At least 37 records · Page 2

Oxidation of ZrB2-SiC

In this paper the oxidation behavior of ZrB2-20 vol% SiC is examined. Samples were exposed in stagnant air in a zirconia furnace (Deltech, Inc.) at temperatures of 1327, 1627, and 1927 C for ten ten-minute cycles. Samples were removed from the furnace after one, five, and ten cycles. Oxidized material was characterized by mass change when possible, x-ray diffraction (XRD), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS). Oxidation kinetics, oxide scale development, and matrix recession were monitored as a function of time and temperature. Oxidation and recession rates of ZrB2 - 20 vol% SiC were adequately modeled by parabolic kinetics. Oxidation rates of this material are rapid, allowing only very short-term application in air or other high oxygen partial pressure environments.

Opila, Elizabeth J.↗

Kinetics of Cyclic Oxidation and Cracking and Finite Element Analysis of MA956 and Sapphire/MA956 Composite System

Sapphire fiber-reinforced MA956 composites hold promise for significant weight savings and increased high-temperature structural capability, as compared to unreinforced MA956. As part of an overall assessment of the high-temperature characteristics of this material system, cyclic oxidation behavior was studied at 1093 C and 1204 C. Initially, both sets of coupons exhibited parabolic oxidation kinetics. Later, monolithic MA956 exhibited spallation and a linear weight loss, whereas the composite showed a linear weight gain without spallation. Weight loss of the monolithic MA956 resulted from the linking of a multiplicity of randomly oriented and closely spaced surface cracks that facilitated ready spallation. By contrast, cracking of the composite's oxide layer was nonintersecting and aligned nominally parallel with the orientation of the subsurface reinforcing fibers. Oxidative lifetime of monolithic MA956 was projected from the observed oxidation kinetics. Linear elastic, finite element continuum, and micromechanics analyses were performed on coupons of the monolithic and composite materials. Results of the analyses qualitatively agreed well with the observed oxide cracking and spallation behavior of both the MA956 and the Sapphire/MA956 composite coupons.

Lee, Kang N.↗

A Model of Reduced Kinetics for Alkane Oxidation Using Constituents and Species for N-Heptane

The reduction of elementary or skeletal oxidation kinetics to a subgroup of tractable reactions for inclusion in turbulent combustion codes has been the subject of numerous studies. The skeletal mechanism is obtained from the elementary mechanism by removing from it reactions that are considered negligible for the intent of the specific study considered. As of now, there are many chemical reduction methodologies. A methodology for deriving a reduced kinetic mechanism for alkane oxidation is described and applied to n-heptane. The model is based on partitioning the species of the skeletal kinetic mechanism into lights, defined as those having a carbon number smaller than 3, and heavies, which are the complement of the species ensemble. For modeling purposes, the heavy species are mathematically decomposed into constituents, which are similar but not identical to groups in the group additivity theory. From analysis of the LLNL (Lawrence Livermore National Laboratory) skeletal mechanism in conjunction with CHEMKIN II, it is shown that a similarity variable can be formed such that the appropriately non-dimensionalized global constituent molar density exhibits a self-similar behavior over a very wide range of equivalence ratios, initial pressures and initial temperatures that is of interest for predicting n-heptane oxidation. Furthermore, the oxygen and water molar densities are shown to display a quasi-linear behavior with respect to the similarity variable. The light species ensemble is partitioned into quasi-steady and unsteady species. The reduced model is based on concepts consistent with those of Large Eddy Simulation (LES) in which functional forms are used to replace the small scales eliminated through filtering of the governing equations; in LES, these small scales are unimportant as far as the overwhelming part of dynamic energy is concerned. Here, the scales thought unimportant for recovering the thermodynamic energy are removed. The concept is tested by using tabular information from the LLNL skeletal mechanism in conjunction with CHEMKIN II utilized as surrogate ideal functions replacing the necessary functional forms. The test reveals that the similarity concept is indeed justified and that the combustion temperature is well predicted, but that the ignition time is over-predicted, a fact traced to neglecting a detailed description of the processes leading to the heavies chemical decomposition. To palliate this deficiency, functional modeling is incorporated into this conceptual reduction in addition to the modeling the evolution of the global constituent molar density, the enthalpy evolution of the heavies, the contribution to the reaction rate of the unsteady lights from other light species and from the heavies, the molar density evolution of oxygen and water, and the mole fractions of the quasisteady light species. The model is compact in that there are only nine species-related progress variables. Results are presented showing the performance of the model for predicting the temperature and species evolution. The model reproduces the ignition time over a wide range of equivalence ratios, initial pressure, and initial temperature.

Harstad, Kenneth G.↗

Oxidative vaporization kinetics of chromium (III) oxide in oxygen from 1270 to 1570 K

Rates of oxidative vaporization of Cr2O3 on preoxidized resistively heated chromium were determined in flowing oxygen at 0.115 torr for temperatures from 1270 to 1570 K. Reaction controlled rates were obtained from experimental rates by a gold calibration technique. These rates were shown to agree with those predicted by thermochemical analysis. The activation energy obtained for the oxidative vaporation reaction corresponded numerically with the thermochemical enthalpy of the reaction. A theoretical equation is given for calculating the rate from thermodynamic data by using boundary layer theory.

Stearns, C. A.↗

Chemical kinetics of homogeneous atmospheric oxidation of sulfur dioxide

A systematic evaluation of known homogeneous SO2 reactions which might be important in air pollution chemistry is carried out. A mechanism is developed to represent the chemistry of NOx/hydrocarbon/SO2 systems, and the mechanism is used to analyze available experimental data appropriate for quantitative analysis of SO2 oxidation kinetics. Detailed comparisons of observed and predicted concentration behavior are presented. In all cases, observed SO2 oxidation rates cannot be explained solely on the basis of those SO2 reactions for which rate constants have been measured. The role of ozone-olefin reactions in SO2 oxidation is elucidated.

Sander, S. P.↗

A new approach to the oxidational theory of mild wear

The wear and friction of 316 stainless steel was investigated in relation to oxidation at the real area of contact. An approach describing the oxidation characteristics of mild wear in terms of linear oxidation kinetics is presented. Linear oxidation kinetics more closely approaches the physical conditions involved where oxide growth on asperities is continuously interrupted by spalling and removal. The mild wear rate may now be described mathematically by two empirical equations in terms of the operational variables and the oxidational constants without using the critical oxide thickness, which is dependent on asperity size, shape and temperature, and is difficult to measure. The resulting activation energy for oxidational wear was significantly lower than that for static oxidation governed by diffusion controlled kinetics.

Hong, H.↗

Fundamental kinetics and mechanistic pathways for oxidation reactions in supercritical water

Oxidation of the products of human metabolism in supercritical water has been shown to be an efficient way to accomplish the on-board water/waste recycling in future long-term space flights. Studies of the oxidation kinetics of methane to carbon dioxide in supercritical water are presented in this paper in order to enhance the fundamental understanding of the oxidation of human waste compounds in supercritical water. It is concluded that, although the elementary reaction models remain the best hope for simulating oxidation in supercritical water, several modifications to existing mechanisms need to be made to account for the role of water in the reaction mechanism.

Webley, Paul A.↗

Oxidation of C/SiC Composites at Reduced Oxygen Partial Pressures

T-300 carbon fibers and T-300 carbon fiber reinforced silicon carbide composites (C/SiC) were oxidized in flowing reduced oxygen partial pressure environments at a total pressure of one atmosphere (0.5 atm O2, 0.05 atm O2 and 0.005 atm O2, balance argon). Experiments were conducted at four temperatures (816deg, 1149deg, 1343deg, and 1538 C). The oxidation kinetics were monitored using thermogravimetric analysis. T-300 fibers were oxidized to completion for times between 0.6 and 90 h. Results indicated that fiber oxidation kinetics were gas phase diffusion controlled. Oxidation rates had an oxygen partial pressure dependence with a power law exponent close to one. In addition, oxidation rates were only weakly dependent on temperature. The C/SiC coupon oxidation kinetics showed some variability, attributed to differences in the number and width of cracks in the SiC seal coat. In general, weight losses were observed indicating oxidation of the carbon fibers dominated the oxidation behavior. Low temperatures and high oxygen pressures resulted in the most rapid consumption of the carbon fibers. At higher temperatures, the lower oxidation rates were primarily attributed to crack closure due to SiC thermal expansion, rather than oxidation of SiC since these reduced rates were observed even at the lowest oxygen partial pressures where SiC oxidation is minimal.

Opila, E. J.↗

Oxidation of SiC Fiber-Reinforced SiC Matrix Composites with a BN Interphase

SiC-fiber reinforced SiC matrix composites with a BN interphase were oxidized in reduced oxygen partial pressures of oxygen to simulate the environment for hypersonic vehicle leading edge applications. The constituent fibers as well as composite coupons were oxidized in oxygen partial pressures ranging from 1000 ppm O2 to 5% O2 balance argon. Exposure temperatures ranged from 816 C to 1353 C (1500 F to 2450 F). The oxidation kinetics of the coated fibers were monitored by thermogravimetric analysis (TGA). An initial rapid transient weight gain was observed followed by parabolic kinetics. Possible mechanisms for the transient oxidation are discussed. One edge of the composite coupon seal coat was ground off to simulate damage to the composite which allowed oxygen ingress to the interior of the composite. Oxidation kinetics of the coupons were characterized by scanning electron microscopy since the weight changes were minimal. It was found that sealing of the coupon edge by silica formation occurred. Differences in the amount and morphology of the sealing silica as a function of time, temperature and oxygen partial pressure are discussed. Implications for use of these materials for hypersonic vehicle leading edge materials are summarized.

Opila, Elizabeth↗

The Oxidation of AlN in Dry and Wet Oxygen

The oxidation kinetics of AlN containing 3.5 wt% Y2O3 were studied by thermogravimetric analysis in dry oxygen and 10% H2O/balance oxygen at temperatures between 1000 and 1200 C for times between 48 and 100 h. The oxidation kinetics for AlN in dry oxygen were parabolic and of approximately the same magnitude and temperature dependence as other alumina forming materials. In this case, diffusion of oxygen and/or aluminum through the alumina scale is the rate limiting mechanism. The oxidation kinetics for AlN in wet oxygen were nearly linear and much more rapid than rates observed in dry oxygen. Numerous micropores were observed in the alumina formed on AIN in wet oxygen. These pores provide a fast path for oxygen transport. The linear kinetics observed in this case suggest that the interface reaction rate of AlN with wet oxygen is the oxidation rate limiting step.

Opila, Elizabeth↗

Grain boundary oxidation and low-cycle fatigue at elevated temperatures

Fatigue life consists of fatigue crack nucleation and propagation periods. In order to predict fatigue life accurately, a methodology for the quantitative assessment of these two fatigue damage processes had to be devised. Grain boundary oxidation penetrates faster than does oxidation within a grain. This faster oxidation penetration causes intergranular fatigue failures at elevated temperatures. Grain boundary oxidation accelerates both crack nucleation and propagation. Grain boundary oxidation kinetics and the statistical distribution of grain boundary oxide penetration depth were measured. Quantitative applications of the grain boundary oxidation kinetics to fatigue crack nucleation and propagation were analyzed. A method, based on the Weibull distribution, of extrapolating the laboratory oxidation data measured with small samples to large engineering structures is presented.

Liu, H. W.↗

Oxidative vaporization kinetics of Cr2O3 in oxygen from 1000 to 1300 C

Rates of oxidative vaporization of Cr2O3 on preoxidized resistively heated chromium were determined in flowing oxygen at a pressure of 0.115 Torr for temperatures from 1000 to 1300 C. Reaction controlled rates were obtained from experimental rates by a gold calibration technique, and these rates were shown to agree with those predicted by thermochemical analysis. The activation energy obtained for the oxidative vaporization reaction corresponded numerically with the thermochemical enthalpy of the reaction. A theoretical equation is given for calculating the rate from thermodynamic data using boundary-layer theory.

Stearns, C. A.↗

Thermal barrier coating life prediction model development

A life prediction model for correlating the spallation life of ceramic thermal barrier coatings is developed which includes both cyclic and time-dependent damage. The cyclic damage is related to the calculated cyclic inelastic strain range, while the time-dependent damage is related to the oxidation kinetics at the bond-ceramic interface. The cyclic inelastic strain range is calculated using a modified form of the Walker viscoplastic material model; calculation of the oxidation kinetics is based on traditional oxidation algorithms using experimentally determined parameters. The correlation between the actual and predicted spallation lives is within a factor of 3.

Cruse, T. A.↗