SEARCH · Search NASA
Results for “sintering preparation”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Phase evolution during reactive flash sintering of Li 6.25 Al 0.25 La 3 Zr 2 O 12 starting from a chemically prepared powder
Here, reactive flash sintering (RFS) of a chemically prepared multiphase precursor powder was performed to fabricate Li 6.25 Al 0.25 La 3 Zr 2 O 12 (Al-LLZO) ceramics. This approach allowed for obtaining single-phase dense samples in a remarkably short processing time of 30 s, at a furnace temperature of 600 °C, with an electric field of 50 V cm -1 and a current limit of 150 mA mm -2 . The ceramics display high bulk conductivity of 0.18 mS cm -1 at room temperature. Furthermore, phase evolution is studied by in-situ X-ray diffraction during: i) conventional heating and ii) RFS under current rate mode. As expected, the intermediate phases progressively dissolved into the Al-LLZO matrix by conventional heating. On the other hand, RFS promoted the growth of the intermediate La 2 Zr 2 O 7 , an effect that was overcome by the thermally driven formation of Al-LLZO at higher temperatures. The observed different reaction pathway suggests that RFS can be used for stabilizing phases that are not thermodynamically favored upon conventional heating.
TEM observations on grain boundaries in sintered silicon, part 1
Grain boundaries in silicon with a predetermined orientation were prepared by the sintering of two single crystals. A combination of standard transmission electron microscopy and lattice imaging was used to investigate the structure of the boundaries produced. Low angle grain boundaries on (100) and (111) planes, and twin boundaries on (111) planes are discussed in detail.
Microwave Sintering Lunar Landing Pads & Horizontal Infrastructure
Moon to Mars Planetary Autonomous Construction Technology’s (MMPACT) Microwave Structure Construction Capability (MSCC) team is developing the ability to prepare the lunar regolith and densify it into glass-ceramic landing pads and horizontal infrastructure. Microwave energy will be utilized to densify the lunar regolith. Some of the concept of operations, simulant and synthetic minerals, site preparation, design, microwave sintering, testing, & ancillary instrument technical challenges were listed. A current status of the MSCC project is also provided.
W-ZrC composites prepared by reactive melt infiltration of Zr 2 Cu alloy into binder jet 3D printed WC preforms
W-ZrC composites were successfully prepared by reactive melt infiltration (RMI) of stoichiometric and excess amounts of Zr 2 Cu into sintered and un-sintered WC preforms made from binder jet 3D printing. The focus of this work was to study the conversion of reactant powders and liquid infiltrant with varying preform density and infiltrant amount by controlling the processing time to reach high conversion yield while understanding the phase composition, microstructure, and hardness. To investigate the effect of time, the reactive melt infiltration was conducted at 1400 °C for 2, 4 and 8 h in a furnace with 96% Ar - 4% H2 gas atmosphere. The increase in reaction time from 2 to 8 h increased the W and W 2 C phase contents and decreased the ZrC phase content when using sintered WC preforms. Samples prepared from un-sintered WC preforms exhibited improved reactive melt infiltration compared to sintered samples, and there was no detectable W 2 C phase and nearly full consumption of WC. Similar to sintered WC samples, the content of W and ZrC phases increased with the increase in time from 2 to 8 h. The interfaces and phases at reaction interfaces were investigated using electron diffraction analysis and S/TEM-EDS to understand material stability; the phases were identified and consistent with XRD analysis. Additionally, there was no Cu present at the interfaces. Increasing the amount of infiltrant led to better reactive melt infiltration. In general, the hardness increased with reaction time and the highest Vickers hardness was found in the W-ZrC sample formed from sintered WC reacted with excess Zr 2 Cu. Finally, this research addresses the critical comparison of sintering and RMI time and shows that by using un-sintered samples for 8 h we are able to achieve W-ZrC composites with fewer undesired phases.
Ammonia formation caused by the presence of water in the wet grinding of silicon nitride powder
Si3 N4 powder (amorphous, alpha-, and beta-Si3 N4) was mixed with MeOH containing 8.87 mol. % H2O and ground. The NH3 generation rapidly increased after a grinding time of 100 hours. Silicon nitride sintered material was chosen as one of the high temperature, high strength structural materials and studies of the control of the raw material powder, preparation of the sintered body (finding the right assistant, hot press, high pressure sintering, fracture toughness and oxidation at high temperature were performed.
Improved plaque materials for aerospace nickel-cadmium cells
Improved cadmium electrode substrates with precisely controlled microstructures for possible use in aerospace nickel-cadmium cells were prepared. The preparative technique was a powder metallurgical process in which a fugitive pore-former and a nickel powder were blended, then isostatically compacted, and subsequently sintered. Cadmium electrodes prepared from such substrates were cycle tested using an accelerated tortuous test regime. It was discovered that plaques of 60% or 80% porosity prepared with a 25 micron pore-former were better than state-of-the-art electrodes in terms of efficienty and/or mechanical strength. The 60% structures were particularly outstanding in this respect in that they had efficiencies only 5-10 percentage points lower than state-of-the-art electrodes and vastly superior mechanical properties. This added strength was observed to eliminate cracking and physical degradation of the electrodes during processing and cycling. The cadmium electrodes prepared from the 80% porous substrates proved to be the best electrodes made during the course of the work from the point of view of highest efficiency. Three-point bend tests were used to measure mechanical properties of the plaques produced and also as a general characterization tool. In addition, the BET surface areas of selected specimens was determined. The SEM was used for judging microscopic uniformity and quantitatively determining the induced pore size and various other fine structures in the substrates. The technique of X-ray radiography was used to follow the bulk uniformity of the substrates at various stages of their processing.
Demonstration of the Reproducibility Challenges in the Sintering Behavior of Lithium‐Stuffed Garnets in Scaling up Synthesis
Lithium-stuffed garnets, such as Li 7 La 3 Zr 2 O 12 (LLZO), are promising candidates for next-generation solid-state batteries because of their high room-temperature ionic conductivity and chemical stability against lithium metal anodes, which are crucial for achieving higher energy density. However, realizing LLZO's potential in practical devices requires synthesis methods that can be scaled reliably to large batch sizes for manufacturing. Herein, we investigate the sintering reproducibility of LLZO synthesized at larger scales using ultrasonic spray pyrolysis, a cost-effective and scalable synthesis route. Two 100 g batches of Al-doped LLZO are prepared and their sintering behavior is examined in detail. Both Al-LLZO batches contain over 90 wt.% cubic-phase LLZO, and both batches exhibit room temperature conductivities greater than 1 × 10 −4 S cm −1 at a relative density above 0.8. However, variations in secondary phases and subtle differences in Al content lead to significant differences in densification and microstructure. These results demonstrate that LLZO's sintering behavior is highly sensitive to small changes in secondary phases and Al content, creating reproducibility challenges when moving from laboratory- to manufacturing-scale synthesis.
Heat-sterilized silver oxide-zinc cells: Cycle life studies
A JPL study was conducted to evaluate the cell design parameters that contribute to the cycle life of sealed, heat-sterilized silver oxide-zinc cells. Test cells having a rated capacity of 4.2 A-h were fabricated using zinc oxide electrodes prepared by the sintered Teflon process. Two separator variations were evaluated, one having acrylic acid and the other methacrylic acid grafted to irradiated polyethylene film. Significant results of this study include the following: (1) cycle life in excess of 300 cycles was attained; (2) a zinc oxide/silver stoichiometric ratio of 1.5 resulted in greater cycle life than a ratio of 1.1, and similar cycle life to cells having a ratio of 2; (3) cells having methacrylic acid grafted separators suffered somewhat less in capacity loss due to zinc electrode shape change than cells having acrylic acid type; (4) use of acrylic acid grafted separators was slightly superior to the methacrylic acid type in respect to silver penetration; and (5) the inclusion of a layer of potassium titanate paper adjacent to the zinc electrodes resulted in cells that achieved higher cycle life before any of the group failed than that reached by cells of any other construction.
Millimeter wave surface resistance of RBa2Cu3O(7-delta) (R=Y,Eu,Dy,Sm,Er) superconductors
The measurements are reported of the millimeter wave surface resistance R(sub s) at 58.6 GHz of bulk samples of RBa2Cu3O(7-delta) (R = Y,Eu,Dy,Sm,Er) and of YBa2Cu3O(7-delta) superconducting films, in the temperature range from 20 to 300 K. The bulk samples were prepared by cold pressing the powders of RBa2Cu3O(7-delta) into one in. disks. The powders were prepared by several sinterings in one atmosphere of oxygen at 925 C, with grindings between sinterings, to obtain the superconducting phase. The thin films were deposited on SrTiO3 and LaGaO3 substrates by pulsed laser ablation. Each sample was measured by replacing the end wall of a gold-plated Te sub 013 circular mode copper cavity with the sample and determining the cavity quality factor . From the difference in the Q-factor of the cavity, with and without the sample, the R(sub s) of the sample was determined.
Novel processing route for design and manufacturing of metal toughened nanoceramics: Al–Al 2 O 3 nanocermets
Monolithic alumina is a highly brittle ceramic with a very low fracture toughness, making it an unreliable material for mechanical and structural applications. Ceramic-metal composites (cermets) are the subject of intensive interest to obtain materials which can address the intrinsic brittleness of ceramics without compromising their high strength and light weight. In the present investigation, aluminium-alumina (Al–Al 2 O 3 ) nanocermets were developed. The nanocermets possessed the toughness of Al phase and the strength of reinforced nano Al 2 O 3 particles. Here, the nanocermets green bodies were prepared such that upon sintering each adjacent Al 2 O 3 grain was conformally coated with a continuous Al film. Mechanical milling via a combination of cryo-milling and ball-milling was used to prepare Al–Al 2 O 3 nano-powder mixture. Spark plasma sintering was used to consolidate the green nanocermets. Results show that specimens prepared from 35 h milled powders exhibited superior mechanical properties as compared to other nanocermets, with an improvement in microhardness, elastic modulus, compressive strength, and flexural strength by 88%, 78%, 69% and 40% with respect to sintered pure Al. The indentation toughness of 35 h milled nanocermet showed an increment of 12.5% with respect to sintered pure Al 2 O 3 . Characterization techniques such as XRD, SEM, HR-TEM, X-ray tomography were employed to investigate the phase evolution and structural morphology, while FEM simulations were performed for understanding the crack propagation mechanisms in nanocermets.
In-situ Lunar Launch and Landing Pad Construction with Regolith-Thermoset Polymer Composite Materials
Lunar launch and landing pads are necessary to mitigate risks to lander/ascent vehicles and surrounding surface assets from rocket plume ejected regolith. The current state of the art of landing and launching from the lunar surface is to land/launch on unprepared regolith surfaces. Though this has been a relatively successful approach, significant risks exist for the Artemis Program due to higher thrust levels leading to increased ejecta and cratering, presence of co-located assets in the ejecta path, and potential strict surface levelness requirements. Regolith-thermoset polymer composite materials were developed and evaluated for off Earth launch and landing pad applications. Performance under hot fire conditions was assessed for two simulated Starship lunar launch/landing environments, one targeting thermal conditions and the second targeting pressure conditions. Paver test articles were prepared at 20% and 11% polymer mass fractions. Sintered paver test articles were prepared with 20% polymer grouting filling the seams between pavers. Though significant erosion was experienced during the more extreme thermal testing conditions, all test articles successfully mitigated regolith ejecta from plume effects. A concept for preparing and emplacing the materials was developed and tested in laboratory conditions. The testing evaluated the feasibility of using twin and single screw extruder technology to mix, convey and deposit materials. Both the twin and single screw extruders were capable of processing and extruding the composite with a maximum of 90% mass fraction of regolith achieved by the twin screw extruder.A primary risk for application of regolith-thermoset polymer composites as lunar launch/landingpad is the mass of polymer required to be landed on the moon. Calculations were performed that show that a 100 m diameter, 0.025 m thick pad with polymer mass fraction of 15% will require a payload mass of 72 mt to the Lunar surface. This is below the planned Starship payload capacity to the lunar surface of 100 mt. The regolith-thermoset polymer composite based construction approach proved feasibility in three critical areas: performance under launch/landing conditions, demonstration of a mixing and depositing strategy, and fitting within the planned lunar payload capacity. It is recommended that materials and systems be developed to TRL 6 for a small-scale lunar demonstration of emplacement of a launch/landing pad via a CLPS mission to support Artemis Program roadmap gap closure activities.
Dislocation density in fine grain-size spark-plasma sintered aluminum measured using high brightness synchrotron radiation
In this study, three-dimensional orientation mapping of samples of aluminum prepared by spark plasma sintering (SPS) with average grain sizes of 5 μm and 1 μm has been carried out using high-brightness synchrotron radiation, from which the geometrically necessary dislocation (GND) density has been determined. The low average measured GND density values confirm that the SPS process can be used to produce samples containing grains with dislocation density similar to that of fully recrystallized coarse-grained samples. Values of GND density are also compared to those obtained from electron back-scatter diffraction studies on the same material, highlighting the significantly higher angular resolution of the synchrotron data. For the 5 μm grain-size sample the measured GND density can account for a large fraction of the previously observed positive Hall-Petch deviation of this material. For the 1 μm grain-size sample, however, the GND-based strengthening contribution is much smaller than the reported positive Hall-Petch deviation, such that the additional strength may be reliably associated with dislocation source-limited strengthening.
Si-Ge Nano-Structured with Tungsten Silicide Inclusions
Traditional silicon germanium high temperature thermoelectrics have potential for improvements in figure of merit via nano-structuring with a silicide phase. A second phase of nano-sized silicides can theoretically reduce the lattice component of thermal conductivity without significantly reducing the electrical conductivity. However, experimentally achieving such improvements in line with the theory is complicated by factors such as control of silicide size during sintering, dopant segregation, matrix homogeneity, and sintering kinetics. Samples are prepared using powder metallurgy techniques; including mechanochemical alloying via ball milling and spark plasma sintering for densification. In addition to microstructural development, thermal stability of thermoelectric transport properties are reported, as well as couple and device level characterization.
WSi2 in Si(1-x)Ge(x) Composites: Processing and Thermoelectric Properties
Traditional SiGe thermoelectrics have potential for enhanced figure of merit (ZT) via nano-structuring with a silicide phase, such as WSi2. A second phase of nano-sized silicides can theoretically reduce the lattice component of thermal conductivity without significantly reducing the electrical conductivity. However, experimentally achieving such improvements in line with the theory is complicated by factors such as control of silicide size during sintering, dopant segregation, matrix homogeneity, and sintering kinetics. Samples were prepared using powder metallurgy techniques; including mechano-chemical alloying, via ball milling, and spark plasma sintering for densification. Processing, micro-structural development, and thermoelectric properties will be discussed. Additionally, couple and device level characterization will be introduced.
Fabrication of thin layer beta alumina
Beta alumina tubes having walls 700 microns, 300 microns, and 140 microns were processed by extrusion and sintering utilizing Ford proprietary binder and fabrication systems. Tubes prepared by this method have properties similar to tubes prepared by isostatic pressing and sintering, i.e. density greater than 98% of theoretical and a helium leak rate less than 3 x 10 to the -9th power cc/sq cm/sec. Ford ultrasonic bonding techniques were used for bonding beta alumina end caps to open ended beta -alumina tubes prior to sintering. After sintering, the bond was hermetic, and the integrity of the bonded area was comparable to the body of the tube.
The Grain Boundary Relaxation (GBR) Approach for Manufacturing High Strength Nanocrystalline Lightweight Metals
The overarching goal of the project was to conduct research and development work as proposed in the Statement of Project Objective (SOPO) of the award document DE-FE-0009116. The project had 4 tasks and 12 milestones. All the milestone deliverables were completed. The accomplishments of the project objectives and technical discussions are described in Sections 3 and 4, respectively. The modeling and simulation work indicated that to increase the strength and stability of nanocrystalline aluminum (Al), selection of dopants, such as Mg, is necessary. It was predicted that the crystallite size should be less than 50 nm to give high strength. On the basis of modeling, cryo-milling of Al was conducted with the addition of Mg as a function of different times. The crystallite size of the cryo-milled powders was determined by XRD and TEM. Both measurements showed that the actual crystallite size of the grain was <40 nm. The thermal stability of the grain size was established as a function of temperature. It was established that the grain size was < 50 nm up to 500C. The crystallite size of the bulk sample prepared by spark plasma sintering (SPS) and cold spray (CS) additive manufacturing was less than <40 nm. The mechanical properties of the bulk samples prepared by SPS and CS, showed excellent microhardness, good tensile properties (>200 MPa) with moderate ductility and improved fatigue performance. Adding yttria stabilized zirconia (YSZ) improved the build thick of the CS sample, however the YSZ was getting embedded into the sample. A highly dense SPS samples sent for 3rd party testing to the Innovation Testing Services showed a minimum hardness of 180 HV with an average tensile strength of 512.5 MPa. The high cycle fatigue tests also showed an endurance limit of 179.5 MPa. The Energy cost evaluations showed an overall energy cost of around $\$$17.05 for the cryomilling and SPS processes and the total manufacturing cost calculations of $\$$78.14 for 1 kg of sample. The energy cost to prepare a Kg of CS sample is $\$$17.60 and the overall manufacturing cost is $\$$86.85.
A study of the oxide dispersion and recrystallization in NiCrAl prepared from preoxidized powder
The sintered aluminum powder (SAP) technique of dispersion strengthening (formation of an oxide dispersion by preoxidation of metal powders) was applied to atomized powder of a nickel alloy containing, by weight, 17% Cr, 5% Al, and 0.2% Y. The SAP-NiCrAl alloy (without the ytterbium removed by oxdation) was worked by extrusion and rod rolling at 1205 C and by swaging at 760 C. Annealing treatments were applied after working to determine the recrystallization response. The NiCrAlY alloy, similarly prepared from atomized powder, but without a preoxidation treatment, was examined for comparison. The SAP-NiCrAl alloy exhibited oxide particle size and spacing much larger than that usually observed in oxide dispersion strengthened alloys; nonetheless, it was possible to achieve abnormal (secondary) recrystallization in the SAP-NiCrAl alloy as has been reported for other oxide dispersion strengthened alloys. In contrast, the unoxidized NiCrAlY alloy exhibited only primary recrystallization.