Search NASA⌕ Search

SEARCH · Search NASA

Results for “plastic debris”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Role of plastic deformation in wear of copper and copper - 10-percent-aluminum alloy in cryogenic fuels

High-purity copper specimens and a copper-aluminum (10%) alloy specimen were subjected to sliding against Type 440 C in cryogenic fuel environments. It was found that virtually all wear occurred by the plastic deformation of a recrystallized layer extending to about 10 micrometers below the wear scar surface of the copper or copper alloy. The wear debris was in the form of a layered structure adhering to the exit region of the wear scar. Measurements on the high purity copper specimens indicated that the wear rate was proportional to the applied load and to the sliding velocity squared. A physical model of the wear process is proposed to account for these observations.

Bill, R. C.↗

Sliding induced crystallization of metallic glass

Sliding friction and wear experiments, electron microscopy, and diffraction studies were conducted with an Fe67Co18B14Si1 ferrous-base metallic glass in sliding contact with aluminum oxide at room temperature in air. The results indicate that the amorphous alloy can be crystallized during the sliding process. Crystallization of the wear surface causes high friction. Plastic flow occurred on the amorphous alloy with sliding, and the flow film of the alloy transferred to the aluminum oxide surface. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and powdery and whiskery oxide debris. Generation of oxide wear debris particles on an alloy can cause transitions in friction behavior.

Miyoshi, K.↗

Low Density Sabot Catcher for Hypervelocity Impact Tests

The monolithic steel plate traditionally used to intercept sabot pieces during light-gas gun operations was replaced by low density material. The idea was to decrease the shock stress in these plastic sabot pieces to values below the vaporization threshold, thereby reducing the prominent soot-deposits that characterize typical target surfaces. The project was a collaboration between Orbital Debris and Planetary Science interests at JSC/ARES.

Horz, Friedrich↗

The use of tethered satellites for the collection of cosmic dust and the sampling of man made orbital debris far from the space station

The use of a tethered subsatellite employed downward into the earth's upper atmosphere to an altitude of about 110 km above the earth would eliminate the orbital contamination problem while at the same time affording a measure of atmospheric braking to reduce the velocities of many particles to where they may be captured intact or nearly so with properly designed collectors. The same technique could also be used to monitor the flux of all types of man-made orbital debris out to a distance of more than a hundred kilometers in any direction from the space station. In this way the build up of any debris belt orbiting earth could be determined. The actual collecting elements used for both purposes could be of several different materials and designs so as to optimize the collection of different types of particles with different densities. Stacks of foils, films, plastics, and foams, as well as simple capture cells would be mounted in clusters around the outside of a tethered satellite and protected by iris covers until the tethered had been fully deployed. If the orientation history of the satellite were known the direction of the incoming material could be infered. A chief advantage in deploying such tethered collectors from the Space Station instead of from the shuttle is the ability to maintain deployment of the tether for days instead of hours resulting in much greater yields of intact particles and impact debris.

Corso, G. J.↗

Phenomena after meteoroid penetration of a bumper plate

The analysis of hypervelocity impact of particles on a detector in space, with flow and shock penetration through fluid, plastic, and elastic zones was studied. The original paper and computer program on this topic is presented. Improvements in the program for the study of the formation of a cone of debris are discussed. The truncated apex of the cone is at the hole formed by the penetration of an initially spherical rock through a thin plate. A solution for the penetration of the thin plate was sought.

Todd, F. C.↗

Fretting wear in titanium, Monel-400, and cobalt 25-percent-molybdenum using scanning electron microscopy

Damage scar volume measurements taken from like metal fretting pairs combined with scanning electron microscopy observations showed that three sequentially operating mechanisms result in the fretting of titanium, Monel-400, and cobalt - 25-percent molybdenum. Initially, adhesion and plastic deformation of the surface played an important role. This was followed after a few hundred cycles by a fatigue mechanism which produced spall-like pits in the damage scar. Finally, a combination of oxidation and abrasion by debris particles became most significant. Damage scar measurements made on several elemental metals after 600,000 fretting cycles suggested that the ratio of oxide hardness to metal hardness was a measure of the susceptibility of a metal to progressive damage by fretting.

Bill, R. C.↗

Friction and Wear Properties of Selected Solid Lubricating Films: Ion-Plated Lead Films - Part 2

To evaluate commercially developed dry solid film lubricants for aerospace bearing applications, an investigation was conducted to examine the friction and wear behavior of ion-plated lead films in sliding contact with 6-mm-diameter American Iron and Steel Institute (AISI) 440C stainless steel balls. Unidirectional sliding friction experiments were conducted with a load of 5.9 N (600 g), a mean Hertzian contact pressure of 0.79 GPa (maximum Hertzian contact pressure of 1.2 GPa), and a sliding velocity of 0.2 m/s. The experiments were conducted at room temperature in three environments: ultrahigh vacuum (vacuum pressure, 7 x 10(exp -7 Pa), humid air (relative humidity, approx. 20 percent), and dry nitrogen (relative humidity, less then 1 percent). The resultant films were characterized by scanning electron microscopy, energy-dispersive X-ray spectroscopy, and surface profilometry. Marked differences in the friction and wear of the ion-plated lead films investigated herein resulted from the environmental conditions. The main criteria for judging the performance of the ion-plated lead films were coefficient of friction and wear rate, which had to be less than 0.3 and on the order of 1(exp -6) cu mm/N.m or less, respectively. The ion-plated lead films met both criteria only in ultrahigh vacuum but failed in humid air and in dry nitrogen, where the coefficient of friction was higher than the criterion. Both the lead film wear rate and the ball wear rate met that criterion in all three environments. Adhesion and plastic deformation played important roles in the friction and wear of the ion-plated lead films in contact with 440C stainless steel balls in the three environments. All sliding involved adhesive transfer of materials: transfer of lead wear debris to the counterpart 440C stainless steel and transfer of 440C stainless steel wear debris to the counterpart lead.

Miyoshi, Kazuhisa↗

A unique nozzle cover for the Shuttle booster separation motors

The stringent requirements imposed upon the Shuttle booster separation system led to the development of two unique nozzle cover concepts with potential applications in other space propulsion systems. Major requirements were to (1) protect the booster separation motors (BSMs) from the ascent aerothermal environment; (2) provide a humidity seal for the BSM during storage and readiness on the launch pad; (3) open completely during the ignition transient; and (4) produce no debris during ascent, separation, and booster reentry. The nozzle cover concepts included (1) a frangible reinforced elastomeric cover with a retraction mechanism to remove the cover sections away from the plume, and (2) a stainless steel cover hinged by a plastically deforming torsion pin.

Dettling, J. R.↗

Acoustic fluidization and the scale dependence of impact crater morphology

A phenomenological Bingham plastic model has previously been shown to provide an adequate description of the collapse of impact craters. This paper demonstrates that the Bingham parameters may be derived from a model in which acoustic energy generated during excavation fluidizes the rock debris surrounding the crater. Experimental support for the theoretical flow law is presented. Although the Bingham yield stress cannot be computed without detailed knowledge of the initial acoustic field, the Bingham viscosity is derived from a simple argument which shows that it increases as the 3/2 power of crater diameter, consistent with observation. Crater collapse may occur in material with internal dissipation Q as low as 100, comparable to laboratory observations of dissipation in granular materials. Crater collapse thus does not require that the acoustic field be regenerated during flow.

Melosh, H. J.↗

Mechanical contact induced transformation from the amorphous to the crystalline state in metallic glass

Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.

Miyoshi, K.↗

Mechanical-contact-induced transformation from the amorphous to the partially crystalline state in metallic glass

Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.

Miyoshi, K.↗

Mechanical-contact-induced transformation from the amorphous to the partially crystalline state in metallic glass

Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.

Miyoshi, K.↗

Evaluation of Contact Separation Force Testing as a Screening Methodology for Electrical Socket Contacts

During system level testing intermittent and permanent open circuit failures of mated, crimp removable, electrical contact pairs were experienced. The root cause of the failures was determined to be low (but not zero) contact forces applied by the socket contact tines against the engaging pin. The low contact force reduces the effectiveness of the wiping action of the socket tines against the pin. The observed failure mode may be produced when insufficient wiping during mate, demate and small relative movement in use allows for the accumulation of debris or insulating films that electrically separate the contact pair. The investigation identified at least three manufacturing process control problems associated with the socket contacts that enabled shipment of contacts susceptible to developing low contact forces: (1) Improper heat treatment of the socket tines resulting in plastic rather than elastic behavior; (2) Overly thinned socket tines at their base resulting in reduced pin retention forces; (3) Insufficient screening tests to identify parts susceptible to the aforementioned failure mechanisms. The results from an extensive screening program of socket contacts utilizing the industry standard contact separation force test procedures are described herein. The investigation shows this method to be capable of identifying initially weak sockets. However, sockets whose contact retention forces may degrade during use may not be screened out by pin retention testing alone. Further investigations are required to correlate low contact retention forces with increased electrical contact resistance in the presence of insulating films that may accumulate in the use environment.

Christopher Green↗

Impact gages for detecting meteoroid and other orbital debris impacts on space vehicles.

Impacts on space vehicles have been simulated using the McDonnell Douglas Aerophysics Laboratory (MDAL) Light-Gas Guns to launch particles at hypervelocity speeds into scaled space structures. Using impact gages and a triangulation technique, these impacts have been detected and accurately located. This paper describes in detail the various types of impact gages (piezoelectric PZT-5A, quartz, electret, and off-the-shelf plastics) used. This description includes gage design and experimental results for gages installed on single-walled scaled payload carriers, multiple-walled satellites and space stations, and single-walled full-scale Delta tank structures. A brief description of the triangulation technique, the impact simulation, and the data acquisition system are also included.

Mastandrea, J. R.↗

Dynamic SEM wear studies of tungsten carbide cermets

Dynamic friction and wear experiments were conducted in a scanning electron microscope. The wear behavior of pure tungsten carbide and composite with 6 and 15 weight percent cobalt binder was examined. Etching of the binder was done to selectively determine the role of the binder in the wear process. Dynamic experiments were conducted as the WC and bonded WC cermet surfaces were transversed by a 50 micron radiused diamond stylus. These studies show that the predominant wear process in WC is fracture initiated by plastic deformation. The wear of the etched cermets is similar to pure WC. The presence of the cobalt binder reduces both friction and wear. The cementing action of the cobalt reduces granular separation and promotes a dense polished layer because of its low shear strength film-forming properties. The wear debris generated from unetched surface is approximately the same composition as the bulk.

Brainard, W. A.↗

Dynamic SEM wear studies of tungsten carbide cermets

Dynamic friction and wear experiments were conducted in a scanning electron microscope. The wear behavior of pure tungsten carbide and composite with 6 and 15 weight percent cobalt binder was examined, and etching of the binder was done to selectively determine the role of the binder in the wear process. Dynamic experiments were conducted as the tungsten carbide (WC) and bonded WC cermet surfaces were transversed by a 50 micron radiused diamond stylus. These studies show that the predominant wear process in WC is fracture initiated by plastic deformation, and the wear of the etched cermets is similar to pure WC. The presence of the cobalt binder reduces both friction and wear. The cementing action of the cobalt reduces granular separation, and promotes a dense polished layer because of its low shear strength film-forming properties. The wear debris generated from unetched surface is approximately the same composition as the bulk.

Brainard, W. A.↗

Laser Surface Preparation and Bonding of Aerospace Structural Composites

Adhesive bonds are critical to the integrity of built-up structures. Disbonds can often be detected but the strength of adhesion between surfaces in contact is not obtainable without destructive testing. Typically the number one problem in a bonded structure is surface contamination, and by extension, surface preparation. Standard surface preparation techniques, including grit blasting, manual abrasion, and peel ply, are not ideal because of variations in their application. Etching of carbon fiber reinforced plastic (CFRP) panels using a neodymium-doped yttrium aluminum garnet (Nd:YAG) laser appears to be a highly precise and promising way to both clean a composite surface prior to bonding and provide a bond-promoting patterned surface akin to peel ply without the inherent drawbacks from the same (i.e., debris and curvature). CFRP surfaces prepared using laser patterns conducive to adhesive bonding were compared to typical prebonding surface treatments through optical microscopy, contact angle goniometry, and post-bonding mechanical testing.

Belcher, M. A.↗

Laser Surface Preparation for Adhesive Bonding of Aerospace Structural Composites

Adhesive bonds are critical to the integrity of built-up structures. Disbonds can often be detected but the strength of adhesion between surfaces in contact is not obtainable without destructive testing. Typically the number one problem in a bonded structure is surface contamination, and by extension, surface preparation. Standard surface preparation techniques, including grit blasting, manual abrasion, and peel ply, are not ideal because of variations in their application. Etching of carbon fiber reinforced plastic (CFRP) panels using a neodymium-doped yttrium aluminum garnet (Nd:YAG) laser appears to be a highly precise and promising way to both clean a composite surface prior to bonding and provide a bond-promoting patterned surface akin to peel ply without the inherent drawbacks from the same (i.e., debris and curvature). CFRP surfaces prepared using laser patterns conducive to adhesive bonding were compared to typical pre-bonding surface treatments through optical microscopy, contact angle goniometry, and post-bonding mechanical testing.

Belcher, M. A.↗