Search NASA⌕ Search

SEARCH · Search NASA

Results for “helium irradiation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Nanoscale friction of CVD single-layer MoS 2 with controlled defect formation

Two-dimensional (2D) layered nanomaterials such as graphene, molybdenum disulfide (MoS 2 ), or tungsten disulfide offer a promising solution in areas of solid-state lubrication, due to their excellent mechanical properties as well as low friction. However, defects can influence their friction and reduce their superior tribological properties. Thus, it is crucial to understand the effects of defects on sliding behavior in 2D nanomaterials, to foster a functional strategy for utilizing 2D nanomaterials as solid-state tribological films. In this study, frictional effects of defects, grain boundaries, and atomic-scale structural defects were explored on chemical vapor deposition (CVD) grown single layer MoS 2 . Selective patterning of defects into MoS 2 was accomplished via controlled irradiation of helium ions with varying ion doses. The friction of MoS 2 was characterized by friction force microscopy (FFM) and was found that friction depends on the defect formation controlled by helium ion irradiation. This approach offers a correlation between surface topography, defects and friction. Understanding the relative friction of MoS 2 in the presence of different levels of defects is foundational to studying tribological properties of a single layer MoS 2 at both nanoscales and macroscales.

36 MATERIALS SCIENCE↗

Temperature-dependent model of helium bubble expansion and bursting in tungsten

Continuum-scale models that can reliably predict the behavior of helium in tungsten are of interest to the fusion community due to the projected impact of these materials on fusion reactor operation. In this work, we perform molecular dynamics simulations of spherical helium bubbles of various sizes in tungsten at different temperatures and depths with the goal of determining a mathematical model of the pressure and density at which the bubbles initially expand or burst as a function of depth, size, temperature, and surface orientation. The bubbles are small enough that their loop-punching pressures cannot be accurately predicted with continuum mechanics, and their expansion behavior is important, as it appears to cause many of the features observed on helium-irradiated tungsten surfaces. We vary the temperature, bubble size, bubble depth, and surface orientation in each case, recording the bubble pressure and density that result in bubble expansion. An exponential function with three adjustable parameters is found to fit the results well; the parameters that best fit our results are provided.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Performance of the Friction Stir Welds Made on Neutron-Irradiated Steel with Helium

This report describes new experimental results on the microstructure and mechanical performance of the friction stir welds made on neutron-irradiated steel with helium. The report focuses on helium-related issues, specifically, helium-induced degradation in the welded joint, aiming to repair irradiated components of nuclear power plants (NPPs). The friction stir welds analyzed here were produced at Oak Ridge National Laboratory previously, and limited characterization work was performed, mostly addressing the presence or absence of macroscopic cracks. The present work attempts to perform a more comprehensive study to assess microstructure conditions, grain size, plastic strain gradients, the morphology of the helium-induced damage, and deformation behavior.

42 ENGINEERING↗

Effect of Helium Flux on Near-surface Helium Accumulation in Plasma-Exposed Tungsten

We report results of object kinetic Monte Carlo (OKMC) simulations aimed at understanding the effect of helium flux on the near-surface helium accumulation in plasma-facing tungsten, which is initially defect-free and has a W(100) surface orientation. These OKMC simulations are performed at 933 K for fluxes ranging from 10 22 to 4 × 10 25 He/m 2 s, with 100 eV helium atoms impinging on a W(100) surface up to a maximum fluence of 4×10 19 He/m 2 . In the near-surface region, helium clusters interact elastically with the free surface. The interaction is attractive and results in the drift of mobile helium clusters towards the surface as well as increased trap mutation rates. The associated kinetics and energetics of the above-mentioned processes obtained from molecular dynamics simulations are also considered. The OKMC simulations indicate that as the flux decreases, the retention of implanted helium decreases, and its depth distribution shifts to deeper below the surface in initially pristine tungsten. Furthermore, the fraction of retained helium diffusing into the bulk increases as well, so much so that for 10 22 He/m 2 s, almost all of the retained helium diffused into the bulk with minimal/negligible near-surface helium accumulation. At a given flux, with increasing fluence, the fraction of retained helium initially decreases and then starts to increase after reaching a minimum. The occurrence of the retention minimum shifts to higher fluences as the flux decreases. Although the near-surface helium accumulation spreads deeper into the material with decreasing flux and increasing fluence, the spread appears to saturate at depths between 80 and 100 nm. Finally, we present a detailed analysis of the influence of helium flux on the size and depth distribution of total helium and helium bubbles.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Suppression of Helium Induced Cracking in Laser Repair Welding of Highly Irradiated Stainless Steels

Welding repair of irradiated nuclear reactor materials such as austenitic stainless steels used for the reactor internals has been challenging due to irradiation generated helium in the material matrix over an extended period of time. In this study, improved laser welding techniques, including the novel Auxiliary Beam Stress Improved (ABSI) technique that proactively manages the stresses during laser repair welding is investigated to substantially reduce or avoid the occurrence of intergranular helium-induced cracking (HeIC). Here, laser weld cladding, with and without ABSI technique, was applied to deposit weld metal on irradiated stainless steel (Type 304 L) blocks with various helium concentrations up to approximately 20 atomic parts per million (appm). Welded samples were cross-sectioned and analyzed using optical and electron microscopes. It was found that, with the improved laser welding techniques, no macroscopic (millimeter-sized) cracks were observed in any of the samples. Microscopic (less than 50 μm) cracks were present in the heat affected zone. Statistical analysis on the sample with the highest helium concentration (~20 appm) reveals that the ABSI technique could effectively reduce the size and amounts of microscopic cracks.

36 MATERIALS SCIENCE↗

Helium 10830 Angstrom Irradiance: 1975-1983

A fairly complete time series from late 1974 to mid-1983 is available of values of the equivalent width of the He I 10830A chromospheric spectrum line averaged over the visible solar disk. Variation from about 25 mA in 1975 to about 80 mA in late 1981 is the major component of the signal. The 10830 variation reaches minimum about a year before the sunspot minimum and reaches maximum about a year after sunspot maximum. Superposed on the solar cycle variation is a modulation of up to + or - 13 mAdu to the passage of active regions across the disk. Power spectral analysis of the time series shows a major peak at a synodic rotation period of 27.42 days and smaller peaks at 1/2, 1/4 and 1/6 of this period. The spectrum is well modeled by a basic fluctuating component with an exponentially decaying autocovariance function of scale time of 43 days. Analysis of the data indicates that the rotational modulation occurs in episodes that last from 4 to 10 rotations. These episodes arise when active regions tend to occur in a limited longitude range. The analysis also shows that the apparent rotation period increased from 1977 to 1981. The apparent rotation period since 1981 is markedly shorter.

Harvey, J. W.↗

Microstructure and mechanical properties of friction stir weld performed on neutron-irradiated 304L steel with helium

As nuclear power plants (NPPs) approach or exceed 40–60 years of service, it may become necessary to repair damaged neutron-irradiated components to prolong longevity. However, fusion welding repair of irradiated steels and metallic materials is challenging because of helium-induced cracking. This study used friction stir welding (FSW) to address helium-related issues, such as helium bubble formation and grain boundary cracking. The microstructure, helium-induced degradation, and mechanical properties of a friction stir weld produced on neutron-irradiated 304L stainless steel with approximately 5.2 appm of helium were characterized. The analysis focused on variations in grain size, texture, and the morphology of helium-induced damage in the friction stir weld. Mechanical properties were characterized on the irradiated base metal (BM) and metallurgical zones of the friction stir weld: the stir zone (SZ), the thermo-mechanically affected zone (TMAZ), and the heat affected zone (HAZ). Only minor scattered porosity in the SZ and TMAZ and a few short microcracks (below 20 μm in length) in the TMAZ were observed, indicating limited helium-induced degradation. Tensile tests revealed good mechanical properties and fractography analysis demonstrated predominantly ductile fracture. In conclusion, the results highlight the immediate and substantial benefits of the FSW approach for repairing or joining helium-containing irradiated materials in NPPs.

36 MATERIALS SCIENCE↗

Behavior of helium cavities in ion-irradiated W-Ni-Fe ductile-phase toughened tungsten

This study reports on the distribution of helium (He) cavities in a hot-rolled W-Ni-Fe ductile-phase toughened tungsten (DPT W) composite irradiated to a dose and a helium concentration that are comparable to those in the material after 5-year irradiation in a conceptual fusion power plant. Here, the DPT W sample consists of W particles embedded in a ductile-phase NiFeW matrix with a nominal composition of 90W-7Ni-3Fe by weight. It was hot-rolled to a thickness reduction by 87% (87R DPT W). Sequential irradiation of the material with 1.2 MeV Ni + ions to a fluence of 2.15×10 16 Ni + /cm 2 and 90 keV He + ions to 6.5×10 15 He + /cm 2 was performed at 973 K. Larger He cavities with a lower number density are observed in NiFeW than W. Helium cavities are aggregated preferentially along the NiFeW/W interphase boundary. This behavior is not observed along the W/W grain boundary under the same irradiation conditions. A similar distribution of He cavities with comparable sizes is observed in 87R DPT W irradiated with He + ions only, suggesting that the He cavity distribution is not significantly affected by pre-irradiation of Ni + ions at 973 K. The data from this study does not provide any evidence for formation of visible voids or Ni precipitates in W phase irradiated with Ni + ions only. Diffusion and clustering of He atoms and mobile vacancies during ion irradiation at 973 K are responsible for the formation and growth of the He cavities.

36 MATERIALS SCIENCE↗

MX precipitate behavior in an irradiated advanced Fe-9Cr steel: Helium effects on phase stability

As part of an ongoing series aimed at optimizing Fe-9Cr reduced activation ferritic/martensitic (RAFM) alloys for fusion energy systems, this study explores MX precipitate behavior under dual-ion irradiations, specifically examining correlations between helium transmutation and irradiation-induced damage. Utilizing single and dual-beam ion irradiation, the research explores the combined effects of helium (10–25 appm He/dpa), temperature (400–600 °C), and damage levels (15–100 dpa) on the microstructural evolution of CNA9 steel, a variant of Castable Nanostructured Alloys (CNAs). The study demonstrates that helium co-implantation hinders radiation-enhanced coarsening of MX-TiC precipitates at 500 and 600 °C, maintaining MX-TiC precipitate stability at moderate damage levels (15 dpa) but failing to prevent complete precipitate dissolution at higher damage levels (≥50 dpa) when irradiated at 500 °C. Here, a generalized precipitate stability model suggests that helium-induced suppression of diffusion alters the balance between recoil resolution and back diffusion for MX-TiC precipitates, enhancing the current understanding of precipitate behavior under damage and transmutation simulated dual-ion irradiation conditions.

Characterization↗

Helium partitioning to the core-shelled Ta nanoclusters in nanocrystalline Cu-Ta alloy

In this work, a nanocrystalline (NC) Cu-10at.%Ta alloy is irradiated with helium at different temperatures to assess the stability and effectiveness of Ta nanoclusters in trapping helium and suppressing swelling. Advanced microstructural characterization of the room-temperature irradiated specimens indicated the presence of small He-bubbles (∼1-2 nm) at the peak damage depth mainly at the core and along the interface of Ta nanoclusters with Cu matrix. Few bubbles were found along grain boundaries, with much smaller bubbles homogenously distributed within the copper lattice. High-temperature irradiation exhibited bubbles of ∼3-5 nm, which were primarily associated with nanoclusters as compared to other locations, with no observed faceting of the bubbles. In conclusion, atom probe analysis confirmed helium partitioning to the Ta nanoclusters indicating the effective entrapment of these He atoms.

36 MATERIALS SCIENCE↗

Anterior segment sparing to reduce charged particle radiotherapy complications in uveal melanoma

PURPOSE: The purpose of this investigation is to delineate the risk factors in the development of neovascular glaucoma (NVG) after helium-ion irradiation of uveal melanoma patients and to propose treatment technique that may reduce this risk. METHODS AND MATERIALS: 347 uveal melanoma patients were treated with helium-ions using a single-port treatment technique. Using univariate and multivariate statistics, the NVG complication rate was analyzed according to the percent of anterior chamber in the radiation field, tumor size, tumor location, sex, age, dose, and other risk factors. Several University of California San Francisco-Lawrence Berkeley National Laboratory (LBNL) patients in each size category (medium, large, and extralarge) were retrospectively replanned using two ports instead of a single port. By using appropriate polar and azimuthal gaze angles or by treating patients with two ports, the maximum dose to the anterior segment of the eye can often be reduced. Although a larger volume of anterior chamber may receive a lower dose by using two ports than a single port treatment. We hypothesize that this could reduce the level of complications that result from the irradiation of the anterior chamber of the eye. Dose-volume histograms were calculated for the lens, and compared for the single and two-port techniques. RESULTS: NVG developed in 121 (35%) patients. The risk of NVG peaked between 1 and 2.5 years posttreatment. By univariate and multivariate analysis, the percent of lens in the field was strongly correlated with the development of NVG. Other contributing factors were tumor height, history of diabetes, and vitreous hemorrhage. Dose-volume histogram analysis of single-port vs. two-port techniques demonstrate that for some patients in the medium and large category tumor groups, a significant decrease in dose to the structures in the anterior segment of the eye could have been achieved with the use of two ports. CONCLUSION: The development of NVG after helium-ion irradiation is correlated to the amount of lens, anterior chamber in the treatment field, tumor height, proximity to the fovea, history of diabetes, and the development of vitreous hemorrhage. Although the influence of the higher LET deposition of helium-ions is unclear, this study suggests that by reducing the dose to the anterior segment of the eye may reduce the NVG complications. Based on this retrospective analysis of LBNL patients, we have implemented techniques to reduce the amount of the anterior segment receiving a high dose in our new series of patients treated with protons using the cyclotron at the UC Davis Crocker Nuclear Laboratory (CNL).

NASA Discipline Radiation Health↗

MX precipitate behavior in an irradiated advanced Fe-9Cr steel: Helium sequestration and cavity swelling performance

This work is the third and final part in an initial series on addressing the behavior of MX precipitate stability in an advanced Fe-9Cr reduced activation ferritic/martensitic (RAFM) alloy under fusion-relevant ion irradiation conditions. Here, the helium trapping properties of MX precipitates are investigated across varying damage levels (15–100 dpa), temperatures (400–600 °C), and helium doses (10–25 appm He/dpa) using sophisticated dual ion beam experiments and electron microscopy. Results indicate that individual MX precipitates efficiently sequester helium in the form of nanoscale bubbles at the precipitate-matrix interfaces near the peak swelling temperature (∼5 bubbles/precipitate at 500 °C). Swelling was primarily due to matrix cavities. The Fe-9Cr alloy reached 2% swelling by 100 dpa, suggesting a shift to steady-state swelling around 50 dpa at 500 °C. Furthermore, MX precipitate dissolution beginning at 15 dpa did not coincide with this onset of steady-state swelling.

Dual ion irradiation↗

Helium-bubble-enhanced disordering of intermetallic phase under irradiation

Understanding and controlling phase transformations in metals and alloys under irradiation is vital to the design of irradiation-tolerant materials. The L1 2 -ordered intermetallic phase in nickel-based superalloys provides superior high-temperature mechanical properties and corrosion resistance. Here, we studied the order-disorder transformation kinetics of an L1 2 -structured gamma-prime phase in nickel-based superalloy Rene N4 under krypton ion irradiation and the effect of pre-implanted helium gas bubbles on the kinetics of phase transformation. Furthermore, the presence of pre-implanted helium gas bubbles significantly enhances the order-disorder transformation of L1 2 -structured gamma-prime phase under irradiation at 300 °C. The evolution of pre-implanted helium gas bubbles under irradiation implies that helium gas bubbles could effectively trap irradiation-induced vacancies and impede the reordering process of anti-site defects in gamma-prime phase.

36 MATERIALS SCIENCE↗

Helium effects on the surface and subsurface evolutions in single-crystalline tungsten

Tungsten (W) has been perceived as one of the most promising plasma facing materials (PFMs) for future fusion reactors. In the past decade, its behavior under irradiation and helium (He) plasma interaction has been extensively studied. However, some key knowledge gaps still exist, such as the influence of crystallographic orientation on the surface and subsurface evolutions. In this work, we focus on the He ion-beam irradiation damage effects in mirror-polished single-crystalline W samples with three different surface planes of {100}, {110} and {111}. Irradiation was performed at room temperature using 40 keV He+ to a fluence of 1 × 10 16 /cm 2 , followed by thermal desorption spectroscopy (TDS) up to ~1920 K. The microstructures of He-irradiated W before and after TDS heat treatment were characterized by scanning and transmission electron microscopy. Subsurface He bubbles were imaged in all irradiated samples, but newly formed <111>-oriented surface grains and surface blisters were only observed in W {100} and {110} starting orientations. These results reveal that radiation damage, He thermal desorption, and surface/subsurface evolution are all strongly dependent on crystallographic orientation. Underlying physical mechanisms are discussed based on ion channeling effects, He-vacancy interactions, and surface diffusion. In conclusion, these findings provide new insights into He effects in W.

36 MATERIALS SCIENCE↗

Primary and Low-Strain Creep Models for 9Cr Tempered Martensitic Steels Including the Effects of Irradiation Softening and High-Helium Re-Hardening

Primary and low-strain creep represents a very important integrity challenge to large, complex structures, like fusion reactors. Here, we develop a predictive empirical primary creep model for 9Cr tempered martensitic steels (TMS), relating the applied stress (σ) to strain (ε), time (t) and temperature (T). The most accurate model is based on the applied σ normalized by the steel’s T-dependent ultimate tensile stress (σo), σ/σo(T). The model, fit to 17 heats of 9Cr TMS, yielded a σ root mean square error (RMSE) of ≈±11 MPa. Notably, the model also provides robust predictions for all the other TMS, when calibrated only by the fusion candidate Eurofer97 database. The model was extended to explore two possible effects of neutron irradiation, which produces both displacements per atom (dpa) and helium (He in atomic parts per million, appm) damage. These effects, which have not been previously considered, include: (a) softening, as a function of dpa, at T > ≈400–450 °C, in low-He fission environments (<1 He/dpa); and (b) subsequent re-hardening in high-He (≥10 He/dpa) fusion first-wall environments. The irradiation effect models predict (a) accelerated primary creep due to irradiation softening; and (b) fully arrested creep due to high-He re-hardening.

Alam, Md Ershadul (ORCID:0000000345968026)↗