Search NASA⌕ Search

SEARCH · Search NASA

Results for “perfluoropolyether”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

The properties of perfluoropolyethers used for space applications

The perfluoropolyether (PFPE) class of liquid lubricants has been used for space applications for over two decades. At first, these fluids performed satisfactorily as early spacecraft placed few demands on their performance. However, as other spacecraft components have become more reliable and lifetimes have been extended, PFPE lubricant deficiencies have been exposed. Therefore, the objective of this paper is to review the PFPE properties that are important for successful long term operation in space.

Jones, William R., Jr.↗

XPS analysis of 440C steel surfaces lubricated with perfluoropolyethers under sliding conditions in high vacuum

This work presents the results of the X-Ray Photoelectron Spectroscopy (XPS) analysis of AISI 440C ball surfaces lubricated with perfluoropolyether (PFPE) oils after friction experiments under sliding conditions at high load in air and vacuum environments. The PFPE lubricants tested were Demnum S100, Fomblin Z-25, and Krytox 143AB. It was found that all the PFPE lubricants were degraded by sliding contact causing the formation of inorganic fluorides on the metallic surfaces and a layer of organic decomposition products. KRYTOX 143AB was the least reactive of the three lubricants tested. It was also found that metal fluoride formed at off-scar areas. This suggests the formation of reactive species, such as COF2 or R(sub f)COF, during sliding experiments, which can diffuse through the lubricant film and react with the metallic surfaces away from the contact region. Comparison of reference specimens before sliding with those that had undergone the sliding tests showed that the amount of non-degraded PFPE remaining on the surface of the balls after the sliding experiments was greater than that of the balls without sliding.

Herrera-Fierro, Pilar↗

Properties of Perfluoropolyethers for Space Applications

The perfluoropolyether (PFPE) class of liquid lubricants has been used for space applications for over two decades. At first, these fluids performed satisfactorily as early spacecraft placed few demands on their performance. However, as other spacecraft components have become more reliable and lifetimes have been extended, PFPE lubricant deficiencies have been exposed. Therefore, the objective of this paper is to review the PFPE properties that are important for successful long term operation in space.

Jones, William R., Jr.↗

Enhancement of perfluoropolyether boundary lubrication performance: I. Preliminary results

A ball bearing simulator operating under starved conditions was used to evaluate the boundary lubrication performance of a perfluoropolyether (PFPE) Krytox 143 AB. Several approaches to enhance boundary lubrication were studied. These included: (1) soluble boundary additives, (2) bearing surface modifications, (3) 'run-in' surface films, and (4) ceramic bearing components. In addition, results were compared with two non-perfluorinated liquid lubricant formulations. Based on these preliminary tests, the following tentative conclusions can be made: (1) substantial improvements in boundary lubrication performance were observed with a beta-diketone boundary additive and a tricresyl phosphate (TCP) liquid surface pretreatment; (2) the use of rough Si3N4 balls (Ra = 40 micro-in) also provided substantial improvement but with concomitant abrasive wear; (3) marginal improvements were seen with two boundary additives (a phosphine and a phosphatriazine) and a neat (100%) fluid (a carboxylic acid terminated PFPE); and surface pretreatments with a synthetic hydrocarbon, a PTFE coating, and TiC coated 440C and smooth Si3N4 balls (R(sub a) less than 1 micro-in); and (4) two non-PFPE lubricant formulations (a PAO and a synthetic hydrocarbon) yielded substantial improvements.

Jones, W. R., Jr.↗

The effects of ion implantation on the tribology of perfluoropolyether-lubricated 440C stainless steel couples

The lubricating lifetime of thin films of a perfluoropolyether (PFPE) based on hexafluoropropene oxide in the presence of ion implanted 440C stainless steel is presented. Stainless steel discs, either unimplanted or implanted with N2, C, Ti, Ti + N2, or Ti + C had a thin film of PFPE (60-400 A) applied to them reproducibly (+/- 20 percent) and uniformly (+/- 15 percent) using a device developed for this study. The lifetimes of these films were quantified by measuring the number of sliding-wear cycles required to induce an increase in the friction coefficient from an initial value characteristic of the lubricated wear couple to a final, or failure value, characteristic of an unlubricated, unimplanted couple. The tests were performed in a dry nitrogen atmosphere (less than 1 percent RH) at room temperature using a 3 N normal load with a relative sliding speed of 0.05 m/s. The lubricated lifetime of the 440C couple was increased by an order of magnitude by implanting the disc with Ti. Ranked from most to least effective, the implanted species were: Ti; Ti+C; unimplanted; N2; C approximately equals Ti+N2. The mechanism postulated to explain these results involves the formation of a passivating or reactive layer which inhibits or facilitates the production of active sites. The corresponding surface microstructures induced by ion implantation, obtained using x-ray diffraction and conversion electron Mossbauer spectroscopy, ranked from most to least effective in enhancing lubricant lifetime were: amorphous Fe-Cr-Ti; amorphous Fe-Cr-Ti-C + TiC; unimplanted; epsilon-(Fe,Cr)(sub x)N, x = 2 or 3; amorphous Fe-Cr-C approximately equals amorphous Fe-Cr-Ti-N.

Shogrin, Bradley↗

Spontaneous dewetting of a perfluoropolyether

Eight different production lots of a commercial perfluoropolyether (PFPE) based on hexafluoropropene oxide (HFPO) were applied to polished metal surfaces by spinning. One of the lots repeatedly dewetted from a clean 440C steel surface, forming droplets on the surface, whereas the other seven did not dewet. This dewetting phenomenon also repeatedly occurred on 2024 aluminum and 1018 steel, but not on copper or gold. Fourier transform infrared microspectroscopy (mu-FTIR) was used to determine thickness and uniformity of the PFPE films. The dewetting lot was found to dewet from 440C steel at a film thickness greater than 520 A. A portion of the dewetting lot was heated at 316 C for 12 days in the presence of oxygen and M-50 steel. This fluid did not dewet. Sequentially, samples of the dewetting lot were filtered either with an alumina or a silica cartridge which can remove polar impurities. Neither of the filtered samples dewetted from 440C steel. It was concluded that an unknown impurity, both thermally labile and polar, present at very low concentration and undetected by our analytical techniques (FTIR, proton NMR, or F-19 NMR), was responsible for the dewetting phenomenon.

Shogrin, Bradley↗

Properties of Perfluoropolyethers for Space Applications

The perfluoropolyether (PEPE) class of liquid lubricants has been used for space applications for over two decades. At first, these fluids performed satisfactorily, as early spacecraft placed few demands on their performance. However, as other spacecraft components have become more reliable and lifetimes have been extended, PEPE lubricant deficiencies have been exposed. Therefore, the objective of this paper is to review the PEPE properties that are important for successful long term operation in space.

Jones, William R., Jr.↗

Enhancement of Perfluoropolyether Boundary Lubrication Performance

A ball bearing simulator operating under starved conditions was used to perform screening tests to evaluate the boundary lubrication performance of a branched perfluoropolyether (PFPE), K-143 AB. Several approaches to enhance boundary lubrication were studied. These included: (1) soluble boundary additives, (2) bearing surface modifications, (3) 'run-in' surface films, and (4) ceramic bearing components. In addition, results were compared with two non-perfluorinated liquid lubricant formulations. Based on these tests, the following tentative conclusions can be made: (1) Substantial improvements in boundary lubrication performance were observed with a beta-diketone boundary additive and a tricresyl phosphate (TCP) liquid surface pretreatment, (2) the use of rough Si3N4 balls (R(sub a) = 40 micro-inch) also provided increases in test duration, but with concomitant abrasive wear, (3) moderate improvements were seen with two boundary additives (a phosphine and a phosphatriazine) and a neat (100%) fluid (a carboxylic acid terminated PFPE); and small improvements with surface pretreatments with synthetic hydrocarbons, a polytetrafluoroethylene (PTFE) coating, and TiC coated 440 C and smooth Si3N4 balls (R(sub a) = 1 micro-inch), and (4) two non-PFPE lubricant formulations (a polyalphaolefin (PAO) and synthetic hydrocarbon) yielded substantial improvements.

Jones, W. R., Jr.↗

Spectroscopic Analysis of Perfluoropolyether Lubricant Degradation During Boundary Lubrication

The degradation of a branched perfluoropolyether (PFPE) under boundary lubrication conditions was studied using mu-FTIR and mu-Raman spectroscopies. Stainless steel (440C) discs coated with thin (600A), uniform films of the PFPE were tested in a ball-on-disc apparatus until various levels of friction coefficient were attained. Discs were then examined using the above techniques. When the friction coefficient surpassed the value obtained with an un-lubricated control, the lubricant film had either been physically displaced or partially transformed in to a 'friction polymer'. Infrared analysis of this 'friction polymer' indicated the presence of a polymeric fluorinated acid species (R(sub f)COOH). Raman spectroscopy indicated the presence of amorphous carbon in the wear track and in the friction polymer. Some reaction mechanisms are suggested to explain the results.

Herrera-Fierro, Pilar↗

The Effects of Acid Passivation, Tricresyl Phosphate Pre-Soak, and UV/Ozone Treatment on the Tribology of Perfluoropolyether-Lubricated 440C Stainless Steel Couples

The boundary-lubrication performance of perfluoropolyether (PFPE) thin films in the presence of passivated 440 C stainless steel is presented. The study utilized a standard ball-on-disc tribometer. Stainless steel surfaces were passivated with one of four techniques: 1) submersion in a chromic acid bath for 30 minutes at 46 C, 2) submersion in a chromic acid bath for 60 minutes at 56 C, 3) submersion in a tricresyl phosphate (TCP) bath for 2 days at 107 C, or 4) UV/Ozone treated for 15 minutes. After passivation, each disc had a 400 A film of PFPE (hexafluoropropene oxide) applied to it reproducibly (+/- 20%) and uniformly (+/- 15%) using a film deposition device. The lifetimes of these films were quantified by measuring the number of sliding wear cycles required to induce an increase in the friction coefficient from an initial value characteristic of the lubricated wear couple to a final, or failure value, characteristic of an unlubricated, unpassivated wear couple. The lubricated lifetime of the 440 C couple was not altered as a result of the various passivation techniques. The resulting surface chemistry of each passivation technique was examined using X-ray Photoelectron Spectroscopy (XPS). It was found that chromic acid passivation altered the Cr to Fe ratio of the surface. TCP passivation resulted in a FePO4 layer on the surface, while UV/Ozone passivation only removed the carbonaceous contamination layer. None of the passivation techniques were found to dramatically increase the oxide film thickness.

Shogrin, Bradley A.↗

An Additive to Improve the Wear Characteristics of Perfluoropolyether Based Greases

The friction and wear characteristics of two formulated perfluoropolyether based greases were compared to their non-additive base greases. One grease was developed for the electronics industry (designated as GXL-296A) while the other is for space applications (designated as GXL-320A). The formulated greases (GXL-296B and GXL-320B) contained a proprietary antiwear additive at an optimized concentration. Tests were conducted using a vacuum four-ball tribometer. AISI 52100 steel specimens were used for all GXL-296 tests. Both AISI 52100 steel and 440C stainless steel were tested with the GXL-320 greases. Test conditions included: a pressure less than 6.7 x 10(exp )-4 Pa, a 200N load, a sliding velocity of 28.8 mm/sec (100 rpm) and room temperature (approximately equal to 23 C). Wear rates for each grease were determined from the slope of the wear volume as a function of sliding distance. Both non-additive base greases yielded relatively high wear rates on the order of 10(exp -8) cu mm using AISI 52100 steel specimens. Formulated grease GXL-296B yielded a reduction in wear rate by a factor of approximately 21, while grease GXL-320B had a reduction of approximately 12 times. Lower wear rates (-50%) were observed with both GXL-320 greases using 440C stainless steel. Mean friction coefficients were slightly higher for both formulated greases compared to their base greases. The GXL-296 series (higher base oil viscosity) yielded much higher friction coefficients compared to their GXL-320 series (lower base oil viscosity) counterparts.

Jones, David G. V.↗

The Effects of Acid Passivation, Tricresyl Phosphate Presoak, and UV/Ozone Treatment on the Tribology of Perfluoropolyether-Lubricated 440C Stainless Steel Couples

The boundary-lubrication performance of two perfluoropolyether (PFPE) thin films in the presence of passivated 440C stainless steel is presented. The study used a standard ball on disk (BoD) tribometer in dry nitrogen and a vacuum spiral orbit tribometer (SOT). Stainless steel surfaces were passivated with one of four techniques: high and low temperature chromic acid bath, a tricresyl phosphate (TCP) soak, or UV/Ozone treated for 15 min. After passivation, each BoD disk had a 400A film of Krytox 16256 (PFPE) applied to it. The lifetimes of these films were quantified by measuring the number of sliding cycles before an increase in friction occurred. The lubricated lifetime of the 440C couple was not altered as a result of the various passivation techniques. The resulting surface chemistry of each passivation technique was examined using X-ray photoelectron spectroscopy (XPS). The SOT was used to examine the effects of the TCP treatment on the lubricated lifetime of another PFPE, Brayco 815Z, under rolling conditions. None of the passivation techniques were found to dramatically increase the oxide film thickness or lubricated lifetimes.

Shogrin, Bradley A.↗

Ion Implantation of Perfluoropolyether-Lubricated Surfaces for Improved Tribological Performance

For over 30 years, perfluoropolyethers (PFPE's) have been the liquid lubricants of choice for space applications because of their proven tribological performance and desirable properties, such as low vapor pressure and a wide liquid temperature range. These oils are used in such space mechanisms as gyroscopes, scanning mirrors, actuators, and filter wheels. In the past few years, there have been several incidents during which PFPE-lubricated space mechanisms have shown anomalous behavior. These anomalies are thought to be the result of PFPE degradation. Investigative research focused on understanding and modeling the degradation of PFPE lubricants has shown that PFPE's degrade and lose their desirable properties while under boundary-lubricated, sliding/rolling contacts and at elevated temperatures. These performance deficiencies are strongly dependent on the surface chemistry and reactivity of the lubricated contacts, which dictate the formation of harmful catalytic by-products. One way to inhibit tribo-induced degradation may be to use passivated surfaces that do not promote the formation of harmful by-products. Such a passivated surface would inhibit PFPE degradation and increase the lifetime of the lubricated mechanism. Ion implantation is one such passivation technique. This surface-treatment technique can modify the surface properties of materials without affecting either the properties or dimensions of the bulk material beneath the treated layer. By introducing a foreign species into a submicron surface layer, ion implantation can induce unique surface microstructures.

Shogrin, Brad↗

Lubricated Bearing Lifetimes of a Multiply Alkylated Cyclopentane and a Linear Perfluoropolyether Fluid in Oscillatory Motion at Elevated Temperatures in Ultrahigh Vacuum

Bearing life tests in vacuum with three space liquid lubricants, two multiply alkylated cyclopentanes (MACs) and a linear perfluoropolyether (PFPE) were performed. Test conditions included: an 89 N axial load (mean Hertzian stress 0.66 GPa), vacuum level below 7x10(exp -4) Pa, and a +/-30deg dither angle. Dither rate was 75 cycles per minute. Higher (110 to 122 C) and lower temperature tests (75 C) were performed. For the higher temperature tests, the PFPE, Fomblin (Ausimont SpA) Z25 outperformed Pennzane (Shell Global Solutions) X-2000 by more than an order of magnitude. Lubricant evaporation played a key role in these high temperature results. At 75 C, the order was reversed with both Pennzane X-1000 and X-2000 outperforming Fomblin Z25 by more than an order of magnitude. Most Pennzane tests were suspended without failure. The primary failure mechanism in these lower temperature tests was lubricant consumption in the tribocontacts.

Braza, Joseph↗

Experimental density and PC-SAFT modeling of Krytox (R) (perfluoropolyether) at pressures to 275 MPa and temperatures to 533 K

Density data from 298 to 533 K and to 275 MPa are reported for Krytox® GPL 102, a poly(perfluoropropyl ether) (PFPE) with a CF3-branched fluoropropylether repeat group. The Tait equation fit to each density isotherm have mean absolute percent deviations (MAPD) between 0.11 and 0.30% with standard deviations (SD) not exceeding 0.20%. The perturbed-chain statistical associating fluid theory (PC-SAFT) fit to the density data has an MAPD of 0.67% and an SD of 0.67%. Likewise the PC-SAFT fit to previously reported density data of Demnum®, a PFPE with an n-fluoropropylether repeat group, has an MAPD of 0.22% and a SD of 0.21% for Demnum® S-20 and an MAPD of 0.27% with a SD of 0.14% for Demnum® S-65. The trends exhibited by the PC-SAFT pure component parameters obtained from the fits of these three PFPEs are similar to those reported for linear and branched hydrocarbons with the same number of carbons.

42 ENGINEERING↗

Preparation of perfluoropolyether prepolymers

Fluorinated prepolymers are used to generate highly fluorinated polymers which possess most of the desirable properties of polytetrafluoroethylene, such as nonflammability and high corrosion resistance, while retaining good low temperature flexibility.

Rochow, S. E.↗