At least 37 records · Page 2

Large-Angle Rocking Beam Electron Diffraction of Large Unit Cell Crystals Using Direct Electron Detector

We report a large-angle rocking beam electron diffraction (LARBED) technique for electron diffraction analysis. Diffraction patterns are recorded in a scanning transmission electron microscope (STEM) using a direct electron detector with large dynamical range and fast readout. We use a nanobeam for diffraction and perform the beam double rocking by synchronizing the detector with the STEM scan coils for the recording. Using this approach, large-angle convergent beam electron diffraction (LACBED) patterns of different reflections are obtained simultaneously. By using a nanobeam, instead of a focused beam, the LARBED technique can be applied to beam-sensitive crystals as well as crystals with large unit cells. Here, this paper describes the implementation of LARBED and evaluates the performance using silicon and gadolinium gallium garnet crystals as test samples. We demonstrate that our method provides an effective and robust way for recording LARBED patterns and paves the way for quantitative electron diffraction of large unit cell and beam-sensitive crystals.

4DSTEM↗

Persistence of crystal orientations across sub-micron-scale "super-grains" in self-organized Cu-W nanocomposites

We use precession electron diffraction to investigate the crystallographic character of copper (Cu)-tungsten (W) nanocomposites fabricated via physical vapor co-deposition at 400 oC. We observe sub-micron-scale regions, where apparently disconnected Cu and W grains have near identical crystallographic orientations. This persistence of grain orientations suggests Cu and W grains within these regions are interconnected in 3-D when they first form and may be considered as intercalated, sub-micron-scale "super-grains". Indeed, atom probe tomography provides direct evidence of 3-D interconnectivity of W domains. Our findings shed light on the structure and self organization mechanisms of nanocomposites formed by spontaneous phase separation of co-deposited metals.

Yadav, Digvijay↗

Structure of the pellet-cladding interaction layer of a high-burnup Zr-Nb-O nuclear fuel cladding

Here, structure of the pellet/cladding-interaction (PCI) layer of a high-burnup nuclear fuel with niobium-bearing cladding was investigated using modern transmission electron microscopy (TEM) techniques. Morphology of the PCI consisted of uniform zirconia layer on the cladding side and finger-like features towards to the ceramic fuel. The PCI layer showed a complex microstructure that constitutes three distinct zirconia layers formed by two zirconia phases. From cladding to fuel, monoclinic, tetragonal, and another tetragonal phase were determined via TEM diffraction patterns and precession electron diffraction (PED) using ASTAR microscopy platform (AMP). Characterizations showed that monoclinic and tetragonal phases close to the cladding were crack-free, but the tetragonal layer adjacent to the fuel contained cracks and pores. Presence of the monoclinic layer suggested that its formation involved the gaseous diffusion of oxygen below threshold dose of fission product damage before the fuel/cladding contact occurred. Furthermore, high-resolution TEM revealed compound phase of (U,Zr)O 2 at fringes of zirconia fingers on the fuel side.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermal stability of titanate nanorods and titania nanowires formed from titanate nanotubes by heating

The structure of titanate nanowires was studied by a combination of powder X-ray diffraction (XRD) and 3D precession electron diffraction. Titania nanowires and titanate nanorods were prepared by heating of titanate nanotubes. The structure of final product depended on heating conditions. Titanium nanotubes heated in air at a temperature of 850 °C decomposed into three phases — Na{sub 2}Ti{sub 6}O{sub 13} (nanorods) and two phases of TiO{sub 2} — anatase and rutile. At higher temperatures the anatase form of TiO{sub 2} transforms into rutile and the nanorods change into rutile nanoparticles. By contrast, in the vacuum only anatase phases of TiO{sub 2} were obtained by heating at 900 °C. The anatase transformation into rutile began only after a longer time of heating at 1000 °C. For the description of anisotropic XRD line broadening in the total powder pattern fitting by the program MSTRUCT a model of nanorods with elliptical base was included in the software. The model parameters — rod length, axis size of the elliptical base, the ellipse flattening parameter and twist of the base could be refined. Variation of particle shapes with temperature was found. - Highlights: • Titanate nanotubes changed to particles of TiO{sub 2} and nanorods of Na{sub 2}Ti{sub 6}O{sub 13} at 850 °C. • With heating time and temperature nanorods transformed to rutile nanoparticles. • X-ray diffraction powder pattern fitting indicated an elliptical shape of nanorod base. • No transition of titanate nanotubes to Na{sub 2}Ti{sub 6}O{sub 13} was found after heating in vacuum. • Heating of titanate nanotubes in vacuum leads to appearance of anatase nanowires.

36 MATERIALS SCIENCE↗

In-situ 3D characterization of He bubble and displacement damage in dense and nanoporous thin films.

This initial work attempted to determine the feasibility of using advanced in-situ, electron tomography, and precession electron diffraction techniques to determine the structural evolution that occurs during advanced aging of Pd films with nanometer resolution. To date, significant progress has been made in studying the cavity structures in sputtered, evaporated, and pulsed-laser deposited Pd films that result from both the deposition parameters, as well as from He ion implantation. In addition, preliminary work has been done to determine the feasibility of performing precession electron diffraction (PED) and electron tomography in these type of systems. Significant future work is needed to determine the proper conditions such that relevant advanced aging protocols can be developed.

Hattar, Khalid Mikhiel↗

Microstructure, microtexture and precipitation in the ultrafine-grained surface layer of an Al-Zn-Mg-Cu alloy processed by sliding friction treatment

Precipitate redistribution and texture evolution are usually two concurrent aspects accompanying grain refinement induced by various surface treatment. However, the detailed precipitate redistribution characteristics and process, as well as crystallographic texture in the surface refined grain layer, are still far from full understanding. In this study, we focused on the microstructural and crystallographic features of the sliding friction treatment (SFT) induced surface deformation layer in a 7050 aluminum alloy. With the combination of transmission electron microscopy (TEM) and high angle angular dark field scanning TEM (HAADF-STEM) observations, a surface ultrafine grain (UFG) layer composed of both equiaxed and lamellar ultrafine grains and decorated by high density of coarse grain boundary precipitates (GBPs) were revealed. Further precession electron diffraction (PED) assisted orientation mapping unraveled that high angle grain boundaries rather than low angle grain boundaries are the most favorable nucleation sites for GBPs. The prominent precipitate redistribution can be divided into three successive and interrelated stages, i.e. the mechanically induced precipitate dissolution, solute diffusion and reprecipitation. The quantitative prediction based on pipe diffusion along dislocations and grain boundary diffusion proved the distribution feasibility of GBPs around UFGs. Based on PED and electron backscatter diffraction (EBSD) analyses, the crystallographic texture of the surface UFG layer was identified as a shear texture composed of major rotated cube texture (001) 〈110〉 and minor (111) 〈112〉, while that of the adjoining lamellar coarse grained matrix was pure brass. The SFT induced surface severe shear deformation is responsible for texture evolution. - Highlights: •The surface ultrafine grain layer in a 7050 aluminum alloy was focused. •Precipitate redistribution and texture evolution were discussed. •The quantitative prediction proved the distribution feasibility of GBPs. •Precession electron diffraction orientation mapping showed a shear texture.

36 MATERIALS SCIENCE↗

Nanoscale elastic strain mapping of polycrystalline materials

Measuring elastic strain with nanoscale resolution has historically been very difficult and required a marriage of simulations and experiments. Nano precession electron diffraction provides excellent strain and spatial resolution but has traditionally only been applied to single-crystalline semiconductors. The present study illustrates that the technique can also be applied to polycrystalline materials. The strain resolution was determined to be 0.15% and 0.10% for polycrystalline copper and boron carbide, respectively. Local strain maps were obtained near grain boundaries in boron carbide and dislocations in magnesium and shown to correlate with expected values, thus demonstrating the efficacy of this technique. This study demonstrates that nano precession electron diffraction can be extended from semiconductor devices to polycrystalline metals and ceramics to map nanoscale elastic strain fields with high strain resolution.

36 MATERIALS SCIENCE↗

Study of titanate nanotubes by X-ray and electron diffraction and electron microscopy

The structure of titanate nanotubes (Ti-NTs) was studied by a combination of powder X-ray diffraction (PXRD), electron diffraction and high resolution transmission electron microscopy (HRTEM). Ti-NTs are prepared by hydrothermal treatment of TiO{sub 2} powder. The structure is identified by powder X-ray diffraction as the one based on the structure of H{sub 2}Ti{sub 2}O{sub 5}·H{sub 2}O phase. The same structure is obtained by projected potential from HRTEM through-focus image series. The structure is verified by simulated PXRD pattern with the aid of the Debye formula. The validity of the model is tested by computing Fourier transformation of a single nanotube which is proportional to measured electron diffraction intensities. A good agreement of this calculation with measured precession electron diffraction data is achieved. - Highlights: • Titanate nanotubes were prepared by hydrothermal method. • X-ray powder diffraction indicated their structure based on that of H{sub 2}Ti{sub 2}O{sub 5}·H{sub 2}O. • Structural model was created with the aid of high-resolution electron microscopy. • The model was verified with electron diffraction data. • X-ray powder diffraction pattern was calculated with the aid of the Debye formula.

36 MATERIALS SCIENCE↗

The structure of nano-twinned rhombohedral YCuO 2.66 solved by electron crystallography

In the search for frustrated spin interactions, a YCuO 2.66 phase has been synthesized by a treatment under oxygen pressure of YCuO 2.5 . X-ray powder diffraction and electron diffraction studies have been conducted. Electron diffraction shows that the sample is twinned on a 10 nm scale. Precession electron diffraction data obtained from a twinned crystal was treated in order to obtain intensities corresponding to only one of the orientations of the twins. From this data a structure solution was obtained where, as in YCuO 2.5 , the Cu atoms form triangular planes. The Cu atoms are linked in two dimensions by oxygen atoms in the present structure whereas in YCuO 2.5 they are only linked in one-dimensional chains.

36 MATERIALS SCIENCE↗

Deformation of Diopside Single Crystal at Mantle Pressure 2 TEM Characterization of Deformation Microstructures

The dislocation microstructures of diopside single crystals deformed at high-pressure (4 {<=} P {<=} 9 GPa), high-temperature (1100{sup o} {<=} T {<=} 1400 {sup o}C) using a Deformation-DIA high-pressure apparatus (D-DIA) have been characterized by transmission electron microscopy using weak-beam dark-field (WBDF), precession electron diffraction (PED), large-angle convergent-beam electron diffraction (LACBED) and the thickness-fringe method. Dislocation glide is the dominant deformation mechanism under these conditions. The 1/2<110>{l_brace}110{r_brace} glide is controlled by lattice friction on the edge segments and shows extensive cross-slip. The [001] glide occurs mostly on {l_brace}110{r_brace}; no evidence for [001](010) glide has been found. The [100] dislocations bear a strong lattice friction probably due to complex (out of glide) core structures.

58 GEOSCIENCES↗

Lattice rotations in precipitate free zones in an Al-Mg-Si alloy

Highlights: • Recovery processes in precipitate free zones differ from those in grain interiors. • Most precipitate free zones contain few dislocations, after deformation. • Deformation can induce large misorientations in precipitate free zones. • Some deformed precipitate free zones contain nanoscale grains. - Abstract: Scanning precession electron diffraction and automated crystal orientation mapping in a transmission electron microscope (TEM) have been applied to quantitatively study the crystal orientation of precipitate free zones (PFZs) of four GB regions in an AA6060 alloy in peak aged condition (temper T6) after uniaxial compression to 20% engineering strain. The PFZ width in the alloy was found to be w = 170 ± 40 nm. The results show that some PFZs develop significant misorientations relative to their parent grain, and represent, to the best knowledge of the authors, the first quantitative evidence of this. This misorientation may either be constant inside a particular PFZ, making it appear like a band or a very elongated subgrain, or be partitioned in discrete regions with a diameter comparable to the PFZ width, making the former PFZ into a collection of small grains. The band-like PFZ observed in this work had a misorientation relative to its parent grain of ≈ 7°, while the grain-like PFZ had grains with misorientations between ≈ 12° and ≈ 20° relative to its parent grain. The other PFZs that were observed had only limited misorientations relative to their parent grains, and had either dislocations perpendicular to the GB plane or a dislocation wall at the transition region. A general TEM study of the material at various engineering strains was also conducted and suggests that grain-like PFZs are more frequent for larger strains, indicating that the different PFZ features are likely due to different strain localisation in individual PFZs. This localisation is expected to be influenced by the orientation of the loading axis relative to crystal orientations and GB planes. It is also suggested that the different PFZ features engender different work hardening rates and possibly affect nucleation of intergranular fracture. The results support previous studies on the microstructure evolution of PFZs in age-hardenable aluminium alloys during deformation.

36 MATERIALS SCIENCE↗

The onset and evolution of fatigue-induced abnormal grain growth in nanocrystalline Ni–Fe

Conventional structural metals suffer from fatigue-crack initiation through dislocation activity which forms persistent slip bands leading to notch-like extrusions and intrusions. Ultrafine-grained and nanocrystalline metals can potentially exhibit superior fatigue-crack initiation resistance by suppressing these cumulative dislocation activities. Prior studies on these metals have confirmed improved high-cycle fatigue performance. In the case of nano-grained metals, analyses of subsurface crack initiation sites have indicated that the crack nucleation is associated with abnormally large grains. But, these post-mortem analyses have led to only speculation about when abnormal grain growth occurs (e.g., during fatigue, after crack initiation, or during crack growth). In this study, a recently developed synchrotron X-ray diffraction technique was used to detect the onset and progression of abnormal grain growth during stress-controlled fatigue loading. Our study provides the first direct evidence that the grain coarsening is cyclically induced and occurs well before final fatigue failure—our results indicate that the first half of the fatigue life was spent prior to the detectable onset of abnormal grain growth, while the second half was spent coarsening the nanocrystalline structure and cyclically deforming the abnormally large grains until crack initiation. Post-mortem fractography, coupled with cycle-dependent diffraction data, provides the first details regarding the kinetics of this abnormal grain growth process during high-cycle fatigue testing. Finally, precession electron diffraction images collected in a transmission electron microscope after the in situ fatigue experiment also confirm the X-ray evidence that the abnormally large grains contain substantial misorientation gradients and sub-grain boundaries.

36 MATERIALS SCIENCE↗

A Rutile Chevron Modulation in Delafossite-Like Ga 3– x In 3 Ti x O 9+ x /2

The structure solution of the modulated, delafossite-related, orthorhombic Ga 3–x In 3 Ti x O 9+x/2 for x = 1.5 is reported here in conjunction with a model describing the modulation as a function of x for the entire system. Previously reported structures in the related A 3–x In 3 Ti x O 9+x/2 (A = Al, Cr, or Fe) systems use X-ray diffraction to determine that the anion lattice is the source of modulation. Neutron diffraction, with its enhanced sensitivity to light atoms, offers a route to solving the modulation and is used here, in combination with precession electron diffraction tomography (PEDT), to solve the structure of Ga 1.5 In 3 Ti 1.5 O 9.75 . We construct a model that describes the anion modulation through the formation of rutile chevrons as a function of x. This model accommodates the orthorhombic phase (1.5 ≤ x ≤ 2.1) in the Ga 3-x In 3 Ti x O 9+x/2 system, which transitions to a biphasic mixture (2.2 ≤ x ≤ 2.3) with a monoclinic, delafossite-related phase (2.4 ≤ x ≤ 2.5). The optical band gaps of this system are determined, and are stable at ~3.4 eV before a ~0.4 eV decrease between x = 1.9 and 2.0. After this decrease, stability resumes at ~3.0 eV. Resistance to oxidation and reduction is also presented.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The evolution of precipitate crystal structures in an Al-Mg-Si(-Cu) alloy studied by a combined HAADF-STEM and SPED approach

Highlights: • Scanning electron diffraction and machine learning complement lattice imaging • Developed approach gives increased objectivity in precipitate phase analysis • Precipitate phase fractions and solute content obtained with superior statistics • 0.01 at.% Cu changes the Al-Mg-Si system precipitation during overageing • Q’-phase eventually dominates precipitate structures and shows varying Cu-occupancy - Abstract: This work presents a detailed investigation into the effect of a low Cu addition (0.01 at.%) on precipitation in an Al-0.80Mg-0.85Si alloy during ageing. The precipitate crystal structures were assessed by scanning transmission electron microscopy combined with a novel scanning precession electron diffraction approach, which includes machine learning. The combination of techniques enabled evaluation of the atomic arrangement within individual precipitates, as well as an improved estimate of precipitate phase fractions at each ageing condition, through analysis of a statistically significant number of precipitates. Based on the obtained results, the total amount of solute atoms locked inside precipitates could be approximated. It was shown that even with a Cu content close to impurity levels, the Al-Mg-Si system precipitation was significantly affected with overageing. The principal change was due to a gradually increasing phase fraction of the Cu-containing Q′-phase, which eventually was seen to dominate the precipitate structures. The structural overtake could be explained based on a continuous formation of the thermally stable Q′-phase, with Cu atomic columns incorporating less Cu than what could potentially be accommodated.

36 MATERIALS SCIENCE↗

Influence of SiC grain boundary character on fission product transport in irradiated TRISO fuel

The relationship between grain boundary character and fission product migration is identified as an important knowledge gap in order to advance the understanding of fission product release from TRISO fuel particles. Precession electron diffraction (PED), a TEM-based technique, was used in this study to quickly and efficiently provide the crystallographic information needed to identify grain boundary misorientation, grain boundary type (low or high angle) and whether the boundary is coincident site lattice (CSL) – related, in irradiated SiC. Analysis of PED data showed the grain structure of the SiC layer in an irradiated TRISO fuel particle from the AGR-1 experiment to be composed mainly of twin boundaries with a small fraction of low angle grain boundaries (<10%). In general, fission products favor precipitation on random, high angle grain boundaries but can precipitate out on low angle and CSL-related grain boundaries to a limited degree. Pd is capable of precipitating out on all types of grain boundaries but most prominently on random, high angle grain boundaries. Pd-U and Pd-Ag precipitates were found on CSL-related as well as random high angle grain boundaries but not on low angle grain boundaries. In contrast, precipitates containing only Ag were found only on random, high angle grain boundaries but not on either low angle or CSL-related grain boundaries.

36 MATERIALS SCIENCE↗

Laser weld-induced formation of amorphous Mn–Si precipitate in 304 stainless steel

In this paper, we report the formation of partially amorphous Mn-Si precipitates due to laser welding of face centered cubic (fcc) 304 stainless steel. Transmission electron microscopy and precession electron diffraction studies in the heat affected zone (HAZ) of the weldment indicate the formation of these precipitates in grain interiors. Precipitates have MnSi stoichiometry and the partially crystalline regions have a lattice constant of 0.45 nm. It is surmised that the rapid cooling rates during the laser weld melt pool solidification process may be sufficient to inhibit the complete crystallization of these precipitates.

304 stainless steel↗

Grain subdivision and structural modifications by high-energy heavy ions in UO 2 with different initial grain size

Irradiation with 84 MeV Xe ions at peak fluence above 7 × 10 17 ions/cm 2 has been carried out on two UO 2 samples with different initial grain sizes at 300 °C and 500 °C. Characterization of both grain structure and bubble morphology has been performed using transmission electron microscopy, image analysis and precession electron diffraction. The bubble size in the large-grained sample was smaller than that in the standard-grain sample, confirming fission gas precipitation resistance in the former. The ion irradiation in the high electronic energy deposition range has caused formation of a large density of dislocations which resulted in grain polygonization for the sample with standard grain size, which was observed in multiple lamellas extracted next to each other at peak dose. The sample with large grains showed inconsistent behavior. In one case, dislocation pile-up occurred, but no sub-grain formation was observed. An adjacent location showed sub-grain formation, even if to less extent compared to the standard grain-size sample. Furthermore, these findings suggest a limited polygonization resistance in large-grained UO 2 compared to standard-grain UO 2 . Recrystallization of both sample surfaces was present, leaving unclear if this is a surface effect or a consequence of the highest energy deposition rate in this area.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High cycle fatigue in the transmission electron microscope

One of the most common causes of structural failure in metals is fatigue induced by cyclic loading. Historically, microstructure-level analysis of fatigue cracks has primarily been performed post mortem. However, such investigations do not directly reveal the internal structural processes at work near micro- and nanoscale fatigue cracks and thus do not provide direct evidence of active microstructural mechanisms. In this paper, the tension–tension fatigue behavior of nanocrystalline Cu was monitored in real time at the nanoscale by utilizing a new capability for quantitative cyclic mechanical loading performed in situ in a transmission electron microscope (TEM). Controllable loads were applied at frequencies from one to several hundred hertz, enabling accumulations of 10 6 cycles within 1 h. The nanometer-scale spatial resolution of the TEM allows quantitative fatigue crack growth studies at very slow crack growth rates, measured here at ~10 –12 m·cycle –1 . This represents an incipient threshold regime that is well below the tensile yield stress and near the minimum conditions for fatigue crack growth. Evidence of localized deformation and grain growth within 150 nm of the crack tip was observed by both standard imaging and precession electron diffraction orientation mapping. Finally, these observations begin to reveal with unprecedented detail the local microstructural processes that govern damage accumulation, crack nucleation, and crack propagation during fatigue loading in nanocrystalline Cu.

36 MATERIALS SCIENCE↗