Unveiling the Liquid Electrolyte Solvation Structure by Small Angle X-ray Scattering

The fundamental understanding of the liquid electrolyte (LE) solvation structure and electrode–electrolyte interface behavior will bring more in-depth thinking and revolutionary changes to the entire electrochemical energy storage field. Regardless of the variety of techniques available, the methods employed to investigate electrolyte solvation structures over a long-range are severely limited. Small-angle X-ray scattering (SAXS) is an ideal complement to Raman spectroscopy, Fourier transform infrared spectroscopy, or nuclear magnetic resonance, which offers a unique perspective from a larger scale on clusters or networks in electrolytes. Understanding the solvation structures from a few angstroms to hundreds of nanometers will undoubtedly lay a good foundation for studying the macroscopic transport properties, such as viscosity and ionic conductivity, of the LEs. Here, in this Perspective, we discuss the use of SAXS to investigate the solvation structures in different electrolyte systems, a prospect for the SAXS broader application in the electrolyte study, and some challenges that need to be solved in the SAXS application.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Investigation of electrode-electrolyte interfaces to enable non-flammable Li-ion batteries operating up to 125°C with liquid electrolyte

Non-flammable and high-temperature stable ionic liquid (IL)-based electrolytes could eliminate catastrophic battery failures and improve battery safety, but their poor electrochemical interaction with the LiNi x Mn y Co z O 2 (NMC) family of cathodes is a long-standing problem due to severe parasitic reactions at high temperature. Understanding surface and bulk structural mechanisms of NMC-type cathodes at elevated operational temperature is of paramount importance to facilitate stable electrochemical performance. Here, we report a non-flammable phosphonium IL-based cell chemistry that offers stable electrode-electrolyte interfaces, leading to electrochemical performance up to 125°C and high-temperature safety. We combine electrochemistry with multimodal X-ray spectroscopy methods to understand interfaces at elevated temperature (100°C). This nanoscale understating enables a proof-of-concept high-temperature cylindrical cell (14500), and the design achieves an average Coulombic efficiency of ≈99.5% up to 300 cycles at 100°C. The results ascertain the significance of depth-dependent degradation at the interface, guiding room-temperature Li-ion technology toward extreme-temperature applications.

36 MATERIALS SCIENCE↗

Structure–Capacitance Relationships of Graphene/Ionic Liquid Electrolyte Double Layers

The differential capacitance profile of electrochemical interfaces reflects the physical properties of the double layer. For carbon electrodes and ionic liquid based electrolytes, these capacitance profiles are not fully understood. In this work, we utilize constant voltage molecular dynamics simulations to compute differential capacitance profiles of ionic liquids [BMIm + ][BF 4 - ] and [BMIm + ][TFSI - ] mixed with acetonitrile and 1,2-dichloroethane, at model graphene electrodes. We find that both pure and 10% mole fraction ionic liquid electrolytes exhibit camel shaped capacitance profiles with two peaks on either side of a minimum centered at the potential of zero charge. This profile shape results from electric field induced rearrangement of ion structure within the inner layer closest to the electrode interface. At low potential, the ionic liquid inner layer is concentrated with non-polar tri-fluoromethyl and butyl functional groups of the anions and cations, corresponding to the minimum of the capacitance profiles. With increasing voltage, electrostatic interactions of polar/charged functional groups with the electrode surface compete with these non-polar interactions, leading to ion rearrangement that increases the inner layer charge density and results in higher capacitance. After the ion restructuring is complete, the response saturates and capacitance diminishes. The presence of organic solvent significantly changes the composition of the inner layer. For example, strong non-polar interactions between dichloroethane molecules and the graphene surface substantially block ion/electrode contact at moderate potentials. Overall, our simulations highlight the dynamic nature of the inner region of organic electrolyte double layers, and the sensitive dependence on electrolyte composition and applied voltage.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Spatially resolved structural order in low-temperature liquid electrolyte

Determining the degree and the spatial extent of structural order in liquids is a grand challenge. Here, we are able to resolve the structural order in a model organic electrolyte of 1 M lithium hexafluorophosphate (LiP 6 ) dissolved in 1:1 (v/v) ethylene carbonate:diethylcarbonate by developing an integrated method of liquid-phase transmission electron microscopy (TEM), cryo-TEM operated at -30°C, four-dimensional scanning TEM, and data analysis based on deep learning. This study reveals the presence of short-range order (SRO) in the high–salt concentration domains of the liquid electrolyte from liquid phase separation at the low temperature. Molecular dynamics simulations suggest the SRO originates from the Li + - (PF 6 - ) n (n > 2) local structural order induced by high LiP 6 salt concentration.

42 ENGINEERING↗

Ambipolar Electrochemistry of Pre‐Intercalated Ti 3 C 2 T x MXene in Ionic Liquid Electrolyte

Abstract Cation intercalation with or without redox remains the dominant charge storage mechanism for two‐dimensional (2D) Ti 3 C 2 T x MXene. Anion‐based charge storage remains unexplored due to intrinsic negative surface charge of MXenes preventing spontaneous intercalation of anions and irreversible oxidation of Ti at anodic potentials in aqueous electrolytes. In this work, we report on the ambipolar electrochemical behavior of the Ti 3 C 2 T x in ionic liquid electrolyte over a 2.5 V electrochemically stable window. The experiments are conducted on a thin Ti 3 C 2 T x film current collector coated with an electroactive layer of small flakes (∼150 nm) of Ti 3 C 2 T x pre‐intercalated with 1‐ethyl‐3‐methylimidazolium bis‐(trifluoromethylsulfonyl)‐imide (EMIM‐TFSI) ionic liquid. Couples of redox peaks with a very small potential separation during the voltage sweep are observed at high negative (−0.75 V vs. Ag wire) and high positive (+0.75 V vs. Ag wire) potentials. Our experimental electrochemical data combined with density functional theory (DFT) calculations suggest feasibility of pseudo‐intercalation of TFSI anions between Ti 3 C 2 T x flakes. This study provides a pathway for elucidating anion intercalation for different MXene chemistries in solvent‐free electrolytes, which can lead to development of MXene based energy storage devices with improved performance.

Electrochemistry↗

Effect of Liquid Electrolyte Soaking on the Interfacial Resistance of Li 7 La 3 Zr 2 O 1 2 for All-Solid-State Lithium Batteries

In this work, the impact of liquid electrolyte soaking on the interfacial resistance between the garnet-structured Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte and metallic lithium has been studied. Lithium carbonate (Li 2 CO 3 ) formed by inadvertent exposure of LLZO to ambient conditions is generally known to increase interfacial impedance and decrease lithium wettability. Soaking LLZO powders and pellets in the electrolyte containing lithium tetrafluoroborate (LiBF 4 ) shows a significantly reduced interfacial resistance and improved contact between lithium and LLZO. Raman spectroscopy, X-ray diffraction, and soft X-ray absorption spectroscopy reveal how Li 2 CO 3 is continuously removed with increasing soaking time. On-line mass spectrometry and free energy calculations show how LiBF 4 reacts with surface carbonate to form carbon dioxide. Using a very simple and scalable process that does not involve heat-treatment and expensive coating techniques, we show that the Li–LLZO interfacial resistance can be reduced by an order of magnitude.

25 ENERGY STORAGE↗

Low-Temperature Characterization of a Nonaqueous Liquid Electrolyte for Lithium Batteries

Rechargeable batteries exhibit poor performance at low temperatures due to sluggish ion transport through the electrolytic phase. Ion transport is governed by three transport parameters—conductivity, diffusion coefficient, and the cation transference number with respect to the solvent velocity—and the thermodynamic factor. Understanding how these parameters change with temperature is necessary for designing improved electrolytes. In this work, we combine electrochemical techniques with electrophoretic NMR to determine the temperature dependence of these parameters for a liquid electrolyte, LiTFSI salt dissolved in tetraglyme between −20 and 45 °C. At colder temperatures, all species in the electrolyte tend to move more slowly due to increasing viscosity, which translates to a monotonic decrease in conductivity and diffusion coefficient with decreasing temperature. Surprisingly, we find that the field-induced velocity of solvent molecules at a particular salt concentration is a nonmonotonic function of temperature. The cation transference number with respect to the solvent velocity thus exhibits a complex dependence on temperature and salt concentration. The measured thermodynamic and transport properties are used to predict concentration gradients that will form in a lithium-lithium symmetric cell under a constant applied potential as a function of temperature using concentrated solution theory. The calculated steady current at −20 °C is lower than that at 45 °C by roughly two orders of magnitude.

25 ENERGY STORAGE↗

Identifying High Ionic Conductivity Compositions of Ionic Liquid Electrolytes Using Features of the Solvation Environment

Binary mixtures of ionic liquids with molecular solvents are gaining interest in electrochemical applications due to the improvement in their performance over neat ionic liquids. Dilution with suitable molecular solvents can reduce the viscosity and facilitate faster diffusion of ions, thereby yielding substantially higher ionic conductivity than that for a pure ionic liquid. Although viscosity and diffusion coefficients typically behave as monotonic functions of concentration, ionic conductivity often passes through a peak value at an optimum molar ratio of the molecular solvent to the ionic liquid. The ionic conductivity maximum is generally explained in terms of a balance between the ease of charge transport and the concentration of the charge carriers. In this work, fluctuation in the local environment surrounding an ion is invoked as a plausible explanation for the ionic conductivity mechanism with a binary mixture of 1-ethyl-3-methylimidazolium tetrafluoroborate and ethylene glycol as an example. The magnitude of the dynamism in the local environment is captured by measuring the spatial and temporal features of the solvation environment. Standard deviation in the number of ions in the solvation environment serves as a spatial feature, while the cage correlation lifetimes for oppositely charged ions within the first solvation shell serve as a temporal feature. Large standard deviations in the cluster ion population and short cage correlation lifetimes are indicators of highly dynamic ionic environment at the molecular level and consequently yield high ionic conductivity. Such compositions were found to be in good agreement with the optimum ionic liquid mole fractions obtained through experimental measurement. Short cage correlation lifetimes enable the identification of optimum mixture compositions using simulation trajectories significantly shorter than those required to implement the Nernst–Einstein or Einstein formalisms for calculating ionic conductivity. We validated the applicability of this approach across force fields and in six ionic liquid-molecular solvent electrolytes formed with combination of cations, anions, and solvents. We offer a computationally efficient approach of screening ionic liquid-molecular solvent binary mixture electrolytes to identify molar ratios that yield high ionic conductivity.

25 ENERGY STORAGE↗

Lithium Solvation and Mobility in Ionic Liquid Electrolytes with Asymmetric Sulfonyl-Cyano Anion

The solvation structure and transport properties of Li + in ionic liquid (IL) electrolytes based on n-methyl-n-butylpyrrolidinium cyano(trifluoromethanesulfonyl)imide [PYR 14 ][CTFSI] and [Li][CTFSI] (0 ≤ x Li ≤ 0.7) were studied by Raman and Nuclear Magnetic Resonance (NMR) diffusometry, and molecular dynamics (MD) simulations. At x Li < 0.3, Li + coordination is dominated by the cyano group. As x Li is increased, free cyano-sites become limited, resulting in increased coordination via the sulfonyl group. Here, the 1:1 mixture of the symmetric anions bis(trifluoromethanesulfonyl)imide ([TFSI]) and dicyanamide ([DCA]) results in similar physical properties as the IL with [CTFSI]. However, anion asymmetry is shown to increase Li-salt solubility and promote Li+ transference. The lifetimes of Li + -cyano coordination for [CTFSI] are calculated to be shorter than those for [DCA], indicating that the competition from the sulfonyl group weakens its solvation with Li + . This resulted in higher Li + transference for the electrolyte with [CTFSI]. In relation to the utility of these electrolytes in energy storage, the Li–LiFePO 4 half cells assembled with IL electrolyte (x Li = 0.3, 0.5, and 0.7) demonstrated a nominal capacity of 140 mAh/g at 0.1C rate and 90 °C where the cell with x Li = 0.7 IL electrolyte demonstrated 61% capacity retention after 100 cycles and superior rate capability owing to increased electrochemical stability.

25 ENERGY STORAGE↗

Ionic liquid electrolyte for lithium-ion batteries

The ionic liquids disclosed herein are salts comprising a nitrogen or phosphorus such as a quaternary ammonium ion, a quaternary phosphonium ion, or an N-alkylated nitrogen heterocycle, and which include at least one functional substituent, e.g., a fluoro, cyano, carbonate ester, an alkenyl group, or an alkynyl group bonded to a carbon atom the cation. In a preferred embodiment, the cation is represented by the structure of Formula (I) as described herein.

Zhang, Zhengcheng↗

In Operando Calorimetric Measurements for Activated Carbon Electrodes in Ionic Liquid Electrolytes under Large Potential Windows

This study aims to investigate the effect of the potential window on heat generation in carbon-based electrical double layer capacitors (EDLCs) with ionic-liquid (IL)-based electrolytes using in operando calorimetry. The EDLCs consisted of two identical activated-carbon electrodes with either neat 1-butyl-1-methylpyrrolidinium bis(trifluoromethane-sulfonyl)imide ([Pyr 14 ][TFSI]) electrolyte or 1.0 m [Pyr 14 ][TFSI] in propylene carbonate (PC) as electrolyte. The instantaneous heat generation rate at each electrode was measured under galvanostatic cycling for different potential windows ranging from 1 to 4 V. First, the heat generation rates at the positive and negative electrodes differed significantly in neat IL owing to the differences in the ion sizes and diffusion coefficients. However, these differences were minimized when the IL was diluted in PC. Second, for EDLC in neat [Pyr 14 ][TFSI] at high potential window (4 V), a pronounced endothermic peak was observed at the beginning of the charging step at the positive electrode owing to TFSI - intercalation in the activated carbon. On the other hand, for EDLC in 1.0 m [Pyr 14 ][TFSI] in PC at potential window above 3 V, an endothermic peak was observed only at the negative electrode owing to the decomposition of PC. Third, for both neat and diluted [Pyr 14 ][TFSI] electrolytes, the irreversible heat generation rate increased with increasing potential window and exceeded Joule heating. This was attributed to the effect of potential-dependent charge redistribution resistance. Additionally, a further increase in the irreversible heat generation rate was observed for the largest potential windows owing to the degradation of the PC solvent. Finally, for both types of electrolyte, the reversible heat generation rate increased with increasing potential window because of the increase in the amount of ion adsorbed/desorbed at the electrode/electrolyte interface.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Diffusion coefficient and nucleation density studies on electrochemical deposition of aluminum from chloroaluminate ionic liquid electrolytes

In this study, aluminum was electrodeposited from ionic liquids comprising a melt of alkyl imidazolium chlorides and aluminum chloride (AlCl 3 ). The ionic liquids utilized in this study were 1-ethyl-3-methyl-imidazolium chloride (EMIC)-AlCl 3 , 1-butyl-3-methylimidazolium chloride (BMIC)-AlCl 3 , and 1-hexyl-3-methyl-imidazolium chloride (HMIC)-AlCl 3 at the AlCl 3 mole fraction of 0.667 (molar ratio of 1:2). The electrochemical behavior of chloroaluminate species in the three ionic liquids was investigated by cyclic voltammetry (CV) and chronoamperometry (CA) techniques at different temperatures. The cyclic voltammograms indicated that the reduction of Al 2 Cl 7 – species to metallic aluminum followed a diffusion-controlled phenomenon. Moreover, even at a less negative applied potential, the higher current density was obtained for EMIC-AlCl 3 ionic liquid. That indicates that EMIC-AlCl 3 favors less energy consumption during the electrodeposition. The chronoamperometric analysis revealed that the onset of aluminum deposition from such ionic liquids proceeds via a three-dimensional instantaneous nucleation process. The concentrations of Al 2 Cl 7 – ions in the ionic liquids were calculated based on the thermodynamic data, which were 2520, 2271, and 2035 mol m –3 for EMIC-AlCl 3 , BMIC-AlCl 3 , and HMIC-AlCl 3 , respectively. The diffusion coefficient (D) values of Al 2 Cl 7 – species in such ionic liquids were also calculated at various temperatures. The D values determined from the CA technique at 363 K are 2.16 × 10 –11 , 1.03 × 10 –11 , and 0.87 × 10 –11 m 2 s –1 for EMIC-AlCl 3 , BMICAlCl 3 , and HMIC-AlCl 3 , respectively. In addition, the D value increased as temperature increased and decreased as the hydrocarbon group in the ionic liquid increased. As a result, the calculated grain sizes of nucleation range from 2 to 4 μm for these ionic liquids and are in good agreement with experimental data obtained from SEM micrographs.

42 ENGINEERING↗

High Current Cycling in a Superconcentrated Ionic Liquid Electrolyte to Promote Uniform Li Morphology and a Uniform LiF-Rich Solid Electrolyte Interphase

High-energy-density systems with fast charging rates and suppressed dendrite growth are critical for the implementation of efficient and safe next-generation advanced battery technologies such as those based on Li metal. However, there are few studies that investigate reliable cycling of Li metal electrodes under high-rate conditions. in this work, by employing a superconcentrated ionic liquid (IL) electrolyte, we highlight the effect of Li salt concentration and applied current density on the resulting Li deposit morphology and solid electrolyte interphase (SEI) characteristics, demonstrating exceptional deposition/dissolution rates and efficiency in these systems. Operation at higher current densities enhanced the cycling efficiency, e.g., from 64 ± 3% at 1 mA cm –2 up to 96 ± 1% at 20 mA cm –2 (overpotential <±0.2 V), while resulting in lower electrode resistance and dendrite-free Li morphology. A maximum current density of 50 mA cm –2 resulted in 88 ± 3% cycling efficiency, displaying tolerance for high overpotentials at the Ni working electrode (0.5 V). X-ray photoelectron microscopy (XPS), time-of-flight secondary-ion mass spectroscopy (ToF-SIMS), and scanning electron microscopy (SEM) surface measurements revealed that the formation of a stable SEI, rich in LiF and deficient in organic carbon species, coupled with nondendritic and compact Li morphologies enabled enhanced cycling efficiency at higher currents. Reduced dendrite formation at high current is further highlighted by the use of a highly porous separator in coin cell cycling (1 mAh cm –2 at 50 °C), sustaining 500 cycles at 10 mA cm –2 .

25 ENERGY STORAGE↗

Rational Design of Weakly‐Solvating Molecules for Salt‐In‐Pre‐Ionic‐Liquid Electrolytes for Li Metal Batteries

Lithium metal batteries (LMBs) promise step‐changes in energy densities but suffer from poor cycle life due to unstable electrolyte‐lithium interfaces. Conventional carbonate electrolytes exhibit excessive lithium‐ion solvation and low oxidative stability, leading to rapid capacity loss. Herein, we report a rationally designed weakly‐solvating cyclic sulfonamide, 1‐trifluoromethanesulfonyl)amide pyrrolidine (TFMSPyr), which integrates an electron‐withdrawing trifluoromethanesulfonyl functional group at pyrrolidinic‐N. TFMSPyr acts as a pre‐ionic‐liquid solvent that forms intrinsically localized, anion‐dominated solvation, coupling molecular architecture, solvation topology, and transport dynamics. As a result, LiFSI based salt‐in‐pre‐ionic‐liquid (SIPIL) electrolytes exhibit high lithium‐ion transference number, oxidative stability > 5 V versus Li/Li + and anion‐derived solid electrolyte interphases (SEI). Li||Cu cells with SIPIL deliver a first cycle Coulombic efficiency (CE) of ≈ 99% with average CE of 99.2% for 100 cycles, and lithium half‐cells with lithium iron phosphate (LFP) cathode exhibit 82% capacity retention after 400 cycles with CE of 99.98%. In anode‐free full cells, 95% of initial capacity is retained after 63 cycles with an average CE of 99.5%. These results demonstrate that molecular engineering of solvents offers a powerful pathway to stabilize lithium metal interfaces and enable practical Anodeless LMBs.

25 ENERGY STORAGE↗

Multicomponent Phase Separation in Ternary Mixture Ionic Liquid Electrolytes

We investigate the phase behavior of ternary mixtures of ionic liquid, organic solvent, and lithium salt by molecular dynamics simulations. We find that at room temperature, the electrolyte separates into distinct phases with specific compositions; an ion-rich domain that contains a fraction of solvent molecules and a second domain of pure solvent. Here, the phase separation is shown to be entropy-driven and is independent of lithium salt concentration. Phase separation is only observed at microsecond time scales and greatly affects the transport properties of the electrolyte.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Do Deep Eutectic Solvents Behave Like Ionic Liquid Electrolytes? A Perspective from the Electrode-Electrolyte Interface

The differential capacitance as a function of potential and composition for choline chloride (ChCl) and ethylene glycol (EG) at 1:2,1:4, 1:6, and 1:20 molar ratios were studied using electrochemical impedance spectroscopy (EIS) on glassy carbon. In addition, ChCl:EG at the known ethaline DES composition (1:2) and 1:20 molar ratio were studied on Au and Pt electrodes, and compared to glyceline (ChCl:glycerol, 1:2). The capacitance-potential curves on glassy carbon were best interpreted by the modified Gouy-Chapman model. A dampened U-shape was observed similar to dilute electrolytes, however, the non-negligible ionic and H-bonding interactions in these electrolytes resulted in ambiguity about the point of zero charge where capacitance was weakly dependent on potential. Additionally, the differential capacitance was independent of composition on glassy carbon due to limited availability of mobile free ions and constraints by solvated ion sizes within the interface. Increases in capacitance are observed with Au as a result of desolvation and specific adsorption of Cl, and with Pt upon decreased Cl concentrations. These results indicate DESs and H-bonded electrolytes with high salt concentrations are distinct from ionic liquids and present no pronounced over screening or crowding with applied potential.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Heat generation in electric double layer capacitors with neat and diluted ionic liquid electrolytes under large potential window between 5 and 80 °C

Here, this study investigates the effect of temperature on the heat generation and the associated electrochemical phenomena occurring in IL-based EDLCs. The EDLCs consisted of two identical activated carbon electrodes with neat Pyr14TFSI or Pyr14TFSI diluted in propylene carbonate (PC) as electrolytes. The instantaneous heat generation rate at each electrode was measured by isothermal calorimetry between 5 and 80 °C under constant current cycling and potential window of 2.5 V. First, the instantaneous heat generation rate was similar at each electrode in neat IL. However, it was smaller at the negative electrode in diluted IL and featured endothermic dips growing with increasing temperature > 40 °C due to overscreening effects, ion desolvation, and/or decomposition of PC. The irreversible heat generation was similar in each half-cell and decreased with increasing temperature due to the reduction in internal resistance, particularly with neat IL. The irreversible heat generation exceeded Joule heating in all cases, especially at high temperature and low current. This was attributed to ion desorption and charge redistribution in the porous electrodes. Finally, the reversible heat generation for both electrolytes was larger at the positive than at the negative electrode due to the difference in anion and cation sizes.

25 ENERGY STORAGE↗