Search NASA⌕ Search

SEARCH · Search NASA

Results for “slurry cast”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

3D printing of architected sulfur cathodes with dual-site atomic catalysts for accelerated polysulfide kinetics and Li-ion transport in high areal-loading lithium–sulfur batteries

The practical deployment of lithium–sulfur batteries (LSBs) is hindered by fundamental limitations in conventional slurry-cast cathodes, including poor sulfur utilization, sluggish ion transport, and low areal capacity, particularly in thick electrodes required for high energy density. To address these challenges, we present direct ink writing (DIW) as an additive manufacturing strategy to fabricate advanced current-collector-free, 3D-printed sulfur cathodes (3DP S@CoNi-DSACs/NC) with hierarchically porous architectures that enhance lithium-ion diffusion, promote electrolyte penetration, and reduce interfacial resistance. The synergistic effects of Co/Ni dual-atom sites accelerate redox kinetics and mitigate polysulfide shuttling. As a result, the optimized 3DP cathode with a sulfur loading of 5.4 mg cm −2 demonstrated excellent rate capability, delivering a high reversible capacity of 1041.4 mAh g −1 at 1C with 85.5% capacity retention after 1000 cycles, significantly outperforming its cast counterpart. Remarkably, even at a higher sulfur loading of 8.1 mg cm −2 , the 3DP cathode maintains outstanding performance, achieving a discharge capacity of 1538.4 mAh g −1 and an areal capacity of 12.5 mAh cm −2 at 0.1C. This study not only demonstrates the functional integration of catalytically active materials into 3D printable sulfur cathode architectures but also offers a scalable and transformative platform for building high-performance LSBs beyond conventional electrode manufacturing methods.

3D electrode↗

Impact of fabrication methods on binder distribution and charge transport in composite cathodes of all-solid-state batteries

Abstract The manufacturing process of all-solid-state batteries necessitates the use of polymer binders. However, these binders, being ionic insulators by nature, can adversely affect charge transport within composite cathodes, thereby impacting the rate performance of the batteries. In this work, we aim to investigate the impact of fabrication methods, specifically the solvent-free dry process versus the slurry-cast wet process, on binder distribution and charge transport in composite cathodes of solid-state batteries. In the dry process, the binder forms a fibrous network, while the wet process results in binder coverage on the surface of cathode active materials. The difference in microstructure leads to a notable 20-fold increase in ionic conductivity in the dry-processed cathode. Consequently, the cells processed via the dry method exhibit higher capacity retention of 89% and 83% at C/3 and C/2 rates, respectively, in comparison to 68% and 58% for the wet-processed cells at the same rate. These findings provide valuable insights into the influence of fabrication methods on binder distribution and charge transport, contributing to a better understanding of the binder’s role in manufacturing of all-solid-state batteries.

Emley, Benjamin↗

Highly Loaded Sulfur Cathode, Coated Separator and Gel Electrolyte for High Rate Li-Sulfur Batteries

As one of DOE Battery 500 Seedling projects, Cornell University and EIC Labs investigated and developed i) highly loaded sulfur cathodes (> 3 mg/cm 2 ), ii) hybrid separators, and iii) gel ceramic electrolytes (GCE) to mitigate the low rate capability, shuttling effect and limited cycle life in high performance Li-Sulfur batteries. Scalable nanomanufacturing processes such as air-controlled electrospray (ACES) and gas-assisted electrospinning (GAES) have been utilized to develop directly deposited electrodes and polymer/ceramic hybrid separators. First, in the development of highly loaded cathodes, alternating layers of sulfur impregnated mesoporous carbon and graphene were fabricated via ACES and the resulting layered cathodes and coated separators exhibit higher capacity and capacity retention (about 1,000 mAh/g capacity with less than 0.02% fade/cycles) than single layer cathode or cathode prepared by conventional slurry cast. Alternating layer approach via ACES has been applied to high loading systems (3 - 5 mg S/cm 2 ), demonstrating the potential to increase sulfur utilization and capacity retention. We have also incorporated iron oxides (Fe 3 O 4 ) into S/mesoporous carbon/graphene cathodes to enhance sulfur utilization and mitigation of polysulfide shuttling. and the effect of Fe 3 O 4 in mesoporous carbon and Gr is highly pronounced at high C rates of 1C and 2C cycling performance. To further improve the cathodes at high rates, graphene nanoribbons (GNR) which can promote ion transport were incorporated in the cathode, resulting in 550 mAh/g at 5C/5C rates. Hybrid Li-ion/Li-S cathodes has also been explored to better engage unreacted polysulfides during charge/discharge. S/LFP hybrid cathodes offer higher sulfur utilization and enhanced rate capability, as well as higher areal loading. This study suggests inclusion of iron phosphide (Fe2P) which can chemically interact with polysulfides can further enhance sulfur utilization and mitigation of soluble polysulfides at high rates. Secondly, in the development of hybrid separators, we first employed graphene coating on the commercial polyolefin separators, which exhibits higher capability, better capacity retention and enhanced rate capability. To improve the rate capability with enhanced safety features such as thermal stability and nonflammability, we developed polymer/ceramic hybrids based on thermally stable polyimide (PI) and room temperature curable ceramic precursors such as organopolysilazane (OPSZ) or polysilsesquioxanes (PSSQ), which exhibit no shrinkages up to 300 ºC and non-flammability. To improve mechanical properties and electrochemical stability, polybenzimidazole (PBI) and alumina have been incorporated in polymer/ceramic hybrid separator, replacing PI and OPSZ/PSSQ, respectively. Finally, the gel ceramic electrolyte (GCE) based on ceramic cross linkers have been applied to make Li-S cells even safer and also to mitigate the polysulfide shuttling further. The resulting gel ceramic electrolyte offers improved capacity retention and rate capability, and also effectively mitigates polysulfide shuttling which was also confirmed by modeling. Inclusion of high ion conducting additives into GCE together with polymer/ceramic hybrid separators exhibit the higher ionic conductivity than liquid electrolyte with commercial polyolefin separator. We demonstrated that the developed highly loaded sulfur cathodes, polymer/ceramic hybrid separators and gel ceramic electrolyte can effectively mitigate the low rate capability, shuttling effect and limited cycle life in high performance Li-Sulfur batteries with improved safety.

25 ENERGY STORAGE↗

Synergistic Effect of High Sulfur Loading Layered Cathode, Ceramic Separator and Gel Electrolyte

Lithium sulfur (Li-S) batteries are promising candidates for next-generation energy storage devices as they are capable of providing higher energy density and lower cost in comparison to the state of the art Li-ion batteries. To gain these characteristics, there are challenges such as polysulfide crossover, large volume changes during cycling, and deposition of insulating lithium sulfide that need to be alleviated. A popular approach to address these issues is to control the structure and properties of the carbon cathode in order to influence the transport of polysulfides, surface area for reaction, and lithium sulfide deposition. Ceramic separators on the other hand can drastically affect ion diffusion and overall battery performance. Safety concerns regarding the flammable liquid electrolyte can be reduced by deploying gel electrolyte. Towards this direction, we developed a layer-on-layer cathode structure with sulfur-impregnated activated carbon alternating with graphene layer, which was fabricated by Air-assisted electrospray. A much higher sulfur loading compared to slurry cast cathodes can be provided in this method. Combining the new cathode with gel electrolyte can offer higher safety of the battery and capacity retention. Ceramic separator would compensate the reduced ion conductivity of the gel electrolyte and the combination of these variables will be very promising in improvement of battery performance and safety.

25 ENERGY STORAGE↗

The Role of Metal Oxides in Li-S Batteries: A High-Areal-Capacity Sulfur Composite Cathode Investigation

Compared to lithium-ion batteries (LIB), lithium-sulfur (Li-S) batteries have low cost and high theoretical specific energy (2510 Wh/kg or about 10 times of the LIB). However, Li-S batteries have several challenges, including large volume expansion, poor utilization of the end products, sluggish kinetics of polysulfides, and crossover, so-called the "shuttle effect". To address these issues, we have introduced metal oxides to the Li-S electrode to develop a metal-oxide-sulfur composite electrode. We aim to use metal oxides to assist the Li-S formation (dissociation) during discharge (charge) cycles. We elect to focus on LIB-based metal oxides to ensure that the added material can contribute storage capacity to the battery. Our cathodes are fabricated by both the conventional slurry casting and air-controlled electrospray. LIB electrode materials, such as Li(Ni 0.6 Mn 0.6 Co 0.2 )O 2 , LiMn 2 O 4 , Li 2 TiO 3 , etc, were incorporated with the sulfur-carbon composite and their charge-discharge performances are compared. We found that the presence of metal oxides increased sulfur utilization with stable cycling performance, even in cells with high areal capacities. To unveil the interactions between lithium metal oxides and sulfur, the cathodes were analyzed by various characterization techniques, including scanning electron microscopy, X-ray diffraction, thermogravimetric analysis, and electrochemistry. The analysis of the role of the oxides will be presented along with the reaction mechanism.

25 ENERGY STORAGE↗

High Throughput Solvent-free Manufacturing of Battery Electrodes

The project goal is to develop and demonstrate an advanced solvent-free lithium-ion battery electrode process through proposed Advanced Dry Electrode Process (ADEP) equipment, which is expected to exhibit a better binder fibrillization and high throughput and suitable for high performance electrode manufacturing, and commonize the anode and cathode dry processing equipment, supply chain and operation for lithium-ion battery OEMs for replacing the solvent-based slurry casting. Our proposed approach will facilitate low-cost battery production by addressing the following gaps in present dry electrode processing: • Extend the dry electrode fabrication process to lithium-ion battery anode manufacturing • Increase the active material content for anodes and cathodes • Intensify the process through improved mixing, powder rheology and surface modifications • Enable processing of next-generation electrode materials that are not stable to solvent or ambient air exposure. The project objectives include the development of anode-compatible binder and binder fibrillization promoter for low irreversible capacity loss, low electrode binder content yet higher film mechanical strength, and the optimization of solvent-free anode and cathode process for low cost (>60% electrode cost reduction), high performance (10% increase in energy density without sacrificing cycle life) and high throughput to enable next generation lithium-ion battery electrode production. Solvent-free electrode manufacturing will also enable next-generation cell designs based on prelithiated anodes or solid-state electrolytes.

25 ENERGY STORAGE↗

Electrospun Si and Si/C Fiber Anodes for Li-Ion Batteries

Due to structural changes in silicon during lithiation/delithiation, most Li-ion battery anodes containing silicon show rapid gravimetric capacity fade upon charge/discharge cycling. Herein, we report on a new Si powder anode in the form of electrospun fibers with only poly(acrylic acid) (PAA) binder and no electrically conductive carbon. The performance of this anode was contrasted to a fiber mat composed of Si powder, PAA binder, and a small amount of carbon powder. Fiber mat electrodes were evaluated in half-cells with a Li metal counter/reference electrode. Without the addition of conductive carbon, a stable capacity of about 1500 mAh/g (normalized to the total weight of the anode) was obtained at 1C for 50 charge/discharge cycles when the areal loading of silicon was 0.30 mgSi/cm2, whereas a capacity of 800 mAh/g was obtained when the Si loading was increased to ~1.0 mgSi/cm2. On a Si weight basis, these capacities correspond to >3500 mAh/gSi. The capacities were significantly higher than those found with a slurry-cast powdered Si anode with PAA binder. There was no change in fiber anode performance (gravimetric capacity and constant capacity with cycling) when a small amount of electrically conductive carbon was added to the electrospun fiber anodes when the Si loading was ≤1.0 mgSi/cm2.

Mondal, Abhishek N.↗

High Temperature Tensile Properties and Fatigue Behavior of a Melt-Infiltrated SiC/SiC Composite

High temperature fatigue behavior of a woven, SiC/SiC ceramic matrix composite (CMC) was investigated in air at two temperatures. The reinforcement for the CMC consisted of 5HS Sylramic(Trademark) fabric with a [0deg/90deg]4s lay-up. The SiC matrix material was infiltrated into the fiber-preform with a slurry-cast, melt-infiltration process. Tensile and fatigue test specimens were machined from the CMC plates. Initially tensile tests were conducted to obtain the average values of tensile properties at 1038 and 1204 C. Subsequently, low-cycle fatigue (LCF) tests with zero and two-hour hold-times at the maximum stress were conducted at the same two temperatures. Fatigue life data generated in the LCF tests were used to determine the geometric mean fatigue lives. In this paper, the tensile behavior and the fatigue durability of the CMC determined under different loading conditions are documented. In addition, reductions observed in the cyclic lives of the composite due to the two hour hold-time at maximum tensile stress are discussed.

Kalluri, Sreeramesh↗

An Assessment of Variability in the Average Tensile Properties of a Melt-Infiltrated SiC/SiC Composite

Woven SiC/SiC Ceramic Matrix Composites (CMCs), manufactured by the slurry-cast, melt-infiltration process are under consideration as combustor liner materials in aircraft gas turbine engines. Tensile properties (elastic modulus, proportional limit strength, in-plane tensile strength and strain to failure) of the CMC, manufactured during two separate time periods (9/99 and 1/01) were determined at 816 and 1024 C by conducting tensile tests on specimens machined from the CMC plates. A total of 24 tensile tests were conducted for each temperature and CMC variant combination. In this study average tensile properties of the two cMC variants were statistically compared to evaluate significant differences, if any, within the CMC's properties.

Kalluri, Sreeramesh↗

Melt-infiltrated Sic Composites for Gas Turbine Engine Applications

SiC-SiC ceramic matrix composites (CMCs) manufactured by the slurry -cast melt-infiltration (MI) process are leading candidates for many hot-section turbine engine components. A collaborative program between Goodrich Corporation and NASA-Glenn Research Center is aimed at determining and optimizing woven SiC/SiC CMC performance and reliability. A variety of composites with different fiber types, interphases and matrix compositions have been fabricated and evaluated. Particular focus of this program is on the development of interphase systems that will result in improved intermediate temperature stressed-oxidation properties of this composite system. The effect of the different composite variations on composite properties is discussed and, where appropriate, comparisons made to properties that have been generated under NASA's Ultra Efficient Engine Technology (UEET) Program.

Morscher, Gregory N.↗

Issues on Fabrication and Evaluation of SiC/SiC Tubes With Various Fiber Architectures

SiC/SiC engine components, high-modulus Sylramic-iBN SiC fiber tows were used to form nine different tubular architectural preforms with 13 mm (0.5 in.) inner diameter and lengths of approx. 75 and 230 mm (approx. 3 and approx, 9 in.). The thin-walled preforms were then coated with a BN interphase and densified with a hybrid SiC matrix using nearly the same process steps previously established for slurry-cast melt-infiltrated Sylramic-iBN/BN/SiC flat panels. The as-fabricated CMC tubes were microstructurally evaluated and tested for tensile hoop and flexural behavior, and some of the tubes were also tested in a low-pressure burner rig test with a high thru-thickness thermal gradient. To date, four general tube scale-up issues have been identified: greater CVI deposits on outer wall than inner wall; increased ply thickness and reduced fiber fraction; poor test standards for accurately determining the hoop strength of a small-diameter tube; and poor hoop strength for architectures with seams or ply ends. The underlying mechanisms and possible methods for their minimization are discussed.

Yun, H. M.↗

Hoop Tensile Properties of Ceramic Matrix Composite Cylinders

Tensile stress-strain properties in the hoop direction were obtained for 100-mm diameter SiC/SiC ceramic matrix composite cylinders using ring specimens machined form the cylinder ends. The cylinders were fabricated from 2D balanced SiC fabric with several material variants, including wall thickness (6,8, and 12 plies), SiC fiber type (Sylramic, Sylramic-iBN, Hi-Nicalon, and Hi-Nicalon S), fiber sizing type, and matrix type (full CVI SiC, and partial CVI SiC plus slurry cast + melt-infiltrated SiC-Si). Fiber ply splices existed in all the hoops. Tensile hoop measurements are made at room temperature and 1200 C using hydrostatic ring test facilities. The failure mode of the hoops, determined through microstructural examination, is presented. The hoop properties are compared with in-plane data measured on flat panels using same material variants, but containing no splices.

Verrilli, Michael J.↗

Thermo-Mechanical Properties of SiC/SiC Composites with Hybrid CVI-PIP Matrices

For long term structural service, the upper temperature capability for slurry-cast melt infiltrated (MI) SiC/SiC composites is limited to approx. 1315 C because of silicon reaction with the SiC fibers. For applications requiring material temperatures in excess of 1315 C, alternate methods of manufacturing the SiC matrices without silicon are being investigated, such as a hybrid combination of CVI and PIP. In this study, stacked fabric plies of Sylramic i-BN SiC fibers were coated with a CVI BN interface layer followed by a partial CVI SiC matrix. The remaining porosity in the SiC/SiC preforms was then infiltrated with silicon carbide matrix by PIP. Thermo-mechanical property measurements indicate that these composites are stable to 1700 C in inert environments under no load conditions for 100 h and under load conditions to 1450 C in air for 300 h. The advantages, disadvantages, and potential of this composite system for high temperature applications will be discussed.

Bhatt, R. T.↗

Tensile Creep and Fatigue of Sylramic-iBN Melt-Infiltrated SiC Matrix Composites: Retained Properties, Damage Development, and Failure Mechanisms

An understanding of the elevated temperature tensile creep, fatigue, rupture, and retained properties of ceramic matrix composites (CMC) envisioned for use in gas turbine engine applications are essential for component design and life-prediction. In order to quantify the effect of stress, time, temperature, and oxidation for a state-of-the-art composite system, a wide variety of tensile creep, dwell fatigue, and cyclic fatigue experiments were performed in air at 1204 C for the SiC/SiC CMC system consisting of Sylramic-iBN SiC fibers, BN fiber interphase coating, and slurry-cast melt-infiltrated (MI) SiC-based matrix. Tests were either taken to failure or interrupted. Interrupted tests were then mechanically tested at room temperature to determine the residual properties. The retained properties of most of the composites subjected to tensile creep or fatigue were usually within 20% of the as-produced strength and 10% of the as-produced elastic modulus. It was observed that during creep, residual stresses in the composite are altered to some extent which results in an increased compressive stress in the matrix upon cooling and a subsequent increased stress required to form matrix cracks. Microscopy of polished sections and the fracture surfaces of specimens which failed during stressed-oxidation or after the room-temperature retained property test was performed on some of the specimens in order to quantify the nature and extent of damage accumulation that occurred during the test. It was discovered that the distribution of stress-dependent matrix cracking at 1204 C was similar to the as-produced composites at room temperature; however, matrix crack growth occurred over time and typically did not appear to propagate through thickness except at final failure crack. Failure of the composites was due to either oxidation-induced unbridged crack growth, which dominated the higher stress regime (> 179 MPa) or controlled by degradation of the fibers, probably caused by intrinsic creep-induced flaw growth of the fibers or internal attack of the fibers via Si diffusion through the CVI SiC and/or microcracks at the lower stress regime (< 165 MPa).

Morscher, Greg↗

SiC/SiC Composites: The Effect of Fiber Type and Fiber Architecture on Mechanical Properties

Woven SiC/SiC composites represent a broad family of composites with a broad range of properties which are of interest for many energy-based and aero-based applications. Two important features of SiC/SiC composites which one must consider are the reinforcing fibers themselves and the fiber-architecture they are formed into. The range of choices for these two features can result in a wide range of elastic, mechanical, thermal, and electrical properties. In this presentation, it will be demonstrated how the effect of fiber-type and fiber architecture effects the important property of "matrix cracking stress" for slurry-cast melt-infiltrated SiC matrix composites, which is often considered to be a critical design parameter for this system of composites.

Morscher, Gregory N.↗

SiC Composite Turbine Vanes

Turbine inlet guide vanes have been fabricated from composites of silicon carbide fibers in silicon carbide matrices. A unique design for a cloth made from SiC fibers makes it possible to realize the geometric features necessary to form these vanes in the same airfoil shapes as those of prior metal vanes. The fiber component of each of these vanes was made from SiC-fiber cloth coated with boron nitride. The matrix was formed by chemical-vapor infiltration with SiC, then slurry-casting of SiC, followed by melt infiltration with silicon. These SiC/SiC vanes were found to be capable of withstanding temperatures 400 F (222 C) greater than those that can be withstood by nickel-base-superalloy turbine airfoils now in common use in gas turbine engines. The higher temperature capability of SiC/SiC parts is expected to make it possible to use them with significantly less cooling than is used for metallic parts, thereby enabling engines to operate more efficiently while emitting smaller amounts of NOx and CO. The SiC/SiC composite vanes were fabricated in two different configurations. Each vane of one of the configurations has two internal cavities formed by a web between the suction and the pressure sides of the vane. Each vane of the other configuration has no web (see Figure 1). It is difficult to fabricate components having small radii, like those of the trailing edges of these vanes, by use of stiff stoichiometric SiC fibers currently preferred for SiC/SiC composites. To satisfy the severe geometric and structural requirements for these vanes, the aforementioned unique cloth design, denoted by the term Y-cloth, was conceived (see Figure 2). In the regions away from the trailing edge, the Y-cloth features a fiber architecture that had been well characterized and successfully demonstrated in combustor liners. To form a sharp trailing edge (having a radius of 0.3 mm), the cloth was split into two planes during the weaving process. The fiber tows forming the trailing-edge section were interlocked, thereby enhancing through-thickness strength of the resulting composite material. For vanes of the webless configuration, each made from a layup of six plies of Ycloth, the length of each Y-cloth layer was cut so that the two strips corresponding to the aforementioned two planes would wrap around the perimeter of a graphite vane preform tool with a 10-mm overlap. The overlap was used to join the two strips in a fringe splice. To make the external sixth ply, a standard woven cloth was cut to the required final length and a fringe splice joined the two ends of the cloth at the trailing edge. The cloth was then prepregged. The entire assembly was then placed into an aluminum compaction tool designed to form the outer net shape of the vane. After the prepreg material was allowed to dry, the preform was removed from the aluminum tooling and placed into an external graphite tool before being shipped to a vendor for matrix infiltration. To make the SiC fiber preform for a vane having an internal web, a slightly different initial approach was followed. Each of two sections forming the internal cavities (and ultimately the web) was created by first slipping two concentric layers of a two-dimensional, 2-by-2, 45 - braided tube around a net-shape graphite mandrel. The tubes on both mandrels were prepregged and allowed to dry. The resulting two subassemblies were put together, then four additional plies were wrapped around them in the same fashion as that described above for the six plies of the vaneless configuration. The consolidation of the SiC fiber preforms into SiC/SiC composite parts was performed by commercial vendors using their standard processes. The capability of two of the webless SiC/SiC turbine vanes was demonstrated in tests in a turbine environment. The tests included 50 hours of steady-state operation and 102 two-minute thermal cycles. A surface temperature of 1,320 C was reached during the tests.

Calomino, Anthony M.↗

Binder systems and methods for tape casting lithium garnet electrolytes

Slurry compositions, tape casting binder systems and fabrication methods for the fabrication of lithium-garnet electrolyte scaffolds for use in solid state batteries and other devices are provided. Slurry compositions may be optimized mixtures of LLZO powder, a dispersant, a lithium salt, a wetting agent a binder, a plasticizer and at least one solvent. The optimized ceramic slurry compositions may include MgO as a sintering additive to improve density and ionic conductivity of the doped-LLZO sheets and produce a fine-grained microstructure. Sintering protocols for cast slurries of commercially available doped LLZO powders eliminate the requirement of mother-powder coverings or externally applied pressure. An environmentally friendly water-based system using methylcellulose as a binder is also provided producing green tape and final properties comparable to those obtained with organic solvent-based systems.

Jonson, Robert↗

One-step Tape Casting of Composites via Slurry on Fiber

A process by which metal matrix composites can be made was presented. The process involves putting a powder slurry on fibers to make a precursor green tape. These green tapes are cut, stacked and hot pressed to form the fully dense composite. A computer program was presented which enables complete quantification and control of the process. Once some easily obtained properties of the slurry and its behavior are determined (such as the shrinkage from the wet to green state, and the density of the green tape) modification of the fiber spacing and blade height give the maker precise control of fiber volume fraction, and fiber architecture in the composite. The process was shown to be accurate and flexible through the production of a wide variety of volume fraction fiber composites made from a wide variety of fibers and powders. The most time consuming step of the tape casting process (other than hot pressing) was winding the fiber on the drum. The tape casting techniques developed resulted in high quality metal matrix composites, with ultimate tensile strength in the range of 215 ksi (1477 MPa), a strain at failure of 1.15 percent, and in fatigue at room temperature 0 to 120 ksi, n = 0.3 Hz, a 4-ply Ti-24Al-11Nb/SCS-6, 32 vol% fiber tape cast composite lasted 202,205 cycles with a maximum strain on the 100th cycle of 0.43 percent.

deGroh, Henry C., III↗