34 records · Page 2

Designing with figer-reinforced plastics (planar random composites)

The use of composite mechanics to predict the hygrothermomechanical behavior of planar random composites (PRC) is reviewed and described. These composites are usually made from chopped fiber reinforced resins (thermoplastics or thermosets). The hygrothermomechanical behavior includes mechanical properties, physical properties, thermal properties, fracture toughness, creep and creep rupture. Properties are presented in graphical form with sample calculations to illustrate their use. Concepts such as directional reinforcement and strip hybrids are described. Typical data that can be used for preliminary design for various PRCs are included. Several resins and molding compounds used to make PRCs are described briefly. Pertinent references are cited that cover analysis and design methods, materials, data, fabrication procedures and applications.

Chamis, C. C.↗

Empirical Constraints on Progressive Shock Metamorphism of Magnetite from the Siljan Impact Structure, Sweden

Little is known about the microstructural behavior of magnetite during hypervelocity impact events, even though it is a widespread accessory mineral and important magnetic carrier in terrestrial and extraterrestrial rocks. We report systematic electron backscatter diffraction crystallographic analysis of shock features in magnetite, from a transect across the 52-km diameter ~380 Ma Siljan impact structure in Sweden. Magnetite grains in granitoid samples contain brittle fracturing, crystal-plasticity, and lamellar twins. Deformation twins along {111} with shear direction of <112> are consistent with spinel-law twins. Inferred bulk shock pressures for investigated samples, as constrained by planar deformation features (PDFs) in quartz and shock twins in zircon, range from 0–20 GPa; onset of shock-induced twinning in magnetite is observed at >5 GPa. These results highlight the utility of magnetite to record shock deformation in rocks that experience shock pressures >5 GPa, which may be useful in quartz-poor samples. Despite significant hydrothermal alteration, and variable transformation of host magnetite to hematite, shock effects are preserved, demonstrating that magnetite is a reliable mineral for preserving shock deformation over geologic time.

magnetite↗

Saltation threshold detection in a wind tunnel by the measurement of the net electrostatic charge

The Mars surface wind tunnel (MARSWIT) is an open circuit wind tunnel used for aeolian studies and is located inside a large vacuum chamber allowing testing at Martian surface atmospheric pressure. Since direct access is not available to the tunnel during operation at low pressure, a remote method of saltation detection is needed. The bed is observed by means of closed circuit video, but it is often difficult to determine the initiation of threshold. The measurement by means of an electrometer of the net electric charge produced by the saltating particles has provided a reliable means of saltation threshold detection. Saltating particles become charged several ways, both in wind tunnels and in a natural environment. The most significant of these methods are tribo-charging and contact charging, which always occur. Fracture charging may also occur under the high velocities associated with particle transport on Mars or under simulated Martian conditions. Detection in MARSWIT is achieved by allowing the saltating particles to impinge on a planar conducting surface normal to the flow that is connected to ground through a Keithly electrometer. The signal from the electrometer is connected to a strip chart recorder along with the analog signal from the pitot tube transducer that is used to determine the wind velocity in the tunnel. Thus, a record of wind velocity and the initiation of particle saltation is conveniently displayed together. While both positive and negative charges are produced during saltation, this method measures only the net charge; thus the charge may be either positive or negative depending upon the particles being tested, the size and size distribution of the test material, and the wind velocity. This has proven to be a very trustworthy and sensitive method of saltation threshold detection, being especially useful with the smaller sized particles which are the most difficult to observe visually.

Leach, Rodman N.↗

Determination of cleavage planes and fracture characterization of Ni-based single crystal superalloys

The room temperature fracture behavior of the Ge Rene N-4, CMSX-2, and CMSX-4C single crystal Ni-based superalloys was studied. All crystals were grown along the (001) direction and tensile tested in both helium and hydrogen atmospheres. A stereoscopic technique developed for use with a scanning electron microscope was applied to determine cleavage planes. Planar gamma(') morphologies also were examined to help determine cleavage planes. Helium charged specimens failed on a number of planes including the (111), (110), and (320). In most cases planes of the (111)-type initiated at the notch region and became smaller and smaller as they moved in radially. Tensile strengths in helium averaged 1000 MPa higher than that of the hydrogen charged specimens. Specimens tested in hydrogen generally failed on (100)-type planes originating from the notch region. This (100) region comprised 60 to 80 percent of the total fracture surface on most samples and appeared as large flat planes perpendicular to the growth direction of the crystal. The interior regions contained (100)-type planes as well as (321), (320), (210), and (111)-types. Hydrogen charged specimens also showed a high percentage of large cracks oriented at 90 deg to one another, indicative of the (100)-type fracture. The Ge Rene N4 and the CMSX-4C samples contained 3-5 percent gamma/gamma(') eutectic, while the CMSX-2 samples had little or no gamma/gamma(') eutectic. The relationship between gamma/gamma(') eutectic and the fracture surface has not been fully determined, but it is thought that the gamma/gamma(') eutectic may serve as a possible trapping site for hydrogen.

Merrill, John M.↗

The mechanisms of dispersion strengthening and fracture in Al-based XD(tm) alloys, part 1

The influence of reinforcement size, volume fraction, and matrix deformation behavior on room and elevated temperature strength; the fracture toughness; and the fatigue crack growth rate of metal matrix composites of Al-4(pct)Cu-1.5(pct)Mg with TiB2 were examined. The influence of reinforcement volume fraction was also examined for pure aluminum with TiB2. Higher TiB2 volume fractions increased the tensile yield strength at both room and elevated temperatures, and reduced the elongation to fracture. Tensile tests also indicate that small particles provided a greater increase in strength for a given volume fraction than larger particles, whereas elongation to fracture appeared to be insensitive to reinforcement size. Interparticle spacing appears to be the factor that controls the strength of these alloys, with the exact nature of the dependence relying on the nature of dislocation slip in the matrix (planar vs. diffuse). The isothermal aging response of the precipitation strengthened Al-4(pct)Cu-1.5(pct)Mg alloys was not accelerated by the presence of TiB2. Cold work prior to artificial aging created additional geometrically necessary dislocations which serve as heterogeneous nucleation sites leading to accelerated aging, a finer precipitate size, and an increase in the strength of the alloy.

Aikin, R. M., Jr.↗

Fracture of single crystals of the nickel-base superalloy PWA 1480E in helium at 22 C

The fracture behavior and deformation of He-charged (at 22 C) single crystals of PWA 1480E Ni-base superalloy were investigated using SEM and TEM techniques to observe the behavior of tensile fractures in notched single crystals with seven different crystal growth orientations: 100-line, 110-line, 111-line, 013-line, 112-line, 123-line, and 223-line. To identify the cleavage plane orientation, a stereoscopic technique, combined with the use of planar gamma-prime morphologies, was applied. It was found that gamma-prime particles were orderly and closely aligned with edges along the 100-line, 010-line, and 001-line-oriented directions of the gamma matrix. Different crystal growth orientations were found not to affect the morphology of gamma-prime particles. The accumulation of dislocations around gamma/gamma-prime interfaces formed strong barriers to subsequent dislocation movement and was the primary strengthening mechanism at room temperature.

Chen, P. S.↗

A preliminary characterization of the tensile and fatigue behavior of tungsten-fiber/Waspaloy-matrix composite

A microstructural study and a preliminary characterization of the room temperature tensile and fatigue behavior of a continuous, tungsten fiber, Waspaloy-matrix composite was conducted. A heat treatment was chosen that would allow visibility of planar slip if it occurred during deformation, but would not allow growth of the reaction zone. Tensile and fatigue tests showed that the failed specimens contained transverse cracks in the fibers. The cracks that occurred in the tensile specimen were observed at the fracture surface and up to approximately 4.0 mm below the fracture surface. The crack spacing remained constant along the entire length of the cracked fibers. Conversely, the cracks that occurred in the fatigue specimen were only observed in the vicinity of the fracture surface. In instances where two fiber cracks occurred in the same plane, the matrix often necked between the two cracked fibers. Large groups of slip bands were generated in the matrix near the fiber cracks. Slip bands in the matrix of the tensile specimen were also observed in areas where there were no fiber cracks, at distances greater than 4 mm from the fracture surface. This suggests that the matrix plastically flows before fiber cracking occurs.

Corner, Ralph E.↗

Unit-Sphere Multiaxial Stochastic-Strength Model Applied to Anisotropic and Composite Materials

Models that predict the failure probability of brittle materials under multiaxial loading have been developed by authors such as Batdorf, Evans, and Matsuo. These "unit-sphere" models assume that the strength-controlling flaws are randomly oriented, noninteracting planar microcracks of specified geometry but of variable size. This methodology has been extended to predict the multiaxial strength response of transversely isotropic brittle materials, including polymer matrix composites (PMCs), by considering (1) flaw-orientation anisotropy, whereby a preexisting microcrack has a higher likelihood of being oriented in one direction over another direction, and (2) critical strength, or K (sub Ic) orientation anisotropy, whereby the level of critical strength or fracture toughness for mode I crack propagation, K (sub Ic), changes with regard to the orientation of the microstructure. In this report, results from finite element analysis of a fiber-reinforced-matrix unit cell were used with the unit-sphere model to predict the biaxial strength response of a unidirectional PMC previously reported from the World-Wide Failure Exercise. Results for nuclear-grade graphite materials under biaxial loading are also shown for comparison. This effort was successful in predicting the multiaxial strength response for the chosen problems. Findings regarding stress-state interactions and failure modes also are provided.

Nemeth, Noel, N.↗

Glass/Ceramic Composites for Sealing Solid Oxide Fuel Cells

A family of glass/ceramic composite materials has been investigated for use as sealants in planar solid oxide fuel cells. These materials are modified versions of a barium calcium aluminosilicate glass developed previously for the same purpose. The composition of the glass in mole percentages is 35BaO + 15CaO + 5Al2O3 + 10B2O3 + 35SiO2. The glass seal was found to be susceptible to cracking during thermal cycling of the fuel cells. The goal in formulating the glass/ ceramic composite materials was to (1) retain the physical and chemical advantages that led to the prior selection of the barium calcium aluminosilicate glass as the sealant while (2) increasing strength and fracture toughness so as to reduce the tendency toward cracking. Each of the composite formulations consists of the glass plus either of two ceramic reinforcements in a proportion between 0 and 30 mole percent. One of the ceramic reinforcements consists of alumina platelets; the other one consists of particles of yttria-stabilized zirconia wherein the yttria content is 3 mole percent (3YSZ). In preparation for experiments, panels of the glass/ceramic composites were hot-pressed and machined into test bars.

Bansal, Narottam P.↗

Intrinsic fatigue crack growth rates for Al-Li-Cu-Mg alloys in vacuum

The influences of microstructure and deformation mode on inert environment intrinsic fatigue crack propagation were investigated for Al-Li-Cu-Mg alloys AA2090, AA8090, and X2095 compared to AA2024. The amount of coherent shearable delta-prime (Al3Li) precipitates and extent of localized planar slip deformation were reduced by composition (increased Cu/Li in X2095) and heat treatment (double aging of AA8090). Intrinsic growth rates, obtained at high constant K(max) to minimize crack closure and in vacuum to eliminate any environmental effect, were alloy dependent; da/dN varied up to tenfold based on applied Delta-K or Delta-K/E. When compared based on a crack tip cyclic strain or opening displacement parameter, growth rates were equivalent for all alloys except X2095-T8, which exhibited unique fatigue crack growth resistance. Tortuous fatigue crack profiles and large fracture surface facets were observed for each Al-Li alloy independent of the precipitates present, particularly delta-prime, and the localized slip deformation structure. Reduced fatigue crack propagation rates for X2095 in vacuum are not explained by either residual crack closure or slip reversibility arguments; the origin of apparent slip band facets in a homogeneous slip alloy is unclear.

Slavik, D. C.↗

Impact-induced tensional failure in rock

Planar impact experiments were employed to induce dynamic tensile failure in Bedford limestone. Rock disks were impacted with aluminum and polymethyl methacralate flyer plates at velocities of 10 to 25 m/s. This resulted in tensile stresses in the range of 11 to 160 MPa. Tensile stress durations of 0.5 and 1.3 microsec induced microcrack growth which in many experiments were insufficient to cause complete spalling of the samples. Velocity reduction, and by inference microcrack production, occurred in samples subjected to stresses above 35 MPa in the 1.3-microsec PMMA experiments and 60 MPa in the 0.5-microsec aluminum experiments. Apparent fracture toughnesses of 2.4 and 2.5 MPa m exp 1/2 are computed for the 1.3- and 0.5-microsec experiments. Three-dimensional impact experiments were conducted on 20 cm-sized blocks of Bedford limestone and San Marcos gabbro. Compressional wave velocity deficits up to 50-60 percent were observed in the vicinity of the crater. The damage decreases as about r exp -1.5 from the crater, indicating a dependence on the magnitude and duration of the tensile pulse.

Ahrens, Thomas J.↗

Dynamic tensile-failure-induced velocity deficits in rock

Planar impact experiments were employed to induce dynamic tensile failure in Bedford limestone. Rock disks were impacted with aluminum and polymethyl methacralate (PMMA) flyer plates at velocities of 10 to 25 m/s. Tensile stress magnitudes and duration were chosen so as to induce a range of microcrack growth insufficient to cause complete spalling of the samples. Ultrasonic P- and S-wave velocities of recovered targets were compared to the velocities prior to impact. Velocity reduction, and by inference microcrack production, occurred in samples subjected to stresses above 35 MPa in the 1.3 microsec PMMA experiments and 60 MPa in the 0.5 microsec aluminum experiments. Using a simple model for the time-dependent stress-intensity factor at the tips of existing flaws, apparent fracture toughnesses of 2.4 and 2.5 MPa sq rt m are computed for the 1.3 and 0.5 microsec experiments. These are a factor of about 2 to 3 greater than quasi-static values. The greater dynamic fracture toughness observed may result from microcrack interaction during tensile failure. Data for water-saturated and dry targets are indistinguishable.

Rubin, Allan M.↗

Patterns of brittle deformation under extension on Venus

The development of fractures at regular length scales is a widespread feature of Venusian tectonics. Models of lithospheric deformation under extension based on non-Newtonian viscous flow and brittle-plastic flow develop localized failure at preferred wavelengths that depend on lithospheric thickness and stratification. The characteristic wavelengths seen in rift zones and tessera can therefore provide constraints on crustal and thermal structure. Analytic solutions were obtained for growth rates in infinitesimal perturbations imposed on a one-dimensional, layered rheology. Brittle layers were approximated by perfectly-plastic, uniform strength, overlying ductile layers exhibiting thermally-activated power-law creep. This study investigates the formation of faults under finite amounts of extension, employing a finite-element approach. Our model incorporates non-linear viscous rheology and a Coulomb failure envelope. An initial perturbation in crustal thickness gives rise to necking instabilities. A small amount of velocity weakening serves to localize deformation into planar regions of high strain rate. Such planes are analogous to normal faults seen in terrestrial rift zones. These 'faults' evolve to low angle under finite extension. Fault spacing, orientation and location, and the depth to the brittle-ductile transition, depend in a complex way on lateral variations in crustal thickness. In general, we find that multiple wavelengths of deformation can arise from the interaction of crustal and mantle lithosphere.

Neumann, G. A.↗

Effect of fiber orientation on the fracture toughness of brittle matrix composites

The effective fracture toughness of brittle matrix materials can be increased through the addition of short, poorly bonded fibers which bridge the growing crack. The orientation distribution of the fibers is likely to be biased, and not in an ideal random or aligned state. A micromechanical model is formulated for the postcracking behavior using the force-displacement relation for an arbitrary fiber bridging a crack, the fiber orientation density function, and the fiber location density function. This model is then used to determine an effective traction law for the bridging fibers, as well as the steady state bridging toughness increment. In most cases, the results may be placed in the form of a product of the aligned fiber results times a modifying integrated orientation factor. The frictional shear stress on fiber pull-out is allowed to vary during pull-out, modeling the effects of matrix breakdown, fiber surface smoothing or wear debris accumulation. Results are presented for a variety of representative planar and three-dimensional fiber orientation states.

Jain, L. K.↗

3D Finite Element Analysis of Particle-Reinforced Aluminum

Deformation in particle-reinforced aluminum has been simulated using three distinct types of finite element model: a three-dimensional repeating unit cell, a three-dimensional multi-particle model, and two-dimensional multi-particle models. The repeating unit cell model represents a fictitious periodic cubic array of particles. The 3D multi-particle (3D-MP) model represents randomly placed and oriented particles. The 2D generalized plane strain multi-particle models were obtained from planar sections through the 3D-MP model. These models were used to study the tensile macroscopic stress-strain response and the associated stress and strain distributions in an elastoplastic matrix. The results indicate that the 2D model having a particle area fraction equal to the particle representative volume fraction of the 3D models predicted the same macroscopic stress-strain response as the 3D models. However, there are fluctuations in the particle area fraction in a representative volume element. As expected, predictions from 2D models having different particle area fractions do not agree with predictions from 3D models. More importantly, it was found that the microscopic stress and strain distributions from the 2D models do not agree with those from the 3D-MP model. Specifically, the plastic strain distribution predicted by the 2D model is banded along lines inclined at 45 deg from the loading axis while the 3D model prediction is not. Additionally, the triaxial stress and maximum principal stress distributions predicted by 2D and 3D models do not agree. Thus, it appears necessary to use a multi-particle 3D model to accurately predict material responses that depend on local effects, such as strain-to-failure, fracture toughness, and fatigue life.

Shen, H.↗

Separation of crack extension modes in orthotropic delamination models

In the analysis of an interface crack between dissimilar elastic materials, the mode of crack extension is typically not unique, due to oscillatory behavior of near-tip stresses and displacements. This behavior currently limits the applicability of interfacial fracture mechanics as a means to predict composite delamination. The Virtual Crack Closure Technique (VCCT) is a method used to extract mode 1 and mode 2 energy release rates from numerical fracture solutions. The mode of crack extension extracted from an oscillatory solution using the VCCT is not unique due to the dependence of mode on the virtual crack extension length, Delta. In this work, a method is presented for using the VCCT to extract Delta-independent crack extension modes for the case of an interface crack between two in-plane orthotropic materials. The method does not involve altering the analysis to eliminate its oscillatory behavior. Instead, it is argued that physically reasonable, Delta-independent modes of crack extension can be extracted from oscillatory solutions. Knowledge of near-tip fields is used to determine the explicit Delta dependence of energy release rate parameters. Energy release rates are then defined that are separated from the oscillatory dependence on Delta. A modified VCCT using these energy release rate definitions is applied to results from finite element analyses, showing that Delta-independent modes of crack extension result. The modified technique has potential as a consistent method for extracting crack extension modes from numerical solutions. The Delta-independent modes extracted using this technique can also serve as guides for testing the convergence of finite element models. Direct applications of this work include the analysis of planar composite delamination problems, where plies or debonded laminates are modeled as in-plane orthotropic materials.

Beuth, Jack L.↗