At least 37 records · Page 2

Recrystallization of A Shot Peened Single Crystal Nickel-Base Superalloy

Single crystal nickel-base superalloys used as turbine engine airfoils can have much higher creep and thermal fatigue resistance required for blades and vanes than polycrystalline superalloys due to the absence of weak grain boundaries, as well as the low elastic modulus in the [001] single crystal growth direction (Refs. 1 and 2). This has allowed an increase in the turbine rim inlet temperatures for improved performance and efficiency. However, these advantages in performance require constraints on acceptable levels of single crystal defects, such as macroscopic grain boundaries at low angles to the primary grain (i.e., low angle boundaries or LAB), higher angle boundaries, small new grains nucleated at the blade surface (a.k.a. freckles), larger new grains, and also the single crystal blades’ orientation, typically degrees off of the [001] direction and the orientation of a transverse [010] direction with respect to blade geometry. Therefore, single crystal turbine airfoils, which are frequently used with as-cast surfaces, are grain etched and inspected before and after heat treatments to ensure these aspects conform to acceptability limits.

single crystal↗

Nickel-Based Superalloy Resists Embrittlement by Hydrogen

A nickel-based superalloy that resists embrittlement by hydrogen more strongly than does nickel alloy 718 has been developed. Nickel alloy 718 is the most widely used superalloy. It has excellent strength and resistance to corrosion as well as acceptably high ductility, and is recognized as the best alloy for many high-temperature applications. However, nickel alloy 718 is susceptible to embrittlement by hydrogen and to delayed failure and reduced tensile properties in gaseous hydrogen. The greater resistance of the present nickel-based superalloy to adverse effects of hydrogen makes this alloy a superior alternative to nickel alloy 718 for applications that involve production, transfer, and storage of hydrogen, thereby potentially contributing to the commercial viability of hydrogen as a clean-burning fuel. The table shows the composition of the present improved nickel-based superalloy in comparison with that of nickel alloy 718. This composition was chosen to obtain high resistance to embrittlement by hydrogen while maintaining high strength and exceptional resistance to oxidation and corrosion. The most novel property of this alloy is that it resists embrittlement by hydrogen while retaining tensile strength greater than 175 kpsi (greater than 1.2 GPa). This alloy exhibits a tensile elongation of more than 20 percent in hydrogen at a pressure of 5 kpsi (approximately equal to 34 MPa) without loss of ductility. This amount of elongation corresponds to 50 percent more ductility than that exhibited by nickel alloy 718 under the same test conditions.

Lee, Jonathan↗

Predictive design of novel nickel-based superalloys beyond Haynes 282

Nickel-based superalloys are in great demand for harsh-service conditions involving high temperatures and oxidative environments. Haynes 282 stands out due to its excellent high-temperature properties and easy fabricability. However, the upper operation temperature of Haynes 282 is limited due to its relatively low liquidus temperature. Equipped with high-fidelity density-functional theory calculations and high-throughput experimentation methodology, we explored new compositional spaces that exhibit higher liquidus temperature and higher strength. While maintaining the manufacturability, the newly designed alloy shows improved strength and ductility at room temperature and better oxidation resistance up to 800°C. Here, the new compositions showcase a minor change in the refractory and metalloid content can significantly impact the mechanical and oxidation performance of superalloys.

36 MATERIALS SCIENCE↗

A discrete dislocation dynamics study of precipitate bypass mechanisms in nickel-based superalloys

Order strengthening in nickel-based superalloys is associated with the extra stress required for dislocations to bypass the $\gamma'$ precipitates distributed in the $\gamma$ matrix. Depending on the operating conditions and microstructure, a rich variety of bypass mechanism has been identified, with various shearing and Orowan looping processes gradually giving way to climb bypass as the operating conditions change from the low/intermediate temperatures and high stress regime, to the high temperature and low stress regime. When anti phase boundary (APB) shearing and Orowan looping mechanisms operate, the classical picture is that, at for a given volume fraction, the bypass mechanism changes from shearing to looping with increased particle size and within a broad coexistence size window. Another possibility, which is supported by indirect experimental evidence, is that a third “hybrid” transition mechanism may operate. Here, in this paper we use discrete dislocation dynamics (DDD) simulations to study dislocation bypass mechanisms in Ni-based superalloys. We develop a new method to compute generalized stacking fault forces in DDD simulations, based on a concept borrowed from complex analysis and known as the winding number of a closed curve about a point. We use this method to study the mechanisms of bypass of a square lattice of spherical $\gamma'$ precipitates by $a/2\langle110\rangle$ {111} edge dislocations, as a function of the precipitates volume fraction and size. We show that not only the hybrid mechanism is possible, but also that it operates as the transition mechanism between the shearing and looping regimes over a wide range of precipitates volume fraction and radii. Based on our simulation results, we propose a simple model for the strength of this mechanism. We also consider the effects of a $\gamma$/$\gamma'$ lattice misfit on the bypass mechanisms, which we approximate by an additional precipitate stress computed according to Eshelby’s inclusion theory. We show that in the shearing and hybrid looping-shearing regimes, a lattice misfit generally results in an increased bypass stress. For sufficiently high lattice misfit, the critical bypass configuration in attractive dislocation-precipitates interactions changes dramatically, and the bypass stress is controlled by the pinning of the trailing dislocation on the exit side of the precipitates, similar to what has been reported in the high-temperature creep literature.

36 MATERIALS SCIENCE↗

Effects of silicon on the oxidation, hot-corrosion, and mechanical behavior of two cast nickel-base superalloys

Cast specimens of nickel-base superalloys 713C and Mar-M200 with nominal additions of 0, 0.5, and 1 wt% Si were evaluated for oxidation and corrosion resistance, tensile and stress-rupture properties, microstructure, and phase relations. Results are compared with those of an earlier study of the effects of Si in B-1900. Si had similar effects on all three superalloys. It improves oxidation resistance but the improvement in 713C and Mar-M200 was considerably less than in B-1900. Hot-corrosion resistance is also improved somewhat. Si is, however, detrimental to mechanical properties, in particular, rupture strength and tensile ductility. Si has two obvious microstructural effects. It increases the amount of gamma-prime precipitated in eutectic nodules and promotes a Mo(Ni,Si)2 Laves phase in the alloys containing Mo. These microstructural effects do not appear responsible for the degradation of mechanical properties, however.

Miner, R. V., Jr.↗

Fatigue-resistant nickel-base superalloys

New γ' strengthened nickel-base superalloy compositions are described that, when forged and properly heat treated, demonstrate superior resistance to fatigue crack growth accompanied by very good high temperature properties. Parts can be fabricated (e.g., using conventional cast and wrought processing) from these alloys without encountering difficulty in forging.

Keh-Minn Chang↗

Machine Learning Vacancy Formation Energy in Nickel-Based Superalloys

Creep performance plays a key role in nickel-based superalloys for high temeprature applications. Creep behavior depends on many parameters such as strength, dislocations, diffusivity, and microstructural stability in addition to temeprature, applied stress, and oxidation. This work focuses on predicting vacancy formation energy in nickel-based superalloys using machine learning approach. High-throughput density functional theory (DFT) calculations are performed on Ni-based alloys with the addition of various alloying elements to predict the vacancy formation energy and vacancy concentration. Machine learning is performed using various models including graph neural networks.

creep performance↗

Addition of silicon improves oxidation resistance of nickel based superalloys

Specific weight changes of nickel-base superalloy B-1900 and B-1900 + 1% Si specimens were tested at 1273 K. B-1900 was losing weight at an increasing rate due to spalling of oxide scale while B-1900 + 1% Si was still gaining weight at low, nearly constant rate. Similar comparison in weight change was observed for specimens tested at 1373 K.

Lowell, C. E.↗

Effects of processing and microstructure on the fatigue behaviour of the nickel-base superalloy Rene95

Forms of the nickel-base superalloy Rene95 produced by three processing methods were evaluated in tensile, low cycle fatigue and fatigue crack propagation tests at 540 and 650 C. Two powder-metallurgy (PM) forms, hot-isostatically-pressed and extruded-and-forged, and a conventionally cast-and-wrought form were all given the same heat treatment. The extruded-and-forged form showed superior fatigue life in low strain range tests though the two PM forms exhibited nearly identical mechanical behavior in all other respects. Further, this life difference could not be explained by significant differences in the types, sizes or shapes of the defects initiating failure. The cast-and-wrought Rene95, however, had lower strength, ductility and fatigue life, but higher fatigue crack propagation resistance because of a larger grain size. It did not exhibit the environmentally-assisted intergranular mode of propagation which occurs in PM Rene95 and other fine-grained superalloys at these test temperatures and frequencies.

Miner, R. V.↗

Compositional Effects on Nickel-Base Superalloy Single Crystal Microstructures

Fourteen nickel-base superalloy single crystals containing 0 to 5 wt% chromium (Cr), 0 to 11 wt% cobalt (Co), 6 to 12 wt% molybdenum (Mo), 0 to 4 wt% rhenium (Re), and fixed amounts of aluminum (Al) and tantalum (Ta) were examined to determine the effect of bulk composition on basic microstructural parameters, including gamma' solvus, gamma' volume fraction, volume fraction of topologically close-packed (TCP) phases, phase chemistries, and gamma - gamma'. lattice mismatch. Regression models were developed to describe the influence of bulk alloy composition on the microstructural parameters and were compared to predictions by a commercially available software tool that used computational thermodynamics. Co produced the largest change in gamma' solvus over the wide compositional range used in this study, and Mo produced the largest effect on the gamma lattice parameter and the gamma - gamma' lattice mismatch over its compositional range, although Re had a very potent influence on all microstructural parameters investigated. Changing the Cr, Co, Mo, and Re contents in the bulk alloy had a significant impact on their concentrations in the gamma matrix and, to a smaller extent, in the gamma' phase. The gamma phase chemistries exhibited strong temperature dependencies that were influenced by the gamma and gamma' volume fractions. A computational thermodynamic modeling tool significantly underpredicted gamma' solvus temperatures and grossly overpredicted the amount of TCP phase at 982 C. Furthermore, the predictions by the software tool for the gamma - gamma' lattice mismatch were typically of the wrong sign and magnitude, but predictions could be improved if TCP formation was suspended within the software program. However, the statistical regression models provided excellent estimations of the microstructural parameters based on bulk alloy composition, thereby demonstrating their usefulness.

MacKay, Rebecca A.↗

Slip band characteristics in the presence of grain boundaries in nickel-based superalloy

Shear strain profiles along slip bands in a modified Rolls-Royce nickel superalloy (RR1000) were analyzed for a tensile sample deformed by 2%. The strain increased with distance away from a grain boundary (GB), with maximum shear strain towards the center of the grain, indicating that dislocation nucleation generally occurred in the grain interior. The strain gradients in the neighborhood of the GBs were quantified and generally correlated with rotation about the active slip system line direction. This leads to an ability to determine the active slip system in these regions. The dislocation spacing and pileup stresses were inferred. The dislocation spacing closely follows an Eshelby analytical solution for a single ended pileup of dislocations under an applied stress. The distribution of pileup stress values for GBs of a given misorientation angle follows a log-normal distribution, with no correlation between the pileup stress and the GB misorientation angle. Furthermore, there is no observed correlation between various transmissivity factors and slip band pileup stress. Hence it appears that the obstacle strength of any of the observed GBs is adequate to facilitate the dislocation pileups present in the slip bands. However, slip band transmission does correlate with transmissivity factors, with the current study focusing on the Luster and Morris m’-factor. Observation of strain profiles of transmitted bands indicate dislocation nucleation locations.

36 MATERIALS SCIENCE↗

Requirements of constitutive models for two nickel-base superalloys

The constitutive behavior of two nickel-base superalloys, Rene '80 and Inconel 718, utilized in gas turbine blade and disk components, respectively, is presented. In turbine blade applications, the high homologous temperatures result in strain-rate effects dominating behavior. In turbine disks, the temperatures are cooler so that mean stress effects become important. The impact of these two variables on the overall crack initiation lifetime and analysis methodology is discussed.

Laflen, J. H.↗

The correlation between the temperature dependence of the CRSS and the formation of superlattice-intrinsic stacking faults in the nickel-base superalloy PWA 1480

The PWA 1480 nickel-base superalloy is known to exhibit a unique minimum in the critical resolved shear stress (CRSS) at about 400 C. This paper reports an observation of a deformation mechanism whose temperature dependence correlates exactly with the reduction in the CRSS. It was found that, after monotonic or cyclic deformation of PWA 1480 at 20 C, the deformation substructures typically contain high density of superlattice-intrinsic stacking faults (S-ISFs) within the gamma-prime precipitates. As the temperature of deformation is increased, the density of S-ISFs is reduced, until finally no faults are observed after deformation in the range from 400 to 705 C. The reduction in the fault density corresponds exactly to the reduction in the CRSS, and the temperature at which the fault density is zero corresponds with the minimum in the CRRS. Two possible mechanisms related to the presence of the S-ISFs in the alloy are considered.

Milligan, Walter W.↗

Effects of cobalt in nickel-base superalloys

The role of cobalt in a representative wrought nickel-base superalloy was determined. The results show cobalt affecting the solubility of elements in the gamma matrix, resulting in enhanced gamma' volume fraction, in the stabilization of MC-type carbides, and in the stabilization of sigma phase. In the particular alloy studied, these microstructural and microchemistry changes are insufficient in extent to impact on tensile strength, yield strength, and in the ductilities. Depending on the heat treatment, creep and stress rupture resistance can be cobalt sensitive. In the coarse grain, fully solutioned and aged condition, all of the alloy's 17% cobalt can be replaced by nickel without deleteriously affecting this resistance. In the fine grain, partially solutioned and aged condition, this resistance is deleteriously affected only when one-half or more of the initial cobalt content is removed. The structure and property results are discussed with respect to existing theories and with respect to other recent and earlier findings on the impact of cobalt, if any, on the performance of nickel-base superalloys.

Tien, J. K.↗

Additive manufacturing of nickel-based superalloys: A state-of-the-art review on process-structure-defect-property relationship

Fusion-based additive manufacturing (AM) has significantly grown to fabricate Nickel-based superalloys with design freedom across multiple length scales. Several phenomena such as feedstock/energy source/melt pool interactions, solidification and phase transformations occur during fusion-based AM processes of Nickel-based superalloys, which determine the ultimate microstructure and mechanical performance of the built parts. In this review, here we elaborate a comprehensive discussion on AM Nickel-based superalloys and influential factors including feedstock characteristics (powder morphology, chemistry, contamination, flowability, recycling) and AM processing (parameters, and powder spreading/wall/balling/spattering effects) on their microstructure (micro-segregation, phases formations and grain structures), defect generation (sub-surface/internal defects, microcracks, surface roughness, and residual stress). Furthermore, the mechanical properties of AM Nickel-based superalloys such as tensile, creep and fatigue at room/elevated temperatures are analyzed in accordance with the initial, and post processing effects. Additionally, the commonly utilized modeling approaches in literature to predict the microstructure and mechanical behavior of these alloys are highlighted. Finally, the current challenges and mitigation approaches for future research are identified considering the gaps in the AM Nickel-based superalloys.

36 MATERIALS SCIENCE↗

Computational Thermodynamic Study to Predict Complex Phase Equilibria in the Nickel-Base Superalloy Rene N6

A previous study by Ritzert et al. on the formation and prediction of topologically closed packed (TCP) phases in the nickel-base superalloy Rene' N6 is re-examined with computational thermodynamics. The experimental data on phase distribution in forty-four alloys with a composition within the patent limits of the nickel-base superalloy Rene' N6 provide a good basis for comparison to and validation of a commercial nickel superalloy database used with ThermoCalc. Volume fraction of the phases and partitioning of the elements are determined for the forty-four alloys in this dataset. The baseline heat treatment of 400 h at 1366 K was used. This composition set is particularly interesting since small composition differences lead to dramatic changes in phase composition. In general the calculated values follow the experimental trends. However, the calculations indicated no TCP phase formation when the experimental measurements gave a volume percent of TCP phase less than 2 percent. When TCP phases were predicted, the calculations under-predict the volume percent of TCP phases by a factor of 2 to 8. The calculated compositions of the gamma and gamma' phases show fair agreement with the measurements. However, the calculated compositions of the P Phase do not agree with those measured. This may be due to inaccuracies in the model parameters for P phase and/or issues with the microprobe analyses of these phases. In addition, phase fraction diagrams and sigma and P phase solvus temperatures are calculated for each of the alloys. These calculations indicate that P phase is the primary TCP phase formed for the alloys considered here at 1366 K. Finally, a series of isopleths are calculated for each of the seven alloying elements. These show the effect of each alloying element on creating TCP phases.

Copland, Evan H.↗

Creep Deformation and Damage Mechanisms in an Advanced High-Temperature Additively Manufactured Nickel-Base Superalloy

Abstract This research investigates the processing–structure–properties–performance relationship in a novel nickel-base superalloy, ABD ® -900AM, designed for extreme environments. Specifically tailored for additive manufacturing (AM), ABD ® -900AM maintains mechanical integrity at high temperatures and is comparable to other nickel-based superalloys with a 30–40% gamma-prime volume fraction. A comprehensive study was conducted using laser-beam powder bed fusion and electron-beam powder bed fusion methods. Factors such as heat treatment, porosity, build orientation, and hot isostatic pressing were evaluated to understand their effects on microstructure and mechanical performance. Microstructural characterization revealed significant differences in grain size and orientation across build processes and heat treatments. High-temperature mechanical testing indicated that grain size, heat treatment, and orientation significantly influence creep behavior. A super-solvus heat treatment led to recrystallization and grain growth, significantly improving creep properties compared to a near-solvus heat treatment. Various creep mechanisms were identified across different conditions, and creep rupture models were developed for each build process. Post-test microstructural analysis showed grain boundary damage, with differences in creep cavitation morphology under varying stress conditions. It was shown that MC carbides grow at the expense of gamma-prime near grain boundaries, leading to precipitate-free zones in specimens tested at higher temperatures. This study fills a significant gap in fundamental research by offering a deeper insight into the high-temperature mechanical behavior of additively manufactured nickel-base superalloys. It also explores critical research questions regarding the role of carbides and the significance of heat treatment. The insights gained enhance confidence in the industry adoption of ABD ® -900AM and similar alloys for high-temperature applications, bridging the knowledge gap and supporting the development of reliable AM processes for extreme environments.

Bridges, Alex (ORCID:000000030338759X)↗