FaceSheet Push-off Tests to Determine Composite Sandwich Toughness at Cryogenic Temperatures

A new novel test method, associated analysis, and experimental procedures are developed to investigate the toughness of the facesheet-to-core interface of a sandwich material at cryogenic temperatures. The test method is designed to simulate the failure mode associated with facesheet debonding from high levels of gas pressure in the sandwich core. The effects of specimen orientation are considered, and the results of toughness measurements are presented. Comparisons are made between room and liquid nitrogen (-196 C) test temperatures. It was determined that the test method is insensitive to specimen facesheet orientation and strain energy release rate increases with a decrease in the test temperature.

Gates, Thomas S.↗

Factors influencing the Mode I interlaminar fracture toughness of a rubber toughened thermoplastic matrix composite

The use of a rubber modified thermoplastic resin has been investigated as a method to improve the Mode I interlaminar fracture toughness of a unidirectional continuous carbon fiber composite. Test results show that the improvement in the fracture toughness is less than expected due to rubber particle agglomeration, solvent and molding induced crystallization of the matrix and poor fiber/matrix adhesion. The plastic zone in composites utilizing tough matrices can extend well beyond a single interfibrillar spacing. However, the development of the plastic zone is limited due to the failure of the fiber/matrix interface. In order to fully evaluate the potential of tough composites using toughened matrices, any improvement made in the matrix toughness must be coupled with improvements in the fiber/matrix adhesion.

Parker, D. S.↗

Imparting strength and toughness to brittle composites

Appropriate intermittent coatings of fibers can produce areas of low and high toughness in brittle composites. Experiments using silicon vacuum grease (SVG) and polyurethane varnish (PUV) coatings that achieve weakly and strongly bonded interfaces are described. Tensile strength and edge-crack fracture toughness for both SVG and PUV coatings were plotted against the percentage coating (C). Both coating materials maintain tensile strengths in the order of the rule of mixture strength values up to a large C. It is suggested that both materials produce similar coated interfacial shear strengths while producing different effects on toughness.

Atkins, A. G.↗

New Testing Tool For Composite Interfaces

Mechanical strength of fiber/matrix interface key factor in overall strength and toughness of composite material. Desktop fiber pushout apparatus generates load and acoustic-emission (soundwave) data as function of translation-table displacement. Video camera gives view of specimen. Compact, easy to operate, and inexpensive. Appropriate for wide range of composites, including metal, intermetallic, and ceramic matrix composites. Not restricted to aerospace/aeronautics applications.

Eldridge, Jeffrey I.↗

Characterization of Hybrid CNT Polymer Matrix Composites

Carbon nanotubes (CNTs) have been studied extensively since their discovery and demonstrated at the nanoscale superior mechanical, electrical and thermal properties in comparison to micro and macro scale properties of conventional engineering materials. This combination of properties suggests their potential to enhance multi-functionality of composites in regions of primary structures on aerospace vehicles where lightweight materials with improved thermal and electrical conductivity are desirable. In this study, hybrid multifunctional polymer matrix composites were fabricated by interleaving layers of CNT sheets into Hexcel® IM7/8552 prepreg, a well-characterized toughened epoxy carbon fiber reinforced polymer (CFRP) composite. The resin content of these interleaved CNT sheets, as well as ply stacking location were varied to determine the effects on the electrical, thermal, and mechanical performance of the composites. The direct-current electrical conductivity of the hybrid CNT composites was characterized by in-line and Montgomery four-probe methods. For [0](sub 20) laminates containing a single layer of CNT sheet between each ply of IM7/8552, in-plane electrical conductivity of the hybrid laminate increased significantly, while in-plane thermal conductivity increased only slightly in comparison to the control IM7/8552 laminates. Photo-microscopy and short beam shear (SBS) strength tests were used to characterize the consolidation quality of the fabricated laminates. Hybrid panels fabricated without any pretreatment of the CNT sheets resulted in a SBS strength reduction of 70 percent. Aligning the tubes and pre-infusing the CNT sheets with resin significantly improved the SBS strength of the hybrid composite To determine the cause of this performance reduction, Mode I and Mode II fracture toughness of the CNT sheet to CFRP interface was characterized by double cantilever beam (DCB) and end notch flexure (ENF) testing, respectively. Results are compared to the control IM7/8552 laminate.

Grimsley, Brian W.↗

The Chemical Nature of the Fiber/resin Interface in Composite Materials

Carbon fiber/epoxy resin composites are considered. The nature of the fiber structure and the interaction that occurs at the interface between fiber and matrix are emphasized. Composite toughness can be improved by increased axial tensile and compressive strengths in the fibers. The structure of carbon fibers indicates that the fiber itself can fail transversely, and different transverse microstructures could provide better transverse strengths. The higher surface roughness of lower modulus and surface-treated carbon fibers provides better mechanical interlocking between the fiber and matrix. The chemical nature of the fiber surface was determined, and adsorption of species on this surface can be used to promote wetting and adhesion. Finally, the magnitude of the interfacial bond strength should be controlled such that a range of composites can be made with properties varying from relatively brittle and high interlaminar shear strength to tougher but lower interlaminar shear strength.

Diefendorf, R. J.↗

Interface effects in interlaminar fracture of thermoplastic composites

Mode I interlaminar fracture toughness was determined on a series of unidirectional poly(phenylene oxide)/carbon fiber composites using the double cantilever beam test. Initial toughness for growth of a delamination from an insert depends on fiber type, and ranges from 190 to 440 J/sq m, with intermediate modulus fibers tending to give lower values than high-strain fibers. Low toughness values are attributed to poor fiber-matrix adhesion. As a delamination progress down the beam, fiber bridging increases the apparent toughness by up to a factor of 7, depending on the fiber.

Hinkley, J. A.↗

Deformation and fracture of a directionally solidified NiAl-28Cr-6Mo eutectic alloy

A directionally solidified alloy based on the NiAl-(Cr, Mo) eutectic was examined by transmission and scanning electron microscopy to characterize the microstructure and room temperature deformation and fracture behavior. The microstructure consisted of a lamellar morphology with a group of zone axes (111) growth direction for both the NiAl and (Cr, Mo) phases. The interphase boundary between the eutectic phases was semicoherent and composed of a well-defined dislocation network. In addition, a fine array of coherent NiAl precipitates was dispersed throughout the (Cr, Mo) phase. The eutectic morphology was stable at 1300 K with only coarsening of the NiAl precipitates occurring after heat treatment for 1.8 ks (500 h). Fracture of the aligned eutectic is characterized primarily by a crack bridging/renucleation mechanism and is controlled by the strength of the semicoherent interface between the two phases. However, contributions to the toughness of the eutectic may arise from plastic deformation of the NiAl phase and the geometry associated with the fracture surface.

Chen, X. F.↗

Offset-Stoichiometric Reflowable Composite Bonding Method with Adhesive for Mitigating Strict Faying Surface Tolerances

Inherent susceptibility of adhesive bonds to miniscule quantities of contamination can cause undetectable weakened bonds. For this reason, the Federal Aviation Administration (FAA) places strict regulations on adhesively bonded joints in primary aircraft structures. To meet certification requirements aircraft manufactures resort to redundant load paths in the form of fasteners which inherently add weight to the structure and increase manufacturing time. In prior work, a secondary bonding technique called AERoBOND was developed, which utilized off-stoichiometric epoxymatrix resins to facilitate reflow and diffusion of the resin within the joint interface during a secondary bonding/cure process, thus achieving a bond similar to a co-cured joint. However, the AERoBOND process required tight spatial tolerances between the two parts being joined. This study examined the utilization of conventional adhesive with the AERoBOND method to act as a filler in the joint line, effectively reducing the need for tight tolerances on the joining parts and serving as a flexible alternative for existing manufacturing processes. Ultrasonic inspection, optical microscopy, and ASTM International standard tests were performed to analyze the joints for defects and to quantify the mode-I and mode-II interlaminar fracture toughness and short beam strength of the proposed methodology with varying manufacturing parameters. The comprehensive results indicate that the AERoBOND+ method with and without surface preparation performs comparably to co-cured and conventional, adhesively bonded joints when secondary cured in an autoclave with 791 kPa of pressure. As an example, the AERoBOND+ panel without surface preparation bonded with 791 kPa of pressure (referred to as AB+3 throughout paper) had a mode-I fracture toughness (G Ic ) of 0.643 kJ/m 2 and a mode-II fracture toughness (G IIc ) of 4.000 kJ/m 2 in the non-precracked condition and 4.218 kJ/m 2 in the precracked condition at the adhesive-to-prepreg interface. These results were 96%, 142%, and 217%, respectively, of a co-cured baseline panel (referred to as C1 throughout paper).

Composites↗

Transmission electron microscopy of composites

Since interphase-interfaces are often both the structurally weakest and chemically least stable regions of a composite material, they are critical determinants of such macrostructural characteristics as tensile strength and fracture toughness. Attention is presently given to the use of TEM for the study of interfaces between dissimilar materials; electron-diffraction, analytical, and high-resolution forms of TEM are employed, for the cases of both structural and semiconductor composites. The materials studied are SiC/Si, GaP/Si, and SiC fiber- and whisker-reinforced Si3N4.

Pirouz, P.↗

A fiber-resin micromechanics analysis of the delamination front in a DCB specimen

A 3-D finite element model was developed to analyze the fiber-resin behavior near the delamination front in a graphite-epoxy double cantilever beam (DCB) specimen. The specimen interior was analyzed using a typical one-fiber slice, represented by a local 3-D fiber-resin model. The resin stresses were computed for the resin-rich layer at the ply interface as well as for the regions between the fibers close to the delamination front. However, the computed strain energy release rate G sub I along the delamination front varied by less than two percent, and was within about four percent of the plane-strain value. The von Mises yield criterion was used to estimate the extent of yielding near the delamination front. The yielding extended ahead of the delamination and also developed between the fibers. Although the fibers had only a negligible effect on G sub I, they caused yielding within the ply and therefore could influence delamination fracture toughness. The normal and shear stresses at the fiber-resin interface were computed near the delamination front. These results suggest that multi-axial stress criteria may be required to analyze fiber-resin interfaces.

Crews, J. H.↗

Mullite fiber reinforced reaction bonded Si3N4 composites

Fracture toughnesses of brittle ceramic materials have been improved by introducing reinforcements and carefully tailored interface layers. Silicon carbide and Si3N4 have been emphasized as matrices of structural composites intended for high temperature service because they combine excellent mechanical, chemical, thermal and physical properties. Both matrices have been successfully toughened with SiC fibers, whiskers and particles for ceramic matrix composite (CMC) parts made by sintering, hot pressing or reaction forming processes. These SiC reinforced CMCs have exhibited significantly improved toughnesses at low and intermediate temperature levels, as well as retention of properties at high temperatures for selected exposures; however, they are vulnerable to attack from elevated temperature dry and wet oxidizing atmospheres after the matrix has cracked. Property degradation results from oxidation of interface layers and/or reinforcements. The problem is particularly acute for small diameter (-20 tim) polymer derived SiC fibers used for weavable toes. This research explored opportunities for reinforcing Si3N4 matrices with fibers having improved environmental stability; the findings should also be applicable to SiC matrix CMCs.

Saleh, T.↗

Directionally Solidified Ceramics Produced

Produced Multiphase, interpenetrating structures are an alternative route to obtaining structural ceramic materials with adequate strength, toughness, and stability for high-temperature aerospace applications. The eutectic architecture, a continuous-reinforcing phase within a higher volume phase or matrix, can be described as a naturally occurring, in situ composite. The phases of a eutectic are thermodynamically compatible at high homologous temperatures. Strong and stable materials have been produced. Toughness, however, remains a technical obstacle. The potential for producing materials with enhanced toughness along with adequate strength and stability was demonstrated using the laser-heated float zone (LHFZ) growth method at the NASA Glenn Research Center at Lewis Field. LHFZ growth at Glenn provides a means to efficiently produce and record the underlying growth phenomena associated with two-phase structures. To initiate directional solidification, a seed of single-crystal sapphire (<0001> direction) was lowered onto the molten liquid until wetting occurred and then withdrawn at a constant rate. Neither the crystal nor the source rod was rotated. The materials produced were tested mechanically in tension, and the resulting microstructure was examined with a scanning electron microscope. Both the inherent properties of the constituent phases and the properties of the interface between them affect the mechanical behavior and the fracture surfaces. The following scanning electron micrographs show the microstructures of two different materials that were tested to failure in tension. In the left micrograph, the flat fracture surface is typical of a material that is strong but has low toughness. In the right micrograph, the crack is effectively deflected at the interface between the two phases, achieving higher toughness at moderately lower strength levels. Conducting mechanical tests to determine the high temperature properties of these materials is the next step in determining their eventual suitability.

Farmer, Serene C.↗

Interfaces and failure mechanisms in Al-SiC composites

Aluminum alloys reinforced with silicon carbide whiskers exhibit significantly higher strength and modulus than the unreinforced alloys. However, the composites also exhibit low ductility and poor fracture toughness for reasons which are not well-understood. In this study, high resolution and conventional TEM techniques are used to analyze interface microstructure and failure mechanisms in P/M 2124 and 6061 aluminum alloys reinforced with silicon carbide whiskers. Interfacial oxides are typical of both composite materials, often distributed in clusters or in a discrete layer 2-5 nm thick along the whisker-matrix interface. Highly deformed regions beneath bulk tensile fracture surfaces reveal possible fracture nucleation centers as well as sites of stress concentration where intense plastic strain has occurred. Observations of such highly deformed regions include (1) void initiation at whisker ends, (2) interface decohesion involving the thin oxide layer, (3) transverse cracks in whiskers, and (4) cracks in large constituent particles. TEM results are presented and discussed in relation to mechanisms of composite failure.

Nutt, S. R.↗

NASA Tech Briefs, October 2013

Topics include: A Short-Range Distance Sensor with Exceptional Linearity; Miniature Trace Gas Detector Based on Microfabricated Optical Resonators; Commercial Non-Dispersive Infrared Spectroscopy Sensors for Sub-Ambient Carbon Dioxide Detection; Fast, Large-Area, Wide-Bandgap UV Photodetector for Cherenkov Light Detection; Mission Data System Java Edition Version 7; Adaptive Distributed Environment for Procedure Training (ADEPT); LEGEND, a LEO-to-GEO Environment Debris Model; Electronics/Computers; Millimeter-Wave Localizers for Aircraft-to-Aircraft Approach Navigation; Impedance Discontinuity Reduction Between High-Speed Differential Connectors and PCB Interfaces; SpaceCube Version 1.5; High-Pressure Lightweight Thrusters; Non-Magnetic, Tough, Corrosion- and Wear-Resistant Knives From Bulk Metallic Glasses and Composites; Ambient Dried Aerogels; Applications for Gradient Metal Alloys Fabricated Using Additive Manufacturing; Passivation of Flexible YBCO Superconducting Current Lead With Amorphous SiO2 Layer; Propellant-Flow-Actuated Rocket Engine Igniter; Lightweight Liquid Helium Dewar for High-Altitude Balloon Payloads; Method to Increase Performance of Foil Bearings Through Passive Thermal Management; Unibody Composite Pressurized Structure; JWST Integrated Science Instrument Module Alignment Optimization Tool; Radar Range Sidelobe Reduction Using Adaptive Pulse Compression Technique; Digitally Calibrated TR Modules Enabling Real-Time Beamforming SweepSAR Architectures; Electro-Optic Time-to-Space Converter for Optical Detector Jitter Mitigation; Partially Transparent Petaled Mask/Occulter for Visible-Range Spectrum; Educational NASA Computational and Scientific Studies (enCOMPASS); Coarse-Grain Bandwidth Estimation Scheme for Large-Scale Network; Detection of Moving Targets Using Soliton Resonance Effect; High-Efficiency Nested Hall Thrusters for Robotic Solar System Exploration; High-Voltage Clock Driver for Photon-Counting CCD Characterization; Development of the Code RITRACKS; and Enabling Microliquid Chromatography by Microbead Packing of Microchannels.

Source record↗

Effects of fiber, matrix, and interphase on carbon fiber composite compression strength

The major goal of this project was to obtain basic information on compression failure properties of carbon fiber composites. To do this, we investigated fiber effects, matrix effects, and fiber/matrix interface effects. Using each of nine fiber types, we prepared embedded single-fiber specimens, single-ply specimens, and full laminates. From the single-fiber specimens, in addition to the standard fragmentation test analysis, we were able to use the low crack density data to provide information about the distribution of fiber flaws. The single-ply specimens provided evidence of a correlation between the size of kink band zones and the quality of the interface. Results of the laminate compression experiments mostly agreed with the results from single-ply experiments, although the ultimate compression strengths of laminates were higher. Generally, these experiments showed a strong effect of interfacial properties. Matrix effects were examined using laminates subjected to precracking under mixed-mode loading conditions. A large effect of precracking conditions on the mode 1 toughness of the laminates was found. In order to control the properties of the fiber/matrix interface, we prepared composites of carbon fiber and polycarbonate and subjected these to annealing. The changes in interfacial properties directly correlated with changes in compression strength.

Nairn, John A.↗

Fracture behavior of the Space Shuttle thermal protection system

Stable crack-growth and fracture-toughness experiments were conducted using precracked specimens machined from LI-900 reusable surface insulation (RSI) tiles of the Space Shuttle thermal protection system (TPS) at room temperature. Similar fracture experiments were conducted on fracture specimens with preexisting cracks at the interface of the tile and the strain isolation pad (SIP). Stable crack growth was not observed in the LI-900 tile fracture specimens which had a fracture toughness of 12.0 kPa sq rt of m. The intermittent subcritical crack growth at the tile-pad interface of the fracture specimens was attributed to successive local pull-outs due to tensile overload in the LI-900 tile and cannot be characterized by linear elastic fracture mechanics. No subcritical interfacial crack growth was observed in the fracture specimens with densified LI-900 tiles where brittle fracture initiated at an interior point away from the densification.

Komine, A.↗

Fracture Toughness Evaluation of Space Shuttle External Tank Thermal Protection System Polyurethane Foam Insulation Materials

Experimental evaluation of the basic fracture properties of Thermal Protection System (TPS) polyurethane foam insulation materials was conducted to validate the methodology used in estimating critical defect sizes in TPS applications on the Space Shuttle External Fuel Tank. The polyurethane foam found on the External Tank (ET) is manufactured by mixing liquid constituents and allowing them to react and expand upwards - a process which creates component cells that are generally elongated in the foam rise direction and gives rise to mechanical anisotropy. Similarly, the application of successive foam layers to the ET produces cohesive foam interfaces (knitlines) which may lead to local variations in mechanical properties. This study reports the fracture toughness of BX-265, NCFI 24-124, and PDL-1034 closed-cell polyurethane foam as a function of ambient and cryogenic temperatures and knitline/cellular orientation at ambient pressure.

McGill, Preston↗