Search NASA⌕ Search

SEARCH · Search NASA

Results for “hydrogenated amorphous silicon”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Development of CIGS2 Thin Films on Ultralightweight Flexible Large Area Foil Sunstrates

The development of thin film solar cells is aimed at reducing the costs for photovoltaic systems. Use of thin film technology and thin foil substrate such as 5-mil thick stainless steel foil or 1-mil thick Ti would result in considerable costs savings. Another important aspect is manufacturing cost. Current single crystal technology for space power can cost more than $ 300 per watt at the array level and weigh more than 1 kg/sq m equivalent to specific power of approx. 65 W/kg. Thin film material such as CuIn1-xGaxS2 (CIGS2), CuIn(1-x)Ga(x)Se(2-y)S(y) (CIGSS) or amorphous hydrogenated silicon (a-Si:H) may be able to reduce both the cost and mass per unit area by an order of magnitude. Manufacturing costs for solar arrays are an important consideration for total spacecraft budget. For a medium sized 5kW satellite for example, the array manufacturing cost alone may exceed $ 2 million. Moving to thin film technology could reduce this expense to less than $ 500K. Earlier publications have demonstrated the potential of achieving higher efficiencies from CIGSS thin film solar cells on 5-mil thick stainless steel foil as well as initial stages of facility augmentation for depositing thin film solar cells on larger (6 in x 4 in) substrates. This paper presents the developmental study of achieving stress free Mo coating; uniform coatings of Mo back contact and metallic precursors. The paper also presents the development of sol gel process, refurbishment of selenization/sulfurization furnace, chemical bath deposition (CBD) for n-type CdS and scrubber for detoxification of H2S and H2Se gases.

Dhere, Neelkanth G.↗

Status and applications of diamond and diamond-like materials: An emerging technology

Recent discoveries that make possible the growth of crystalline diamond by chemical vapor deposition offer the potential for a wide variety of new applications. This report takes a broad look at the state of the technology following from these discoveries in relation to other allied materials, such as high-pressure diamond and cubic boron nitride. Most of the potential defense, space, and commercial applications are related to diamond's hardness, but some utilize other aspects such as optical or electronic properties. The growth processes are reviewed, and techniques for characterizing the resulting materials' properties are discussed. Crystalline diamond is emphasized, but other diamond-like materials (silicon carbide, amorphous carbon containing hydrogen) are also examined. Scientific, technical, and economic problem areas that could impede the rapid exploitation of these materials are identified. Recommendations are presented covering broad areas of research and development.

Source record↗

A solar power system for an early Mars expedition

As NASA looks at missions that will expand human presence in the solar system, the power requirements for such missions need to be defined, developed and analyzed. One mission under consideration consists of a 40 day manned Mars surface expedition to perform science experiments. The mission time was centered around an aerocentric longitude (Ls) of 90 deg to lessen the probability of an occurrence of a local or planetary dust storm. The mission site was arbitrarily located at the Martian equator. The power requirements were assumed to be 40 kWe for life support and experiment power during the Martian day and 20 kWe for life support during the Martian night. A solar energy system consisting of roll-out amorphous silicon arrays and a hydrogen-oxygen regenerative fuel cell energy storage system was chosen for the study. The power available from a roll-out array, when plotted against time, approaches a cosine-like curve and depends on both array area and the amount of solar irradiance impinging on its horizontal surface. The array is sized to provide at least 20 KWe when the sun is 12.5 deg above the horizon and ramp up to 140 kWe peak power at Martian noon. In this configuration, the array is capable of supplying 40 KWe continuously to the user for the majority of the Martian day while supplying the excess energy to the electrolyzer portion of the energy storage system. A roll-out, pumped loop radiator system is used to dissipate the waste heat produced by the fuel cell. The power management and distribution system inverts the power from the individual solar array sub-modules and the fuel cell stacks and connects them to a 440 VAC single phase 20 kHz main bus. The total power system is comprised of 80 individual solar array modules with an integral bus and three energy storage modules consisting of fuel cell and electrolyzer stacks, reactant storage tanks, and a roll-out radiator. Power system mass, stowed volume, and deployed area were determined. Day/night power splits of 40/10 kWe, 40/30 kWe, and 40/40 kWe were also considered to determine the impact of a range of nighttime power requirements on the baseline system.

Mckissock, Barbara I.↗

Studies of mechano-chemical interactions in the tribological behavior of materials

Mechano-chemical interaction studies can contribute to the understanding of wear and friction of materials. Specific examples of experimental results relative to the subject are discussed. There are two parts: one describes the synergistic effect of corrosion and wear of iron sliding on sapphire in sulfuric acid, and the other describes the effect of surface films on the wear and friction of plasma-deposited diamondlike carbon (amorphous hydrogenated carbon) films in sliding contact with silicon nitride. The concentration of acid (pH) is an important factor in controlling the iron loss caused by wear-corrosion processes in sulfuric acid. The mechanical action can cause chemical reactions to proceed much faster than they would otherwise. The diamondlike carbon (DLC) films are shown to behave tribologically much like bulk diamond. In a dry nitrogen environment, a mechano-chemical reaction produces a substance which greatly decreases the coefficient of friction. In a moist air environment, mechano-chemical interactions drastically reduce the wear life of DLC films and water vapor greatly increases friction.

Miyoshi, Kazuhisa↗

Studies of mechanochemical interactions in the tribological behavior of materials

Mechanochemical interaction studies can contribute to the understanding of wear and friction of materials. Specific examples of experimental results relative to the subject are discussed. There are two parts: one describes the synergistic effect of corrosion and wear of iron sliding on sapphire in sulfuric acid, and the other describes the effect of surface films on the wear and friction of plasma-deposited diamondlike carbon (amorphous hydrogenated carbon) films in sliding contact with silicon nitride. The concentration of acid (pH) is an important factor in controlling the iron loss caused by wear-corrosion processes in sulfuric acid. The mechanical action can cause chemical reactions to proceed much faster than they would otherwise. The diamondlike carbon (DLC) films are shown to behave tribologically much like bulk diamond. In a dry nitrogen environment, a mechanochemical reaction produces a substance which greatly decreases the coefficient of friction. In a moist air environment, mechanochemical interactions drastically reduce the wear life of DLC films and water vapor greatly increases friction.

Miyoshi, Kazuhisa↗

Rapid thermal annealing of Amorphous Hydrogenated Carbon (a-C:H) films

Amorphous hydrogenated carbon (a-C:H) films were deposited on silicon and quartz substrates by a 30 kHz plasma discharge technique using methane. Rapid thermal processing of the films was accomplished in nitrogen gas using tungsten halogen light. The rapid thermal processing was done at several fixed temperatures (up to 600 C), as a function of time (up to 1800 sec). The films were characterized by optical absorption and by ellipsometry in the near UV and the visible. The bandgap, estimated from extrapolation of the linear part of a Tauc plot, decreases both with the annealing temperature and the annealing time, with the temperature dependence being the dominating factor. The density of states parameter increases up to 25 percent and the refractive index changes up to 20 percent with temperature increase. Possible explanations of the mechanisms involved in these processes are discussed.

Alterovitz, Samuel A.↗

Outdoor performance testing of thin-film devices

The Advanced Systems Research Group supports the photovoltaic advanced R&D (PV AR&D) project by providing outdoor (global) testing of PV cells, submodules, modules, and arrays. The group also provides in house engineering and analysis to identify and determine how technical issues such as cell/module/system adaptations, long term stability, reliability, economics, materials availability, safety, and environmental impacts affect the development and ultimate use of advanced PV thin film, innovative cell, and material technologies. A major thrust of the research effort is to develop and utilize instrumentation and procedures for monitoring and analyzing PV cells and submodules including outdoor performance and stability testing and life cycle accelerated stress testing. To accomplish the above, the solar energy research institute (SERI) outdoor PV test facility was established in 1982. The group has designed testing systems and analysis procedures for, and has tested, numerous amorphous silicon thin film submodules provided by SERI subcontractors and has performed long term outdoor stability tests on CdS/CuIr Se sub 2 and hydrogen passivated silicon solar cells. A significant contribution from this facility over the past year was the testing of large area amorphous silicon submodules.

Source record↗

Deposition Of Diamondlike Films By ECR Microwave Plasma

Hard, amorphous hydrogenated carbon films of diamondlike quality deposited at room temperature on silicon, optical glass, and quartz through decomposition of CH4 in electron-cyclotron-resonance (ECR) microwave plasma of CH4 diluted with H2. Technique provides hard, abrasion-resistant coatings for lenses and other optical components. Films chemically inert and posses high electrical resistivity and breakdown fields, valuable properties in microelectronics applications.

Pool, Frederick S.↗

New Interstellar Dust Models Consistent with Interstellar Extinction, Emission and Abundances Constraints

We present new interstellar dust models that are consistent with both, the FUV to near-IR extinction and infrared (IR) emission measurements from the diffuse interstellar medium. The models are characterized by different dust compositions and abundances. The problem we solve consists of determining the size distribution of the various dust components of the model. This problem is a typical ill-posed inversion problem which we solve using the regularization approach. We reproduce the Li Draine (2001, ApJ, 554, 778) results, however their model requires an excessive amount of interstellar silicon (48 ppM of hydrogen compared to the 36 ppM available for an ISM of solar composition) to be locked up in dust. We found that dust models consisting of PAHs, amorphous silicate, graphite, and composite grains made up from silicates, organic refractory, and water ice, provide an improved fit to the extinction and IR emission measurements, while still requiring a subsolar amount of silicon to be in the dust. This research was supported by NASA Astrophysical Theory Program NRA 99-OSS-01.

Zubko, V.↗

The growth of cubic silicon carbide on a compliant substrate

Research has shown that silicon carbide grown on silicon and 6H silicon carbide has problems associated with these substrates. This is because silicon and silicon carbide has a 20% lattice mismatch and cubic silicon carbide has not been successfully achieved on 6H silicon carbide. We are investigating the growth of silicon carbide on a compliant substrate in order to grow defect free silicon carbide. This compliant substrate consists of silicon/silicon dioxide with 1200 A of single crystal silicon on the top layer. We are using this compliant substrate because there is a possibility that the silicon dioxide layer and the carbonized layer will allow the silicon lattice to shrink or expand to match the lattice of the silicon carbide. This would improve the electrical properties of the film for the use of device fabrication. When trying to grow silicon carbide, we observed amorphous film. To investigate, we examined the process step by step using RHEED. RHEED data showed that each step was amorphous. We found that just by heating the substrate in the presence of hydrogen it changed the crystal structure. When heated to 1000 C for 2 minutes, RHEED showed that there was an amorphous layer on the surface. We also heated the substrate to 900 C for 2 minutes and RHEED data showed that there was a deterioration of the single crystalline structure. We assumed that the presence of oxygen was coming from the sides of the silicon dioxide layer. Therefore, we evaporated 2500 A of silicon to all four edges of the wafer to try to enclose the oxygen. When heating the evaporated wafer to 900 C the RHEED data showed single crystalline structure however at 1000 C the RHEED data showed deterioration of the single crystalline structure. We conclude that the substrate itself is temperature dependent and that the oxygen was coming from the sides of the silicon dioxide layer. We propose to evaporate more silicon on the edges of the wafer to eliminate the escape of oxygen. this will allow us to grow single crystal cubic silicon carbide.

Mitchell, Sharanda↗

Ion beam deposition of amorphous carbon films with diamond like properties

Carbon films were deposited on silicon, quartz, and potassium bromide substrates from an ion beam. Growth rates were approximately 0.3 micron/hour. The films were featureless and amorphous and contained only carbon and hydrogen in significant amounts. The density and carbon/hydrogen ratio indicate the film is a hydrogen deficient polymer. One possible structure, consistent with the data, is a random network of methylene linkages and tetrahedrally coordinated carbon atoms.

Angus, John C.↗

Degradation of the lunar vacuum by a moon base

Several industrial processes requiring high and ultra-high vacuum similar to the lunar vacuum are outlined. The effects of a 20-person lunar base and a 250-person industrial facility on this vacuum are discussed. It is shown that exhaust from transport spacecraft and leakage from the habitat will be comparable to the daytime gas pressure for the 20-person base, and will degrade the vacuum to the range of 2 x 10 to the -9th torr for the use of 250-person facility. This will result in replacing the mostly nonreactive gases hydrogen, helium, and neon with more reactive gases containing carbon and oxygen. This vacuum is still good enough to perform many important vacuum processes such as plasma-deposition of amorphous silicon for solar cells, but processes such as molecular beam epitaxy or locating an intersecting beam accelerator on the moon will require additional vacuum pumping.

Landis, Geoffrey↗

Tribological studies of amorphous hydrogenated carbon films in a vacuum, spacelike environment

Recent work on the adhesion and friction properties of plasma-deposited amorphous hydrogenated carbon films and their dependence on preparation conditions are reviewed. The results of the study indicate that plasma deposition enables one to deposit a variety of amorphous hydrogenated carbon (a-C:H) exhibiting diamondlike friction behavior. The plasma-deposited a-C:H films can be effectively used as hard lubricating films on ceramic materials such as silicon nitride in vacuum.

Kazuhisa Miyoshi↗

Diagnostics of silane and germane radio frequency plasmas by coherent anti-Stokes Raman spectroscopy

In situ plasma diagnostics using coherent anti-Stokes Raman spectroscopy have shown different dissociation characteristics for GeH4 and SiH4 in radio frequency (rf) plasma-enhanced chemical vapor deposition of amorphous silicon germanium alloy (a-SiGe:H) thin films. The GeH4 dissociation rate in rf plasmas is a factor of about 3 larger than that of SiH4. Plasma diagnostics have revealed that the hydrogen dilution of the SiH4 and GeH4 mixed plasma plays a critical role in suppressing the gas phase polymerization and enhancing the GeH4 dissociation.

Perry, Joseph W.↗

Silicon carbon alloy thin film depositions using electron cyclotron resonance microwave plasmas

Amorphous and microcrystalline silicon carbon films (a-SiC:H, micro-c-SiC:H) have been deposited using SiH4, CH4 and H2 mixed gas ECR (electron cyclotron resonance) plasmas. The optical bandgap of a-SiC:H films is not dependent on the hydrogen dilution in the ECR plasma. The deposition rate of a-SiC:H films is found to be strongly dependent on the ECR magnetic field and the hydrogen dilution. The hydrogen dilution effect on the deposition rate indicates that the etching in ECR hydrogen plasmas plays an important role in the deposition of a-SiC:H films. The optical constants n and k of ECR-deposited a-SiC:H films in the wavelength region of 0.4 to 1.0 micron are determined to be 2.03-1.90 and 0.04-0.00, respectively. The microstructures of ECR-deposited micro-c-SiC:H films are shown by X-ray diffraction and SEM (scanning electron microscopy) to be composed of 1000-A alpha-SiC microcrystallites and amorphous network structures.

Shing, Y. H.↗

Modelling of Laser-Enhanced Chemical Vapor Deposition

Research is directed at development of a detailed model of mass and heat transfer and chemical reaction in the pyrolysis of silane for the growth of thin amorphous silicon substrates incorporating laser heating of the gas phase above the film. The model will be the basis for evaluation of the relative importances of the decomposition of SiH4 in the vapor phase, mass transfer of the intermediate species, e.g., SiH2, and the evolution of hydrogen gas. Plans are also underway for developing a model for homogeneous nucleation of Si in the vapor phase to model the rate limitations observed at high gas-phase temperatures and high partial pressures of silane. Work was concentrated on an almost one-dimensional model for the coupling of the CO2 laser beam for heat transfer of the vapor phase with simple kinetic models for SiH4 decomposition and subsequent absorption of Si vapor on the substrate. Mass transfer in the vapor phase is assumed to be solely by diffusion. The role of convection in the vapor phase caused by the large changes in density in and around the center of the laser beam will be analyzed to evaluate the potential of microgravity experiments for increasing the uniformity of the film and the deposition rate.

Brown, R. A.↗

Synthesis of silane and silicon in a non-equilibrium plasma jet

The feasibility of using a non-equilibrium hydrogen plasma jet as a chemical synthesis tool was investigated. Four possible processes were identified for further study: (1) production of polycrystalline silicon photovoltaic surfaces, (2) production of SiHCl3 from SiCl4, (3) production of SiH4 from SiHCl3, and (4) purification of SiCl4 by metal impurity nucleation. The most striking result was the recognition that the strongly adhering silicon films, amorphous or polycrystalline, produced in our studies could be the basis for preparing a photovoltaic surface directly; this process has potential advantages over other vapor deposition processes.

Calcote, H. F.↗

Tribological evaluation and analysis of coating materials

A physical characterization of coating materials by analytical techniques such as XPS, AES, ellipsometry, and nuclear reaction analysis can contribute to the understanding of adhesion and friction of the coatings and can partially predict the tribological properties of the coatings. This two-part paper describes the tribological properties and physical characteristics of (1) diamondlike carbon (DLC) films and (2) silicon nitride (SiN(x)) films. Emphasis is to relate plasma deposition conditions to the film chemistry and composition and to the adhesion and friction of the films. With the DLC films, the higher the plasma deposition power, the less the hydrogen concentration and the greater the film density and the hardness. The friction behavior of DLC films deposited at higher deposition powers (200 to 300 W) is similar to that of bulk diamond. Even in a vacuum, the DLC films effectively lubricate ceramic surfaces (Si3N4) at temperatures to 500 C. With SiN(x) films, the silicon to nitrogen ratios and the amount of amorphous silicon depend on deposition frequency. The presence of rich amorphous silicon in the high-frequency plasma-deposited SiN(x) films increases their adhesion and friction above 500 C in vacuum.

Miyoshi, Kazuhisa↗