Search NASA⌕ Search

SEARCH · Search NASA

Results for “nanocrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Improving Corrosion Resistance and Corrosive Wear Resistance of Aluminum Alloy Drill Pipe by Surface Nanocrystallization and Micro-arc Oxidation

To improve the corrosion and wear resistance performance of aluminum alloy drill pipes in geological and petroleum drilling applications, a strengthening coating was prepared on the surface of the 2618 aluminum alloy by combining treatment with ultrasonic cold forging technology (UCFT) and micro-arc oxidation (MAO). The effects of the strengthening coating on the corrosion and wear resistance of the aluminum alloy were evaluated by electrochemical and tribological tests. The results demonstrated that the corrosion and wear resistance of the aluminum alloy were improved by the UCFT and MAO technologies, especially the salt corrosion resistance. The corrosion morphology of the strengthening coating primarily included pitting, micro-cracks and NaCl attachment. In addition, the UCFT + MAO composite coating exhibited the best wear performance. The wear rate of the UCFT + MAO composite coating was lower than that of the aluminum alloy by 94%. The results provided support for this excellent surface treatment technology for the corrosion and wear resistance of aluminum alloy drill pipes, and they also present a feasible evaluation method for drill pipes.

36 MATERIALS SCIENCE↗

Amorphization and nanocrystallization of silcon under shock compression

High-power, short-duration, laser-driven, shock compression and recovery experiments on [001] silicon unveiled remarkable structural changes above a pressure threshold. Two distinct amorphous regions were identified: (a) a bulk amorphous layer close to the surface and (b) amorphous bands initially aligned with {111} slip planes. Further increase of the laser energy leads to the re-crystallization of amorphous silicon into nanocrystals with high concentration of nano-twins. This amorphization is produced by the combined effect of high magnitude hydrostatic and shear stresses under dynamic shock compression. Shock-induced defects play a very important role in the onset of amorphization. Calculations of the free energy changes with pressure and shear, using the Patel-Cohen methodology, are in agreement with the experimental results. Molecular dynamics simulation corroborates the amorphization, showing that it is initiated by the nucleation and propagation of partial dislocations. As a result, the nucleation of amorphization is analyzed qualitatively by classical nucleation theory.

36 MATERIALS SCIENCE↗

Kinetics of Mg[subscript 6]Ni nanocrystallization in amorphous Mg[subscript 83]Ni[subscript 17]

A comprehensive crystallization kinetics study was carried out in order to understand the mechanism of formation of a Mg-rich nanocrystalline Mg{sub 6}Ni phase in a metallic glass with similar overall composition, Mg{sub 83}Ni{sub 17}. Adequate description of the transformation kinetics was obtained by the JMKA equation with an integer Avrami exponent n = 4, associated with nucleation and three-dimensional linear growth crystallization mechanism. To study the nanocrystals growth mechanism separately a controlled heat treatment of the amorphous alloy was applied and thus a three-dimensional growth with a constant rate was obtained (n = 3) for the pre-annealed alloys. For all transformation curves the dependence of n on the degree of transformation {alpha}, n({alpha}), was analyzed and the regions with constant n were defined. The correct separation of the processes of nucleation and crystal growth allowed reliable values for the activation energies of both nucleation and growth processes to be determined.

36 MATERIALS SCIENCE↗

Synthesis and characterization of rare-earth doped SrBi{sub 2}Nb{sub 2}O{sub 9} phase in lithium borate based nanocrystallized glasses

Glass composites comprising of un-doped and samarium-doped SrBi{sub 2}Nb{sub 2}O{sub 9} nanocrystallites are fabricated in the glass system 16.66SrO-16.66[(1-x)Bi{sub 2}O{sub 3}-xSm{sub 2}O{sub 3}]-16.66Nb{sub 2}O{sub 5}-50Li{sub 2}B{sub 4}O{sub 7} (0<=x<=0.5, in mol%) via the melt quenching technique. The glassy nature of the as-quenched samples is established by differential thermal analyses. Transmission electron microscopic studies reveal the presence of about 15 nm sized spherical crystallites of the fluorite-like SrBi{sub 1.9}Sm{sub 0.1}Nb{sub 2}O{sub 9} phase in the samples heat treated at 530 deg. C. The formation of layered perovskite-type un-doped and samarium-doped SrBi{sub 2}Nb{sub 2}O{sub 9} nanocrystallites with an orthorhombic structure through the intermediate fluorite phase is confirmed by X-ray powder diffraction and micro-Raman spectroscopic studies. The influence of samarium doping on the lattice parameters, lattice distortions, and the Raman peak positions of SrBi{sub 2}Nb{sub 2}O{sub 9} perovskite phase is clarified. The dielectric constants of the perovskite SrBi{sub 2}Nb{sub 2}O{sub 9} and SrBi{sub 1.9}Sm{sub 0.1}Nb{sub 2}O{sub 9} nanocrystals are relatively larger than those of the corresponding fluorite-like phase and the precursor glass. - Graphical Abstract: This figure shows the XRD patterns at room temperature for the as-quenched and heat treated samples in Sm{sub 2}O{sub 3}-doped (x=0.1) glass. Based on these results, it is concluded that the formation of samarium-doped perovskite SBN phase takes place via an intermediate fluorite-like phase in the crystallization of this glass.

36 MATERIALS SCIENCE↗

Surface nanocrystallization of Mg-3 wt.% Li-6 wt.% Al alloy by surface mechanical attrition treatment

A nanocrystalline surface layer was produced on Mg-3 wt.% Li-6 wt.% Al alloy by means of surface mechanical attrition treatment (SMAT). Microstructure features of various sections were systematically characterized by transmission electron microscopy. The results indicate that grain refinement induced by SMAT is dominated mainly by dislocation slip. Twinning is active at the early stage of grain refinement process when the grain size is large. The dislocation-dominated deformation mechanism is attributed to the change of c/a ratio due to the alloying of Li in Mg matrix and the suppression of twinning due to grain refinement. Nanoindentation results show that the hardness of the surface is enhanced by SMAT. - Highlights: •Nanocrystalline surface layer was produced on Mg-3 wt.%Li-6 wt.%Al alloy by SMAT. •Grain refinement induced by SMAT is dominated mainly by dislocation slip. •Twinning is active at the early stage of grain refinement process. •The hardness of the surface was enhanced by SMAT.

36 MATERIALS SCIENCE↗

Improving Er{sup 3+} 1.53 {mu}m luminescence by CeF{sub 3} nanocrystallization in aluminosilicate glass

In order to develop promising materials for the Er{sup 3+}-doped fiber amplifier, transparent glass ceramics containing hexagonal CeF{sub 3} nanocrystals were prepared by melt-quenching and subsequent heating. The obvious Stark splitting in the absorption and emission spectra, the intensification of the 1.53 {mu}m emission, and the prolongation of the Er{sup 3+}:{sup 4}I{sub 13/2} decay lifetime demonstrated the partition of Er{sup 3+} ions into the CeF{sub 3} nanocrystals. Evidently, the efficient cross-relaxation between Ce{sup 3+} and Er{sup 3+}, i.e., Er{sup 3+}:{sup 4}I{sub 11/2}+Ce{sup 3+}:{sup 2}F{sub 5/2}{yields}Er{sup 3+}:{sup 4}I{sub 13/2}Ce{sup 3+}:{sup 2}F{sub 7/2} led to the quenching of the upconversion and the enhancing of the desired Er{sup 3+} 1.53 {mu}m emission. Based on the emission and absorption spectra, it was further calculated that the glass ceramic possesses broad bandwidth as that of the ZBLAN glass, and large emission cross-section close to the silicate glass, for the 1.53 {mu}m emission.

36 MATERIALS SCIENCE↗

Nanocrystallization in a shear band: An in situ investigation

Preferential nanocrystal formation in shear bands that occurred upon applying a tensile strain on an Al-rich metallic glass has been analyzed in situ in a transmission electron microscope as a function of time after the shear band initiation and as a function of local heating. The results indicate the presence of a transient period before nanocrystal formation sets in, as well as the necessity of thermal activation and further show that nanocrystals developed only within the shear bands. These results support models that explain nanocrystal formation in shear bands based on an increased local mobility.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Low temperature magnetic behaviour of glass-covered magnetic microwires with gradient nanocrystalline microstructure

Slow nanocrystallization driving dynamics can be affected by the combination of two factors: sample residual stresses and sample geometry. This effect is evidenced at the initial stages of nanocrystallization of amorphous CoFeSiBCuNb magnetic microwires. Transmission electron microscopy observations indicate how crystallization at temperatures between 730 and 780 K results in a graded microstructure where the crystallization at the surface skin of the microwire, which remains almost amorphous, differs from that of the middle, where elongated grains are observed, and inner regions. However, samples annealed at higher temperatures present a homogeneous microstructure. The effect of gradient microstructure on magnetic properties has been also analyzed and a loss of bistable magnetic behaviour at low temperatures, from that obtained in the amorphous and fully nanocrystallized sample, has been observed and ascribed to changes in sign of magnetostriction for measuring temperatures below 100 K.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of geometrical constraint condition on the formation of nanoscale twins in the Ni-based metallic glass composite

We investigated the effect of geometrically constrained stress-strain conditions on the formation of nanotwins in alpha-brass phase reinforced Ni59Zr20Ti16Si2Sn3 metallic glass (MG) matrix deformed under macroscopic uniaxial compression. The specific geometrically constrained conditions in the samples lead to a deviation from a simple uniaxial state to a multi-axial stress state, for which nanocrystallization in the MG matrix together with nanoscale twinning of the brass reinforcement is observed in localized regions during plastic flow. The nanocrystals in the MG matrix and the appearance of the twinned structure in the reinforcements indicate that the strain energy is highly confined and the local stress reaches a very high level upon yielding. Both the effective distribution of reinforcements on the strain enhancement of composite and the effects of the complicated stress states on the development of nanotwins in the second-phase brass particles are discussed.

36 MATERIALS SCIENCE↗

Characterization of atomic-level structure in Fe-based amorphous and nanocrystalline alloy by experimental and modeling methods

The atomic structure of Fe{sub 70}Nb{sub 10}B{sub 20} alloy in “as-cast” state and after annealing was investigated using high-energy X-ray diffraction (XRD), Mössbauer spectroscopy (MS) and high resolution transmission electron microscopy (HRTEM). The HRTEM observations allowed to indicate some medium-range order (MRO) regions about 2 nm in size and formation of some kinds of short-range order (SRO) structures represented by atomic clusters with diameter ca. 0.5 nm. The Reverse Monte Carlo (RMC) method basing on the results of XRD measurements was used in modeling the atomic structure of Fe-based alloy. The structural model was described by peak values of partial pair correlation functions and coordination numbers determined by Mössbauer spectroscopy investigations. The three-dimensional configuration box of atoms was obtained from the RMC simulation and the representative Fe-centered clusters were taken from the calculated structure. According to the Gonser et al. approach, the measured spectra of alloy studied were decomposed into 5 subspectra representing average Fe–Fe coordination numbers. Basing on the results of disaccommodation of magnetic permeability, which is sensitive to the short order of the random packing of atoms, it was stated that an occurrence of free volume is not detected after nanocrystallization process. - Highlights: • Atomic cluster model of amorphous structure was proposed for studied glassy alloy. • Short range order (ca. 0.5 nm) regions interpreted as clusters were identified by HREM. • Clusters correspond to coordination numbers (N = 4,6,8,9) calculated by using Gonser approach. • Medium-range order (ca. 2 nm) could be referred to few atomic clusters. • SRO regions are able to grow up as nuclei of crystalline bcc Fe and iron borides. • Crystalline particles have spherical morphology with an average diameter of 20 nm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study of the scale formed on super 304H boiler tube steels after long-term steam oxidation at high temperatures

Highlights: • Steam oxidation tests were performed on the conventional and shot-peened Super304H boiler tube. • A continuous amorphous SiO{sub 2} layer separated the metal from the scale in shot-peened specimen. • The SiO{sub 2} layer enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} layers. • The scale on shot-peened specimens is stable upon steam temperature and time increase. Steam oxidation of a Super 304H boiler tube was performed at steam temperatures of 650 °C and 700 °C for time durations up to 5000 h. The oxidation scale outcomes which formed on as-received untreated and shot-peened (SP) tubes were studied using X-ray diffraction (XRD), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM). γ-Grain nanocrystallization on the surface of the SP specimen generated an abundant fraction of grain boundary that guaranteed the formation of a continuous amorphous SiO{sub 2} layer at the metal-scale interface that enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} in the scale. Scale breakaway along defects in the outer layer of the scale was accelerated by the steam temperature in the untreated specimens, whereas the scale that formed on the SP specimens appeared to be stable.

36 MATERIALS SCIENCE↗