Search NASA⌕ Search

SEARCH · Search NASA

Results for “reciprocating wear”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

29 records · Page 2

Interaction of sulfuric acid corrosion and mechanical wear of iron

Friction and wear experiments were conducted with elemental iron sliding on aluminum oxide in aerated sulfuric acid at concentrations ranging from very dilute (0.00007 N; i.e., 4 ppm) to very concentrated (96 percent acid). Load and reciprocating sliding speed were kept constant. With the most dilute acid concentration of 0.00007 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At slightly higher concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent (1 N), the well-established high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid and decreased somewhat to 50 percent acid in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It was apparent that the normal passivating film was being worn away and a galvanic cell established that rapidly attacked the wear area. Under the conditions where direct corrosion losses were highest, the coefficient of friction was the lowest.

Rengstorff, G. W. P.↗

Interaction of sulfuric acid corrosion and mechanical wear of iron

Friction and wear experiment were conducted with elemental iron sliding on aluminum oxide in aerated sulfuric acid at concentrations ranging from very dilute (0.00007 N; i.e., 4 ppm) to very concentrated (96 percent acid). Load and reciprocating sliding speed were kept constant. With the most dilute acid concentration of 0.00007 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At slightly higher concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent (1 N), the well-established high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid and decreased somewhat to 50 percent acid in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It was apparent that the normal passivating film was being worn away and a galvanic cell established that rapidly attacked the wear area. Under the conditions where direct corrosion losses were highest, the coefficient of friction was the lowest.

Rengstorff, G. W. P.↗

Design and use of multiple blade slurry sawing in a production atmosphere

The technique and uses of the multiple blade slurry (MBS) saw are considered. Multiple bands of steel are arranged in a frame and the frame is reciprocated with the steel bands to a workpiece, while simultaneously applying abrasive at the point of contact. The blades wear slots in the workpiece and progress through the piece resulting in several parts of wafers. The transition to MBA from diamond slicing is justified by savings resulting from minimized kerf losses, minimized subsurface damage, and improved surface quality off the saw. This allows wafering much closer to finished thickness specifications. The current state of the art MBS technology must be significantly improved if the low cost solar array (LSA) goals are to be attained. It is concluded that although MBS will never be the answer to every wafering requirement, the economical production of wafers to LSA project specifications will be achieved.

Lynah, F. P., Jr.↗

A High Temperature Vapor Phase Lubrication Study Utilizing a Thioether Liquid Lubricant

Much of the experimental work on vapor phase lubrication has employed certain organo phosphorous compounds as the vapor phase lubricant. Graham and Klaus, for instance, used tricresyl phosphate (TCP) and tributyl phosphate to vapor phase lubricate a four-ball wear tester using M50 steel balls at 370 C. Makki and Graham were able to vapor phase lubricate a reciprocating pin on plate tribometer using 1018 steel at 280 C with TCP vapor. Although a few organo phosphorous compounds, such as TCP, have been successfully used as vapor phase lubricants in many laboratory experiments, many problems remain unsolved. Two areas of concern relate to the 'durability' of phosphate deposited films and to the ability of the lubricating system to "self-recover" when vapor phase lubricated with an organo phosphorous compound. Durability refers to the ability of the deposited film to provide effective lubrication, for a period of time, after the vapor flow to the lubricating surfaces has been interrupted. Vapor phase lubrication tests, conducted at Cleveland State University with their high temperature tribometer, revealed that when TCP vapor flow to the lubricating surfaces was interrupted the frictional coefficient of the system rapidly increased from a value less than 0.1 to a value of 0.3 which was selected as our failure point. Self-recovery means the ability of the vapor phase lubricant to reduce the frictional coefficient of the lubricating system back down to value less than 0.1 after startup of the interrupted vapor flow. Lubrication tests conducted at Cleveland State University revealed that the high temperature tribometer could not self-recover after startup of the interrupted TCP vapor flow.

Morales, Wilfredo↗

Tribological Performance of PM400 Bushings in Oscillatory Sliding from 25 to 927 °C

Small bore (6.35 millimeter) bushings, made from NASA PM400 solid lubricant composite, were evaluated in oscillatory sliding contact against a nickel-based superalloy shaft. Tests were conducted in air from 25 to 900 degrees Centigrade for extended periods (1 million cycles, plus or minus 15 degrees, 1 hertz) to assess the suitability of PM400 in gas turbine and reciprocating engine exhaust gas path control valve applications. Operating torque and estimated friction was monitored throughout the test duration and wear was measured at the end of test. In general, friction, torque and wear was low. At temperatures above 600 degrees Centigrade, bushing dimensional stability was achieved via short duration pre-test furnace exposure heat treatments. Preliminary test results show that bushings made from NASA PM400 are feasible for aerospace and industrial applications.

high temperature solid lubricants↗

Lubricous Deposit Formed In Situ Between Wearing Surfaces at High Temperatures

Many components of future aircraft will be constructed from novel high-temperature materials, such as superalloys and ceramic composites, to meet expected operating temperatures in excess of 300 C. There are no known liquid lubricants that can lubricate above 300 C without significant decomposition. Solid lubricants could be considered, but problems caused by the higher friction coefficients and wear rates of the solid lubricant film make this an undesirable approach. An alternative method of lubrication is currently being investigated: vapor phase lubrication. In vapor phase lubrication, an organic liquid (in our studies a thioether was used) is vaporized into a flowing air stream that is directed to sliding surfaces where lubrication is needed. The organic vapor reacts at the concentrated contact sliding area generating a lubricous deposit. This deposit has been characterized as a thin polymeric film that can provide effective lubrication at temperatures greater than 400 C. Initial tribological studies were conducted at the NASA Lewis Research Center and Cleveland State University with a high-temperature friction and wear tribometer. A cast iron rod was loaded (a 4-kg mass was used to generate a contact pressure of 1.2 MPa) against a reciprocating, cast iron plate at 500 C. This system was then lubricated with the vapor phase of thioether.

Source record↗

Comparison of seal materials for use in Stirling engines

In a dry, reciprocating sliding test, rods of 12 different surface materials rubbed against a glass filled PTFE gas seal. To simulate operation in a Stirling engine a gas (N2) pressure of 1 MPa differential pressure was applied across the seal. Gas leakage rates, rods surface temperatures, changes in the surface finish of the rod, surface hardness of the rod and wear rate of the seals were measured. The rod surface materials that produced the least seal were: plasma sprayed molybdenum (75 Mo 18 Ni 4 Cr), gas nitrided steel, and plasma sprayed aluminum oxide (94 Al2O3 6 TiO2). In contrast to almost all other mating surfaces, the surface roughness of the rods coated with Mo did not decrease during wear. This property is very important for the formation of a PTFE transfer film on the mating surface. The presence of a stable transfer film gives a low PTFE wear rate.

Lundholm, G.↗

Workpiece positioning vise

A pair of jaw assemblies simultaneously driven in opposed reciprocation by a single shaft has oppositely threaded sections to automatically center delicate or brittle workpieces such as lithium fluoride crystal beneath the blade of a crystal cleaving machine. Both jaw assemblies are suspended above the vise bed by a pair of parallel guide shafts attached to the vise bed. Linear rolling bearings, fitted around the guide shafts and firmly held by opposite ends of the jaw assemblies, provide rolling friction between the guide shafts and the jaw assemblies. A belleville washer at one end of the drive shaft and thrust bearings at both drive shaft ends hold the shaft in compression between the vise bed, thereby preventing wobble of the jaw assemblies due to wear between the shaft and vise bed.

Hallberg, F. C.↗

The tribology of PS212 coatings and PM212 composites for the lubrication of titanium 6A1-4V components of a Stirling engine space power system

The Stirling space power machine incorporates a linear alternator to generate electrical power. The alternator is a reciprocating device that is driven by a solar or nuclear-powered Stirling engine. The power piston and cylinder are made of titanium 6A1-4V (Ti6-4) alloy, and are designed to be lubricated by a hydrodynamically-generated gas film. Rubbing occurs during starts and stops and there is a possibility of an occasional high speed rub. Since titanium is known to have a severe galling tendency in sliding contacts, a 'backup,' self-lubricating coating on the cylinder and/or the piston is needed. This report describes the results of a research program to study the lubrication of Ti6-4 with the following chromium carbide based materials: plasma-sprayed PS212 coatings and sintered PM212 counterfaces. Program objectives are to achieve adherent coatings on Ti6-4 and to measure the friction and wear characteristics of the following sliding combinations under conditions simulative of the Stirling-driven space power linear alternator: Ti6-4/Ti6-4 baseline, Ti6-4/PS212 coated Ti6-4, and Ps212 coated Ti6-4/PM212

Sliney, Harold E.↗

The tribology of PS212 coatings and PM212 composites for the lubrication of titanium 6Al-4V components of a Stirling engine space power system

The Stirling space power machine incorporates a linear alternator to generate electrical power. The alternator is a reciprocating device that is driven by a solar or nuclear-powered Stirling engine. The power piston and cylinder are made of titanium 6Al-4V (Ti6-4) alloy, and are designed to be lubricated by a hydrodynamically-generated gas film. Rubbing occurs during starts and stops and there is the possibility of an occasional high speed rub. Since titanium is known to have a severe galling tendency in sliding contacts, a 'back-up', self-lubricating coating on the cylinder and/or the piston is needed. This report describes the results of a research program to study the lubrication of Ti6-4 with the following chromium carbide based materials: plasma-sprayed PS212 coatings and sintered PM212 counterfaces. Program objectives are to achieve adherent coatings on Ti6-4 and to measure the friction and wear characteristics of the following sliding combinations under conditions simulative of the Stirling-driven space power linear alternator: Ti6-4/Ti6-4 baseline, Ti6-4/PS212-coated Ti6-4, and PS212-coated Ti6-4/PM212.

Sliney, Harold E.↗