contact angle and surface tension measurements of a five-ring polyphenyl ether

Contact angle measurements were performed for a five-ring polyphenyl ether isomeric mixture on M-50 steel in a dry nitrogen atmosphere. Two different techniques were used: (1) a tilting plate apparatus, and (2) a sessile drop apparatus. Measurements were made for the temperature range 25 to 190 C. Surface tension was measured by a differential maximum bubble pressure technique over the range 23 to 220 C in room air. The critical surface energy of spreading (gamma /sub c/) was determined for the polyphenyl ether by plotting the cosine of the contact angle (theta) versus the surface tension (gamma /sub LV/). The straight line intercept at cosine theta = 1 is defined as gamma (sub c). Gamma (sub c) was found to be 30.1 dyn/cm for the tilting plate technique and 31.3 dyn/cm for the sessile drop technique. These results indicate that the polyphenyl ether is inherently autophobic (i.e., it will not spread on its own surface film until its surface tension is less than gamma /sub c/). This phenomenon is discussed in light of the wettability and wear problems encountered with this fluid.

Jones, W. R., Jr.↗

Toughening of BIS maleimide resins: Synthesis and characterization of maleimide terminated poly(arylene ether) oligomers and polymers

Amine functional poly(arylene ether) sulfones were previously reported. Herein, the chemistry was extended to amorphous poly(arylene ether) ketones because of their higher fracture toughness values, relative to the polysulfones. It was demonstrated that the amino functional oligomers undergo a self-crosslinking reaction at temperatures above about 220 C. This produces an insoluble, but ductile network that has excellent resistance. A ketamine structure hypothesis was proposed and verified using solid state magic angle NMR. In most cases, the water generated upon ketamine formation is too low to produce porosity and solid networks are obtained. The stability of the ketamine networks towards hydrolysis is excellent. The chemistry was further demonstrated to be able to crosslink preformed nonfunctional poly(arylene ether) ketones if a difunctional amine was utilized. This concept has the possibility of greatly improving the creep resistance of thermoplastics. Also, a new technique was developed for converting the amine functional oligomers cleanly into maleimide structures. This method involves reacting maleic anhydride with monomeric aminophenols in the presence of solvent mixtures.